Resumo:

The inhibitory effect of 2,3,5-triphenyl-2H-tetrazolium chloride (TTC) and 2,4,6-tri(2-pyridyl)-s-triazine (TPT) molecules on the corrosion of mild steel in 1 mol/L HCl and microcosmic inhibitory mechanism were investigated by X-ray photoelectron spectroscopy and ellipsometry. XPS results showed that C Is and N Is peaks of TTC, C Is and N Is peaks of TPT and their integral areas were obtained, which suggested the layer of the inhibitors (TTC or TPT) should have effectively protected the mild steel surface from the corrosion; and the depression from the inhibitors for the corrosion of mild steel surface was studied using ellipsometry combined with potentiodynamic polarization and the phasic difference was gained, which displayed the inhibitory coverage of the inhibitors formed.

Relevância:

40.00% 40.00%

Publicador:

Resumo:

The stress corrosion cracking (SCC) of LambdaISI 321 stainless steel in acidic chloride solution was studied by slow strain rate (SSR) technique and fracture mechanics method. The fractured surface was characterized by cleavage fracture. In order to clarify the SCC mechanism, the effects of inhibitor KI on SCC behaviour were also included in this paper. A study showed that the inhibition effects of KI on SCC were mainly attributed to the anodic reaction of the corrosion process. The results of strain distribution in front of the crack tip of the fatigue pre-cracked plate specimens in air, in the blank solution (acidic chloride solution without inhibitor KI) and in the solution added with KI measured by speckle interferometry (SPI) support the unified mechanism of SCC and corrosion fatigue cracking (CFC).

Relevância:

40.00% 40.00%

Publicador:

Resumo:

Electrochemical measurement, quantum chemical method, and scanning electron microscopy (SEM) were performed to investigate the inhibitive effect of 2,3,5-triphenyl-2H-tetrazolium chloride (TTC) and 2,4,6-tri(2-pyridyl)-s-triazine(TPT) on the corrosion of mild steel in 1mol.L-1 HCl at room temperature. Impedance spectroscopy measurement showed that the polarization resistance increased and that double layer capacitance decreased with the increase in the inhibitive concentration, and the results of potentiodynamic polarization showed that the inhibitors suppressed both cathodic and anodic processes of steel corrosion without change in the mechanism. Higher the orbital density distribution strength of the lowest unoccupied molecular orbital, higher is the molecule dipole, and lower energy gap between the energy of the highest occupied molecular orbital and the energy of the lowest unoccupied molecular orbital resulted in higher inhibitory efficiency. The results of SEM analysis showed that the metal was protected from aggressive corrosion by the addition of TTC and TPT.

Relevância:

30.00% 30.00%

Publicador:

Resumo:

The electrochemical corrosion behavior of Mg-6Al-0.4Mn and Mg-6Al-4RE-0.4Mn (RE = Mischmetal) alloys is investigated in 3.5% NaCl solution. The results of corrosion process, polarization behavior, and electrochemical impedance spectroscopy of the alloys reveal that Mg-6Al-4RE-0.4Mn exhibits enhanced corrosion resistance. The addition of RE stabilizes the solid solution and modifies the passive film through a finer microstructure.

Relevância:

30.00% 30.00%

Publicador:

Resumo:

In corrosion medium, metals can deform under tensile stress and form a new active surface with the anodic dissolution of the metals being accelerated. At the same time, the anodic dissolution may accelerate the deformation of the metals. The synergy can lead to crack nucleation and development and shorten the service life of the component. Austenitic stainless steel in acidic chloride solution was in active dissolution condition when stress corrosion cracking (SCC) occurred. It is reasonable to assume that the anodic dissolution play an important role, so it's necessary to study the synergy between anodic dissolution and deformation of austenitic stainless steels. The synergy between deformation and anodic dissolution of AISI 321 austenitic stainless steel in an acidic chloride solution was studied in this paper. The corrosion rate of the steel increased remarkably due to the deformation-accelerated anodic and cathodic processes. The creep rate was increased while the yield strength was reduced by anodic dissolution. The analysis by thermal activation theory of deformation showed a linear relationship between the logarithm of creep rate and the logarithm of anodic cur-rent. Besides, the reciprocal of yield strength was also linearly dependent on the logarithm of anodic current. The theoretical deductions were in good agreement with experimental results.

Relevância:

30.00% 30.00%

Publicador:

Resumo:

The chloride extraction rules of iron artifacts were studied by immersion methods. Different chloride extraction results between the alkaline solution and a washing solution were obtained. The microstructure and the anti-corrosion performance of the samples before and after treatment, were, respectively studied by the scanning electron microscope (SEM) and the potentiodynamic scanning method. The results indicated that Cl- removed according to the diffusion law. The microstructure of the samples transformed after treatment. The rusts became more compact, and the porosity also increased. The chloride extraction effect in the washing solution was better than that in the NaOH solution.

Relevância:

30.00% 30.00%

Publicador:

Resumo:

The chloride extraction rule of iron artifacts was studied by electrical methods. The effect of the current and potential value on the desalination result of simulated iron artifacts was studied through the galvanostatic and potentiostatic experiments the ingredients of the rust before and after treatments were also analyzed by the X-ray diffraction (XRD). It has been found that the optimal current density was between -0.50 and -0.75 mA/cm(2) and the optimal potential was between -1.175 and -1.200 V. The phase of the samples rusts transformed after treatment, as well as the anti-corrosion performance improved.

Relevância:

20.00% 20.00%

Publicador:

Resumo:

Ceramic coatings are produced on aluminum alloy by autocontrol AC pulse Plasma Electrolytic Oxidation (PEO) with stabilized average current. Transient signal gathering system is used to study the current, voltage, and the transient wave during the PEO process. SEM, OM, XRD and EDS are used to study the coatings evolution of morphologies, composition and structure. TEM is used to study the micro profile of the outer looser layer and inner compact layer. Polarization test is used to study the corrosion property of PEO coatings in NaCl solution. According to the test results, AC pulse PEO process can be divided into four stages with different aspects of discharge phenomena, voltage and current. The growth mechanism of AC PEO coating is characterized as anodic reaction and discharge sintering effect. PEO coating can increase the corrosion resistance of aluminum alloy by one order or two; however, too long process time is not necessarily needed to increase the corrosion resistance. In condition of this paper, PEO coating at 60 min is the most protective coating for aluminum alloy substrate. (C) 2008 Elsevier B.V. All fights reserved.

Relevância:

20.00% 20.00%

Publicador:

Resumo:

Fuzzy reliability methods are used to study the corrosion of pipelines. Three methods are used. They consist of using fracture failure modes, failure assessment diagram (FAD) and residual strength for establishing fuzzy reliability. Calculations are made by application of JC, improved GA-JC and Mente-carlo methods. Examples for oilfield injecting water pipeline show the residual strength well agree with field data. Mente-carlo methods appear to yield results that have better agreement with field data.

Relevância:

20.00% 20.00%

Publicador:

Resumo:

Yb3+Er3+-codoped chloride-modified germanate-bismuth-lead glasses have been synthesized by the conventional melting and quenching method. Structural and thermal stability properties have been obtained on the basis of the Raman spectra and differential thermal analysis, which indicate that the PbCl2 addition has an important influence on the phonon density of states, maximum phonon energy, and thermal stability of host glasses. The Judd-Ofelt intensity parameters and quantum efficiencies were calculated on the basis of the Judd-Ofelt theory and lifetime measurements. For the 1.53 mu m emission band, the full widths at the half-maximum increase and peak wavelengths are blueshifted with increasing PbCl2 content. Moreover, the effect of the PbCl2 addition on the phonon density of states, OH- content, and upconversion luminescence has been discussed and evaluated. Our results reveal that, with increasing PbCl2 content, the decrease of phonon density and OH- content contributes more to the enhanced upconversion emissions than that of maximum phonon energy. (c) 2005 Optical Society of America

Relevância:

20.00% 20.00%

Publicador:

Resumo:

Tm3+-doped oxide-chloride germanate and tellurite glasses have been synthesized by conventional melting method. Intense up-conversion luminescence emissions were simultaneously observed at room temperature in these glasses. The possible up-conversion mechanisms are discussed and estimated. However, in these Tm3+-doped glasses, tellurite glass showed weaker up-conversion emissions than germanate glass, which is inconsistent with the prediction from the difference of maximum phonon energy between tellurite and germanate glasses. In this paper, Raman spectroscopy was employed to investigate the origin of the difference in up-conversion luminescence in the two glasses. Our results confirm that, besides the maximum phonon energy, the phonon density of host glasses is also an important factor in determining the up-conversion efficiency. (c) 2005 Elsevier Ltd. All rights reserved.

Relevância:

20.00% 20.00%

Publicador:

Resumo:

Effect of the substitutions of chloride for fluoride on the chemical and physical properties and the crystallization behavior in heavy metal fluoride glasses has been investigated. The characteristic temperature of the glass does not changed obviously when the fluoride was taken place by chloride. Compared with samples of being free of ErF3, the doping samples are more inclined to be surface crystallization. Optical basicity in the glass system increases with increasing the negative charge provided by the chloride atoms and the absorption peak red shifted is observed in absorption spectra. XRD measurements show that not a single crystalline phase appears in the heated glass samples, which indicate the substitutions of chloride for fluoride with a variety of crystalline precipitation trends. (c) 2007 Elsevier B.V All rights reserved.

Relevância:

20.00% 20.00%

Publicador:

Resumo:

The pigments (melanoidins) in molasses wastewater are refractory to conventional biological treatment. Ferric chloride was used as coagulant to remove color and chemical oxygen demand (COD) from molasses effluent. Using jar test procedure, main operating conditions such as pH and coagulant dosage were investigated. Under the optimum conditions, up to 86% and 96% of COD and color removal efficiencies were achieved. Residual turbidity in supernatant was less than 5 NTU and Fe3+ concentration was negligible because of effective destabilization and subsequent sedimentation. The results of high performance size exclusion chromatography (HPSEC) show that low molecular weight (MW) fraction of melanoidins is more reactive than high MW fraction and increase in the concentration of the lowest MW organic group is related to the capacity of charge neutralization. Aggregate size measurement reveals the size effect on the settleability of flocs formed, with larger flocs settling more rapidly. Charge neutralization and co-precipitation are proposed as predominant coagulation mechanism under the optimum conditions. (C) 2009 Elsevier B.V. All rights reserved.