167 resultados para 340-U1401C
Resumo:
A novel sulfonated diamine monomer, 1,4-bis(4-aminophenoxy)-naphthyl-2,7-disulfonic acid (BAPNDS), was synthesized. A series of sulfonated polyimide copolymers were prepared from BAPNDS, 1,4,5,8-naphthalenetetracarboxylic dianhydride (NTDA) and nonsulfonated diamine 4,4'-diaminodiphenyl ether (ODA). Flexible, transparent, and mechanically strong membranes were obtained. The membranes displayed slightly anisotropic membrane swelling. The dimensional change in thickness direction was larger than that in planar. The novel SPI membranes showed higher conductivity, which was comparable or even higher than Nafion 117. Membranes exhibited methanol permeability from 0.24 x 10(-6) to 0.80 X 10(-6) cm(2)/s at room temperature, which was much lower than that of Nafion (2 x 10-6 CM2/s). The copolymers were thermally stable up to 340 degrees C. These preliminary results have proved its potential availability as proton-exchange membrane for PEMFCs or DMFCs.
Resumo:
Polypeptide/polysaccharide graft copolymers poly(L-lysine)-graft-chitosan (PLL-g-Chi) were prepared by ring-opening polymerization (ROP) of epsilon-benzoxycarbonyl L-lysine N-carboxyanhydrides (Z-L-lysine NCA) in the presence of 6-O-triphenylmethyl chitosan. The PLL-g-Chi copolymers were thoroughly characterized by H-1 NMR, C-13 NMR, Fourier transform infrared (FT-IR), and gel permeation chromatography (GPC). The number-average degree of polymerization of PLL grafted onto the chitosan backbone could be adjusted by controlling the feed ratio of NCA to 6-O-triphenylmethyl chitosan. The particle size of the complexes formed from the copolymer and calf thymus DNA was measured by dynamic light scattering (DLS). It was found in the range of 120 similar to 340 nm. The gel retardation electrophoresis showed that the PLL-g-Chi copolymers possessed better plasmid DNA-binding ability than chitosan. The gene transfection effect in HEK 293T cells of the copolymers was evaluated, and the results showed that the gene transfection ability of the copolymer was better than that of chitosan and was dependent on the PLL grafting ratio. The PLL-g-Chi copolymers could be used as effective gene delivery vectors.
Resumo:
Ultrathin multilayer films of a rare-earth-containing polyoxometalate Na-9[Eu(W5O18)(2)] (EW) and Poly (allyamine hydrochloride) (PAH) have been prepared by layer-by-layer self-assembly from dilute aqueous solutions. The fabrication process of the EW/PAH multilayer films was followed by UV-vis spectroscopy and ellipsometry, which show that the deposition process is linear and highly reproducible from layer to layer. An average EW/PAH bilayer thickness of ca. 2.1 nm was determine,by ellipsometry. In addition, the scanning electron microscopy (SEM) image of the EW/PAH film indicates that the film sufface is relatively uniform and smooth. The photoluminescent properties of these films were also investigated by fluoresence spectroscopy.
Resumo:
玻璃微米管针尖可用于支撑微米级的水/1,2-二氯乙烷(W/DCE)界面,并用来研究二苯基-15-冠-5(DB15C5)加速钠离子和钾离子转移反应的机理和求算其络合物的稳定常数.在两种极限情况下,即水相中金属离子浓度远大于有机相中DB15C5的浓度(DB15C5扩散控制过程)和有机相中DB15C5的浓度远大于水相中金属离子浓度(金属离子扩散控制过程),循环伏安研究表明,加速钠离子转移反应均发生1∶1(金属离子:载体)的界面络合转移过程,相应的一级络合常数分别为logβ1=8.97±0.05和logβ1=8.63±0.03.而对于加速钾离子转移反应,当 DB15C5扩散控制时发生的是一个1:2的界面络合转移过程,当钾离子扩散控制时,在电位窗内却观察到两个过程:一个较低电位的1∶2的界面络合转移过程和一个较高电位的1∶1界面络合转移过程.两种极限条件下所求算的钾离子和DB15C5的二级络合常数分别为logβ1=13.64±0.03和logβ2=11.34±0.24.
Resumo:
The shear-induced spiral-like morphology of a main-chain thermotropic liquid crystalline poly(aryl ether ketone) is observed and characterized by means of polarizing light microscopy, atomic force microscopy, transmission electron microscopy and electron diffraction techniques. The spiral-like texture is formed during shearing in the temperature range of liquid crystalline to isotropic transition (335-340 degreesC), and dispersed discontinuously in the mosaic matrix. Electron diffraction results indicate that the spiral exhibits orthorhombic lateral packing of the crystals and homeotropic alignment of the molecules. The spiral formation process and possible affecting factors are discussed.
Resumo:
A ferrocene-dimyristoyl phosphatidylcholine (DMPC) film electrode was prepared by casting the solution of ferrocene and DMPC in chloroform onto a glassy carbon electrode surface. Ferrocene retained in the biological membrane gave a couple of irreversible peaks of cyclic voltammogram. The electrode exhibited good electrocatalytic activity for the oxidation of ascorbic acid (H(2)A) in phosphate buffer (pH 6.64) with an anodic peak potential of +340 mV (vs. Ag/AgCl). The anodic current was directly proportional to the square root of the scan rate below 150 mV s(-1). The influence of the pH value was investigated and it was observed that pH 6.64 was the suitable value to the anodic peak potential and current. The thickness of the film and the interference of uric acid were also studied. The electrode can be used to determine H(2)A in the presence of equimolar uric acid. The catalytic peak current increased linearly with the concentration of H(2)A in the range of 1 X 10(-4)-5 X 10(-3) mol L-1.
Resumo:
Nanoindentation technique and scanning force microscopy have been used to measure directly the polyethylene modulus along the chain axis. Single crystals of polyethylene were employed in order to obtain well-aligned chain segments. To minimize effects of scanner creep, a Z scan rate of 3 Hz was employed. The "X Rotate" value of 25 degrees was selected to eliminate effects of lateral tip motion. The results were analyzed by the Oliver -Pharr method for which direct observation and measurement of the contact area are not required. Considering the influence of tip roundness on the projected contact area, the nanoindentation results were analyzed by the Sawa method. The chain modulus obtained from the thinner polyethylene single crystal sample was 204 +/- 21 GPa by the Oliver-Pharr method and 168 +/- 17 GPa by the Sawa method. The lower values than expected were due to substrate effects and anisotropy of chain deformation during nanoindentation. An extrapolation of the chain modulus obtained by various strains to zero nanoindentation eliminated the effect of substrate and anisotropy of chain deformation. The corresponding chain modulus obtained from the thicker sample was 278 GPa by the Oliver-Pharr method and 267 GPa by the Sawa method, respectively, in better agreement with the value of 340 Cpa determined theoretically. (C) 2001 Elsevier Science Ltd. All rights reserved.
Resumo:
The fluorescences of BSA and glycosylated BSA were observed respectively. The lambda(cm) of BSA was 340 nm; while the lambda(cm) of glycosylated BSA was 436 nm. Because the fluorescence spectra of them were different greatly, we can observe the suppression of Ge-132 on the Maillard reaction of BSA without any interference of itself. It was showed that the fluorescence intensity of glycosylated BSA increased continuously with the cultured time, Ge-132 may suppress the Maillard reaction of BSA greatly, and the suppressing efficicency would be 32 %. The key site of the Maillard reaction of BSA is free amino groups of alanine residues on N-terminal amino group, besides the epsilon-amino groups of intrachain Lysine residues.
Resumo:
The novel poly(aryl ether ketone)s containing chloro-side group were synthesized by nucleophilic substitution reactions of 4,4'-biphenol and chlorohydroquinone with either 4,4'-difluorobenzophenone(BP/CH/DF) or 1,4-bis(p-fluorobenzoyl)benzene (BP/CH/BF) and their thermotropic liquid crystalline properties were characterized by a variety of experimental techniques. The thermotropic liquid crystalline behavior was observed in the copolymers containing 50 and 70% biphenol. Melting transition (Tm) and isotropization transition (Ti) both appeared in the DSC thermograms. A banded texture was formed after shearing the sample in the liquid crystalline state. The novel poly(aryl ether ketone)s had relatively higher glass transition temperature (Tg) in the range of 168 similar to 200 degrees C and lower melting temperature (Tm) in the range of 290 similar to 340 degrees C. The thermal stability (Td) was in the range of 430 similar to 490 degrees C.
Resumo:
The gold electrodes coated by n-alkanethiol with various chain lengths were used to study the permeability of uric acid, ascorbic acid, 4-aminophenol, paracetanol and phenacetin by means of linear sweep voltammetry. The results show that the optimum chain length is n=10. The improvements in the selectivity and the stability of the amperometric detection of these compounds in a flow stream were obtained by n-alkanethiol self assembled monolayers modified electrodes based on their differences in the hydrophobicity and the permeability.
Resumo:
We study here the reactions between C-60 and planar C5H5+ cations that lead to the formation of [C60C5H5](+) adduct cations in the chemical ionization source of the mass spectrometer. The structures, stabilities and charge locations of some possible isomers of [C60C5H5](+): sigma-adduct, pi-complex, [1,4]- and [1,2]-addition cations, are studied by AM1 semiempirical molecular orbital calculations. We find that the most stable is the sigma-addition cation. Another interesting and stable structure is the pi-complex cation which is bonded by the electrostatic interaction at the inter-ring distance of 1.589 Angstrom with the C-5v symmetry. The C5H5+ cyclopentadienium cation seems to be an ''inverted umbrella'' sitting on a five-membered ring of the C-60 cage.
Resumo:
The states of cytochrome C molecules in aquous solution were studied with synchronous fluorescence spectroscopy, It was found that the synchronous fluorescent spectra of cytochrome C were contributed by tyrosine and tryptophan residues separately at Delta lambda = 20 nm and Delta lambda = 80 nm, The peak position in synchronous fluorescent spectra of tyrosine residues in cytochrome C molecule does not change with its concentration, but that of tryptophan residue changes with its concentration, Only one peak at 340.0 nm was observed in the dilute solution of cytochrome C, With increasing the concentration of cytochrome C, a new peak at 304. 0 nm appeared. The peak at 340.0 nm disappeared and only one peak at 304.0 nm was observed at a higher concentration of cytochrome C, It may originate from the change of aggregation states of cytochrome C molecules and it was considered that the peak at 340.0 nm was attributed to the monomer and peak at 304.0 nm was due to the dimmer or oligomers. When urea was added into cytochrome C solution in which both monomer and dimmer or oligomers exist, cytochrome C molecules do not denature in the range of the specific concentrations of urea. The concentration of monomer of cytochrome C molecules increased and that of aggregation slates decreased by adding urea, Therefore, the synchronous fluorescence spectroscopy can be used to identify monomer and aggregation states of cytochrome C molecules.
Resumo:
Polytetrafluoroethylene (PTFE) has never been reported to form a network structure when subjected to high energy radiation. Results obtained in this work indicates that when irradiation is performed under 330-340-degrees-C in vacuo PTFE can be crosslinked
Resumo:
合成了聚[苯乙烯-甲基丙烯酸β(甲基亚硫酰基)乙酯]载体-三氯化公络合物(PSM·NdCl_3),以红外光谱,X-射线光电子能谱等方法对其作了表征。实验结果表明,PSM·NdCl_3是配键型聚合物戴体-稀土金属络合物;Nd离子在络合物中分布均匀;PSM·NdCl_3和不同烷基铝组成的体系对丁二烯聚合的活性差别很大;在PSM·NdCl_3分子中引入某种Lewis酸可以改善其催化活性,并探讨了催化活性中心的生成机理。