159 resultados para POLYETHYLENE FRACTIONS
Resumo:
Three triblock copolymers of poly[styrene-b-(ethylene-co-butylene)-b-styrene] (SEBS) of different molecular weights and one diblock copolymer of poly[styrene-b-(ethylene-co-butylene)] (SEB) were used to compatibilize high density polyethylene/syndiotactic polystyrene (HDPE/sPS, 80/20) blend. Morphology observation showed that phase size of the dispersed sPS particles was significantly reduced on addition of all the four copolymers and the interfacial adhesion between the two phases was dramatically enhanced. Tensile strength of the blends increased at lower copolymer content but decreased with increasing copolymer content. The elongation at break of the blends improved and sharply increased with increments of the copolymers. Drop in modulus of the blend was observed on addition of the rubbery copolymers. The mechanical performance of the modified blends is strikingly dependent not only on the interfacial activity of the copolymers but also on the mechanical properties of the copolymers, particularly at the high copolymer concentration. Addition of compatibilizers to HDPE/sPS blend resulted in a significant reduction in crystallinity of both HDPE and sPS. Measurements of Vicat softening temperature of the HDPE/sPS blends show that heat resistance of HDPE is greatly improved upon incorporation of 20 wt% sPS.
Resumo:
Metallocene, a newer generation of commercial polymerization catalysts for polyolefins, is best known for its "single sitednss", and the intermolecular structural homogeneity of metallocene polyethylene copolymer is a very interesting research issue. The molecular segregation effects on the crystallization, melting and crystal morphologies of metallocene SCBPE have been investigated with DSC and TEM. The multiple endothermic peaks were observed in the DSC thermograms during heating experiments. The heterogeneity increases as branching content increases, the lamellae becomes thinner, and lamellae distribution becomes broader. Both macroscopic segregation (between two crystal aggregates) and microscopic segreation (between two lamellae) have been observed when SCBPE crystallized from phase separated melt.
Resumo:
The twisting growth of a branched polyethylene single crystal formed from the melt was observed directly by means of transmission electron and atomic force miscroscopy. The surface stress asymmetry arising from the asymmetry of the surface-fold structure and, chain tilting resulted in the twisting growth of the single crystals. The handedness of the twisting lamellae was consistent With the chain-tilting direction. When multilayer lamellae piled up in a thicker film, the lamellar twist would be inevitably causing screw dislocations.
Resumo:
Transition of crystalline structure and morphology of metallocene-catalyzed butyl branched polyethylene with branch content has been studied. It was found that the long periods of the branched polyethylene were controlled by crystallization conditions for the lower branch content samples and by branch contents for the higher branch content samples. When the branch content increased to a critical value the branched polyethylene had no long period because the crystalline morphology was changed from folded chain crystal to a bundled crystal. The TEM observations supported the results. The transition of the crystalline morphology resulted from the reduction of lamellar thickness with increasing of branch content since the branches were rejected from the lattice. The reduction of lamellar thickness with increasing of branch content also resulted in lattice expansion and decrease of melt temperature of the branched polyethylene. (C) 2001 Kluwer Academic Publishers.
Resumo:
Crystallization behavior and spherulitic structure of linear high-density polyethylene (HDPE), after being irradiated in its molten state by gamma -rays, was investigated by small-angle laser scattering (SALS) and differential scanning calorimetry (DSC). Significant changes in the crystallization of HDPE during cooling in air before and after being irradiated in the melt were observed. A critical minimum average molar mass between cross-links (200 carbon-carbon bonds) for spherulite formation in such an irradiated HDPE network was obtained.
Resumo:
The toughness of high-density polyethylene (HDPE)/glass-bead blends containing various glass-bead contents as a function of temperature was studied. The toughness of the blends was determined from the notch Izod impact test. A sharp brittle-ductile transition was observed in impact strength-interparticle distance (ID) curves at various temperatures. The brittle-ductile transition of HDPE/glass-bead blends occurred either with reduced ID or with increased temperature. The results indicated that the brittle-ductile-transition temperature dropped markedly with increasing glass-bead content. Moreover, the correlation between the critical interparticle distance (ID.) and temperature was obtained. Similar to the ID, of polymer blends with elastomers, the ID, nonlinearly increased with increasing temperature. However, this was the first observation of the variation of the ID, with temperature for polymer blends with rigid particles. (C) 2001 John Wiley & Sons, Inc. J Polym. Sci Part B: Polym. Phys 39: 1855-1859, 2001.
Resumo:
The chain structure, spherulite morphology, and theological property of LL-DPE-g-AA were studied by using electronspray mass spectroscopy, C-13-NMR, and rheometer. Experimental evidence proved that AA monomers grafted onto the LLDPE backbone formed multiunit AA branch chains. It was found that AA branch chains could hinder movement of the LLDPE main chain during crystallization. Spherulites of LLDPE became more anomalous because of the presence of AA branch chains. Rheological behavior showed that AA branch chains could act as an inner plasticizer at the temperature range of 170-200 degreesC, which made LLDPE-g-AA easy to further process. (C) 2001 John Wiley & Sons, Inc.
Resumo:
Nanoindentation technique and scanning force microscopy have been used to measure directly the polyethylene modulus along the chain axis. Single crystals of polyethylene were employed in order to obtain well-aligned chain segments. To minimize effects of scanner creep, a Z scan rate of 3 Hz was employed. The "X Rotate" value of 25 degrees was selected to eliminate effects of lateral tip motion. The results were analyzed by the Oliver -Pharr method for which direct observation and measurement of the contact area are not required. Considering the influence of tip roundness on the projected contact area, the nanoindentation results were analyzed by the Sawa method. The chain modulus obtained from the thinner polyethylene single crystal sample was 204 +/- 21 GPa by the Oliver-Pharr method and 168 +/- 17 GPa by the Sawa method. The lower values than expected were due to substrate effects and anisotropy of chain deformation during nanoindentation. An extrapolation of the chain modulus obtained by various strains to zero nanoindentation eliminated the effect of substrate and anisotropy of chain deformation. The corresponding chain modulus obtained from the thicker sample was 278 GPa by the Oliver-Pharr method and 267 GPa by the Sawa method, respectively, in better agreement with the value of 340 Cpa determined theoretically. (C) 2001 Elsevier Science Ltd. All rights reserved.
Resumo:
Metallocene-catalyzed short chain branched polyethylene single crystals, formed from the melt at a higher crystallization temperature of 114 degreesC, were obtained. Highly elongated lamellae were formed, which are different from truncated lozenge or lenticular shaped single crystals formed at a lower crystallization temperature. It was found that there existed a definite line in the lamellae along the longitudinal growth direction and two regions were separated by the definite line. The lateral habits of both the regions were asymmetrical about the b-axis due to the chain tilting, which was the same as that at a lower crystallization temperature. Generally, the highly elongated lamellae were not straight, but curved towards the opposite direction with chain tilting direction due to a series of edge dislocation within a lamella. The inner side of a lamella was serrated and the outer side was smooth due to the lamellar curvature. The thickness of both regions of a lamella was different, the broader region was thicker than the narrower region, which was different from the uniform thickness of the lamellae formed at a lower crystallization temperature. The different thicknesses within a lamella were considered as the result of the initial thickness difference and the impact of isothermal thickening. (C) 2001 Elsevier Science Ltd. All rights reserved.
Resumo:
Ultra high molar mass polyethylene (UHPE) powder as polymerized in a slurry process has been studied, in its nascent state, after recrystallization on rapid cooling from the melt and after hot compression molding to a film, by DSC, effect of annealing the recrystallized specimen at 120 similar to 130 degreesC, morphology by polarizing optical microscopy and small angle X-ray scattering. Based on the experimental results obtained the macromolecular condensed state of the nascent UHPE powder is a rare case of a multi-chain condensed state of non-interpenetrating chains, involving interlaced extended chain crystalline layers and relaxed parallel chain amorphous layers. On melting, a nematic rubbery state of nanometer size domain resulted. The nematic-isotropic transition temperature was judged from literature data to be at least 220 degreesC, possibly higher than 300 degreesC, the exact temperature is however not sue because of chain degradation at such high temperatures. The recrystallization process from the melt is a crystallization from a nematic rubbery state. The drop of remelting peak temperature by 10 K of the specimen recrystallized from its melt as compared to the nascent state has its origin in the decrease both of the crystalline chain stem length and of the degree of crystallinity. The remelting peak temperature could be returned close to that of the nascent state by annealing at 120 similar to 130 degreesC.
Resumo:
Grafting of acrylic acid and glycidyl methacrylate onto low density polyethylene (LDPE) was performed by using a corotating twin-screw extruder. The effects of residence time and concentration of initiator and monomers on degree of grafting and gel content of grafting LDPE were studied systematically. Paraffin, styrene, p-benzoquinone, triphenyl phosphite, tetrachloromethane, and oleic acid were added to try to decrease the extent of crosslinking of LDPE. 4-hydroxyl-2,2,6,6-tetramethyl-1-piperidinyloxy (4-hydroxyl-TEMPO) and dipentamethylenethiuram tetrasulfide were also tried to inhibit crosslinking reaction of LDPE during its extruding grafting process. It was found that p-benzoquinone, triphenyl phosphite and tetrachloromethane were good inhibitors for crosslinking of LDPE. (C) 2000 John Wiley & Sons, Inc.
Resumo:
The effect of potassium thiocyanate on the partitioning of lysozyme and BSA in polyethylene glycol 2000/ammonium sulfate aqueous two-phase system has been investigated. As a result of the addition of potassium thiocyanate to the PEG/ammonium sulfate system, the PEG/mixed salts aqueous two-phase system was formed. It was found that the potassium thiocyanate could alter the pH difference between the two phases, and, thus, influence the partition coefficients of the differently charged proteins. The relationship between partition coefficient of the proteins and pH difference between two phases has been discussed. It was proposed that the pH difference between two phases could be employed as the measurement of electrostatic driving force for the partitioning of charged proteins in polyethylene glycol 2000/ammonium sulfate aqueous two-phase system.
Resumo:
Monte Carlo simulations were used to model A/B/A-B ternary mixtures with different AB diblock copolymer volume fractions for which both the dispersed and continuous phase volume fractions were kept constant. For concentrations of the diblock copolymer below a critical value, the domain size increment of the dispersed phase decreases linearly with the copolymer concentration. This is in agreement with the predictions of Noolandi and Hong. The dependence of the domain size as a function of the copolymer volume fraction can also be fitted by the equation of Tang and Huang. Our simulations indicate, for the first time, that the micelles form before saturation of the interface occurs. This means that the formation of the micelles is not a result of the saturation of the interface.
Resumo:
Blends of polypropylene (PP) and low density polyethylene (LDPE) have been examined for a series of compositions using differential scanning calorimetry and permanganic etching followed by transmission electron microscopy. Thermal analysis of their melting and recrystallization behaviour suggests two possibilities, either that below 15 wt % PP the blends are fully miscible and that PP only crystallizes after LDPE because of compositional changes in the remaining melt, or else that the PP is separated, but in the form of droplets too small to crystallize at normal temperatures. Microscopic examination of the morphology shows that the latter is the case, but that a fraction of the PP is nevertheless dissolved in the LDPE. (C) 1998 Kluwer Academic Publishers.
Resumo:
The compatibilizing effect and mechanism of compatibilization of the diblock copolymer polystyrene-block-poly(4-vinylpyridine) P(S-b-4VPy) on immiscible blends of poly(2,6-dimethyl-1,4-phenylene oxide) (PPO)/chlorinated polyethylene (CPE) were studied by means of scanning electron microscopy (SEM), differential scanning calorimetry (DSC), mechanical properties and FTIR measurements. The block copolymer was synthesized by sequential anionic polymerization and melt-blended with PPO and CPE. The results show that the P(S-b-4VPy) added acts as an effective compatibilizer, located at the interface between the PPO and the CPE phase, reducing the interfacial tension, and improving the interfacial adhesion. The tensile strength and modulus of all blends increase with P(S-b-4VPy) content, whereas the elongation at break increases for PPO-rich blends, but decreases for CPE-rich blends. The polystyrene block of the diblock copolymer is compatible with PPO, and the poly(4-vinylpyridine) block and CPE are partially miscible.