Resumo:
Eu ions doped SiO2 thin films, SiO2( Eu), were prepared by co-sputtering of SiO2 and Eu2O3 and Eu ion implantation into thermally grown SiO2 films. The Eu-L-3-edge X-ray absorption near edge structure (XANES) spectra of SiO2(Eu) films show a doublet absorption peak structure with energy difference of 7 eV, which indicates the conversion of Eu3+ to Eu2+ at high annealing temperature in N-2. The strong blue luminescence of SiO2(Eu) films prepared by ions implantation after films annealed above 1100 degreesC confirms the above argument.
Density functional theory study of triangular molybdenum sulfide nanocluster and CO adsorption on it
Resumo:
The ovaries of Kun-Ming strain mice (3 weeks) were irradiated with different doses of C-12(6+) ion or Co-60 gamma-ray. Chromosomal aberrations were analyzed in metaphase II oocytes at 7 weeks after irradiation. The relative biological effectiveness (RBE) of C C-12(6+) ion was calculated with respect to Co-60 gamma-ray for the induction of chromosornal aberrations. The C-12(6+) ion and Co-60 gamma-ray dose-response relationships for chromosomal aberrations were plotted by linear quadratic models. The data showed that there was a dose-related increase in frequency of chromosomal aberrations in all the treated groups compared to controls. The RBE values for C-12(6+) ions relative to (CO)-C-60 gamma-rays were 2.49, 2.29, 1.57, 1.42 or 1.32 for the doses of 0.5, 1.0, 2.07 4.0 or 6.0 Gy, respectively. Moreover, a different distribution of the various types of aberrations has been found for C-12(6+) ion and Co-60 gamma-ray irradiations. The dose-response relationships for C-12(6+) ion and (CO)-C-60 gamma-ray exhibited positive correlations. The results from the present study may be helpful for assessing genetic damage following exposure of immature oocytes to ionizing radiation.
Resumo:
Sr2Mg(BO3)(2) thermoluminescence (TL) phosphor was synthesized by a high temperature solid state reaction and the effect of Li+, Bi3+, Gd3+ or Ti4+ as a codopant on TL of Sr2Mg(BO3)(2) : Dy was investigated. The results show that Li+ as a codopant improves the emission intensity of high temperature TL peak of Sr2Mg(BO3)(2) : Dy phosphor whereas the addition of Bi3+, Gd3+ or Ti3+ leads to the decrease of TL intensity. The TL emission bands of Sr2Mg(BO3)(2) : Dy phosphors with Li+, Bi3+, Gd3+ or Ti4+ as a codopant are situated at 480, 579, 662 and 755 nm, which were attributed to the characteristic F-4(9/2)-> H-6(15/2), F-4(9/2)-> H-6(13/2), F-4(9/2)-> H-6(11/2) and F-4(9/2)-> H-6(9/2) transitions of Dy3+ ion, consistent with the emission of Sr2Mg(BO3)(2) : Dy phosphors. The kinetics parameters of 234 degrees C TL peak of Sr2Mg(BO3)(2) Dy-0.04(3+), (Li-0.04(+)) phosphor with the values of trap depth E=1.1 eV, frequency factor s=6.3 x 10(9) s(-1) were estimated by a peak shape method, which obey the second order kinetics.
Resumo:
Sr2Mg(BO3)(2) thermoluminescence (TL) phosphor was synthesized by a high temperature solid state reaction and the effect of Li+, Bi3+, Gd3+ or Ti4+ as a codopant on TL of Sr2Mg(BO3)(2) : Dy was investigated. The results show that Li+ as a codopant improves the emission intensity of high temperature TL peak of Sr2Mg(BO3)(2) : Dy phosphor whereas the addition of Bi3+, Gd3+ or Ti3+ leads to the decrease of TL intensity. The TL emission bands of Sr2Mg(BO3)(2) : Dy phosphors with Li+, Bi3+, Gd3+ or Ti4+ as a codopant are situated at 480, 579, 662 and 755 nm, which were attributed to the characteristic F-4(9/2)-> H-6(15/2), F-4(9/2)-> H-6(13/2), F-4(9/2)-> H-6(11/2) and F-4(9/2)-> H-6(9/2) transitions of Dy3+ ion, consistent with the emission of Sr2Mg(BO3)(2) : Dy phosphors. The kinetics parameters of 234 degrees C TL peak of Sr2Mg(BO3)(2) Dy-0.04(3+), (Li-0.04(+)) phosphor with the values of trap depth E=1.1 eV, frequency factor s=6.3 x 10(9) s(-1) were estimated by a peak shape method, which obey the second order kinetics.
Resumo:
A novel method was developed to prepare the highly active Pt-Ru-P/C catalyst. The deposition of phosphorus significantly increased electrochemical active surface (EAS) area of catalyst by reduces Pt-Ru particle size. TEM images show that Pt-Ru-P nanoparticles have an uniform size distribution with an average diameter of 2 nm. Cyclic voltammetry (CV), Chronoamperometry (CA), and CO stripping indicate that the presence of non-metal phosphorus as an interstitial species Pt-Ru-P/C catalyst shows high activity for the electro-oxidation of methanol, and exhibit enhanced performance in the oxidation of carbon monoxide compared with Pt-Ru/C catalyst. At 30 degrees C and pure oxygen was fed to the cathode, the maximum power density of direct methanol fuel cell (DMFC) with Pt-Ru-P/C and Pt-Ru/C catalysts as anode catalysts was 61.5 mW cm(-2) and 36.6 mW cm(-2), respectively. All experimental results indicate that Pt-Ru-P/C catalyst was the optimum anode catalyst for direct methanol fuel cell.