Resumo:
Aqueous conducting polyaniline dispersion was prepared employing acidic phosphate ester bearing hydrophilic ethylene glycol segment as dopant, and conducting film with electrical conductivity of 25 S/cm was obtained from the dispersion. Ordered self-assembly lamellar structure with interlamellar distance of 1.2 nm was observed in the film, which consisted of alternating layers of rigid polyaniline chain and flexible phosphate ester side chains, where the phosphate side chain layer was separated by two rigid polyaniline layers. The lamellar structure leading to high conducting film was formed due to the confinement of polyaniline chain by crystallizable phosphate side chain, since the electrical conductivity decreased by four orders of magnitude once the dopant side chain crystalline was destroyed. The crystallizable side chain forced lamellar structure is expected to be a new chance for highly conducting polyaniline.
Resumo:
Four single polymers with two kinds of attachment of orange chromophore to blue polymer host for white electroluminescence (EL) were designed. The effect of the side-chain attachment and main-chain attachment on the EL efficiencies of the resulting polymers was compared. The side-chain-type single polymers are found to exhibit more efficient white EL than that of the main-chain-type single polymers. Based on the side-chain-type white single polymer with 4-(4-alkyloxy-phenyl)-7-(4-diphenylamino-phenyl)-2,1,3-benzothiadiazoles as the orange-dopant unit and polyfluorene as the blue polymer host, white EL with simultaneous orange (lambda(max) = 545 nm) and blue emission (lambda(max) = 432 nm/460 nm) is realised. A single-layer device (indium tin oxide/poly(3,4-ethylenedioxythiophene)/polymer/Ca/Al) made of these polymers emits white light with the Commission Internationale de l'Eclairage coordinates of (0.30,0.40), possesses a turn-on voltage of 3.5 V, luminous efficiency of 10.66 cd A(-1), power efficiency of 6.68 lm W-1, and a maximum brightness of 21240 cd m(-2).
Resumo:
Two orange phosphorescent iridium complex monomers, 9-hexyl-9-(iridium (III)bis(2-(4'-fluorophenyl)-4-phenylquinoline-N, C-2')(tetradecanedionate-11,13))-2,7-dibromofluorene (Br-PIr) and 9-hexyl-9-(iridium(III)bis(2-(4'-fluorophenyl)-4-methylquinoline-N, C-2')(tetradecanedionate-11,13))-2,7-dibromofluorene (Br-MIr), were successfully synthesized. The Suzuki polycondensation of 2,7-bis(trimethylene boronate)-9,9-dioctylfluorene with 2,7-dibromo-9,9-dioetylfluorene and Br-Plr or Br-MIr afforded two series of copolymers, PIrPFs and MIrPFs, in good yields, in which the concentrations of the phosphorescent moieties were kept small (0.5-3 mol % feed ratio) to realize incomplete energy transfer. The photoluminescence (PL) of the copolymers showed blue- and orange-emission peaks. A white-light-emitting diode with a configuration of indium tin oxide/poly(3,4-ethylenedioxythiophene):poly(styrenesulfonate)/PIr05PF (0.5 mol % feed ratio of Br-PIr)/Ca/Al exhibited a luminous efficiency of 4.49 cd/A and a power efficiency of 2.35 lm/W at 6.0 V with Commission Internationale de L'Eclairage (CIE) coordinates of (0.46, 0.33). The CIE coordinates were improved to (0.34, 0.33) when copolymer MIr10PF (1.0 mol % feed ratio of Br-MIr) was employed as the white-emissive layer. The strong orange emission in the electroluminescence spectra in comparison with PL for these kinds of polymers was attributed to the additional contribution of charge trapping in the phosphorescent dopants.
Resumo:
Electric-field-induced molecular alignments of side-chain liquid-crystalline polyacetylenes [-{HC=C[(CH2)(m)OCO-biph-OC7H15]}-, where biph is 4,4'-biphenylyl and m is 3 (PA3EO7) or 9 (PA9EO7)] were studied with X-ray diffraction and polarized optical microscopy. An orientation as high as 0.84 was obtained for PA9EO7. Furthermore, the molecular orientation of]PA9EO7 was achieved within a temperature range between the isotropic-to-smectic A transition temperature and 115 degreesC, and this suggested that the orientational packing was affected by the thermal fluctuation of the isotropic liquid and the mobility of the mesogenic moieties. The maximum achievable orientation for PA9EO7 was much greater than that for PA3EO7. This was the first time that the electric-field-induced molecular orientation of a side-chain liquid-crystalline polymer with a stiff backbone was studied.
Resumo:
Mesomorphic properties of a side chain liquid crystalline polyacetylene, poly(11-{[(4'-heptyloxy-4-biphenylyl)carbonyl]oxy}-1-undecyne) (PA9EO7), are investigated using polarized optical microscope, X-ray diffraction, and transmission electron microscope. Polymer PA9EO7 forms enantiotropic smectic A and smectic B phases. It also exhibits an additional high order smectic phase, a sandwich structure consisting of different molecular packing of biphenyl mesogenic moieties from that of alkyl spacers and terminals, when it is prepared from its toluene solution. Shearing the polymer film at its smectic A phase generates banded texture with the alignment of the backbones parallel to the direction of shear force. While at its high order smectic phase, the mesogen pendants of the polymer are arranged parallel to the direction of shear. The different mesomorphic behaviors arise from different molecular alignments influenced by the fluidity.
Resumo:
A novel side-chain, liquid-crystalline ionomer (SLCI) with a poly(methyl hydrosiloxane) main chain and side chains containing sulfonic acid groups was used in blends of polyamide-1010 (PA1010) and polypropylene (PP) as a compatibilizer. The morphological structure, thermal behavior, and liquid-crystalline properties of the blends were investigated by Fourier transform infrared, differential scanning calorimetry, thermogravimetric analysis, and scanning electron microscopy. The morphological structure of the interface of the blends containing SLCI was improved with respect to the blend without SLCI. The compatibilization effect of greater than 8 wt % SLCI for the two phases, PA1010 and PP, was better than the effects of other SLCI contents in the blends.
Resumo:
The synthesis of new chiral smectic A (S-A) side-chain liquid crystalline polysiloxanes (LCPs) and ionomers (LCIs) containing 4-allyloxy-benzoyl-4-(S-2-ethylhexanoyl) p-benzenediol his ate (ABB) as mesogenic units and 4-[[4-(2-propenyloxy)phenyl] azo]benzensulfonic acid (AABS) as nonmesogenic units is presented. The chemical structures of the monomers and polymers are confirmed by FTIR spectroscopy or H-1-NMR. Differential scanning calorimetry (DSC), optical polarizing microscopy, and X-ray diffraction measurements reveal that all the polymers P-I-P-IV and ionomers P-V-P-VI exhibit S-A texture. The results seem to demonstrate that the tendency toward the S-A-phase region increases with increasing sulfonic acid concentration, and the thermal stability of the S-A phase is determined by the flexibility of the polymer backbones and the interactions of sulfonic acid groups. (C) 2001 John Wiley & Sons, Inc.
Resumo:
Using poly(styrene-co-maleic anhydride) as a backbone and poly(ethylene glycol) methyl ether (PEGME) with different molecular weights as side chains, three comb-like polymers and their Li salt complexes were synthesized. The dynamic mechanical properties and conductivities were investigated. Results showed that the polymer electrolytes possess two glass transitions: alpha -transition and beta -transition, and the temperature dependence of the ionic conductivity shows WLF (Williams-Landel-Ferry) behavior. Based on the time-temperature equivalence principle, a master curve was constructed by selecting T-beta as reference temperature. The values of the WLF parameters (C-1 and C-2) were obtained and were found to be almost independent of the length of the PEGME side chain and the content of Li salt. By reference to T-0 = 50 degreesC. the relation between log tau (c) and c was found to be linear. The master curves are displaced progressively to higher frequencies as the molecular weight of the side chain is increased. The relation between log tau (n) and the molecular weight of the side chain is also linear. (C) 2001 Elsevier Science B.V. All rights reserved.
Resumo:
A new series of side chain liquid crystal polymers based on the backbone of polymethacrylate containing 4-nitroazobenzene and 4-methoxybiphenyl group as side chain mesogen were prepared and characterized, FTIR, H-1 NMR, POM and WAXD were used to study the structure, phase behavior and mesophase texture of this series of SCLC copolymers. The researches show that polymer PM5MPP and copolymer M5MPP/MMEANB are enantiotropic liquid crystalline polymers, but polymer PMMEANB has no liquid crystalline properties. DSC results showed that the thermal stability of the mesophase of this series of copolymers was enhanced by the existence of intermolecular electron donor-acceptor interaction. It was found that the temperature range of the mesophase of the copolymers was broadened with increasing 4-nitroazobenzene units. The focal-conic texture observed by POM indicated that this series of the copolymers possessed the characteristics of smectic liquid crystal.
Resumo:
Using a graft modification method, a comblike polymer host (CBPE550) was synthesized by reacting monomethyl ether of poly(ethylene glycol) (PEGMA) with ethylene-maleic anhydride copolymer (EMAC) and endcapping the residual carboxylic acid with methanol. The product was characterized by IR and elementary analysis. Result showed that the product was amorphous and semi-ester product is accord with reaction equation. There were two peaks in the plot of the ionic conductivity against Li salt concentration. The plot of log a against 1/(T - T-0) shows a dual VTF behavior when using the glass transition temperature of PEO of side chain as T beta. The comblike polymer is a white rubbery solid. It can be well-dissolved in acetone. (C) 1999 Elsevier Science Ltd. All rights reserved.
Resumo:
Crosslinkable side-chain liquid crystalline polyesters PCn from N-[n-(4-(4-nitrophenylazo)phenyloxy)alkyl]diethanolamine (Cn, n = 3, 5, 6, 10) as mesogenic monomers and maleic anhydride were synthesized and characterized. The thermal properties of PCn's were studied by means of DSC, polarized optical microscopy (POM) and wide angle X-ray diffraction (WAXD), and the results showed that all the polymers studied exhibit enantiotropic liquid crystallinity. In the molar mass independent region, the relatively high content of cis -CH=CH- groups in the polymer backbone of PC3 causes an increase of the melting temperature (T-m) and a decrease of T-g and isotropisation temperature (T-i). The crosslinking of PCn in the radical polymerization with styrene was confirmed by FTIR spectroscopy. The absorption band at 1300 cm(-1) attributed to the in-plane C-H-bending vibration of trans -CH=CH- in the polymer backbone disappeared after crosslinking, indicating that the trans -CH=CH- functions are consumed in the crosslinking polymerization of styrene.
Resumo:
In this paper, phase transition temperatures of side chain liquid crystal polymer were predicted by molecular dynamics simulation. We analyzed the change of energy and the degree of similarity(S) with the temperature varying. The simulated phase transition temperatures agree with the experimental values in a proper deviation.
Resumo:
A series of novel thermotropic side-chain liquid crystalline polymer based on polymethacrylate backbone containing electron-accepting 4-(4'-nitrophenylazo)phenoxy as nonlinear optical active group and electron-donating 4(4'-methoxyphenyl) phenoxy group as mesogen attached covalently to the backbone through the flexible spacer was prepared and characterized, respectively. The results from differential scanning calorimetry showed that these series of copolymers were enantiotropic liquid crystal with single mesophase. The melting points and the relative enthalpy change of the copolymers depressed with increasing the molar percent of 4'-nitroazobenzene monomer units over 0 similar to 50mol%, but the enthalpies change of the transition from mesophase to isotropic state increased for the copolymers containing 0 similar to 50mol% 4'-nitroambenzene units. The texture observed under polarized optical microscope identified that the copolymers containing 24molar% or more than 24mol% 4-nitroambenzene monomer units could form smectic mesophase with the focal-conic texture. The results detected by WAXD were in good agreement with the results observed by POM.
Resumo:
A new side chain liquid crystalline poly[4-(methacryloxy)hexanoloxy-4'-benzyloxy biphenyl] was synthesized. The phase behavior of the monomer and homopolymer was studied. The monomer shows a smectic B phase, while the homopolymer shows a nematic phase. The nonmesogenic nonlinear optical group was introduced to synthesize a series of side chain liquid crystalline copolymers which also show a nematic phase. Owing to the liquid crystallinity of the copolymer has been the orientational stability improved, down the relax of the orientation slowed and the nonlinear optical properties enhanced.
Resumo:
The poly(monoester (6-[4-(p-nitrophenyl) azo]phenoxy-1-hexyloxy) of maleic anhydride) shows a smectic phase with a focal conic fan texture. With the decrease of the monoestering degree the phase transition temperature decreases and the mesomorphic temperature range becomes narrow. The hydrogen bonding between two carboxylic acid groups was found to play a very important role in forming the smectic phase structure. The smectic bilayer structure has been built through self-assembly via. intermolecular hydrogen bonding.