188 resultados para VINYL-POLYMERS
Resumo:
The reactions of freshly prepared Cu(OH)(2).xH(2)O and Cu(OH)(2-2y)(CO3)(y).zH(2)O precipitates with imidazole and adipic acid in CH3OH/H2O at pH = 5.4 yielded CU(C3N2H4)(2)(HL)(2) 1 and CU(C3N2H4)(2)L 2, respectively. Complex 1 consists of ribbon-like polymeric chains (1)(infinity)[CU(C3N2H4)(2)(HL)(4/2)], in which the octahedrally coordinated Cu atoms are doubly bridged by bis-monodentate hydrogen adipato ligands. The interchain N-H...O hydrogen bonding interactions are responsible for supramolecular assembly of the polymeric chains into open 3D frameworks and two-fold interpenetration of the resulting open frameworks completes the crystal structure of 1. Within complex 2, the Cu atoms are penta-coordinated to form CuN2O3 square pyramids and condensed into CU2N4O4 dimers, which are doubly bridged by twisted bis-monodentate adipato ligands into polymeric chains (1)(infinity)([CU(C3N2H4)(2)](2)L-4/2) with 4- and 18-membered rings progressing alternatively. The polymeric chains are assembled due to interchain N-H...O hydrogen bonding interactions. The thermal and magnetic behaviors of 1 and 2 is discussed.
Resumo:
Layer-by-layer electrodeposition of redox polymer/enzyme composition films on screen-printed carbon electrodes for fabrication of reagentless enzyme biosensors has been proposed and the resulting films were found to be very stable and rigid.
Resumo:
Both absolute molecular weight and molecular sizes (radius of gyration and hydrodynamic radius) of a vinyl-type polynorbornene eluting from size-exclusion chromatography columns were determined by combined with a static and dynamic laser light scattering detector. The hydrodynamic radius of polymer fraction eluting from size-exclusion chromatography columns was obtained from dynamic laser light scattering measurements at only a single angle of 900 by introducing a correction factor. According to the scaling relationship between molecular sizes and molecular weight and the ratio between radius of gyration and hydrodynamic radius, the vinyl-type polynorbornene took a random coil conformation in 1,2,4-trichlorobenzene at 150 degreesC.
Resumo:
Efficient blue polymer light-emitting diodes (PLEDs) have been fabricated with a neutral alcohol-soluble polyfluorene, i.e., poly(9,9-bis(6(')-diethoxylphosphorylhexyl)fluorene) (PF-EP), as the emitting layer, high work-function Al as the cathode, and poly(vinyl carbazole) as the hole-transporting layer. The PLEDs display a maximum luminous efficiency of 4.0 cd/A and the luminous efficiency > 2.4 cd/A in a wide range of current densities. It is found that the promising performance of the devices is attributed to the fact that the PF-EP is not only an efficient blue light-emitting polymer, but it also can facilitate efficient electron injection at the Al/PF-EP interface.
Resumo:
A new method for syntheses of hyperbranched poly(ester-amide)s from commercially available A(2) and CBx type monomers has been developed on the basis of a series of model reactions. The aliphatic and semiaromatic hyperbranched poly(ester-amide)s with multihydroxyl end groups are prepared by in situ thermal polycondensation of intermediates obtained from dicarboxylic acids (A(2)) and multihydroxyl primary amines (CBx) in N,N-dimethylformamide. Analyses of FTIR, H-1 NMR, and C-13 NMR spectra revealed the structures of the polymers obtained. The MALDI-TOF MS of the polymers indicated that cyclization side reactions occurred during polymerization. The hyperbranched poly(ester-amide) s contain configurational isomers observed by C-13 and DEPT C-13 NMR spectroscopy. The DBs of the polymers were determined to be 0.38-0.62 by H-1 NMR or quantitive C-13 NMR and DEPT 135 spectra. These polymers exhibit moderate molecular weights, with broad distributions determined by size exclusion chromatography ( SEC), and possess excellent solubility in a variety of solvents such as N, N- dimethylacetamide, dimethyl sulfoxide, tetrahydrofuran, and ethanol, and display glass-transition temperatures (T(g)s) between -2.3 and 53.2 degrees C, determined by DSC measurements.
Resumo:
A novel sulfonated aromatic dichloride monomer was successfully prepared by the reaction of 2, 5-dichlorobenzophenone with fuming sulfuric acid. Copolymerization of this monomer in the form of sodium salt (1) with N-(4-chloro-2-trifluoromethylphenyl)-5-chloro-1,8-naphthalimide (2) or bis(N-(4-chloro-2-trifluoromethylphenyl)1,4,5,8-naphthalimide (3) generated two series of novel poly(arylene-co-naphthalimide) s I-x and II-x where x represents the content of the sulfonated monomer. The synthesized copolymers with the -SO3H group in the side chains possessed high molecular weights revealed by their high viscosity and the formation of tough and flexible membranes. The copolymers exhibited excellent stability toward water and oxidation due to the introduction of the hydrophobic CF3 groups. The sulfonated copolyimides that incorporated with 1,8-naphthalimide (I-x) exhibited better hydrolytic and oxidative stabilities than those with 1,4,5,8-naphthalimide. Copolymer I-50 membrane endured for more than 83 h in Fenton's reagent at room temperature. The mechanical properties of I-50 membrane kept almost unchanged after immersing membrane in boiling water for 196 h. The proton conductivities of copolymer films increased with increasing IEC and temperature, reaching values above 6.8 x 10(-1) S/cm at 80 degrees C.
Resumo:
In this paper, four novel silver(I) sulfonate coordination polymers containing neutral ligands, namely, [Ag(2)Ll (biim)(2)]center dot 2H(2)O (1). AgL2(biim) (2), [Ag(HL3)(Pic)(2)]center dot H2O (3), and [Ag-3(L3)(HL3)(4,4'-bipy)(3)(H2O)(2)]center dot 4H(2)O (4), have been synthesized [L1 = 3-carboxy-4-hydroxybenzenesulfonate, L2 = p-aminobenzenesulfonate, H(2)L3 = p-hydroxybenzenesulfonic acid, biim = 1,1'-(1.4-butanediyl)-bis(imidazole), Pic = beta-picoline, 4,4'-bipy = 4,4'-bipyridine]. For compounds 1 and 2, Ag(I) cations are bridged by biim ligands to form a one-dimensional (1D) "zigzag" chain, and L1 and L2 sulfonate ligands are not coordinated to the silver cation. Compound 3 has a dimeric structure in which two silver cations are bridged by two HL3 ligands. For compound 4, L3 ligand coordinates to a silver cation as a monodentate ligand, and Ag(l) cations are bridged by 4,4'-bipy ligands to form a ID chain. Compound 1 contains water dimers, while compound 4 contains water trimers. Compounds 1-3 display room-temperature photoluminescence.
Phenylene vinylene-based electroluminescent polymers with electron transport block in the main chain
Resumo:
We report a new route for the design of soluble phenylene vinylene (PV) based electroluminescent polymers bearing electron-deficient oxadizole (OXD) and triazole (TZ) moieties in the main chains with the aryloxy linkage. Both series of the PV-based polymers were prepared by Wittig reaction. By properly adjusting the OXD and/or TZ content through copolymerization, we can achieve an enhanced balance of hole- and electron injections, such that the device efficiency is significantly improved. Light-emitting diodes fabricated from P1, P2, P3, P4, P5, P6, and P7 with the configuration of Indium-Tin Oxide (ITO)/Poly (styrene sulfonic acid) doped poly (ethylenedioxythiophene) (PEDOT)/polymer/Ca/Al, emit bright green light with the maximum peak around 500 nm. For the device using the optimal polymer (P4) as emitting layer, a maximum brightness of 1300 cd/m(2) at 20 V and a maximum luminance efficiency of 0.325 cd/A can be obtained.
Resumo:
This paper reports the synthesis of a novel maleimide-terminated thioetherimide oligomer and its copolymefization with reactive solvents bearing vinyl. Starting from 3-chlorophthalic anhydride and 4-chlorophthalic anhydride, 2,2',3,3'-thiodiphenyl tertracaboxylic dianhydride (3,3'-TDPA) and 3,3',4,4'-thiodiphenyl tertracaboxylic dianhydride (4,4'-TDPA) were synthesized. Thereby, a novel maleimide-terminated thioetherimide oligomer was prepared from. 3,3-TDPA, 4,4'-TDPA, 3,3'-dimethyl-4,4-diaminodiphenylmethane (DMMDA) and maleic anhydride. Binary and ternary copolymer resin were derived from corresponding binary and ternary homogeous solution consisting of thioetherimide oligomer, reactive solvent N-vinylpyrrolidone (NVP) or N,N'-dimethylacrylamide (DMAA) and divinylbenzene (DVB) as modifier, initiated either by gamma ray irradiation or by benzoyl peroxide (BPO). Thermal and mechanical properties of copolymer resin are determined and compared in terms of the kind of reactive solvent, addition of modifier DVB. The effect of initiation approach on property of final copolymer resin were studied. Phase separation and sub-transition of ternary copolymer resin induced by BPO are observed, which could be accounted for by thermal movement of DMAA molecules during thermal initiation.
Resumo:
We demonstrated in this paper an electrospinning technique could be employed to prepare the single layer macroporous films and fibrous networks of poly(vinyl alcohol) (PVA). A crucial element using electrospinning on the development of these electrospun structures was to shorten the distance of from the needle tip to the collector (L), which resulted in the bond of the wet fibers deposited on the collector at the junctions. The morphologies and average pore size of electrospun structures of PVA were mainly predominated by L and the time of collecting wet fibers on the collector. In addition, experimental results showed that an increase of the PVA concentration or a decrease of the applied voltage could also diminish slightly the average pore size of electrospun productions. Furthermore, a 60 degrees C absolute ethanol soak to PVA electrospun production led them to be able to stabilize in water for 1 month against disintegration. Differential scanning calorimetry (DSC) demonstrated that the 60 degrees C ethanol soak enhanced the degree of crystallinity of PVA production. The structural characteristic of macroporous films and networks in combination with their easy processability suggests potential utility in issue engineering applications.
Resumo:
Two new Cull coordination polymers, namely [Cu-2(BDC)(2)(L)(4)(H2O)(2)]center dot 14H(2)O (1) and [Cu-1.5(BTC)(L)(1.5)(H2O)(0.5)]center dot 2H(2)O (2), where L = 1,1'-(1,4-butanediyl)bis(imidazole), BDC = 1,4-benzene dicarboxylate, and BTC = 1,3,5-benzenetricarboxylate, have been synthesized at room temperature. Complex 1 exhibits an unusual, square-planar, four-connected 2D (2)(6)4 net, which has been predicated by Wells. Interestingly, three types of water clusters, namely (H2O)(6), (H2O)(8), and (H2O)(10), are observed in the hydrogen-bonded layers constructed by the BDC ligands and water molecules. The BTC anion in compound 2 is coordinated to the Cu" cation as tetradentate ligand to form a (6(6))(2)(4(2)6(4)8(4))(2)(6(4)810) net containing three kinds of nonequivalent points, Thermogravimetric analyses (TGA) and IR spectra for 1 and 2 are also discussed in detail.
Resumo:
A series of binuclear neutral nickel and palladium complexes [(XC6H2CH=NC6H3-iPr(2))MRL](2) 4b-f (X=NO2, M=Ni, R=Ph, L=PPh3, 4b; X=H, M=Pd, R=Me, L=PPh3,4c; X=H,M=Pd, R=Me, L=Py, 4d; X=NO2,M=Pd, R=Me, L=PPh3, 4e; X=NO2, M=Pd, R=Me, L=Py, 4f) and [(C10H7CH=NC6H3-iPr(2))MRL](2) 8a-c (M=Ni, R=Ph, L=PPh3, 8a; M=Pd, R=Me, L=PPh3, 8b; M=Pd, R=Me, L=Py, 8c) have been synthesized and characterized. The structures of complexes 4e and 8b have also been confirmed by X-ray crystallographic analysis. With modified methylalummoxane (MMAO) as cocatalysts, these complexes and complex [(C6H3CH=NC6H3-iPr(2))NiPh(PPh3)](2) 4a are capable of catalyzing the addition polymerization of norbomene (NBE) with the high activity up to 2.3 x 10(8) g PNBE/(mol(M) h). The structure of complexes affects considerably catalytic activity towards norbomene polymerization. The polymers obtained with nickel complexes are soluble, while those obtained with palladium complexes are insoluble. Palladium complexes 4c, 4e and 8b bearing PPh3 ligands exhibit much higher activities than the corresponding complexes 4d, M and 8c bearing pyridine ligands under the same conditions.
Resumo:
A series of acrylic impact modifiers (AIMS) with different particle sizes ranging from 55.2 to 927.0 nm were synthesized by seeded emulsion polymerization, and the effect of the particle size on the brittle-ductile transition of impact-modified poly(vinyl chloride) (PVC) was investigated. For each AIM, a series of PVC/AIM blends with compositions of 6, 8, 10, 12, and 15 phr AIM in 100 phr PVC were prepared, and the Izod impact strengths of these blends were tested at 23 degrees C. For AIMs with particle sizes of 55.2, 59.8, 125.2, 243.2, and 341.1 nm, the blends fractured in the brittle mode when the concentration of AIM was lower than 10 phr, whereas the blends showed ductile fracture when the AIM concentration reached 10 phr. It was concluded that the brittle-ductile transition of the PVC/AIM blends was independent of the particle size in the range of 55.2-341.1 nm. When the particle size was greater than 341.1 nm, however, the brittle-ductile transition shifted to a higher AIM concentration with an increase in the particle size. Furthermore, the critical interparticle distance was found not to be the criterion of the brittle-ductile transition for the PVC/AIM blends.
Resumo:
Two heterometallic chain coordination polymers with the chemical formula {[Cu2Mn2L2(CH3OH)(H2O)] center dot 0.5CH(3)OH center dot 0.5CH(3)CH(2)OH}(n) (1) and {[Cu2Co2L2(H2O)(2)] center dot H2O}(n) (2) have been synthesized and characterized by IR, UV spectroscopy and single-crystal X-ray structural analysis, where H4L = 2-hydroxy-3-[(E)-({2-[(2-hydroxybetizoyl)amino]ethyl}imino)methyl] benzoic acid. Magnetic measurements showed that the two compounds exhibit antiferromagnetic coupling exchange interactions, and satisfactory fittings to the observed magnetic susceptibility data were obtained by assuming a linear four-spin arrangement with two isotropic magnetic exchange interactions.
Resumo:
Copper-zinc heterometallic 1D chain coordination polymer has been synthesized and characterized by elemental analysis, and IR spectra etc. The crystal structure was determined by single-crystal X-ray diffraction analyses. The title complex is 1 D chain coordination polymer with the chemical formula {[CuLZn center dot CuLZn(H2O)]center dot H2O}(n), where H4L=N-(2-hydroxybenzamido)-N'-(3-carboxylsalicylidene)ethylenediamine. Its structural unit is comprosed of two tetranuclear cycles formed by two dissymmetrical tetranuclear units. These units polymerized each other to form 1 D chain coordination polymer.