Resumo:
采用丘克拉斯基(Czochralski)技术生长了掺铥硅酸镥(Tm∶Lu2SiO5,Tm∶LSO)晶体;测量了LSO晶体在室温下的非偏振吸收光谱和非偏振荧光光谱;利用窄得-奥菲特(Judd-Ofelt)理论计算了Tm∶LSO晶体的窄得-奥菲特强度参数、振子强度、自发辐射概率、辐射寿命、积分吸收截面和积分发射截面.Tm∶LSO晶体的强度参数为Ω2=9.1355×10-20cm2,Ω4=8.4103×10-20cm2,Ω6=1.5908×10-20cm2;Tm∶LSO晶体在1.9μm附近有明显的发射峰(3F4→3H6跃迁),相应的辐射寿命为2.03 ms,积分发射截面为5.81×10-18cm2,半峰全宽(FWHM)为250 nm.用Tm∶LSO晶体在77 K温度下实现了激光运转.利用792 nm的激光二极管(LD)作为抽运源,获得中心波长为1960 nm的激光输出,抽运阈值为2.13 kW/cm2.
Resumo:
The Ho:YAP crystal is grown by the Czochralski technique. The room-temperature polarized absorption spectra of Ho:YAP crystal was measured on a c-cut sample with 1 at% holmium. According to the obtained Judd-Ofelt intensity parameters Omega(2) = 1.42 x 10(-20) cm(2), Omega(4) = 2.92 x 10(-20) cm(2), and Omega(6) = 1.71 x 10(-20) cm(2), this paper calculated the fluorescence lifetime to be 6 ms for I-5(7) -> I-5(8) transition, and the integrated emission cross section to be 2.24 x 10(-18) cm(2). It investigates the room-temperature Ho:YAP laser end-pumped by a 1.91-mu m Tm:YLF laser. The maximum output power was 4.1 W when the incident 1.91-mu m pump power was 14.4W. The slope efficiency is 40.8%, corresponding to an optical-to-optical conversion efficiency of 28.4%. The Ho:YAP output wavelength was centred at 2118 nm with full width at half maximum of about 0.8 nm.
Resumo:
The 2 at.% Sm:GdVO4 crystal was grown by the Czochralski method. The segregation coefficient of Sm3+ ion in this crystal is 0.98. The crystal structure of the Sm:GdVO4 crystal was determined by X-ray diffraction analysis. Judd-Ofelt theory was used to calculate the intensity parameters (Omega(i)), the spontaneous emission probability, the luminary branching ratio and the radiative lifetime of the state (4)G(5/2). The stimulated emission cross-sections at 567, 604 and 646 nm are calculated to be 5.92 x 10(-21), 7.62 x 10(-21) and 5.88 x 10(-21) cm(2), respectively. The emission cross-section at 604 nm is 4.4 times lager than that in Sm: YAP at 607 nm. (C) 2007 Elsevier B.V. All rights reserved.
Resumo:
Er-Si-O (Er2SiO5) crystalline films are fabricated by the spin-coating and subsequent annealing process. The fraction of erbium is estimated to be 21.5 at% based on Rutherford backscattering measurement. X-ray diffraction pattern indicates that the Er-Si-O films are similar to Er2SiO5 compound in the crystal structure. The fine structure of room-temperature photoluminescence of Er3+-related transitions suggests that Er has a local environment similar to the Er-O-6 octahedron. Our preliminary results show that the intensity of 1.53 mu m emission is enhanced by a factor of seven after nitrogen plasma treatment by NH3 gas with subsequent post-annealing. The full-width at half-maximum of 1.53 pm emission peak increases from 7.5 to 12.9 nm compared with that of the untreated one. Nitrogen plasma treatment is assumed to tailor Er3+ local environment, increasing the oscillator strength of transitions and thus the excitation/emission cross-section. (c) 2005 Elsevier B.V. All rights reserved.
Resumo:
A novel neodymium pentafluoropropionate binuclear complex, Nd(C(2)F(5)COO)(3)Dipy (Dipy: 2,2'-dipyridyl), was synthesized and characterized by single-crystal X-ray diffraction. At a concentration of 0.2 M in DMSO-d(6), the Judd-Ofelt parameters (Omega(2), Omega(4), Omega(6)) were calculated from the UV-Vis spectrum. According to the small value of Omega(2) and the zero splitting energy of (4)F/(3/2) level, a symmetric ligand field of the complex was confirmed in DMSO-d(6). Strong emission of the complex in DMSO-d(6) at 1057 nm with a decay time about 1.3 mu s were detected when excited at 800 nm pumped by a laser diode. The stimulated emission cross-section of (4)F(3/2) -> (4)I(11/2) fluorescence transition was 2.36 x 10 (20) cm(2) and comparable with some laser glasses, which indicated good radiative properties of this neodymium pentafluoropropionate binuclear complex in liquid matrix. (c) 2008 Elsevier B.V. All rights reserved.
Resumo:
A novel Nd3+-doped lead fluorosilicate glass (NPS glass) is prepared by a two-step melting process. Based on the absorption spectrum a Judd-Ofelt theory analysis is made. The emission line width of NPS glass is 44.2nm. The fluorescence decay lifetime of the 4F3/2 level is 586±20μsec, and the stimulated emission cross-section is 0.87×10-20cm2 at 1056nm. A laser oscillation is occurred at 1062nm when pumped by 808nm Diode Laser. The slope efficiency is 23.7% with a 415mJ threshold. It is supposed that NPS glass is a good candidate for using in ultra-short pulse generation and amplification by the broad emission bandwidth and long fluorescence lifetime.
Resumo:
Ultrashort pulses were generated in passively mode-locked Nd:YAG and Nd:GdVO4 lasers pumped by a pulsed laser diode with 10-Hz repetition rate. Stable mode-locked pulse trains were produced with the pulse width of 10 ps. The evolution of the mode-locked pulse was observed in the experiment and was discussed in detail. Comparing the pulse evolutions of Nd:YAG and Nd:GdVO4 lasers, we found that the buildup time of the steady-state mode-locking with semiconductor saturable absorber mirrors (SESAMs) was relevant to the upper-state lifetime and the emission cross-section of the gain medium.
Resumo:
Condensation of steam in a single microchannel, silicon test section was investigated visually at low flow rates. The microchannel was rectangular in cross-section with a depth of 30 pm, a width of 800 mu m and a length of 5.0 mm, covered with a Pyrex glass to allow for visualization of the bubble formation process. By varying the cooling rate during condensation of the saturated water vapor, it was possible to control the shape, size and frequency of the bubbles formed. At low cooling rates using only natural air convection from the ambient environment, the flow pattern in the microchannel consisted of a nearly stable elongated bubble attached upstream (near the inlet) that pinched off into a train of elliptical bubbles downstream of the elongated bubble. It was observed that these elliptical bubbles were emitted periodically from the tip of the elongated bubble at a high frequency, with smaller size than the channel width. The shape of the emitted bubbles underwent modifications shortly after their generation until finally becoming a stable vertical ellipse, maintaining its shape and size as it flowed downstream at a constant speed. These periodically emitted elliptical bubbles thus formed an ordered bubble sequence (train). At higher cooling rates using chilled water in a copper heat sink attached to the test section, the bubble formation frequency increased significantly while the bubble size decreased, all the while forming a perfect bubble train flowing downstream of the microchannel. The emitted bubbles in this case immediately formed into a circular shape without any further modification after their separation from the elongated bubble upstream. The present study suggests that a method for controlling the size and generation frequency of microbubbles could be so developed, which may be of interest for microfluidic applications. The breakup of the elongated bubble is caused by the large Weber number at the tip of the elongated bubble induced by the maximum vapor velocity at the centerline of the microchannel inside the elongated bubble and the smaller surface tension force of water at the tip of the elongated bubble.
Resumo:
The characteristic Ll, Lα, Lβ and Lγx-rays of Au and energy shifts produced by 20–50MeV 16O5+ beams on a thick Au ilm are measured with a Si (Li) detector. Cross-section ratios of σ(Ll)/σ(Lα), σ(Lβ)/σ(Lα) andσ(Lγ)/σ(Lα) versus O5+ energy show that consistent calculations yield considerably better agreements. Energy shifts Ll, Lα, Lβ and Lγ x-rays of Au target increase with more incidence energy. The main application for these measurements is multi-element trace analysis through particle induced x-ray emission.
Resumo:
An investigation into the three-dimensional propagation of the transmitted shock wave in a square cross-section chamber was described in this paper, and the work was carried out numerically by solving the Euler equations with a dispersion-controlled scheme. Computational images were constructed from the density distribution of the transmitted shock wave discharging from the open end of the square shock tube and compared directly with holographic interferograms available for CFD validation. Two cases of the transmitted shock wave propagating at different Mach numbers in the same geometry were simulated. A special shock reflection system near the corner of the square cross-section chamber was observed, consisting of four shock waves: the transmitted shock wave, two reflection shock waves and a Mach stem. A contact surface may appear in the four-shock system when the transmitted shock wave becomes stronger. Both the secondary shock wave and the primary vortex loop are three-dimensional in the present case due to the non-uniform flow expansion behind the transmitted shock.
Resumo:
Resonant cavity modes in a torus with elliptical cross section are studied by means of a direct variational method. The nonlinear effects of toroidicity and ellipticity on the frequency of the basic mode are analyzed simply and systematically without the restriction of linear theory. It is shown that the toroidicity effect on the m = 0 transverse magnetic mode is less-than-or-equal-to 11%. The frequency of the mode shifts approximately 11-29% when the elongation of the cross section changes from 1 to 2. The effects of toroidicity and ellipticity differ for each resonant mode.
Resumo:
通过对新合成的芴的一种具有对称性衍生物4-2-(7-(4-氨基苯乙烯基)-9,9-二(2-乙基己基)-9H-芴-2-)乙烯基)苯胺(BASF)的DMF溶液的研究,发现其具有很强三光子吸收频率上转换荧光发射特性,实验测出上转换荧光的波长范围是456-775nm,在510nm处的荧光强度与入射光强的三次方成正比.在0.03mol/L的浓度下就有明显的三光子吸收诱导的光限幅效应.非线性吸收系数和吸收截面分别为y=4.34×10^20 cm^3/W^2和σ3=2.4×10^-39 cm^6/W^2.
Resumo:
This paper reports on the steady-state fluorescence, three- photon absorption-induced fluorescence emission and subsequently induced optical limiting behaviour of a fluorene derivative with D-pi-D structural motifs. The lifetime of the steady-state fluorescence is 0.903 ns. Large optical limiting behaviour induced by 3PA has also been demonstrated, and the nonlinear absorption coefficient gamma derived from 3PA fitting curves is 5.92 x 10(-20) cm(3)/W-2 and the corresponding molecular 3PA cross-section sigma(3)' is 1.14 x 10(-76) cm(6) s(2).
Resumo:
测试了不同掺杂浓度和样品厚度下掺铒磷酸盐和碲酸盐玻璃的吸收光谱、荧光光谱和荧光寿命,计算了Er^3+离子在1.53μm处的吸收截面(σa)、发射截面(σe)、自发辐射跃迁概率(Arad)、辐射跃迁寿命(τrad)、以及辐射跃迁量子效率(η)等光谱参数.讨论了荧光俘获效应对掺铒磷酸盐和碲酸盐玻璃光谱性质及光谱参数的影响.结果表明即使在铒离子低掺杂浓度(0.1mol%Er2O3)下,荧光俘获效应也普遍存在于掺铒玻璃材料中,使得荧光寿命(τt)和荧光半高宽(FWHM)随样品的厚度和铒离子掺杂浓度增加而增大,导致
Resumo:
研究了Na2O含量对Na2O-Al2O3-SiO2(NAS)玻璃的光谱性质的影响。利用Judd-Ofelt(J-O)理论和吸收光谱计算了Er^3+掺杂的铝硅酸盐玻璃的Ωt参数、自发辐射几率和自发辐射寿命,分析了Ωt参数与Na2O含量的关系以及与吸收截面,Er^3+离子^4I13 2能级的自发辐射几率和荧光半峰全宽(FWHM)等性质的关系。随Na2O含量的增加.J-O参数Ωt(t=2,4,6)减小,Er^3+离子1533nm的吸收截面和荧光半峰全宽.Er^3+离子^4I13 2能级的自发辐射几率也减小,而E