A comb polymer (CP350) with oligo-oxyethylene side chains of the type -(CH2CH2O)(7)CH3 was prepared from methyl vinyl ether/maleic anhydride copolymer and poly(ethylene glycol) methyl ether. The polymer can dissolve LiNO3 salt to form homogeneous amorphous polymer electrolyte. This electrolyte system was first found to have two class glass transitions, and the two T(g)s were observed to increase with increasing salt content. The ionic conduction was measured by using the complex impedance method, and conductivities were investigated as functions of temperature and salt concentration. At 25 degrees C, the ionic conductivity maximum of this system can get to 3.72 X 10(-5) S/cm at the [Li]/ [EO] ratio of 0.057. The appearance of the conductivity maximum has been interpreted as being due to the effect of T-g and the so called physical crosslinks. The temperature dependence of the ionic conductivity displaying non-Arrhenius behaviour can be analyzed using the Vogel-Tammann-Fulcher equation and interpreted on the basis of the configurational entropy model.

Relevância:

20.00% 20.00%

Publicador:

Resumo:

The microphase separation, glass transition and crystallization of two series of tetrahydrofuran-methyl methacrylate diblock copolymers (PTHF-b-PMMA), one with a given PTHF block of M(n) = 5100 and the other with a given PTHF block of (M) over bar(n) = 7000, were studied in this present work. In the case of solution-cast materials, the microphase separation of the copolymer takes place first, with crystallization then gradually starting in the formed PTHF microphase. The T-g of the PMMA microphase shows a strong dependence on the molecular weight of the PMMA block, while the T-g of the PTHF microphase shows a strong dependence on the copolymer composition. The non-isothermal crystallization temperature (T-c) of the diblock copolymer decreases rapidly and continuously with the increase in the amorphous PMMA weight fraction; the lowest T-c of the copolymer is ca. 35 K lower than the T-c of the PTHF homopolymer. There also exists a T-c dependence on the molecular weight of the PTHF block. In addition, when the major component of the copolymer is PMMA, a strong dependence of the crystallizability of the copolymer on the molecular weight of the PTHF block is observed; the higher the molecular weight, then the stronger its crystallizability. The melting temperature of the block copolymer is dependent on the copolymer composition and the molecular weight of its crystallizable block. Copyright (C) 1996 Elsevier Science Ltd.

Relevância:

20.00% 20.00%

Publicador:

Resumo:

Porphyra yezoensis Ueda (Rhodophyta) is a seaweed of economic importance with a typical dimorphic life cycle consisting of a leafy gametophyte and a filamentous sporophyte. Recently, it has been recognized as a model system for fundamental and applied studies in marine biological sciences. Conchospore, a major spore linking the two distinct multicellular phases in the life cycle, is most widely used in the breeding of P. yezoensis. In this paper, the early-stage development of conchospore, including the attachment and the cell wall formation, was studied with fluorescent reagents staining and Scanning Electron Microscopy detection. Results displayed: (I) the cell wall began to be generated after culturing for 4 h in the attached conchospores; (2) the initially released conchospores were plastids with some filmy, amorphous substance on the surface, and they attached to the fibers firmly via the actively secreted mucilaginous substances after their touch to the fibers; (3) cellulase and pectolase prohibited the attachment of conchospores in the different ways; and (4) only attached conchospores generated cell walls and developed normally, while the suspending ones could not. It indicated that the cellulose played crucial roles in the permanent attachment as the pectin did in the initial attachment. The conchospore attachment seemed to trigger the cell wall formation and the further development. Affects of light on the development of conchospores were also discussed. The results showed that high intensity (200 mu mol.m(-2).s(-1)) and long-wave (>= 580 nm) light facilitated the division rate of conchospores. (C) 2008 Elsevier B.V. All rights reserved.

Relevância:

20.00% 20.00%

Publicador:

Resumo:

A FeNiSiBV amorphous composite coating was developed by laser cladding of metallic powders on AISI 1020 low carbon steel substrate. The coatings were studied using X-ray diffraction, transmission electron microscopy and scanning electron microscopy. The coating reveals different microstructures along the depth of the coating. The transition zone exhibits good metallurgical bonding between the substrate and the coating. The layer consists of amorphous phase in majority and nanocrystalline phase/crystalline phase in minority. Accompanied with the nanocrystalline phase, the amorphous phase is concentrated in the middle of the coating. The crystalline phase in the coating is identified as Fe2B. A gradient distribution of the microhardness ranges from 1208 HV0.2 to 891 HV0.2 in the coating along the depth. The coating shows higher microhardness and better wear property than the substrate.

Relevância:

20.00% 20.00%

Publicador:

Resumo:

The heat capacity of nanostructured amorphous SiO2 (na-SiO2) has been measured by adiabatic calorimetric method over the temperature range 9-354 K. TG and differential scanning calorimeter (DSC) were also employed to determine the thermal stability. Glass transition temperature (T-g) for the two same grain sizes with different specific surface of naSiO(2) samples and one coarse-grained amorphous SiO2 (ca-SiO2) sample were determined to be 1377, 1397 and 1320 K, respectively. The low temperature experimental results show that there are significant heat capacity (C-P) enhancements among na-SiO2 samples and ca-SiO2. Entropy, enthalpy, Gibbs free energy and Debye temperature (theta (D)) were obtained based on the low temperature heat capacity measurement of na-SiO2. The Cp enhancements of na-SiO2 were discussed in terms of configurational and vibrational entropy. (C) 2001 Elsevier Science B.V. All rights reserved.

Relevância:

20.00% 20.00%

Publicador:

Resumo:

Fe-B ultrafine amorphous alloy particles (UFAAP) were prepared by chemical reduction of Fe3+ with NaBHO4 and confirmed to be ultrafine amorphous particles by transmission electron microscopy and X-ray diffraction. The specific heat of the sample was measured by a high precision adiabatic calorimeter, and a differential scanning calorimeter was used for thermal stability analysis. A topological structure of Fe-B atoms is proposed to explain two crystallization peaks and a melting peak observed at T=600, 868 and 1645 K, respectively.

Relevância:

20.00% 20.00%

Publicador:

Resumo:

In this study, a novel sol-gel method is used to synthesize amorphous silica-alumina materials with a narrow mesoporous distribution and various Si/Al molar ratios without using any templates and pore-regulating agents. During the preparation procedure, only inexpensive inorganic salts were used as raw materials, instead of expensive and harmful alkoxides. The precursor sol was dried at room temperature in a vacuum box kept at 60 mmHg until it began to form the gel. The results of a nitrogen sorption experiment indicate that the synthesized materials with different Si/Al molar ratios have similar mesoporous distributions (within 2-12 nm). Moreover, it was found that the material's pore size distribution remains at a similar value during the heat treatment from room temperature to 550 degreesC. On the basis of the nitrogen sorption, TEM, and AFM characterization results, a formation mechanism of mesopores which accounts for the experimental data is also suggested. This suggested mechanism involves rearrangement of the primary particles during the drying process to form the precursors of the similarly sized mesopores. The synthesized materials were characterized by XRD, thermal analysis (TG/DTA), Al-27 and Si-29 MAS NMR spectroscopy, SEM, TEM, and AFM. The results of Al-27 and 29Si MAS NMR indicate that the distribution of silicon and aluminum in the synthesized materials is more uniform and homogeneous than that in the mixed oxides prepared via the traditional sol-gel method even at high alumina contents. The type and density of the acid sites were studied using pyridine adsorption-desorption FTIR spectroscopy. It was shown that the acidity of the synthesized materials is higher than that of the silica-alumina materials prepared by conventional methods.

Relevância:

20.00% 20.00%

Publicador:

Resumo:

The variation of surface compositions on amorphous Ni80.4W1.5P18.1 alloy by O-2 oxidation and H-2 reduction treatments have been studied by XPS, UPS and ISS. It shows that addition of tungsten in the amorphous Ni-P alloy leads to dramatic changes of the relating component distributions in the surface layers before and after these treatments. Oxidation of a Ni80.4W1.5P18.1 amorphous alloy in 1 bar of oxygen at 513 K caused a significant segregation of nickel in different oxide states at the surface. The subsequent reduction of the oxidized surface with I bar hydrogen at 553 K resulted in only a small portion of Ni and P being reduced into elemental states, while most of them was found to combine to form a kind of nickel phosphate compound. On the other hand, under the same conditions, the oxidation and reduction of a Ni80P20 alloy gave rise to metallic Ni and elemental P as the predominate species on the alloy surface. The addition of W in the amorphous alloy might act as nuclei for a favorable formation of the phosphate structure which was proposed to be an active species for hydrogen-relating catalytic reactions. (C) 1999 Elsevier Science B.V. All rights reserved.

Relevância:

20.00% 20.00%

Publicador:

Resumo:

Ultra-fine particle of Ni-B amorphous alloy was prepared by chemical reduction of Ni2+ with NaBH4 and characterized with TEM and XRD. The heat capacity and thermal stability were measured with a high-precision automatic adiabatic calorimeter and DTA. The upper limit of applied temperature of the substance was found to be 684 K for use as catalyst. (C) 1999 Elsevier Science B.V. All rights reserved.