41 resultados para Binary Cyclically Permutable Constant Weight Codes
em Chinese Academy of Sciences Institutional Repositories Grid Portal
Resumo:
Molecular weight dependence of phase separation behavior of the Poly (ethylene oxide) (PEO)/Poly(ethylene oxide-block-dimethylsiloxane) (P(EO-b-DMS)) blends was investigated by both experimental and theoretical methods. The cloud point curves of PEO/P(EO-b-DMS) blends were obtained by turbidity method. Based on Sanchez-Lacombe lattice fluid theory (SLLFT), the adjustable parameter, epsilon*(12)/k (quantifying the interaction energy between different components), was evaluated by fitting the experimental data in phase diagrams. To calculate the spinodals, binodals, and the volume changes of mixing for these blends, three modified combining rules of the scaling parameters for the block copolymer were introduced.
Resumo:
A series of binary SB blend samples with various overall volume fraction of PS (Phi(PS)) and different discrete distribution of the block length (denoted as d(PS) or d(PB)) were prepared by mixing various asymmetric poly(styrene)-block-poly(butadiene) (SB) block copolymers with a symmetric SB block copolymer. The influences of the external solvent field, composition, and the block length distribution on the morphologies of the blends in the thin films were investigated by atomic force microscopy (AFM) and transmission electron microscopy (TEM). The experimental results revealed that after solvent annealing, the interface of the blend thin films depended mainly on the cooperative effects of the annealing solvent and the inherently interfacial curvature of the blends. Upon exposure to the saturated vapor of cyclohexane, which has preferential affinity for the PB block, a "threshold" of Phi(PS) (approximate 0.635-0.707) was found. Below such threshold, the influence of the annealing solvent played an important role on the interfacial curvature of the blend thin film.
Resumo:
A series of reactor blends of linear and branched polyethylenes have been prepared, in the presence of modified methylaluminoxane, using a combination of 2,6-bis[1(2,6-dimethyphenylimino) pyridyl]-cobalt(II) dichloride (1), known as an active catalyst for producing linear polyethylene, and [1,4-bis(2,6-diidopropylphenyl)] acenaphthene diimine nickel(II) dibromide (2), which is active for the production of branched polyethylene. The polymerizations were performed at various levels of catalyst feed ratio at 10 bar. The linear correlation between catalyst activity and concentration of catalyst 2 suggested that the catalysts performed independently from each other. The weight-average molecular weights ((M) over bar (w)), crystalline structures, and phase structures of the blends were investigated, using a combination of gel permeation chromatography, differential scanning calorimetry, wide-angle X-ray diffraction, and small angle X-ray scattering techniques. It was found that the polymerization activities and MWs and crystallization rate of the polymers took decreasing tendency with the increase of the catalyst 2 ratios, while melting temperatures (T-m), crystalline temperatures (T,), and crystalline degrees took decreasing tendency. Long period was distinctly influenced by the amorphous component concentration.
Resumo:
The interfacial tension sigma between two polyisobutylenes (PIB) of dissimilar polydispersity and two polydisperse samples of poly(dimethylsiloxane) (PDMS) was measured as a function of time by means of a pendent drop apparatus at different temperatures ranging from 30 to 110 degreesC. In addition to three of the four possible binary blends, the time evolution of sigma was also determined for one ternary system, where the PIB phase contained 0.03 wt % of a diblock copolymer poly(isobutylene-b-dimethylsiloxane). The pronounced decrease of sigma with advancing time, observed in all cases, is attributed to the migration of the interfacially active lower molecular weight components of the homopolymers and of the compatibilizer into the interphase. Several days are normally required until a becomes constant. These time independent values are not considered as equilibrium data, but accredited to stationary states. A kinetic model is established for sigma(t), which enables a detailed investigation of the rates of transport of the different migrating species of average molar mass of M.
Resumo:
Binary symmetric diblock copolymer blends, that is, low-molecular-weight poly(styrene-block-methyl methacrylate) (PS-b-PMMA) and high-molecular-weight poly(styrene-block-methacrylate) (PS-b-PMA), self-assemble on silicon substrates to form structures with highly ordered nanoholes in thin films. As a result of the chemically similar structure of the PMA and the PMMA block, the PMMA chain penetrates through the large PMA block that absorbs preferentially on the polar silicon substrate. This results in the formation of nanoholes in the PS continuous matrix.
Resumo:
Ordered hexagonal droplets patterns in phase-separating polymeric blend films of polystyrene and poly(2-vinylpyridine) (PS/PVP) formed due to the convection effect by solvent evaporation. The influences of PS molecular weight, solvent evaporation rate, and the weight ratio of PS to PVP on the PVP-rich domains pattern formation and distributions were investigated by atomic force microscope (AFM). Only in an appropriate range of molecular weight of PS, can the ordered pattern form. Too low or too high molecular weight of PS led no ordered pattern due to the viscosity effects. The increase of solvent evaporation rate decreased the mean radius of the PVP-rich domains and the intervals between the centers of the domains due to the enhancement of the viscosity on the top layer of the fluid film. The increase of the weight ratio of PS to PVP decreased mean radius of the PVP-rich domains whereas the intervals between the centers of droplets remained constant. Therefore, the size and the distributions of ordered patterns can be tuned by the polymer molecular weight, the weight ratio of the two components and the solvent evaporation rate.
Resumo:
The glass transition temperature (T-g) of mixtures of polystyrene (PS) with different molecular weight and of blends of poly(2,6-dimethyl-p-phenylene oxide) (PPO) and polystyrene with different molecular weight (DMWPS) was studied by a DSC method. For the whole range of composition, the curves of T-g vs composition obtained by experiment were compared with predictions from the Fox, Gordon-Taylor, Couchman and Lu-Weiss, equations. It was found that the experimental results were not in agreement with those from the Fox, Gordon-TayIor and Couchman equations for the binary mixtures of DMWPS, where the interaction parameter chi was approximately zero. However, for the blends PPO/DMWPS (chi < 0), with an increase of molecular weight of PS, it was shown that the experimental results fitted well with those obtained from the Couchman, Gordon-Taylor and Fox equations, respectively. Furthermore, the Gordon-Taylor equation was nearly identical to the Lu-Weiss equation when \chi\ was not very large. Further, the dependence of the change of heat capacity associated with the glass transition (Delta C-p) on the molecular weight of PS was investigated and an empirical equation was presented. (C) 1997 Elsevier Science Ltd.
Resumo:
The kinetics of the polymerization of isoprene with the heterogeneous rare earth catalyst system isopropoxyneodymium dichloride/triethylaluminium (Nd(OPri)Cl-2-AlEt(3)) was examined in a specially designed dilatometer. The rate of polymerization is expressed as R(p) approximate to -d[M]/dt = k'(p)[Nd](1.40)[M]. The main kinetical parameters such as the concentration of active propagating chain, the efficiency of lanthanide catalyst used (ELCU), the absolute rate constant of propagation as well as the average life time of growing chains, were determined at 30 degrees C, 40 degrees C, 45 degrees C and 50 degrees C.
Resumo:
The glass transition temperature (T(g)) of cyclic polystyrene was measured by differential scanning calorimetry. There was a marked difference in the glass transition behaviour between cyclic and linear polystyrene. In the low molecular weight region (M(n) < 5 x 10(3)), the T(g) of the cyclic polystyrene increased with decreasing M(n), contrary to that of linear polystyrene. With M(n) higher than 5 x 10(3), the T(g) of cyclic polystyrene increased with increasing M(n). The T(g) of cyclic and linear polystyrene approached the same constant value when the M(n) was high enough (M(n) > 10(5)). Combining the results of specific volume, it is believed that the variation of T(g) with molecular weight does not depend only on free volume effects but that configurational entropy is also an important factor.
Resumo:
A method based on capillary zone electrophoresis (CZE) was used to study the interaction between low molecular weight heparin (LMWH) and interleukin 2 (IL-2). The results showed that the increase of the concentration of LMWH led to the decrease of the peak height and the increase of the peak width of IL-2, but the peak areas were kept constant. The binding constant of IL-2 with LMWH was calculated as 1.2 x 10(6) M(-1) by Scatchard analysis, which is in good agreement with the results found in the references using enzyme-linked immunosorbent assay (ELISA). The results demonstrated that the interaction between IL-2 and LMWH is of fast on-and-off kinetic binding reaction. CZE might be used to study not only slow on-and-off rates interactions, but also fast on-and-off rates ones. The binding constant can be calculated easily, and the method can be applied to study a wide range of heparin-protein interactions. (c) 2005 Elsevier B.V. All rights reserved.
Resumo:
It has been reported recently that single carbon nanotubes were attached to AFM tips to act as nanotweezers. In order to investigate its stability, a vertical single-walled carbon nanotube (SWCNT) under its own weight is studied in this paper. The lower end of the carbon nanotube is clamped. Firstly the governing dimensionless numbers are derived by dimensional analysis. Then the theoretical analysis based on an elastic column model is carried out. Two ratios, I.e., the ratio of half wall thickness to radius (t=R) and the ratio of gravity to elastic resilience ($\rho$gR=E), and their influences on the ratio of critical length to radius are discussed. It is found that the relationship between the critical ratio of altitude to radius and ratio of half thickness to radius is approximately linear. As the dimensionless number $\rho$gR=E increases, the compressive force per unit length (weight) becomes larger, thus critical ratio of altitude to radius must become smaller to maintain stability. At last the critical length of SWCNT is calculated. The results of this paper will be helpful for the stability design of nanotweezers-like nanostructures.
Resumo:
The subject of the present work is to report an experimental comparative study of the effect of dispersion-induced turbulence on dust combustion in constant volume vessel, carried out both in normal gravity and in microgravity environment. Dispersion system with small scale of turbulence, creating uniform homogeneous mixture, was used in experiments. To improve reproducibility of the explosion data an ignitor of small energy, with local soft ignition was developed. Both factors contributed to acquisition of more reproducible experimental data. In experiments under microgravity conditions a dust suspension during combustion remains constant. This makes possible to study dust explosion under stationary dust suspension without influence of turbulence.
Resumo:
Forced dissociation of selectin-ligand bonds is crucial to such biological processes as leukocyte recruitment, thrombosis formation, and tumor metastasis. Although the bond rupture has been well known at high loading rate r(f) (>= 10(2) pN/s), defined as the product of spring constant k and retract velocity v, how the low r(f) (< 10(2) pN/s) or the low k regulates the bond dissociation remains unclear. Here an optical trap assay was used to quantify the bond rupture at r(f) <= 20 pN/s with low k (similar to 10(-3)-10(-2) pN/nm) when P-selectin and P-selectin glycoprotein ligand 1 (PSGL-1) were respectively coupled onto two glass microbeads. Our data indicated that the bond rupture force f retained the similar values when r(f) increased up to 20 pN/s. It was also found that f varied with different combinations of k and v even at the same r(f). The most probable force, f