Resumo:

Experiments of laser welding cast nickel-based superalloy K418 were conducted. Microstructure of the welded seam was characterized by optical microscopy (OM), scanning electron microscopy (SEM), X-ray diffraction (XRD), and energy dispersive spectrometer (EDS). Mechanical properties of the welded seam were evaluated by microhardness. The corresponding mechanisms were discussed in detail. Results show that the laser welded seam have non-equilibrium solidified microstructures consisting of Cr-Ni-Fe-C austenite solid solution dendrites as the dominant and some fine and dispersed Ni-3(Al,Ti) gamma' phase as well as little amount of MC needle carbides and particles enriched in Nb, Ti and Mo distributed in the interdendritic regions, cracks originated from the liquation of the low melting points eutectics in the HAZ grain boundary are observed, the average microhardness of the welded seam and HAZ is higher than that of the base metal due to alloy elements' redistribution of the strengthening phase gamma'. (C) 2008 Elsevier B.V. All rights reserved.

Relevância:

20.00% 20.00%

Publicador:

Resumo:

Microstructure characterization is important for controlling the quality of laser welding. In the present work, a detailed microstructure characterization by transmission electron microscopy was carried out on the laser welding cast Ni-based superalloy K418 turbo disk and alloy steel 42CrMo shaft and an unambiguous identification of phases in the weldment was accomplished. It was found that there are gamma-FeCrNiC austenite solid solution dendrites as the matrix, (Nb, Ti) C type MC carbides, fine and dispersed Ni-3 Al gamma' phase as well as Laves particles in the interdendritic region of the seam zone. A brief discussion was given for their existence based on both kinetic and thermodynamic principles. (c) 2007 Elsevier B.V. All rights reserved.

Relevância:

20.00% 20.00%

Publicador:

Resumo:

Exploratory experiments of laser welding cast Ni-based superalloy K418 turbo disk and alloy steel 42CrMo shaft were conducted. Microstructure of the welded seam was characterized by optical microscopy (OM), scanning electron microscopy (SEM), X-ray diffraction (XRD), energy-dispersive spectrometer (EDS). Mechanical properties of the welded seam were evaluated by microhardness and tensile strength testing. The corresponding mechanisms were discussed in detail. Results showed that the laser-welded seam had non-equilibrium solidified microstructures consisting of FeCr0.29Ni0.16C0.06 austenite solid solution dendrites as the dominant and some fine and dispersed Ni3Al gamma' phase and Laves particles as well as little amount of MC short stick or particle-like carbides distributed in the interdendritic regions. The average microhardness of the welded seam was relatively uniform and lower than that of the base metal due to partial dissolution and suppression of the strengthening phase gamma' to some extent. About 88.5% tensile strength of the base metal was achieved in the welded joint because of a non-full penetration welding and the fracture mechanism was a mixture of ductility and brittleness. The existence of some Laves particles in the welded seam also facilitated the initiation and propagation of the microcracks and microvoids and hence, the detrimental effects of the tensile strength of the welded joint. The present results stimulate further investigation on this field. (c) 2006 Elsevier B.V. All rights reserved.

Relevância:

20.00% 20.00%

Publicador:

Resumo:

Experimental trials of autogenous deep penetration welding between dissimilar cast Ni-based superalloy K418 and alloy steel 42CrMo flat plates with 5.0 mm thickness were conducted using a 3 kW continuous wave (CW) Nd:YAG laser. The influences of laser output power, welding velocity and defocusing distance on the morphology, welding depth and width as well as quality of the welded seam were investigated. Results show that full keyhole welding is not formed on both K4.18 and 42CrMo side, simultaneously, due to the relatively low output power. Partial fusion is observed on the welded seam near 42CrMo side because of the large disparity of thermal-physical and high-temperature mechanical properties of these two materials. Tile rnicrohardness of the laser-welded joint was also examined and analyzed. It is suggested that applying negative defocusing in the range of Raylei length can increase the welding depth and improve tile coupling efficiency of the laser materials interaction. (c) 2007 Elsevier Ltd. All rights reserved.

Relevância:

20.00% 20.00%

Publicador:

Resumo:

Experiments of autogenous laser full penetration welding between dissimilar cast Ni-based superalloy K418 and alloy steel 42CrMo flat plates with 3.5 mm thickness were conducted using a 3 kW continuous wave (CW) Nd:YAG laser. The influences of laser welding velocity, flow rate of side-blow shielding gas, defocusing distance were investigated. Microstructure of the welded seam was characterized by optical microscopy (OM), scanning electron microscopy (SEM) and X-ray diffraction (XRD) and energy dispersive spectrometer (EDS). Mechanical properties of the welded seam were evaluated by microhardness and tensile strength testing. Results show that high quality full penetration laser-welded joint can be obtained by optimizing the welding velocity, flow rate of shielding gas and defocusing distance. The laser-welded seam have non-equilibrium solidified microstructures consisting of gamma-FeCr0.29Ni0.16C0.06 austenite solid solution dendrites as the dominant and very small amount of super-fine dispersed Ni3Al gamma' phase and Laves particles as well as MC needle-like carbides distributed in the interdendritic regions. Although the microhardness of the laser-welded seam was lower than that of the base metal, the strength of the joint was equal to that of the base metal and the fracture mechanism showed fine ductility. (c) 2007 Elsevier B.V. All rights reserved.

Relevância:

20.00% 20.00%

Publicador:

Resumo:

A novel high-average-power pulsed CO2 laser with a unique electrode structure is presented. The operation of a 5-kW transverse-flow CO2 laser with the preionized pulse-train switched technique results in pulsation of the laser power, and the average laser power is about 5 kW. The characteristic of this technique is switching the preionized pulses into pulse trains so as to use the small preionized power (hundreds of watts) to control the large main-discharge power (tens of kilowatts). By this means, the cost and the complexity of the power supply are greatly reduced. The welding of LF2, LF21, LD2, and LY12 aluminum alloy plates has been successfully achieved using this laser. (c) 2005 Society of Photo-Optical Instrumentation Engineers.

Relevância:

20.00% 20.00%

Publicador:

Resumo:

A novel high-average-power pulsed CO2 laser with a unique electrode structure is presented. The operation of a 5-kW transverse-flow CO2 laser with the preionized pulse-train switched technique results in pulsation of the laser power, and the average laser power is about 5 kW. The characteristic of this technique is switching the preionized pulses into pulse trains so as to use the small preionized power (hundreds of watts) to control the large main-discharge power (tens of kilowatts). By this means, the cost and the complexity of the power supply are greatly reduced. The welding of LF2, LF21, LD2, and LY12 aluminum alloy plates has been successfully achieved using this laser. (c) 2005 Society of Photo-Optical Instrumentation Engineers.

Relevância:

20.00% 20.00%

Publicador:

Resumo:

Dental variation in the Chinese golden monkey (Rhinopithecus roxellana) is here evaluated by univariate, bivariate, and multivariate analyses. Allometric analyses indicate that canines and P3s are positively, but other dimensions negatively scaled to mandible and maxilla, and to body size. With the exception of the mesiodistal dimensions of I-1 and M-3, and the buccolingual dimension of Pq, mandibular dental variables show similar scaling relative to body size. Analysis of residuals shows that males have significantly larger canine, P-3 and buccolingual dimensions of the postcanine teeth (M-2 and M-3) than females. A significant difference in shape between the sexes is found in the buccolingual dimension of the upper teeth, but not in the mandible. Unlike the situation in some other species, Female golden monkeys do nor exhibit relatively larger postcanine teeth than males, in fact, the reverse is true, especially for M(2)s and M(3)s. The fact that most of the dental variables show low negative allometry to body size might be related a cold environment that has led to the development of larger body size with I-educed energy loss. When the raw data are examined by Discriminant Function Analysis the sexes are clearly distinguishable.

Relevância:

20.00% 20.00%

Publicador:

Resumo:

National Natural Science Foundation of China [40771205]; National Science Fund for Distinguished Young Scholars [40625002]; Chinese Academy of Sciences [KZCX2-YW-315]

Relevância:

20.00% 20.00%

Publicador:

Resumo:

To find the pathologic cause of the children's dental fluorosis in southwestern China, diet structure before the age of 6 and prevalence rate of dental fluorosis (DF) of 405 children were investigated, and the fluorine and arsenic content of several materials were determined. The prevalence rate of DF of children living on roasted corn before the age of 6 is 100% with nearly 95% having the mild to severe DF; while that of children living on non-roasted corn or rice is less than 5% with all having very mild DF. The average fluorine and arsenic concentration are 20.26 mg/kg and 0.249 mg/kg in roasted corn, which are about 16 times and 35 times more than in non-roasted corn, respectively. The average fluorine concentration is 78 mg/kg in coal, 1116 mg/kg in binder clay and 313 mg/kg in briquette (coal mixed with clay). The average arsenic concentration of coal is 5.83 mg/kg, the binder clay is 20.94 mg/kg, with 8.52 mg/kg in the briquette. Living on roasted corn and chili is the main pathologic cause of endemic fluorosis in southwestern China. The main source of fluorine and arsenic pollution of roasted corn and chill is the briquette of coal and binder clay. (C) 2010 Elsevier B.V. All rights reserved.

Relevância:

20.00% 20.00%

Publicador:

Resumo:

Immersion in various media has different effect on the properties of dental composites, such as sorption, solubility, elution of unreacted monomers, flexural strength, and flexural elastic modulus. In the present work, the effect of immersion in various media and the relationship between the variation of these properties and the components of dental composite were investigated.