Resumo:
Aurivillus intergrowth Bi4Ti3O12-5BiFeO(3) was demonstrated to be ferroelectric that evoked the possibility of achieving high temperature magnetoelectric property in this family of compounds. X-ray diffraction studies confirmed its structure to be orthorhombic [Fmm2; a=5.5061(11) A degrees, b=5.4857(7) A degrees, c=65.742(12) A degrees]. However, transmission electron microscopy established the random incidence of intergrowth at nanoscale corresponding to n=6 and n=7 members of the Aurivillius family. Diffuse ferroelectric orthorhombic to paraelectric tetragonal phase transition around 857 K was confirmed by dielectric and high temperature x-ray diffraction studies. Polarization versus electric field hysteresis loops associated with 2P(r) of 5.2 mu C/cm(2) and coercive field of 42 kV/cm were obtained at 300 K.
Resumo:
The electrical conductivity and electrical relaxation for ferroelectric Bi4Ti2.98Nb0.01Ta0.01O12 (BTNT) ceramics have been reported in the frequency range 0.1 Hz to 1 MHz and in the 300-550 degrees C temperature range. The electrical data was analyzed in the framework of the dielectric as well as the electric modulus formalisms. The bulk dc conductivity at various temperatures was extracted from the electrical relaxation data. The activation energy associated with the electrical relaxation determined from the electric modulus spectra was found to be 0.93 +/- 0.03 eV, close to that of the activation energy for dc conductivity (1.03 +/- 0.02 eV). It suggests that the movements of oxygen ions are responsible for both ionic conduction as well as the relaxation process. The pyroelectric coefficient was found to be 12 mu C m(-2) K-1 at room temperature which is higher than that of the reported value of pyroelectric coefficient for undoped Bi4Ti3O12 ceramics. (C) 2010 Elsevier B.V. All rights reserved.
Resumo:
Li-doped ZnO thin films (Zn1-xLixO, x=0.05-0.15) were grown by pulsed-laser ablation technique. Highly c-axis-oriented films were obtained at a growth temperature of 500 degrees C. Ferroelectricity in Zn1-xLixO was found from the temperature-dependent dielectric constant and from the polarization hysteresis loop. The transition temperature (T-c) varied from 290 to 330 K as the Li concentration increased from 0.05 to 0.15. It was found that the maximum value of the dielectric constant at T-c is a function of Li concentration. A symmetric increase in memory window with the applied gate voltage is observed for the ferroelectric thin films on a p-type Si substrate. A ferroelectric P-E hysteresis loop was observed for all the compositions. The spontaneous polarization (P-s) and coercive field (E-c) of 0.6 mu C/cm(2) and 45 kV/cm were obtained for Zn0.85Li0.15O thin films. These observations reveal that partial replacement of host Zn by Li ions induces a ferroelectric phase in the wurtzite-ZnO semiconductor. The dc transport studies revealed an Ohmic behavior in the lower-voltage region and space-charge-limited conduction prevailed at higher voltages. The optical constants were evaluated from the transmission spectrum and it was found that Li substitution in ZnO enhances the dielectric constant.
Resumo:
Monophasic Na0.5La0.5Bi4Ti4O15 powders were synthesized via the conventional solid-state reaction route. The X-ray powder diffraction (XRD), selected area electron diffraction (SAED) and high resolution transmission electron microscopy (HRTEM) studies carried out on the as synthesized powdered samples confirmed the phase to be a four-layer Aurivillius that crystallizes in an orthorhombic A2(1)am space group. The microstructure and the chemical composition of the sintered sample were examined by scanning electron microscope (SEM) equipped with an energy dispersive X-ray analyzer (EDX). The dielectric properties of the ceramics have been studied in the 27-700 degrees C temperature range at various frequencies (100 Hz to 1 MHz). A sharp dielectric anomaly was observed at 580 degrees C for all the frequencies corresponding to the ferroelectric to paraelectric phase transition. Saturated ferroelectric hysteresis loops were observed at 200 degrees C and the associated remnant polarization (P-r) and coercive field (E-c) were found to be 7.4 mu C/cm(2) and 34.8 kV/cm, respectively. AC conductivity analysis confirmed the existence of two different conduction mechanisms in the ferroelectric region. Activation energies calculated from the Arrhenius plots were similar to 0.24 eV and similar to 0.84 eV in the 300-450 degrees C and 450-580 degrees C temperature ranges, respectively. (C) 2010 Elsevier B.V. All rights reserved.
Resumo:
Polarization switching processes in TAAP and DTAAP have been studied by the Merz method. The switching process in DTAAP is slower than in TAAP. The temperature dependence of switching time indicates that the crystal might contain groups of domain nuclei with different activation energies. X-ray irradiation causes an increase in the threshold field below which switching could not occur and decrease in the mobility of domain walls. Irradiation decreases the peak value of dielectric constant, Tc and increases the value of coercive field. Domain structure studies on TAAP crystals have shown that the crystals grow as both predominantly single domain and multi domains, depending on which the internal bias increases or remains unaffected upon irradiation.
Resumo:
Multilayer lithium tantalate thin films were deposited on Pt-Si Si(111)/SiO2/TiO2/Pt(111)]substrates by sol-gel process. The films were annealed at different annealing temperatures (300, 450 and 650 degrees C) for 15 min. The films are polycrystalline at 650 degrees C and at other annealing conditions below 650 degrees C the films are in amorphous state. The films were characterized using X-ray diffraction, atomic force microscopy (AFM) and Raman spectroscopy. The AFM of images show the formation of nanograins of uniform size (50 nm) at 650 degrees C. These polycrystalline films exhibit spontaneous polarization of 1.5 mu C/cm(2) at an application of 100 kV/cm. The dielectric constant of multilayer film is very small (6.4 at 10 kHz) as compared to that of single crystal. (C) 2010 Elsevier B.V. All rights reserved.
Resumo:
Ferroelectric bismuth vanadate Bi2VO5.5 (BVO) thin films have been grown on LaAlO3 (LAO) and SiO2/Si substrates with LaNiO3 (LNO) base electrodes by the pulsed laser deposition technique. The effect of substrate temperature on the ferroelectric properties of BVO thin films, has been studied by depositing the thin films at different temperatures. The BVO thin films grown on LNO/LAO were textured whereas the thin films grown on LNO/SiO2/Si were polycrystalline. The BVO thin films grown at 450?°C exhibited good ferroelectric properties indicating that LNO acts as a good electrode material. The remanent polarization Pr and coercive field Ec obtained for the BVO thin films grown at 450?°C on LNO/LAO and LNO/SiO2/Si were 2.5 ?C/cm2, 37 kV/cm and 4.6?C/cm2, 93 kV/cm, respectively. © 1995 American Institute of Physics.
Resumo:
Large single crystal of triglycine sulphate (dimension 100 mm along monoclinic b-axis and 15 mm in diameter) was grown using the unidirectional solution growth technique. The X-ray diffraction studies confirmed the growth/long axis to be b-axis (polar axis). The dielectric studies were carried out at various temperatures to establish the phase transition temperature. The frequency response of the dielectric constant, dielectric loss and impedance of the crystal along the growth axis, was monitored. These are typically characterized by strong resonance peaks in the kHz region. The piezoelectric coefficients like stiffness constant (C), elastic coefficient (S), electromechanical coupling coefficient (k) and d (31) were calculated using the resonance-antiresonance method. Polarization (P)-Electric field (E) hysteresis loops were recorded at various temperatures to find the temperature-dependent spontaneous polarization of the grown crystal. The pyroelectric coefficients were determined from the pyroelectric current measurement by the Byer and Roundy method. The ferroelectric domain patterns were recorded on (010) plane using scanning electron microscopy and optical microscopy.
Resumo:
Novel ferroelectric bismuth vanadate, Bi2VO5.5 (BVO), thin films have been grown between lattice matched metallic LaNiO3 (LNO) layers deposited on SrTiO3 (STO) by the pulsed laser deposition technique. LNO/BVO/LNO/STO and Au/BVO/LNO/STO trilayer structures exhibited c‐oriented (001) growth of BVO. LNO has been found to be a good metallic electrode with sheet resistance ∼20 Ω in addition to aiding c‐axis oriented BVO growth. The dielectric constant, ϵr of LNO/BVO/LNO/STO, at 300 K was about 12. However, when an Au electrode was used on top of BVO/LNO/STO film, it showed a significant improvement in the dielectric constant (ϵr=123). The ferroelectric properties of BVO thin films have been confirmed by hysteresis behavior with a remnant polarization, Pr=4.6×10−8 C/cm2 and coercive field, Ec=23 kV/cm at 300 K.
Resumo:
Aurivillus intergrowth Bi4Ti3O12–5BiFeO3 was demonstrated to be ferroelectric that evoked the possibility of achieving high temperature magnetoelectric property in this family of compounds. X-ray diffraction studies confirmed its structure to be orthorhombic [Fmm2; a = 5.5061(11) Å, b = 5.4857(7) Å, c = 65.742(12) Å]. However, transmission electron microscopy established the random incidence of intergrowth at nanoscale corresponding to n = 6 and n = 7 members of the Aurivillius family. Diffuse ferroelectric orthorhombic to paraelectric tetragonal phase transition around 857 K was confirmed by dielectric and high temperature x-ray diffraction studies. Polarization versus electric field hysteresis loops associated with 2Pr of 5.2 μC/cm2 and coercive field of 42 kV/cm were obtained at 300 K.
Resumo:
A capillary-enforced template-based method has been applied to fabricate Pb(0.76)Ca(0.24)TiO(3) (PCT24) nanotubes via filling PCT24 precursor solution, prepared by modified sol-gel method, into nanochannels of anodic aluminum oxide templates. The morphology and structure of as-prepared PCT24 were examined by scanning electron microscopy, transmission electron microscopy (TEM) and X-ray diffraction techniques. The obtained PCT24 nanotubes with diameter of similar to 200 nm and wall thickness of similar to 20 nm exhibited a tetragonal perovskite structure. High resolution TEM (HRTEM) analysis confirmed that as-obtained PCT24 nanotubes made up of nanoparticles (5-8 nm) which were randomly aligned in the nanotubes. Formation of some solid crystalline PCT24 nanorods, Y-junctions and multi-branches were observed. Interconnections in the pores of template are responsible for the growth of Y-junctions and multi-branches. The possible formation mechanism of PCT24 nanotubes/nanorods was discussed. Ferroelectric hysteresis loops of PCT24 nanotube arrays were measured, showing a room temperature ferroelectric characteristic of as-prepared PCT24 nanotubes. (C) 2011 Elsevier B.V. All rights reserved.
Resumo:
Boron oxide (B2O3) addition to pre-reacted K0.5Na0.5NbO3 (KNN) powders facilitated swift densification at relatively low sintering temperatures which was believed to be a key to minimize potassium and sodium loss. The base KNN powder was synthesized via solid-state reaction route. The different amounts (0.1-1 wt%) of B2O3 were-added, and ceramics were sintered at different temperatures and durations to optimize the amount of B2O3 needed to obtain KNN pellets with highest possible density and grain size. The 0.1 wt% B2O3-added KNN ceramics sintered at 1,100 A degrees C for 1 h exhibited higher density (97 %). Scanning electron microscopy studies confirmed an increase in average grain size with increasing B2O3 content at appropriate temperature of sintering and duration. The B2O3-added KNN ceramics exhibited improved dielectric and piezoelectric properties at room temperature. For instance, 0.1 wt% B2O3-added KNN ceramic exhibited d (33) value of 116 pC/N which is much higher than that of pure KNN ceramics. Interestingly, all the B2O3-added (0.1-1 wt%) KNN ceramics exhibited polarization-electric field (P vs. E) hysteresis loops at room temperature. The remnant polarization (P (r)) and coercive field (E (c)) values are dependent on the B2O3 content and crystallite size.
Resumo:
The effects of various processing conditions, like annealing, poling, mechanical rolling and their combinations, on the dielectric and ferroelectric properties of PVDF poly(vinylidene fluoride)] were systematically studied in this work. Further, the effect of processing sequence on the structure and properties was investigated. While all the processing conditions adopted here resulted in phase transformation of the alpha- to electroactive beta-polymorph in PVDF, the fraction of beta-phase developed was observed to be strongly contingent on the adopted process. The transformation of alpha- to electroactive beta-polymorph was determined by X-ray diffraction and FTIR. The neat PVDF showed only beta-phase, whereas mechanically rolled samples exhibited the highest ca. 85% beta-phase in PVDF. Both the permittivity and the loss tangent decreased in the samples which had undergone different processing conditions. The polarization-electric field (P-E) loops for all the samples were evaluated. Interestingly, the energy density, estimated from the electrical displacement-electric field (D-E) loops, was observed to be highest for the poled samples which were initially rolled. The results indicate that various processing conditions can influence the dielectric and the ferroelectric properties differently.
Resumo:
Bi1-xCaxMnO3 (BCMO) thin films with x = 0, 0.1, 0.2, 0.3 and 0.4 are successfully deposited on the n-type Si (100) substrate at two different temperatures of 400 degrees C and 800 degrees C using RF magnetron sputtering. The stoichiometry of the films and oxidation state of the elements have been described by X-ray photoelectron spectroscopy analysis. Dielectric measurement depicts the insulating property of BCMO films. Magnetic and ferroelectric studies confirm the significant enhancement in spin orientation as well as electric polarization at room temperature due to incorporation of Ca2+ ions into BiMnO3 films. The BCMO (x = 0.2) film grown at 400 degrees C shows better magnetization (M-sat) and polarization (P-s) with the measured values of 869 emu / cc and 6.6 mu(C)/cm(2) respectively than the values of the other prepared films. Thus the realization of room temperature ferromagnetic and ferroelectric ordering in Ca2+ ions substituted BMO films makes potentially interesting for spintronic device applications. (C) 2014 Author(s).