Resumo:
In conventional metals, there is plenty of space for dislocations-line defects whose motion results in permanent material deformation-to multiply, so that the metal strengths are controlled by dislocation interactions with grain boundaries(1,2) and other obstacles(3,4). For nano-structured materials, in contrast, dislocation multiplication is severely confined by the nanometre-scale geometries so that continued plasticity can be expected to be source-controlled. Nano-grained polycrystalline materials were found to be strong but brittle(5-9), because both nucleation and motion of dislocations are effectively suppressed by the nanoscale crystallites. Here we report a dislocation-nucleation-controlled mechanism in nano-twinned metals(10,11) in which there are plenty of dislocation nucleation sites but dislocation motion is not confined. We show that dislocation nucleation governs the strength of such materials, resulting in their softening below a critical twin thickness. Large-scale molecular dynamics simulations and a kinetic theory of dislocation nucleation in nano-twinned metals show that there exists a transition in deformation mechanism, occurring at a critical twin-boundary spacing for which strength is maximized. At this point, the classical Hall-Petch type of strengthening due to dislocation pile-up and cutting through twin planes switches to a dislocation-nucleation-controlled softening mechanism with twin-boundary migration resulting from nucleation and motion of partial dislocations parallel to the twin planes. Most previous studies(12,13) did not consider a sufficient range of twin thickness and therefore missed this strength-softening regime. The simulations indicate that the critical twin-boundary spacing for the onset of softening in nano-twinned copper and the maximum strength depend on the grain size: the smaller the grain size, the smaller the critical twin-boundary spacing, and the higher the maximum strength of the material.
Resumo:
Nano-fibrillar adhesives can adhere strongly to surfaces as a gecko does. The size of each fiber has significant effects on the adhesion enhancement, especially on rough surfaces. In the present study, we report the size effects on the normal and shear strength of adhesion for a single viscoelastic fiber. It is found that there exists a limited region of the critical sizes under which the interfacial normal or tangential tractions uniformly attain the theoretical adhesion strength. The region for a viscoelastic fiber under tension with similar material constants to a gecko's spatula is 135-255 nm and that under torque is 26.5-52 nm. This finding is significant for the development of artificial biomimetic attachment systems.
Resumo:
The catastrophic failure of heterogeneous brittle materials under impact loading is not fully understood. To describe the catastrophic failure behavior of heterogeneous brittle materials under impact loading, an elasto-statistical-brittle (ESB) model is proposed in this paper. The ESB model characterizes the disordered inhomogeneity of material at mesoscopic scale with the statistical description of the shear strength of mesoscopic units. If the applied shear stress reaches the strength, the mesoscopic unit fails, which causes degradation in the shear modulus of the material. With a simplified ESB model, the failure wave in brittle material under uni-axial compression is analyzed. It is shown that the failure wave is a wave of strain or particle velocity resulted from the catastrophic fracture in an elastically stressed brittle media when the impact velocity reaches a critical value. In addition, the failure wave causes an increase in the rear surface velocity, which agrees well with experimental observations. The critical condition to generate failure wave and the speed of failure wave are also obtained.
Resumo:
IEECAS SKLLQG
Resumo:
The emittance of an extracted ion beam can be estimated to first order by a series of three linear independent profile measurements. This estimation is restricted to the evaluation of an upper limit of the emittance value for a homogeneous, nonfilamented beam. The beam is assumed to be round, respectively elliptical, without any structure of the intensity distribution, no space charge has been assumed for the drifting beam, and the optics is assumed to be linear. Instead of using three different drift sections, a linear focusing element with three different focusing strengths can be used. Plotting the beam radius as function of focusing strength, three independent solutions can be used to calculate the Twiss parameters alpha, beta, and gamma and furthermore the emittance epsilon. Here we describe the measurements which have been performed with the SECRAL ion source at Institute of Modern Physics Lanzhou.
Resumo:
Acid strength distribution and the distribution of aromatics formed in the FCC gasoline conversion reaction on a ZSM-5 zeolite with different Na contents have been studied. With increasing Na content in the ZSM-5 zeolite, the acid sites determined by NH3-TPD technique, especially the strong acid sites, clearly decrease. When used as catalyst for the aromatization reaction, the transformation of olefins in the FCC gasoline into aromatics is governed directly by the strong acid sites on the ZSM-5 catalyst. Only under the conditions that a ZSM-5 catalyst possesses suitable strong acid sites is reaction temperature favorable for the aromatics formed.
Resumo:
A novel poly-l-arginine microcapsule was prepared due to its nutritional function and pharmacological efficacy. A high-voltage electrostatic droplet generator was used to make uniform microcapsules. The results show that the membrane strength and permeating property are both remarkably affected with the changes of sodium alginate concentration. With the sodium alginate concentration increasing, gel beads sizes increase from 233 mum to 350 mum, release ratio is also higher at the same time, but the membrane strength decreases.
Resumo:
It has been generally agreed that pyridine can be effectively mineralized in aerated TiO2 slurries using near-UV irradiation. The knowledge on the kinetics of the system possesses both practical and theoretical values. The present study, on the base of Langmuir-Hinshewood mechanism, illustrates a pseudo first-order kinetic model of the degradation with the limiting rate constant of 3.004 mg l(-1) min(-1) and equilibrium adsorption constant 2.763 x 10(-2) l mg(-1), respectively. The degradation efficiency in alkali is a little higher than that in acid with a minimum at about pH = 5, which is explained by the formation of acid-pyridine in acidic surrounding together with the amphoteric nature of the TiO2 surface. The promotion of H2O2 on the photo-degradation ties in its supplying proper amount of (OH)-O-. radicals for the inducement stage before surface redox reactions. (C) 2004 Elsevier B.V. All rights reserved.
Resumo:
The role of acid strength of zeolites in liquid-phase alkylation of benzene with ethylene was studied over beta, MCM-22, and USY zeolites by means of adsorbing NH3 at different temperatures. The strong acid sites are active centers, while the weak acid sites are inactive. The selectivity behavior of the strong acid sites varies with the relative acid strength as well as the types of the zeolites.
Resumo:
The lifetime behavior of a H-2/O-2 proton exchange membrane (PEM) fuel cell with polystyrene sulfonic acid (PSSA) membrane have been investigated in order to give an insight into the degradation mechanism of the PSSA membrane. The distribution of sulfur concentration in the cross section of the PSSA membrane was measured by energy dispersive analysis of X-ray, and the chemical composition of the PSSA membrane was characterized by infrared spectroscopy before and after the lifetime experiment. The degradation mechanism of the PSSA membrane is postulated as: the oxygen reduction at the cathode proceeds through some peroxide intermediates during the fuel cell operation, and these intermediates have strong oxidative ability and may chemically attack the tertiary hydrogen at the a carbon of the PSSA; the degradation of the PSSA membrane mainly takes place at the cathode side of the cell, and the loss of the aromatic rings and the SO3- groups simultaneously occurs from the PSSA membrane. A new kind of the PSSA-Nafion composite membrane, where the Nafion membrane is bonded with the PSSA membrane and located at the cathode of the cell, was designed to prevent oxidation degradation of the PSSA membrane in fuel cells. The performances of fuel cells with PSSA-Nafion101 and PSSA-recast Nafion composite membranes are demonstrated to be stable after 835 h and 240 h, respectively.