5 resultados para Material properties

em eResearch Archive - Queensland Department of Agriculture


Relevância:

60.00% 60.00%

Publicador:

Resumo:

Arthropods are known to use silk for a number of different purposes including web construction, shelter building, leaf tying, construction of pupal cocoons, and as a safety line when dislodged from a substrate (Alexander, 1961; Fitzgerald, 1983; Common, 1990). Across the arthropods, silk displays a diversity of material properties and chemical constituents and is produced from glands with different evolutionary origins (Craig, 1997). Among insects, larval Lepidoptera are prolific producers of silk. Because many lepidopteran larvae are pests, an ability to interfere with silk production or, at the very least, an understanding of how silk is used, could provide new options for pest control. After testing many known fluorescent dyes, we found that Fluorescent Brightener 28 (also known as Calcofluor White M2R) (Sigma-Aldrich Pty Ltd, Sydney, NSW, Australia), an optical brightener used in the textile industry, binds to arthropod silk in a simple staining reaction, causing it to fluoresce under ultraviolet (UV) light. Such brighteners have also been used in insect gut content analysis (Schlein & Muller, 1995; Hugo et al., 2003). Here we describe the method of visualizing arthropod silk on plant surfaces, using as a model the thin, barely visible, single strands of silk produced by Helicoverpa armigera (Hübner) (Lepidoptera: Noctuidae) neonates.

Relevância:

30.00% 30.00%

Publicador:

Resumo:

Characterisation and investigation of a number of key wood properties, critical for further modelling work, has been achieved. The key results were: • Morphological characterisation, in terms of fibre cell wall thickness and porosity, was completed. A clear difference in fibre porosity, size, wall thickness and orientation was evident between species. Results were consistent with published data for other species. • Viscoelastic properties of wood were shown to differ greatly between species and in the radial and tangential directions, largely due to anatomical and chemical variations. Consistent with published data, the radial direction shows higher stiffness, internal friction and glass transition temperature than the tangential directions. The loss of stiffness over the measured temperature range was greater in the tangential direction than the radial direction. Due to time dependant molecular relaxation, the storage modulus and glass transition temperature decreased with decreasing test frequency, approaching an asymptotic limit. Thus the viscoelastic properties measured at lower frequencies are more representative of static material. • Dynamic interactions between relative humidity, moisture content and shrinkage of four Australian hardwood timbers can be accurately monitored on micro-samples using a specialised experimental device developed by AgroParisTech – ENGREF. The device generated shrinkage data that varied between species but were consistent (repeatable) within a species. Collapse shrinkage was clearly evident with this method for Eucalyptus obliqua, but not with other species, consistent with industrial seasoning experience. To characterise the wood-water relations of this species, free of collapse, thinner sample sections (in the R-T plane) should be used.

Relevância:

30.00% 30.00%

Publicador:

Resumo:

Khaya senegalensis, African mahogany, a high-value hardwood, was introduced in the Northern Territory (NT) in the 1950s; included in various trials there and at Weipa, Q in the 1960s-1970s; planted on ex mine sites at Weipa (160 ha) until 1985; revived in farm plantings in Queensland and in trials in the NT in the 1990s; adopted for large-scale, annual planting in the Douglas-Daly region, NT from 2006 and is to have the planted area in the NT extended to at least 20,000 ha. The recent serious interest from plantation growers, including Forest Enterprises Australia Ltd (FEA), has seen the establishment of some large scale commercial plantations. FEA initiated the current study to process relatively young plantation stands from both Northern Territory and Queensland plantations to investigate the sawn wood and veneer recovery and quality from trees ranging from 14 years (NT – 36 trees) to 18-20 years (North Queensland – 31 trees). Field measures of tree size and straightness were complemented with log end splitting assessment and cross-sectional disc sample collection for laboratory wood properties measurements including colour and shrinkage. End-splitting scores assessed on sawn logs were relatively low compared to fast grown plantation eucalypts and did not impact processing negatively. Heartwood proportion in individual trees ranged from 50% up to 92 % of butt cross-sectional disc area for the visually-assessed dark coloured central heartwood and lighter coloured transition wood combined. Dark central heartwood proportion was positively related to tree size (R2 = 0.57). Chemical tests failed to assist in determining heartwood – sapwood boundary. Mean basic density of whole disc samples was 658 kg/m3 and ranged among trees from 603 to 712 kg/m3. When freshly sawn, the heartwood of African mahogany was orange-red to red. Transition wood appeared to be pinkish and the sapwood was a pale yellow colour. Once air dried the heartwood colour generally darkens to pinkish-brown or orange-brown and the effect of prolonged time and sun exposure is to darken and change the heartwood to a red-brown colour. A portable colour measurement spectrophotometer was used to objectively assess colour variation in CIE L*, a* and b* values over time with drying and exposure to sunlight. Capacity to predict standard colour values accurately after varying periods of direct sunlight exposure using results obtained on initial air-dried surfaces decreased with increasing time to sun exposure. The predictions are more accurate for L* values which represent brightness than for variation in the a* values (red spectrum). Selection of superior breeding trees for colour is likely to be based on dried samples exposed to sunlight to reliably highlight wood colour differences. A generally low ratio between tangential and radial shrinkages was found, which was reflected in a low incidence of board distortion (particularly cupping) during drying. A preliminary experiment was carried out to investigate the quality of NIR models to predict shrinkage and density. NIR spectra correlated reasonably well with radial shrinkage and air dried density. When calibration models were applied to their validation sets, radial shrinkage was predicted to an accuracy of 76% with Standard Error of Prediction of 0.21%. There was also a strong predictive power for wood density. These are encouraging results suggesting that NIR spectroscopy has good potential to be used as a non-destructive method to predict shrinkage and wood density using 12mm diameter increment core samples. Average green off saw recovery was 49.5% (range 40 to 69%) for Burdekin Agricultural College (BAC) logs and 41.9% (range 20 to 61%) for Katherine (NT) logs. These figures are about 10% higher than compared to 30-year-old Khaya study by Armstrong et al. (2007) however they are inflated as the green boards were not docked to remove wane prior to being tallied. Of the recovered sawn, dried and dressed volume from the BAC logs, based on the cambial face of boards, 27% could potentially be used for select grade, 40% for medium feature grade and 26% for high feature grades. The heart faces had a slightly higher recovery of select (30%) and medium feature (43%) grade boards with a reduction in the volume of high feature (22%) and reject (6%) grade boards. Distribution of board grades for the NT site aged 14 years followed very similar trends to those of the BAC site boards with an average (between facial and cambial face) 27% could potentially be used for select grade, 42% for medium feature grade, 26% for high feature grade and 5% reject. Relatively to some other subtropical eucalypts, there was a low incidence of borer attack. The major grade limiting defects for both medium and high feature grade boards recovered from the BAC site were knots and wane. The presence of large knots may reflect both management practices and the nature of the genetic material at the site. This stand was not managed for timber production with a very late pruning implemented at about age 12 years. The large amount of wane affected boards is indicative of logs with a large taper and the presence of significant sweep. Wane, knots and skip were the major grade limiting defects for the NT site reflecting considerable amounts of sweep with large taper as might be expected in younger trees. The green veneer recovered from billets of seven Khaya trees rotary peeled on a spindleless lathe produced a recovery of 83% of green billet volume. Dried veneer recovery ranged from 40 to 74 % per billet with an average of 64%. All of the recovered grades were suitable for use in structural ply in accordance to AS/NZ 2269: 2008. The majority of veneer sheets recovered from all billets was C grade (27%) with 20% making D grade and 13% B grade. Total dry sliced veneer recovery from the logs of the two largest logs from each location was estimated to be 41.1%. Very positive results have been recorded in this small scale study. The amount of colour development observed and the very reasonable recoveries of both sawn and veneer products, with a good representation of higher grades in the product distribution, is encouraging. The prospects for significant improvement in these results from well managed and productive stands grown for high quality timber should be high. Additionally, the study has shown the utility of non-destructive evaluation techniques for use in tree improvement programs to improve the quality of future plantations. A few trees combined several of the traits desired of individuals for a first breeding population. Fortunately, the two most promising trees (32, 19) had already been selected for breeding on external traits, and grafts of them are established in the seed orchard.

Relevância:

30.00% 30.00%

Publicador:

Resumo:

This study provides information about wood quality, structural properties, processing characterists and product suitability of wood harvested from fast-grown hardwood plantations. Wood quality attributes tested included density, extractive content, unit shrinkage, heartwood proportion and sapwood width. Structural properties tested included small clear and full section strength and stiffness, hardness, joint group, visual grade assessment and natural vibration-based grade assessment. The variation between the inner, intermediate and outer heartwood zones and the variation between provenances was also tested. Overall, the wood qualtiy attributes measured for 19 year-old E. cloeziana and 15 year-old E. pellita plantation material fall between those expected from the wood of mature, native forest trees and those found in younger plantation material of the same species.

Relevância:

30.00% 30.00%

Publicador:

Resumo:

Characterisation of mass transfer properties was achieved in the longitudinal, radial, and tangential directions for four Australian hardwood species: spotted gum, blackbutt, jarrah and messmate. Measurement of mass transfer properties for these species was necessary to complement current vacuum drying modelling research. Water-vapour diffusivity was determined in steady state using a specific vapometer. Permeability values of some species and material directions were extremely low and undetectable by the mass flow meter device. Hence, a custom system based on volume evolution was conceived to determine very low, previously unpublished, wood permeability values. Mass diffusivity and permeability were lowest for spotted gum and highest for messmate. Except for messmate, in the radial direction, the four species measured were less permeable in all directions than the lowest published figures, demonstrating the high impermeability of Australian hardwoods and partly accounting for their relatively slow drying rates. Premeability, water-vapour diffusivity, and associated anisotropic ratio data obtained for messmate were extreme or did not follow typical trends and is consequently the most difficult of the four woods to dry in terms of collapse and checkinng degradation.