231 resultados para ionic alloys
Resumo:
This paper describes a new strategy to make a full solid-state, flexible, dye-sensitized solar cell (DSSC) based on novel ionic liquid gel, organic dye, ZnO nanoparticles and carbon nanotube (CNT) thin film stamped onto a polyethylene terephthalate (PET) substrate. The CNTs serve both as the charge collector and as scaffolds for the growth of ZnO nanoparticles, where the black dye molecules are anchored.
Resumo:
Binary melts of S-ethyltetrahydrothiophenium iodide and dicyanoamide (or tricyanomethide) have been employed for dye-sensitized solar cells with high power conversion efficiencies up to 6.9% under the illumination of AM 1.5G full sunlight. We have further shown that the transport of triiodide in ionic liquids with high iodide concentration is viscosity-dependent in terms of a physical diffusion coupled bond exchange mechanism apart from the simple physical diffusion.
Resumo:
We report a high molar extinction coefficient heteroleptic polypyridyl ruthenium sensitizer, featuring an electron-rich 3,4-ethylenedioxythiophene unit in its ancillary ligand. A nanocrystalline titania film stained with this sensitizer shows an improved optical absorption, which is highly desirable for practical dye-sensitized solar cells with a thin photoactive layer, facilitating the efficient charge collection.
Resumo:
We report a high molar extinction coefficient metal-free sensitizer composed of a triarylamine donor in combination with the 2-(2,2'-bithiophen-5-yl)acrylonitrile conjugation unit and cyanoacrylic acid as an acceptor. In conjugation with a volatile acetonitrile-based electrolyte or a solvent-free ionic liquid electrolyte, we have fabricated efficient dye-sensitized solar cells showing a corresponding 7.5% or 6.1% efficiency measured under the air mass 1.5 global sunlight. The ionic liquid cell exhibits excellent stability during a 1000 h accelerated test under the light-soaking and thermal dual stress. Intensity-modulated photocurrent and photovolatge spectroscopies were employed along with the transient photoelectrical decay measurements to detail the electron transport in the mesoporous titania films filled with these two electrolytes.
Resumo:
We systematically studied the temperature-dependent physicochemical properties, such as density, conductivity, and fluidity, of 1,3-dialkylimidazolium iodides. In combination with the amphiphilic Z907Na sensitizer, we have found that it is important to use low-viscosity iodide melts with small cations to achieve high-efficiency dye-sensitized solar cells. By employing high-fluidity eutectic-based melts the device efficiencies considerably increased compared to those for cells with the corresponding state of the art ionic liquid electrolytes.
Resumo:
A new kind of bismuth film modified electrode to sensitively detect trace metal ions based on incorporating highly conductive ionic liquids 1-butyl-3-methyl-imidazolium hexafluorophosphate (BMIMPF6) in solid matrices at glassy carbon (GC) was investigated. Poly(sodium 4-styrenesulfonate) (PSS), silica, and Nafion were selected as the solid matrices. The electrochemical properties of the mixed films modified GC were evaluated. The electron transfer rate of Fe(CN)(6)(4-)/Fe(CN)(6)(3-) can be effectively improved at the PSS-BMIMPF6 modified GC.
Resumo:
The copolymer of acrylonitrile (AN), methyl methacrylate (MMA) and poly(ethylene glycol) methyl ether methacrylate (PEGMEMA) is synthesized in 1-butyl-3-methylimidazolium tetrafluoroborate (BMImBF(4)). The dynamic mechanical properties of the resulting gel polymer electrolytes containing ionic liquid are measured.
Resumo:
The Mg-8Gd-0.6Zr-xHo (x = 1, 3 and 5, mass%) alloys were prepared by casting technology, and structures, aging strengthening mechanism and mechanical properties of the alloys were investigated. The age behaviors and the mechanical properties are improved by adding Ho addition. The structures of the alloys are characterized by the present of rosette-shaped equiaxed grains. The peak hardness value of the Mg-8Gd-0.6Zr-3Ho alloy is 100 Hv, which is about 30% higher than that of Mg-8Gd-0.6Zr alloy.
Resumo:
The influence of the addition of mischmetal (MM) and tin (Sn) (total content of mischmetal and tin = 4 wt.%) on the microstructure, aging behavior and mechanical properties of Mg-6Zn-5Al-based alloys has been investigated. The microstructure of the as-cast alloys consists of alpha-Mg. Mg-32(Al,Zn)(49), Al2Mg5Zn2, Mg2Sn and Al2MMZn2 phases, and the morphology of these intermetallic phases varies with different MM and Sri additions.
Resumo:
Mg-8Gd-2Y-Nd-0.3Zn (wt%) alloy was prepared by the high pressure die-cast technique. The microstructure, mechanical properties in the temperature range from room temperature to 573 K, and strengthening mechanism were investigated. It was confirmed that the Mg-Gd-based alloy with high Gd content exhibited outstanding die-cast character. The die-cast alloy was mainly composed of small cellular equiaxed dendrites and the matrix. The long lamellar-shaped stacking compound of Mg3X (X: Gd, Y, Nd, and Zn) and polygon-shaped.
Resumo:
Mg-5Al-0.4Mn-xNd (x=0, 1, 2 and 4wt.%) alloys were prepared by metal mould casting method. The microstructures and mechanical properties were investigated. The results demonstrated that Al11Nd3 phase was formed and mainly aggregated along the grain boundaries with the addition of Nd. Meanwhile, the grain sizes were greatly reduced with the increasing Nd content.
Resumo:
The electrochemical corrosion behavior of Mg-6Al-0.4Mn and Mg-6Al-4RE-0.4Mn (RE = Mischmetal) alloys is investigated in 3.5% NaCl solution. The results of corrosion process, polarization behavior, and electrochemical impedance spectroscopy of the alloys reveal that Mg-6Al-4RE-0.4Mn exhibits enhanced corrosion resistance. The addition of RE stabilizes the solid solution and modifies the passive film through a finer microstructure.
Resumo:
Mg-8Gd-0.6Zr-1RE (RE = La or Ce, wt.%) alloys were prepared by casting. The microstructures, age hardening behavior and mechanical properties were investigated. The results show that the addition of 1 wt.% La or Ce to a Mg-8Gd-0.6Zr alloy reduces the dendrite arm spacing and slightly improves the mechanical properties and age hardening response.
Resumo:
Microstructure and mechanical properties of Mg-4.5Zn-xNd (x = 0, 1 and 2, wt%) alloys heat-treated at 603 K for 2 It have been investigated. T-phase (an Mg-Zn-Nd ternary phase) was observed in the Nd containing alloys. The optimal mechanical properties were obtained in the Mg-4.5Zn-1Nd alloy, and the ultimate tensile strength and yield strength were 228 and 79 MPa, respectively. Through comparing with the Mg-4.5Zn alloy, the increments of ultimate tensile strength and yield strength were 51 and 17 MPa.
Resumo:
Microstructures and mechanical properties of the peak-aged Mg-4.5Zn-xGd (x = 0, 2, 3 and 5 wt.%) alloys have been investigated. The results showed that grain size increased with increasing Gd. Phase analysis showed that MgZn2 phase was observed in the Mg-4.5Zn alloy. While with Gd additions, Mg3Gd and Mg3Gd2Zn3 phases formed, and the volume fraction of the Mg3Gd2Zn3 phase increased with increasing Gd. Tensile test results indicated that the optimal mechanical properties were obtained in the Mg-4.5Zn-2Gd alloy, and the ultimate tensile strength and yield strength were 215 MPa and 121 MPa, respectively.