130 resultados para Thermal study
Resumo:
In this study, conventional TiO2 powder was heated in hydrogen (H-2) gas at a high temperature as pretreatment. The photoactivity of the treated TiO2 samples was evaluated in the photodegradation of sulfosalicylic acid (SSA) in aqueous suspension. The experimental results demonstrated that the photodegradation rates of SSA were significantly enhanced by using the H-2-treated TiO2 catalysts and an optimum temperature for the H-2 treatment was found to be of 500-600 degreesC. The in situ electron paramagnetic resonance (EPR) signal intensity of oxygen vacancies (OV) and trivalent titanium (Ti3+) associated with the photocatalytic activity was studied. The results proved the presence of OV and Ti3+ in the lattice of the H2-treated TiO2 and indicated that both were contributed to the enhancement of photocatalytic activity. Moreover, the experimental results presented that the EPR signal intensity of OV and Ti3+ in the H-2-treated TiO2 samples after 10 months storage was still significant higher than that in the untreated TiO2 catalyst. The experiment also demonstrated that the significant enhancement occurred in the photodegradation of phenol using the H-2-treated TiO2. (C) 2002 Elsevier Science Ltd. All rights reserved.
Resumo:
New types of templates and novel interactive mechanisms between template and framework are very important for creating porous materials. In this work, by using neutral dibutyl methylphosphonate as a template, an inorganic-organic hybrid mesoporous material, aluminum methylphosphonate, was prepared. The as-synthesized material was studied by P-31 magnetic angle spinning nuclear magnetic resonance (MAS NMR), Al-27 MAS NMR, C-13 CP/MAS, FT-IR spectroscopy, thermogravimetry (TG), differential thermal analysis (DTA), and transmission electron microscopy. After thermal treatment at 673 K and 10 mmHg for 2 h, hybrid mesoporous foam was obtained. The transformation process was investigated by FT-IR. TG-DTA results indicate that the methyl group bonded to the framework keeps intact up to 792 K under air and 823 K under nitrogen. The characterization results from nitrogen gas adsorption-desorption measurements show that the BET surface area and the Barrett-Joyner-Halenda desorption cumulative pore volume of the foam are 90 m(2) g(-1) and 0.32 cm(3) g(-1) respectively. (C) 2003 Elsevier Inc. All rights reserved.
Resumo:
In this study, melt blends of poly(butylene terephthalate) (PBT) with epoxy resin were characterized by dynamic mechanical analysis, differential scanning calorimetry, tensile testing, Fourier transform infrared spectroscopy, and wide-angle X-ray diffraction. The results indicate that the presence of epoxy resin influenced either the mechanical properties of the PBT/epoxy blends or the crystallization of PBT. The epoxy resin was completely miscible with the PBT matrix. This was beneficial to the improvement of the impact performance of the PBT/epoxy blends.
Resumo:
Polylactide (PLA) was melt blended with a biodegradable hyperbranched poly(ester amide) (HBP) to enhance its flexibility and toughness without sacrificing comprehensive performance. The advantage of using HBP was due to its unique spherical shape, low melt viscosity, and abundant functional end groups together with its easy access. Rheological measurement showed that blending PLA with as little as 2.5% HBP resulted in a 40% reduction of melt viscosity. The glass transition temperature (T-g) of PLA in the blends decreased slightly with the increase of HBP content, indicating partial miscibility which resulted from intermolecular interactions via H-bonding. The H-bonding involving CO of PLA with OH and NH of HBP was evidenced by FTIR analysis for the first time. The HBP component, as a heterogeneous nucleating agent, accelerated the crystallization rate of PLA. Remarkably, with the increase of HBP content, the elongation at break of PLA blends dramatically increased without severe loss in tensile strength, even the tensile strength increased within 10% content of HBP. The stress-strain curves and the SEM photos of impact-fractured surface showed the material changed from brittle to ductile failure with the addition of HBP. Reasonable interfacial adhesion via H-bonding and finely dispersed particulate structure of HBP in PLA were proposed to be responsible for the improved mechanical properties.
Resumo:
For the purpose of manufacturing cigarette filter tows and filter rods, the melt-spinning, adhesion and adsorption properties of poly(lactic acid) were studied. The rheological measurements were performed to examine the effects of various processing conditions on the melt flowability and spinnability, including those of residual moisture. The melt spinning and post-processings were followed by determining the molecular weight, thermal and mechanical properties of the fibers. The results obtained were useful to establishing the specification of the PLA resins for filter tows and filter rods manufacturing and to choosing proper melt-spinning and post-processing technologies.
Resumo:
A systematic investigation by FTIR spectroscopy was undertaken on blends of poly(propylene carbonate) (PPC) and bisphenol A (BPA). It provided direct evidence of the hydrogen bond (H-bond) between BPA O-H groups and PPC C=O groups. Using a curve-fitting method, qualitative as well as quantitative information concerning this H-bond interaction was obtained. The inter-H-bond in PPC/BPA blends was weaker than the self-H-bond in BPA. The absorptivities of the free and the H-bonded C=O groups were nearly equal. The fraction of H-bonded C=O in the blends increased with BPA content and leveled off at a value close to 40%. Finally, FTIR-temperature measurements of pure PPC and a representative blend were reported: by monitoring the peak areas of C=O absorptions, the dissociation of the inter-H-bonds and the thermal degradation of PPC were observed. It revealed that the presence of BPA clearly retarded the thermal degradation of PPC.
Resumo:
Notch Izod impact strength of poly(propylene) (PP)/glass bead blends was studied as a function of temperature. The results indicated that the toughness for various blends could undergo a brittle-ductile transition (BDT) with increasing temperature. The BDT temperature (T-BD) decreased with increasing glass bead content. Introducing the interparticle distance (ID) concept into the study, it was found that the critical interparticle distance (IDc) reduced with increasing test temperature correspondingly. The static tensile tests showed that the Young's modulus of the blends decreased slightly first and thereafter increased with increasing glass bead content. However, the yield stress decreased considerably with the increase in glass bead content. Dynamic mechanical analysis (DMA) measurements revealed that the heat-deflection temperature of the PP could be much improved by the incorporation of glass beads. Moreover, the glass transition temperature (T-g) increased obviously with increasing glass beads content. Differential scanning calorimetry (DSC) results implied that the addition of glass beads could change the crystallinity as well as the melting temperature of the PP slightly.
Resumo:
Ni0.65Zn0.35Cu0.1Fe1.9O4/SiO2 nanocomposites with different weight percentages of NiZnCu-ferrite dispersed in silica matrix were successfully fabricated by the sol-gel method using tetraethylorthosilicate (TEOS) as a precursor of silica, and metal nitrates as precursors of NiZnCu ferrite. The thermal decomposition process of the dried gel was studied by thermogravimetric analysis (TGA) and differential thermal analysis (DTA). The obtained Ni0.65Zn0.35Cu0.1Fe1.9O4/SiO2 nanocomposites were characterized by X-ray diffraction (XRD), transmission electron microscope (TEM), scanning electron microscope (SEM), Mossbauer spectroscopy and vibrating sample magnetometry (VSM). The formation of stoichiometric NiZnCu-ferrite dispersed in silica matrix is confirmed when the weight percentage of ferrite is not more than 30%. Samples with higher ferrite content have small amount of alpha-Fe2O3. The transition from the paramagnetic to the ferromagnetic state is observed as the ferrite content increases from 20 to 90wt%.
Resumo:
High-performance polyimide fibers possess man), excellent properties, e.g., outstanding thermal stability and mechanical properties and excellent radiation resistant and electrical properties. However, the preparation of fibers with good mechanical properties is very difficult. In this report, a biphenvl polyimide from 3,3',4,4'-biphenyltetracarboxylic dianhydride and 4,4'-oxydianiline is synthesized in p-chlorophenol by one-step polymerization. The solution is spun into a coagulation bath of water and alcohol via dry-jet wet-spinning technology. Then, the fibers are drawn in two heating tubes. Thermal gravimetric analysis, thermal mechanical analysis, and dynamic mechanical analysis (DMA) are performed to study the properties of the fibers. The results show that the fibers have a good thermal stability at a temperature of more than 400degreesC. The linear coefficient of thermal expansion is negative in the solid state and the glass transition temperature is about 265degreesC. DMA spectra indicate that the tandelta of the fibers has three transition peaks, namely, alpha, beta, and gamma transition. The alpha and gamma transition temperature, corresponding to the end-group motion and glass transition, respectively, extensively depends on the applied frequency, while the beta transition does not.
Resumo:
By using the study of the lattice energy and the structural parameters of binary inorganic crystals, a new parameter reflecting the thermal expansion property has been found, the relation between the linear expansion coefficient and new parameter has been established. A semiempirical method for evaluation of linear expansion coefficient from the lattice energy is presented, and developed to the complex crystals. The estimated values of the linear expansion coefficients of both simple and complex crystals are in good agreement with the experimental values.
Resumo:
The blends of low molecular weight triacetin (TAC) and oligomeric poly(1,3-butylene glycol adipate) (PBGA) were used as multiple plasticizers to lubricate poly(lactic acid) (PLA) in this study. The thermal and mechanical properties of plasticized polymers were investigated by means of dynamic mechanical analysis and differential scanning calorimetry. Atomic force microscopy (AFM) was used to analyze the morphologies of the blends. Multiple plasticizers were effective in lowering the glass transition temperature (T-g) and the melting temperature (T-m) of PLA. Moreover, crystallinity of PLA increased with increasing the con-tent of multiple plasticizers. Tensile strength of the blends decreased following the increasing of the plasticizers, but increased in elongation at break. AFM topographic images showed that the multiple plasticizers dispersed between interfibrillar regions. Moreover, the fibrillar crystallite formed the quasicrosslinkings, which is another cause for the increase in elongation at break.
Resumo:
The PVT data of five kinds of biaxially oriented polypropylene (BOPP) Resins was measured by the PVT-100 apparatus. Thermal expansion coefficients (alpha) and isothermal compressibility (beta) were evaluated from Tait equation in the melting state and then compared with those fitted with the value of experiment. The results showed that it was reasonable to calculate alpha and beta with Tait equation in the melting state. At the same time, it was found that thermal expansion coefficients, isothermal compressibility and the melting temperature (T-m) of one of BOPP melts (S28C) were lower than those of the others in the same test conditions, indicating that the volume deformation of S28C resin is' less so that it could be realized to avoid arising surface defects of the film (biaxially oriented polypropylene film) due to. contracting, thereby decrease damage to the film in the subsequence process. Accordingly superior processing properties of S28C resin are confirmed from PVT. speciality.
Resumo:
The transesterification of poly(beta-hydroxybutyrate) (PHB) and poly(epsilon-caprolactone) (PCL) was carried out by using stannous octoate as catalyzer in liquid phase. The effects of reaction conditions on the transesterification, including reaction temperature, reaction time and catalyzer content, were investigated. The sequence distribution, crystallization behavior and thermal stability of PHB-co-PCL copolyesters were studied by C-13-NMR, FTIR, DSC, WAXD and TGA. The results showed that the transesterification of PHB with PCL was confirmed to produce a block copolymer, and enhancing reaction temperature and increasing reaction time were advantageous to the transesterification. With the increase in PCL content in the block copolymer, the crystallization behavior of PHB-co-PCL copolyesters changed evidently. On the other hand, the introduction of PCL segment into PHB chains did not change its crystalline structure; moreover, thermal stability of PHB-co-PCL copolyesters was a little improved in air, comparing with that of pure PHB.
Resumo:
Using the Bridgeman-Stockbarger method, the KMgF3:EU2+ single crystal was grown. The color centers in unirradiated KMgF3:Eu crystal were studied. By thermal annealing, we confirmed the 422-nm emission resulted from color centers and oxygen centers, and we proved the energy transfer from EU2+ to color centers. From spectra, the relative oxygen content in crystal was calculated, and the relationships of oxygen displacing fluorine were studied.