159 resultados para ZnO:Al
Resumo:
A uniform submicron periodic square structure was fabricated on the surface of ZnO by a technique of two linearly polarized femtosecond laser beams with orthogonal polarizations ablating material alternately. The formed two-dimensional ordering submicron structure consists of close-packed submicron squares with a spacial periodicity of 290 nm, which arises from the intercrossing of two orthogonal submicron ripple structures induced by the two beams respectively. The result demonstrates a noninterference effect of two-beam ablation based on the alternate technique, which should come from the polarization-dependent enhancement of the subwavelength ripple structure and the large interval of two alternate pulses. This two-beam alternate ablation technique is expected to open up prospects for the submicron fabrication of wide-bandgap materials.
Resumo:
Near-infrared to UV and visible upconversion luminescence was observed in single-crystalline ZnO under an 800 nm infrared femtosecond laser irradiation. The optical properties of the crystal reveal that the UV and VIS emission band are due to the exciton transition (D0X) bound to neutral donors and the deep luminescent centers in ZnO, respectively. The relationship between the upconversion luminescence intensity and the pump power of the femtosecond laser reveals that the UV emission belongs to three-photon sequential band-to-band excitation and the VIS emission belongs to two-photon simultaneous defect-absorption induced luminescence. A saturation phenomenon and polarization-dependent effect are also observed in the upconversion process of ZnO. A very good optical power limiting performance at 800 nm has been demonstrated. The two- and three-photon absorption coefficients of ZnO crystal were measured to be 0.2018 cm GW(-1) and 7.102 x 10(-3) cm(3) GW(-2), respectively. The two- and three-photon cross sections were calculated to be 1.189 x 10(-51) cm(4) s and 1.040 x 10(-80) cm(6) s(2), respectively. (c) 2007 Elsevier B.V. All rights reserved.
Resumo:
采用传统熔融冷却的方法制备了透明Ni^2+掺杂ZnO-Al2O3-SiO2系玻璃,结合X-射线、吸收和荧光等测试手段,研究了不同热处理温度对Ni^2+掺杂透明ZnO-Al2O3-SiO2系微晶玻璃光学性质的影响。由X-射线衍射谱鉴定出微晶玻璃中析出的晶相为ZnAl2O4微晶,其尺寸在13nm以下。玻璃中没有发现近红外发光,而在微晶玻璃中存在宽带近红外发光,其可归属为八面体六配位Ni^2+离子的^3T2g(^3F)激发态向^3A2g(^3F)基态的跃迁。随热处理温度升高发光强度增强,而发射峰位则发生蓝移;荧
Resumo:
烧蚀条件对飞秒激光脉冲诱导氧化锌纳米结构有重要影响。研究了800nm,150fs,250kHz的飞秒激光脉冲分别在空气中,去离子水中以及无水乙醇中垂直聚焦于氧化锌晶体表面,诱导形成不同形态的纳米结构。实验结果表明,在空气中利用飞秒激光脉冲辐照样品表面,形成了周期为180nm的纳米线;在去离子水中辐照诱导形成了由氧化锌纳米线聚集而成的"纳米球";在无水乙醇中形成出现分叉结构的纳米线。拉曼光谱分析辐照前后晶体晶相结果表明,形成的纳米结构相对于辐照前特征峰437cm-1强度有所下降,在570cm-1处的峰值则显著增强。分析了在各种烧蚀条件下诱导形成纳米结构的演化过程以及物理机理。
Resumo:
采用20μm的狭缝配平面晶体谱仪构成空间分辨光谱测量系统,对Al激光等离子体的K壳层发射谱进行测量。利用Al的Ly-α线谱的翼部Stark展宽效应推得电子密度空间分布轮廓.建立了翼部Stark展宽法测量高密度等离子体电子密度的诊断技术。
Resumo:
报道了在20 TW皮秒激光器上完成的p偏振激光与等离子体相互作用过程中产生的快电子的角分布和能谱测量结果.实验得到:当激光功率密度小于1017 W/cm^2时,电子发射没有明显定向性,在激光入射面内多峰发射;当激光功率密度大于1017 W/cm^2,小于1018 W/cm^2时,电子主要沿靶面法线方向发射;当激光功率密度达到相对论强度时,电子主要沿激光传播方向发射;激光功率密度未达到相对论强度时,靶后表面法线方向快电子能谱拟合平均温度符合共振吸收温度定标率;激光功率密度达相对论强度以上时,靶后表面法线方向
Resumo:
The Er3+-Yb3+ codoped Al2O3 has been prepared by the sol-gel method using the aluminium isopropoxide [Al(OC3H7)(3)]-derived Al2O3 sols with addition of the erbium nitrate [Er(NO3)(3) center dot 5H(2)O] and ytterbium nitrate [Yb(NO3)(3) center dot 5H(2)O]. The phase structure, including only two crystalline types of doped Al2O3 phases, theta and gamma, was obtained for the 1 mol% Er3+ and 5 mol% Yb3+ codoped Al2O3 at the sintering temperature of 1,273 K. By a 978 nm semiconductor laser diodes excitation, the visible up-conversion emissions centered at about 523, 545, and 660 nm were obtained. The temperature dependence of the green up-conversion emissions was studied over a wide temperature range of 300-825 K, and the reasonable agreement between the calculated temperature by the fluorescence intensity ratio (FIR) theory and the measured temperature proved that Er3+-Yb3+ codoped Al2O3 plays an important role in the application of high temperature sensor.
Resumo:
采用燃烧法制备了Nd:YSAG粉体,经过成型、素烧,最终在氢气气氛中烧结制备了Nd:YSAG透明陶瓷.测试结果表明,Nd:YSAG透明陶瓷具有荧光谱线较宽,荧光寿命较长的特点.激光实验得到的激光输出,斜率效率为23.6%,输出功率为0.36W,输出激光的谱线分布较宽.
Resumo:
1999年,Cao等用皮秒级激光脉冲抽运ZnO颗粒(直径约为100nm)制成的粉末薄层,观察到了谱线宽度非常窄的激光辐射。本文初步研究了在纳秒级(脉宽8ns,频率30Hz)Nd:YAG脉冲激光器的抽运下,纳米ZnO粉末的发散光。
Resumo:
实验采用三倍频Nd:YAG(波长355nm,脉宽8ns,频率30Hz)脉冲激光器作为抽运光源,在ZnO纳米粉末(直径~100nm)中发现了类似激光现象.并用环形腔理论模拟了ZnO的颗粒密度对平均自由程的影响,从理论上证明在纳秒级激光器的抽运下,ZnO纳米粉末也可以发射激光.
Resumo:
Thermal effects in Nd:YAG planar waveguide lasers with non-symmetrical claddings are discussed. The heat generated in the active core can be removed more efficiently by directly contacting the active core to the heat sink. Several cladding materials are compared to optimize the heat removal. Furthermore, uniform pumping is achieved with oblique edge-pumping technique. Using quasi-CW pumping at 1 KHz repetition rate, an average output power of 280 W with a slope efficiency of 38% is obtained with a positive unstable resonator. (C) 2008 Elsevier B.V. All rights reserved.
Resumo:
In this paper, we demonstrated a dual-wavelength competitive output in Nd:Y3SC1.5Al3.5O12 ceramic disk laser. Different dual-wavelength output behaviors for Nd:YSAG and Nd:YAG ceramic disk laser were investigated and discussed. By applying the energy transfer model, we suggested the reasonable explanation for this new phenomenon as the disordered replacing of Al3+ ions by Sc3+ ions. The main advantage of the dual-wavelength ceramic laser is the possibility to serve as the seed source to generate Terahertz radiation. (C) 2008 Elsevier B.V. All rights reserved.
Resumo:
Ce3+ ions were introduced into the Er3+/Yb3+ -codoped TeO2-WO3-ZnO glasses, and the effect of Ce3+ on the emission properties at 1.5 mu m band and the upconversion luminescence of Er3+ in the glasses was investigated. With the increasing of Ce3+ concentration, the emission intensity of Er3+ at 1.5 mu m band increases firstly, and then decreases. The optimal doping concentration of Ce3+ is about 2.07 x 10(20)/cm(3). As for the Er3+ emission at 1.5-mu m band, the fluorescence lifetime decreases a little from 3.4ms to 3.0ms, while the full width at half maximum (FWHM) hardly changes with the increase of Cc 3+ concentration. Due to the effective cross relaxation between Ce3+ and Er3+ : Er3+ (I-4(11/2)) + Ce3+ (F-2(5/2)) -> Er3+ (I-4(13/2)) + Ce3+ (F-2(7/2)), the upconversion emission intensity of Er3+ is reduced greatly. But when Ce3+ -doping concentration is too high, the other cross relaxation between Ce3+ and Er3+ : Er3+ (4I(13/2)) + Ce3+ (F-2(5/2)) -> Er3+ (I-4(15/2)) + Ce3+ (F-2(7/2)) happens, which depopulates the I-4(13/2) level of Er3+ and results in the decrease of the emission intensity and fluorescence lifetime of Er3+ at 1.5 mu m band.