本文报道了太行花属(Taihangia Yu et Li)的种群分布、生物学特性和离体培养的初步结果。 太行花种群由于环境和生物等方面的原因仅在太行山区有狭小分布。来源于不同地区种群的太行花其形态特征具有丰富的表型,在引种条件下更为显著。而酯酶同工酶和过氧化物酶同工酶分析进一步证实了其遗传的稳定性和同源性。 实验表明,太行花在北纬39°58',最低温度-11℃的北京北京植物园,露地越冬正常。温度提高至40℃时生长发育受抑制而迟滞,以25℃最为适宜,增殖率最高。太行花对土壤的适应范围较广,在泥炭培养土上移殖的幼苗成活率达97.20%,主根须根发达,叶生长良好。不同强度光照处理12000Lux效果最好。 太行花生育期为230多天,生长积温为3763℃左右。物候期受环境条件和当年气候的影响,不同种群和个体之间有一定的差异。花的性别、花期和开花量等与纬度、海拔主要与温湿度相关。 太行花的茎尖、花芽、花梗、萼片、花瓣和叶子等外植体均能在MS附加不同种类和浓度植物激素的培养基中分化,其分化途径和分化效果因附加成分、外植体类别而异。在含有0.1mg/L IAA和0.5mg/L 6-BA的培养基中,不但能启动花芽正常生长、开花、形成合子胚,而且也能诱导花芽、花梗、茎尖产生花芽和营养芽。在芽的继代培养中,细胞分裂素能大量诱导芽的分化,最好的配比是0.5mg/L 6-BA、0.1mg/L ZJ;只含生长素时可以诱导生根或脱分化,其中生根最好的是0.5mg/L IAA;2.4-D单独使用时,能较好地使花芽、叶等脱分化,其最佳浓度为1.0mg/L。
Resumo:
Re-examination of the syntypes of the capillariid nematode Neocapillaria phoxini Yu et Wang, 1994, the type species of Neocapillaria Yu et Wang, 1994, described from the intestine of the freshwater fish Phoxinus lagowskii variegatus Gunther (Cyprinidae) from China, confirmed its morphological similarity with species of Freitascapillaria Moravec, 1987, to which it is transferred as Freitascapillaria phoxini (Yu et Wang, 1994) comb. n. Consequently, Neocapillaria Yu et Wang, 1994 (a homonym to Neocapillaria Moravec, 1987) and Sinocapillaria Moravec et Spratt, 1998 become junior synonyms of Freitascapillaria. Skrjabinocapillaria gigantea is transferred to Freitascapillaria as F. gigantea (Wang, 1984) comb. n.
Resumo:
Composite coatings were obtained on A3 steel by hot dipping aluminum(HDA) at 720 ℃ for 6 min and micro-plasma oxidation(MPO) in alkali electrolyte. The surface morphology, element distribution and interface structure of composite coatings were studied by means of XRD, SEM and EDS. The results show that the composite coatings obtained through HDA/MPO on A3 steel consist of four layers. From the surface to the substrate, the layer is loose Al2O3 ceramic, compact Al2O3 ceramic, Al and FeAl intermetallic compound layer in turn. The adhesions among all the layers are strengthened because the ceramic layer formed at the Al surface originally, FeAl intermetallic compound layer and substrate are combined in metallurgical form through mutual diffusion during HDA process.Initial experiment results disclose that the anti-corrosion performance and wear resistance of composite coating are obviously improved through HDA/MPO treatment.
Resumo:
Using a refined two-dimensional hybrid-model with self-consistent microwave absorption, we have investigated the change of plasma parameters such as plasma density and ionization rate with the operating conditions. The dependence of the ion current density and ion energy and angle distribution function at the substrate surface vs. the radial position, pressure and microwave power were discussed. Results of our simulation can be compared qualitatively with many experimental measurements.
Resumo:
To accomplish laser-induced thermal loading simulation tests for pistons,the Gaussian beam was modulated into multi-circular beam with specific intensity distribution.A reverse method was proposed to design the intensity distribution for the laser-induced thermal loading based on finite element(FE) analysis.Firstly,the FE model is improved by alternating parameters of boundary conditions and thermal-physical properties of piston material in a reasonable range,therefore it can simulate the experimental resul...
Resumo:
An improved electromechanical model of the RF MEMS (radio frequency microelectromechanical systems) switches is introduced, in which the effects of intrinsic residual stress from fabrication processes, axial stress due to stretching of beam, and fringing field are taken into account. Four dimensionless numbers are derived from the governing equation of the developed model. A semi-analytical method is developed to calculate the behavior of the RF MEMS switches. Subsequently the influence of the material and geometry parameters on the behavior of the structure is analyzed and compared, and the corresponding analysis with the dimensionless numbers is conducted too. The quantitative relationship between the presented parameters and the critical pull-in voltage is obtained, and the relative importance of those parameters is given.
Resumo:
The growth of highly lattice-mismatched InAs0.3Sb0.7 films on (100) GaAs Substrates by magnetron Sputtering has been investigated and even epitaxial lnAs(0.3)Sb(0.7) films have been successfully obtained. A strong effect of the growth conditions on the film structure was observed, revealing that there was a growth mechanism transition from three-dimensional nucleation growth to epitaxial layer-by-layer growth mode when increasing the substrate temperature. A qualitative explanation for that transition was proposed and the critical conditions for the epitaxial layer-by-layer growth mode were also discussed.
Resumo:
The aggregation behaviors of two surfactants with the same hydrophobic tail, sodium bis(2-ethylhexyl)sulfosuccinate (AOT) and sodium bis(2-ethylhexyl)phosphate (NaDEHP), have been investigated by the fluorescence technique and z-potential (ζ) measurements. Five fine peaks of the pyrene molecule fluorescence spectroscopy appear in the surfactant solution, and the micropolarity at which pyrene locates is monitored from the intensity ratio of the first (I1) and the third peak (I3). A wide peak around 475 nm, the emission spectra of the excimer of pyrene molecules, is observed in the NaDEHP solution, while this is not found for the AOT system. The value of I1/I3 decreases in a more limited concentration range for the AOT system than for NaDEHP, indicating that small aggregates can be more easily formed by NaDEHP molecules. The z-potential results for the aggregates formed by the two surfactants show that the interaction between AOT and PVP is stronger than that between NaDEHP and PVP.
Resumo:
Carbon-nanotube sCNTd-reinforced hydroxyapatite composite coatings have been fabricated by laser surface alloying. Microstructural observation using high-resolution transmission electron microscopy showed that a large amount of CNTs remained with their or
Resumo:
Cowper-Symonds and Johnson-Cook dynamic constitutive relations are used to study the influence of both strain rate effect and temperature variation on the material intrinsic length scale in strain gradient plasticity. The material intrinsic length scale decreases with increasing strain rates, and this length scale increases with temperature.
Resumo:
A new approach is developed to the fabrication of high-quality three-dimensional macro-porous copper films. A highly-ordered macroporous copper film is successfully produced on a polystyrene sphere (PS) template that has been modified by sodium dodecyl sulfate (SDS). It is shown that this procedure can change a hydrophobic surface of PS template into a hydrophilic surface. The present study is devoted to the influence of the electrolyte solution transport on the nucleation process. It is demonstrated that the permeability of the electrolyte solution in the nanochannels of the PS template plays an important role in the chemical electrodeposition of high-quality macroporous copper film. The permeability is drastically enhanced in our experiment through the surface modi. cation of the PS templates. The method could be used to homogeneously produce a large number of nucleations on a substrate, which is a key factor for the fabrication of the high-quality macroporous copper film.
Resumo:
Cylindrical specimens (4 mm diameter and 4 mm height) of titanium alloy bar were given various heat treatments to provide a wide range of microstructures and mechanical parameters. These specimens were then subjected to high plastic strain at a large strain rate (103 s-1 ) during dynamic compression by a split Hopkinson bar at ambient temperature. The microstructures of the localised shear bands were examined by optical and transmission electron microscopy. The results show that there are two types of localised shear bands: deformed and white shear bands. A detailed observation reveals that there is no difference in the nature of the deformed and white shear bands, but they occur at different stages of localised deformation. It is found that there is a burst of strain, corresponding to a critical strain rate at which the white shear band occurs and no phase transformation occurs in the shear bands.