A complete electrical characterization of hydrogenated amorphous silicon layers (a-Si:H) deposited on crystalline silicon (c-Si) substrates by electron cyclotron resonance chemical vapor deposition (ECR-CVD) was carried out. These structures are of interest for photovoltaic applications. Different growth temperatures between 30 and 200 °C were used. A rapid thermal annealing in forming gas atmosphere at 200 °C during 10 min was applied after the metallization process. The evolution of interfacial state density with the deposition temperature indicates a better interface passivation at higher growth temperatures. However, in these cases, an important contribution of slow states is detected as well. Thus, using intermediate growth temperatures (100–150 °C) might be the best choice.
Resumo:
Amorphous silicon thin films were deposited using the high pressure sputtering (HPS) technique to study the influence of deposition parameters on film composition, presence of impurities, atomic bonding characteristics and optical properties. An optical emission spectroscopy (OES) system has been used to identify the different species present in the plasma in order to obtain appropriate conditions to deposit high purity films. Composition measurements in agreement with the OES information showed impurities which critically depend on the deposition rate and on the gas pressure. We prove that films deposited at the highest RF power and 3.4 × 10^−2 mbar, exhibit properties as good as the ones of the films deposited by other more standard techniques.