The variations of unit cell parameters and crystallite size of nine PEEK samples treated at various temperatures have been studied by using Wide-Angle X-ray Diffraction (WAXD), The results indicate a decrease in unit cell parameter a,b and c but an increase in crystallite size L(hkl) With the increase beat treatment temperature. Based on X-ray scattering intensity theory and using the graphic multipeak resolution method, the formula of degree of crystallinity (W-c,W-X) for PEEK is derived. The results calculated are compatible with the density measurement and calorimetry.

Relevância:

100.00% 100.00%

Publicador:

Resumo:

The miscibility and phase behavior of polysulfone (PSF) and poly(hydroxyether of bisphenol A) (phenoxy) with a series of copoly(ether ether ketone) (COPEEK), a random copolymer of poly(ether ether ketone) (PEEK), and phenolphthalein poly(ether ether ketone) (PEK-C) was studied using differential scanning calorimetry. A COPEEK copolymer containing 6 mol % ether ether ketone (EEK) repeat units is miscible with PSF, whereas copolymers containing 12 mol % EEK and more are not. COPEEK copolymers containing 6 and 12 mol % EEK are completely miscible with phenoxy, but those containing 24 mol % EEK and more are immiscible with phenoxy. Moreover, a copolymer containing 17 mol % EEK is partially miscible with phenoxy; the blends show two transitions in the midcomposition region and single transitions at either extreme. Two T(g)s were observed for the 50/50 blend of phenoxy with the copolymer containing 17 mol % EEK, whereas a single composition-dependent T-g appeared for all the other compositions. An FTIR study revealed that there exist hydrogen-bonding interactions between phenoxy and the copolymers. The strengths of the hydrogen-bonding interactions in the blends of the COPEEK copolymers containing 6 and 12 mol % EEK are the same as that in the phenoxy/PEK-C blend. However, for the blends of copolymers containing 17, 24, and 28 mol % EEK, the hydrogen-bonding interactions become increasingly unfavorable and the self-association of the hydroxyl groups of phenoxy is preferable as the content of EEK units in the copolymer increases. The observed miscibility was interpreted qualitatively in terms of the mean-field approach. (C) 1996 John Wiley & Sons, Inc.

Relevância:

100.00% 100.00%

Publicador:

Resumo:

Poly-o-methylaniline (poly-o-toluidine) was doped by some protonic acids. It was found that the acidity, molecular size and oxidizing ability of protonic acids affected the doping level and conductivity of polymer obtained to some extent. The organic acid

Relevância:

100.00% 100.00%

Publicador:

Resumo:

The excimer fluorescence of a triblock copolymer, styrene-butadiene-styrene (SBS) containing 48 wt% polystyrene was used to investigate its miscibility with poly(vinyl methyl ether) (PVME). The excimer-to-monomer emission intensity ratio I(M)/I(E) can be used as a sensitive probe to determine the miscibility level in SBS/PVME blends: I(M)/I(E) is a function of PVME concentration, and reaches a maximum when the blend contains 60% PVME. The cloud point curve determined by light scattering shows a pseudo upper critical solution temperature diagram, which can be attributed to the effect of PB segments in SBS. The thermally induced phase separation of SBS/PVME blends can be observed by measuring I(M)/I(E), and the phase dissolution process was followed by measuring I(M)/I(E) at different times.

Relevância:

100.00% 100.00%

Publicador:

Resumo:

The miscibility of poly(hydroxyether of bisphenol A) (phenoxy) with a series of poly(ethylene oxide-co-propylene oxide) (EPO) has been studied. It was found that the critical copolymer composition for achieving miscibility with phenoxy around 60-degrees-C is about 22 mol % ethylene oxide (EO). Some blends undergo phase separation at elevated temperatures, but there is no maximum in the miscibility window. The mean-field approach has been used to describe this homopolymer/copolymer system. From the miscibility maps and the melting-point depression of the crystallizable component in the blends, the binary interaction energy densities, B(ij), have been calculated for all three pairs. The miscibility of phenoxy with EPO is considered to be caused mainly by the intermolecular hydrogen-bonding interactions between the hydroxyl groups of phenoxy and the ether oxygens of the EO units in the copolymers, while the intramolecular repulsion between EO and propylene oxide units in the copolymers contributes relatively little to the miscibility.

Relevância:

100.00% 100.00%

Publicador:

Resumo:

Surface fluorination of poly (trimethylsilylpropyne) (PTMSP) membranes by CF4 plasma was studied. The surface fluorination of the membranes was carried out in an atmosphere of CF4 in a capacitively coupled discharge apparatus with external electrodes. Dramatic increase in selectivity (P(O2)/P(N2)) was observed. The effect of fluorination conditions such as duration of treatment and discharge power on the permeabilities of the membranes was studied. X-ray photoelectron spectrometric data of modified PTMSP membranes showed a drastic alternation in the surface layer. The P(O2) and P(O2)/P(N2) of the membranes were observed to be dependent on the F/C atomic ratio. At F/C > 1, the P(O2/P(N2) value of the membranes could be more than four.

Relevância:

100.00% 100.00%

Publicador:

Resumo:

We investigated the electron paramagnetic resonance (EPR) spectra of undoped, FeCl3- and iodine-doped poly(para-phenylene) (PPP) prepared by the method of Kovacic. EPR measurements are used to characterize electronic states relevant for carrier transport in doped PPP. We found a novel dependence of room temperature linewidth (DELTAH(pp)) and spin density (N(spin)) on the dopant concentrations for iodine-doped PPP, namely, DELTAH(pp) first decreased and increased, and then decreased and increased again with increasing iodine concentration in the iodine-doped PPP. The corresponding value of N(spin) first increased and decreased, and then increased and decreased again with increasing iodine concentration in PPP. However, the changes in DELTAH(pp) and N(spin) with FeCl3 concentration in FeCl3-doped PPP differ from those of iodine-doped PPP. We explain the different EPR properties in FeCl3-doped and iodine-doped PPP.

Relevância:

100.00% 100.00%

Publicador:

Resumo:

Dysprosium and ytterbium monophosphides have been prepared by the solid state reaction. The optical and electrical properties have been studied. Evidence that DyP and YbP are semiconductors has been obtained from the study of the absorption spectrum, the negative temperature coefficient of resistance and the rectifying effect. Their energy gaps are determined as 1.15 eV for DyP and 1.30 eV for YbP, electric conduction type is n-type, resistivities are about 10(-2) ohm cm and Hall mobility is 8.5-80 cm2/Vs. The p-n junction is formed on the LnP/Si.

Relevância:

100.00% 100.00%

Publicador:

Resumo:

The phase behaviours of poly(vinyl acetate) (PVAc) and poly(styrene-co-acrylonitrile)s (SAN) with poly(epichlorohydrin) (PECH) were examined using differential scanning calorimetry and an optical method using a hot plate. The PECH/PVAc blends showed LCST behaviour. The observed miscibility is thought to be a result of hydrogen-bonding interactions between the alpha-hydrogen atoms of PECH and the carbonyl groups of PVAc. Two SAN copolymers with an acrylonitrile (AN) content of 18 wt% (SAN18) and 25 wt% (SAN25), respectively, were also found to exhibit miscibility with PECH. No phase separation occurred by heating up to about 280-degrees-C, and the individual blend has a single, composition-dependent glass transition temperature. The formation of miscible PECH/SAN blends can be considered as a result of the intramolecular repulsion between styrene and AN units in SAN.

Relevância:

100.00% 100.00%

Publicador:

Resumo:

The catalytic performances of Mn-based catalysts have been investigated for the oxidative dehydrogenation of both ethane (ODE) and propane (ODP). The results show that a LiCl/MnOx/PC (Portland cement) catalyst has an excellent catalytic performance for oxidative dehydrogenation of both ethane and propane to ethylene and propylene, more than 60% alkanes conversion and more than 80% olefins selectivity could be achieved at 650 degrees C. In addition, the results indicate that Mn-based catalysts belong to p-type semiconductors, the electrical conductivity of which is the main factor in influencing the olefins selectivity. Lithium, chlorine and PC in the LiCl/MnOx/PC catalyst are all necessary components to keep the excellent catalytic performance at a low temperature.