188 resultados para Solid phase reaction


Relevância:

80.00% 80.00%

Publicador:

Resumo:

The heat capacities (C-p) of three types of gasohol (which consisted of 20 wt % ethanol and 80 wt % unleaded gasoline 93(#) (system S1), 30 wt % ethanol and 70 wt % unleaded gasoline 931 (system S2), 40 wt % ethanol and 60 wt % unleaded gasoline 930 (system S3), where "93(#)" denotes the octane number) were measured by adiabatic calorimetry in the temperature range of 80320 K. A glass transition was observed at 94.24, 95.15, and 95.44 K for system S1, S2, and S3, respectively. A solid-solid phase transition and solid-liquid phase transition were observed at 135.18 and 151.30 K for system S1, 131.82 and 152.10 K for system S2, and 121.29 and 155.09 K for S3, respectively. The polynomial equations for C, with respect to the thermodynamic temperature (T), and with respect to the content of ethanol (x), were established through the least-squares fitting. The thermodynamic functions and the excess thermodynamic functions of the three samples were derived using these thermodynamic relationships and equations.

Relevância:

80.00% 80.00%

Publicador:

Resumo:

8-hydroxy-2'-deoxyguanosine (8OHdG) has been widely used as a biomarker of oxidative DNA damage in both animal models and human studies. To evaluate the effect of cigarette smoking on oxidative stress, we studied the levels of urinary 8OHdG from smokers and non-smokers and investigated the association with cigarette smoking. The urinary 8OHdG concentrations were determinated by capillary electrophoresis with end-column amprometric detection (CE-AD) after a single-step solid phase extraction (SPE), and then quantitatively expressed as a function of creatinine excretion. To increase the concentration sensitivity, a dynamic pH junction was used and the focusing effect was obvious when using 30 mM phosphate (pH 6.50) as sample matrix. The limit of detection is 4.3 nM (signal-to-noise ratio S/N = 3). The relative standard deviation (R.S.D.) was 1.1% for peak current, and 2.3% for migration time. Based on the selected CE-AD method, it was found that the mean value of urinary 8OHdG levels in the smokers significantly higher than that in non-smokers (31.4 +/- 18.9 nM versus 14.4 +/- 7.6 nM, P = 0.0004; 23.5 +/- 21.3 mug g(-1) creatinine versus 12.6 +/- 13.2 mug g(-1) creatinine, P = 0.028). (C) 2004 Elsevier B.V. All rights reserved.

Relevância:

80.00% 80.00%

Publicador:

Resumo:

Increased oxidative stress induced by hyperglycemia may contribute to the pathogenesis of diabetic complications. Urinary 8-hydroxydeoxyguanosine (8-OHdG) has been reported to serve as a sensitive biomarker of oxidative DNA damage and also of oxidative stress. This article studied oxidative DNA damage in patients with diabetic nephropathy and in healthy control subjects by urinary 8-OHdG evaluations. Contents of 8-OHdG in urine were analyzed by capillary electrophoresis with end-column amperometric detection (CE-AD) after a single-step solid-phase extraction (SPE). Levels of urinary 8-OHdG in diabetic nephropathy patients with macroalbuminuria was significant higher than in control subjects (5.72 +/- 6.89 mumol/mol creatinine versus 2.33 +/- 2.83 mumol/mol creatinine, P = 0.018). A significant difference of 24 h urinary 8-OHdG excretions exists between the patients with macroalbuminuria and the patients with nonnoalbuminuria (19.2 +/- 16.8 mug/24 h versus 8.1 +/- 1.7 mug/24 h, P = 0.015). There was a positive correlation between urinary excretion of 8-OHdG and glycosylated hemoglobin (HbA(1)c) (r = 0.287, P = 0.022). A weak correlation exists between the levels of 8-OHdG and triglyceride (r = 0.230, P = 0.074). However, the urinary 8-OHdG contents are not correlated with blood pressure and total cholesterol. The increased excretion of urinary 8-OHdG is seen as indicating an increased systemic level of oxidative DNA damage in diabetic nephropathy patients. (C) 2004 Elsevier B.V. All rights reserved.

Relevância:

80.00% 80.00%

Publicador:

Resumo:

Melatonin is a highly conserved molecule that not only exists in animals, but also is present in bacteria, unicellular organisms and in plants. Since melatonin is an antioxidant, in plants melatonin was speculated to protect them from intrinsic and environmental oxidative stress. More importantly, melatonin in edible plants inevitably enters animals and human through feed and food. In this study, more than 100 Chinese medicinal herbs were analyzed using the methods of solid phase extraction and HPLC-FD on-line with MS to determine whether melatonin is present in these commonly used herbs. Melatonin was detected in majority of these plants. Sixty-four of them contain melatonin in excess of 10 ng per gram dry mass. Melatonin levels in several herbs are in excess of 1000 ng/g. It is well known that normal average physiological plasma levels of melatonin are only 10-60 pg/mL. These high level-melatonin containing plants are traditionally used to treat diseases which presumably involve free radical damage. The current study provides new information concerning one potentially effective constituent present in a large number of medicinal herbs. The results suggest that these herbs should be reevaluated in reference to their nutritional and medicinal value. (C) 2003 Elsevier Science Inc. All rights reserved.

Relevância:

80.00% 80.00%

Publicador:

Resumo:

Due to a low mineral content, the sapropelic sediments depositing in Mangrove Lake, Bermuda, provide an excellent opportunity to explore for possible additions of sulfur to organic matter during the early stages of diagenesis. We evaluated early diagenetic organic sulfur transformations by monitoring the concentrations and stable isotopic compositions of a number of inorganic and organic sulfur pools, thereby accounting for all of the sulfur in the sediments. We have identified and quantified the following sulfur pools: porewater sulfate, porewater sulfide, elemental sulfur, pyrite sulfur, hydrolyzable organic sulfur (HYOS), chromium-reducible organic sulfur (CROS), and nonchromium-reducible organic sulfur (Non-CROS). Of the organic sulfur pools, the Non-CROS pool is by far the largest, followed by CROS, and finally HYOS. By 60 cm depth these pools contribute, respectively, to 85, 7.9, and 3.6% of the total solid phase sulfur. The HYOS pool is probably of biological origin and shows no interaction with the sulfur compounds produced during diagenesis. By contrast, CROS is produced, most likely, from the diagenetic addition of polysulfides to functionalized lipids in the upper, H2S-poor, elemental sulfur-rich, region of the sediment. A portion of this sulfur pool is unstable and decomposes on contact with the H2S-rich porewaters. The portion of CROS that remains in the sulfidic waters appears to readily exchange sulfur isotopes with H2S. While some of the Non-CROS pool is of biological origin, some is also formed by the diagenetic addition of sulfur to organic compounds in the upper H2S-poor region of the sediment. By contrast with CROS, Non-CROS is not diagenetically active in the H2S-rich porewaters. Overall, somewhere between 27 and 53 % of the organic sulfur buried in Mangrove Lake sediments is of diagenetic origin, with the remaining organic sulfur derived from biosynthesis. We extrapolate our Mangrove Lake results and calculate that in typical coastal marine sediments between 11 and 29 μmol g−1 of organic sulfur will form during early diagenesis, of which 2–5 μmol g−1 will be chromium reducible.

Relevância:

80.00% 80.00%

Publicador:

Resumo:

(Y0.95Ln(0.01)Ce(0.04))(3)Al5O12 phosphors were synthesized by high-temperature solid state reaction under reducing atmosphere and the doping effects of lanthanide ions (Ln(3+)) on the luminescence properties of phosphors were studied. YAG: Ce, Ln spectra of excitation and emission show that the influence between Ce3+ and Ln(3+) can be divided into the following three types

Relevância:

80.00% 80.00%

Publicador:

Resumo:

Rectangular AgIn(WO4)(2) nanotubes with a diameter range of 80 to 120 nm and length up to 2 mu m have been synthesized by a hydrothermal method. These nanotubes exhibit interesting white light emissions when using 320 nm as the excitation wavelength. A photocatalytic reaction for water decomposition to evolve K, was performed under UV irradiation, and the rate of H, evolution is nearly seven times that of the sample prepared by a solid-state reaction, which shows much higher photocatalytic activities compared with their bulk counterparts.

Relevância:

80.00% 80.00%

Publicador:

Resumo:

Bulk and nano-materials Sr2CeO4 were prepared by solid-state reaction and sol-gel technique, respectively. Photoluminescence shows that luminescence has the characteristic of a ligand-to-metal charge transfer (CT) emission. Compared with bulk Sr2CeO4, the nano-material exhibits stronger emission intensity, longer decay time, and higher CT excitation energy. Three CT excitation peaks were observed in both bulk and nano samples.

Relevância:

80.00% 80.00%

Publicador:

Resumo:

Amphetamines including methamphetamine, 3,4-methylenedioxyamphetamine and 3,4-methylenedioxymethamphetamine were separated and detected by CE using simultaneous electrochemical (EC) and electrochemiluminescence (ECL) detection (CE-EC/ ECL). Factors that influenced the separation and detection performance, such as the detection potential, the pH value and concentration of the running buffer, the separation voltage and the pH of the detection buffer, were investigated.

Relevância:

80.00% 80.00%

Publicador:

Resumo:

A new approach for fast and sensitive electrochemiluminescence (ECL) detection of narcotic drugs on a microchip after separation by micellar electrokinetic chromatography (MEKC) is presented, taking the cocaine and its hydrolysate ecgonine as the test analytes. The mixture of hydrophilic BMIMBF4 ionic liquid (IL) and sodium dodecyl sulfate (SDS) was used directly as the buffer of MEKC with less noisy baselines, lower electrophoretic current and satisfactory separation performance.

Relevância:

80.00% 80.00%

Publicador:

Resumo:

LiCaBO3 was synthesized by high-temperature solid-state reaction. The influence of different rare earth dopants, i.e. Dy3+, Tb3+. TM3+ and Ce3+, on thermoluminescence (TL) of LiCaBO3 phosphor was discussed. We studied the TL properties and some dosimetric characteristics of Ce3+-activated LiCaBO3 phosphor in detail. The effect of the concentration of Ce3+ on TL was investigated, the result of which showed that the optimum Ce3+ concentration was 1 mol%. The TL kinetic parameters of LiCaBO3:0.01 Ce3+ were studied by computer glow curve deconvolution (CGCD) method.

Relevância:

80.00% 80.00%

Publicador:

Resumo:

Lanthanum magnesium hexaaluminate is a very important ceramic material for high temperature applications. In this paper lanthanum magnesium hexaaluminate has been synthesized directly by solid-state reaction. The forming mechanism was investigated by XRD. The SEM photographs show that the prepared powders are made of hexagonal plates. These powders can be well sintered at the high temperature (1600 degrees C) under the high pressure (4.5 GPa), and the relative density reaches 94.8%.

Relevância:

80.00% 80.00%

Publicador:

Resumo:

Lanthanum magnesium hexaalumminate (LMA) is an important candidate for thermal barrier coatings due to its thermal stability and low thermal conductivity. On the other hand, laser glazing method can potentially make thermal barrier coatings impermeable, resistant to corrosion on the surface and porous at bulk. LMA powder was synthesized at 1600 degrees C by solid-state reaction, pressed into tablet and laser glazed with a 5-kW continuous wave CO2 laser.

Relevância:

80.00% 80.00%

Publicador:

Resumo:

Polycrystalline powder sample of KSr4(BO3)(3) was synthesized by high-temperature solid-state reaction. The influence of different rare earth dopants, i.e. Tb3+, TM3+ and Ce3+, on thermoluminescence (TL) of KSr4(BO3)(3) Phosphor was discussed. The TL, photoluminescence (PL) and some dosimetric properties of Ce3+-activated KSr4(BO3)(3) phosphor were studied. The effect of the concentration of Ce3+ on TL intensity was investigated and the result showed that the optimum Ce3+ concentration was 0.2 mol%. The TL kinetic parameters of KSr4(BO3)(3):0.002 Ce3+ phosphor were calculated by computer glow curve deconvolution (CGCD) method. Characteristic emission peaking at about 407 and 383 nm due to the 4f(0)5d(1) -> F-2((5/2),(7/2)) transitions of Ce3+ ion were observed both in PL and three-dimensional (3D) TL spectra. The dose-response of KSr4(BO3)(3):0.002 Ce3+ to gamma-ray was linear in the range from 1 to 1000 mGy. In addition, the decay of the TL intensity of KSr4(BO3)(3):0.002 Ce3+ was also investigated.

Relevância:

80.00% 80.00%

Publicador:

Resumo:

The thermoluminescence (TL) properties of Ce3+ doped NaSr4(BO3)(3) phosphor under the beta-ray irradiation were reported. The polycrystalline sample was synthesized by high temperature solid-state reaction. The TL glow curve of NaSr4(BO3)(3):Ce3+ phosphor was composed of only one peak. TL kinetic parameters of NaSr4(BO3)(3):Ce3+ were deduced by the peak shape method, the activation energy (E) was 0.590 eV and the frequency factor was 1.008x10(6) s(-1). TL dose response was linear in the range of measurement. The 3-dimensional (3D) TL emission spectrum was also recorded, the emission spectrum consisted of two bands located at 441 and 479 nm respectively, corresponding to the characteristic 4f(0)5d(1)-> F-2((5/2,7/2)) transitions of the Ce3+ ion. The fading behavior of the NaSr4(BO3)(3):Ce3+ phosphor over a period of 15 d was also studied.