We prepare bismuth-doped borosilicate glasses and the luminescence properties in infrared wavelength region are investigated. Transmission spectrum, fluorescence spectrum and fluorescence decay curve are measured. The glasses exhibit a broad infrared luminescence peaking at 1340nm with the full width at half maximum of about 205nm, and lifetime of 273 mu s when excited by an 808-nm laser diode. The glasses are promising materials for broadband optical amplifiers and tunable lasers.

Relevância:

20.00% 20.00%

Publicador:

Resumo:

We report near infrared broadband emission of bismuth-doped barium-aluminum-borate glasses. The broadband emission covers 1.3 mum window in optical telecommunication systems. And it possesses wide full width at half maximum (FWHM) of similar to 200nm and long lifetime as long as 350 mus. The luminescent properties are quite sensitive to glass compositions and excitation wavelengths. Based on energy matching conditions, we suggest that the infrared emission may be ascribed to P-3(1) --> P-3(0) transition of Bi+. The broad infrared emission characteristics of this material indicate that it might be a promising candidate for broadband optical fiber amplifiers and tunable lasers. (C) 2005 Optical Society of America.

Relevância:

20.00% 20.00%

Publicador:

Resumo:

Writing computer-generated holograms has been achieved by using near infrared femtosecond laser selective ablation of metal film deposited on glass substrate. The diffraction features with data reconstruction of fabricated computer-generated holograms were evaluated. Both transmission and reflection holograms can be fabricated in a single process. The process required no mask, no pre- or post-treatment of the substrate. (C) 2005 Optical Society of America.

Relevância:

20.00% 20.00%

Publicador:

Resumo:

The broadband emission in the 1.2 similar to 1.6 mu m region from Li2O-Al2O3-ZnO-SiO2 ( LAZS) glass codoped with 0.01mol.% Cr2O3 and 1.0mol.% Bi2O3 when pumped by the 808nm laser at room temperature is not initiated from Cr4+ ions, but from bismuth, which is remarkably different from the results reported by Batchelor et al. The broad similar to 1300nm emission from Bi2O3-containing LAZS glasses possesses a FWHM ( Full Width at Half Maximum) more than 250nm and a fluorescent lifetime longer than 500 mu s when excited by the 808nm laser. These glasses might have the potential applications in the broadly tunable lasers and the broadband fiber amplifiers. (c) 2005 Optical Society of America.

Relevância:

20.00% 20.00%

Publicador:

Resumo:

Broadband infrared luminescence covering the optical telecommunication wavelength region of 0, E and S bands was observed in GeO2: Bi, M (M = Ga, B) glasses prepared by conventional melting-quenching technique. The luminescence with a maximum at around 1320 nm possesses a full width at half maximum larger than 300 nm and mean fluorescent lifetime longer than 500 mus when excited by an 808 nm-laser. These glasses may have potential applications in widely tunable laser and super-broadband optical amplifier for the optical communications. (C) 2005 Elsevier B.V. All rights reserved.

Relevância:

20.00% 20.00%

Publicador:

Resumo:

Blue frequency-upconversion fluorescence emission has been observed in Ce3+-doped Gd2SiO5 single crystals, pumped with 120-fs 800 nm IR laser pulses. The observed fluorescence emission peaks at about 440nm is due to 5d -> 4f transition of Ce3+ ions. The intensity dependence of the blue fluorescence emission on the IR excitation laser power obeys the cubic law, demonstrating three-photon absorption process. Analysis suggested that three-photon simultaneous absorption induced population inversion should be the predominant frequency upconversion mechanism. (c) 2006 Optical Society of America.

Relevância:

20.00% 20.00%

Publicador:

Resumo:

Broadband neat-infrared emission from transparent Ni2+-doped sodium aluminosilicate glass-cermaics is observed. The broad emission is centered at 1290 nm and covers the whole telecommunication wavelength region (1100-1700 nm) with full width at half maximum of about 340 nm. The observed infrared emission could be attributed to the T-3(2)(F) -> (3)A(2)(F) transition of octahedral Ni2+ ions that occupy high-field sites in nanocrystals. The product of the lifetime and the stimulated emission cross section is 2.15 x 10(-24) cm(2)s. It is suggested that Ni2+-doped sodium aluminosilicate glass ceramics have potential applications in tunable broadband light sources and broadband amplifiers.

Relevância:

20.00% 20.00%

Publicador:

Resumo:

Absorption spectrum from 400 to 2000 run and upconversion fluorescence spectra under 940 nm pumping of YAG single crystal codoped with 5 at.% Yb3+ and 4 at.% Tm3+ were studied at room temperature. The blue upconversion emission centered at 483 nm corresponds to the transition (1)G(4) -> H-3(6), the emission band around 646 nm corresponds to the transition (1)G(4) -> F-3(4) of Tm3+. Energy transfer from Yb3+ to Tm3+ is mainly nonradiative and the transfer efficiency was experimentally assessed. The line strengths, transition probabilities and radiative lifetimes of (1)G(4) level were calculated by using Judd-Ofelt theory. Gain coefficient calculated from spectra shows that the upconversion corresponding with transitions (1)G(4) -> H-3(6) in YAG doped with Yb3+ and Tm3+ is potentially useful for blue light Output. (c) 2006 Elsevier B.V. All rights reserved.