Using a graft modification method, a comblike polymer host (CBPE550) was synthesized by reacting monomethyl ether of poly(ethylene glycol) (PEGMA) with ethylene-maleic anhydride copolymer (EMAC) and endcapping the residual carboxylic acid with methanol. The product was characterized by IR and elementary analysis. Result showed that the product was amorphous and semi-ester product is accord with reaction equation. There were two peaks in the plot of the ionic conductivity against Li salt concentration. The plot of log a against 1/(T - T-0) shows a dual VTF behavior when using the glass transition temperature of PEO of side chain as T beta. The comblike polymer is a white rubbery solid. It can be well-dissolved in acetone. (C) 1999 Elsevier Science Ltd. All rights reserved.

Relevância:

10.00% 10.00%

Publicador:

Resumo:

Blends of nylon-6 and epoxidised ethylene propylene diene (eEPDM) rubber were prepared through reactive mixing. It is found that the toughness of nylon-6 can be much improved by this method, and that the particle size of eEPDM is much smaller than that of unexpoxidised EPDM (uEPDM) rubber in a nylon-6 matrix. This indicates that the epoxy group in eEPDM could react with a nylon-6 end group to form a graft copolymer which could act as an interfacial compatibiliser between the nylon-6 and the eEPDM rubber dispersed phase. (C) 1998 Elsevier Science Ltd. All rights reserved.

Relevância:

10.00% 10.00%

Publicador:

Resumo:

In this paper, unepoxidized ethylene propylene diene rubber (uEPDM) was first epoxidized with formic acid and H2O2, and then the epoxidized ethylene propylene diene rubber (eEPDM) was melt-mixed with PET resin in a Brabender-like apparatus. Toughening of PET matrix was achieved by this method. The dispersion of rubber particles and phase structure of the blends were also observed by SEM. It has been suggested that the epoxy groups in the eEPDM could react with PET end groups to form a graft copolymer which could act as an interfacial compatibilizer between the PBT matrix and eEPDM rubber dispersed phase. This is beneficial to the improvement of the impact performance of PBT. (C) 1997 Elsevier Science Ltd.

Relevância:

10.00% 10.00%

Publicador:

Resumo:

Grafting of acrylamido tertiary butyl sulfonic acid (ATBS) onto ethylene-polypropylene copolymer (EPM) was carried out by using a reactive processing method. The grafting copolymer was characterized by means of WAXD, FT-IR, ESCA, and DSC. Improved thermal stability was observed for graft copolymer. Effects of the monomer and the initiator concentrations, reactive temperature, and time on grafting degree were investigated. (C) 1997 John Wiley & Sons, Inc.

Relevância:

10.00% 10.00%

Publicador:

Resumo:

The compatibilization of high density polyethylene (HDPE)/polyisoprene (PI) blends with polyethylene/polyisoprene (PE/PI) ''thread-through'' copolymers was investigated. The proliferating structure of PE/PI with segments chemically identical to HDPE and PI, respectively, is different from that of graft copolymers. Studies showed that the dispersed domain size in the blends was significantly reduced and interfacial adhesion was improved by the compatibilization action of the copolymer. In the differential scanning calorimetry (DSC) analysis, the crystallization peak of HDPE in the blends became broad with adding the copolymer and fractionated crystallization appeared in the HDPE/PI blend compatibilized with the copolymer at a weight ratio of 30/70 while it appeared in the blend without copolymer at a weight ratio of 20/80. DMA results showed that by adding the copolymer, both the glass transition temperature (T-g) of the PI component and the alpha-relaxation of HDPE shifted to lower temperature, demonstrating the enhanced penetration of the two components. Mechanical properties of the blends were improved, especially the elongation at break, by the presence of the copolymers. The characteristic yielding at the fractured surface of the blends compatibilized with the copolymer indicates the fractural behavior of the material changed from brittle to tough.

Relevância:

10.00% 10.00%

Publicador:

Resumo:

In this paper, the graft copolymers of styrene to nascent linear polyethylene reactor powders were prepared through plasma graft polymerization. The grafting reaction was initiated by the alkyl radicals formed on the surface of nascent polyethylene with plasma treatment as indicated by electron spin resonance spectra. In graft copolymerization by alkyl radicals, the grafting yield increased with either the plasma power or the plasma treatment lime. Compared with ordinary polyethylene powders, nascent polyethylene reactor powders were found to be more easily plasma-grafted. This has been attributed to the greater sensitivity to irradiation in producing reactive centres under the same conditions. High density polyethylene showed almost the same grafting yield as linear low density polyethylene at 50 degrees C. The surface morphology of nascent polyethylene observed by scanning electron microscope before and after the grafting showed that the silk-like fibrils were not destroyed by plasma treatment.

Relevância:

10.00% 10.00%

Publicador:

Resumo:

The melting behavior of poly(methyl methacrylate)-grafted nascent polyethylene reactor powder by plasma irradiation was studied by differential scanning calorimetry (DSC). The grafting yield ranged hom 11 to 190%. Grafting was found to lower both melting point and heat of fusion during the first run of DSC determination. The heat of fusion was used to calculate the apparent grafting yield of the samples. There was little strain induced by plasma-irradiated grafting on the surface of the polyethylene crystals. A method to determine the covalent grafting yield in the graft copolymer systems was developed. (C) 1995 John Wiley & Sons, Inc.

Relevância:

10.00% 10.00%

Publicador:

Resumo:

This paper reports a study of compatibilization and the mechanism of compatibilization of polypropylene (PP)/thermoplastic polyurethane (TPU) blends with maleated polypropylene (PP-MA) and its graft copolymer with polyethylene oxide (PEO), (PP-MA)-g-PEO.

Relevância:

10.00% 10.00%

Publicador:

Resumo:

The compatibilization of incompatible polypropylene (PP)/poly(ethylene oxide) (PEO) blends was studied. The experimental results showed that the graft copolymer [(PP-MA)-g-PEO] of maleated PP (PP-MA) and mono-hydroxyl PEO (PEO-OH) was a good compatibilize

Relevância:

10.00% 10.00%

Publicador:

Resumo:

Graft copolymers of polyethylene (PE) with polyisoprene (PI) were synthesized through polymerization of ethylene in toluene solution of PI (cis-1,4-: 95%; 3,4-: 5%) using a homogeneous V(acac)3/Et3Al2Cl3 catalyst. Copolymers are formed when the growing po

Relevância:

10.00% 10.00%

Publicador:

Resumo:

A new graft copolymer (PP-MA)-g-PEO was synthesized by means of the chemical reaction between maleated polypropylene (PP-MA) and mono hydroxyl poly(ethylene oxide) (PEO-OH). The effect of reaction conditions on the degree of grafting of PEO-OH was studied

Relevância:

10.00% 10.00%

Publicador:

Resumo:

A novel comb-like amphiphilic polymer, poly (2-acrylamidohexadecylsulfonic acid) (PAMC16S), was synthesized by free radical polymerization of the corresponding amphiphilic monomer in 1,4-dioxane-water mixed solvents. Depending on the ratio of water/dioxane in the solvent, the reaction proceeded by either precipitation polymerization or micellar polymerization. The molecular weight of the polymer obtained under similar conditions decreased and subsequently increased with the increase of water content in the mixed solvent. The polyion nature of PAMC16S was confirmed by viscosity data of ethanolic solutions. In addition, the polymer was characterized by solubility, IR, TG and wide angle X-ray diffraction methods.

Relevância:

10.00% 10.00%

Publicador:

Resumo:

A novel matrix of macropore cellulose membrane was prepared by chemical graft, and immobilized the cationic charged groups as affinity ligands. The prepared membrane Fan be used for the removal of endotoxin from human serum albumin (HSA) solutions. With a cartridge of 20 sheets affinity membrane of 47 mm diameter, the endotoxin level in HSA solution can be reduced ro 0.027 eu/mL. Recovery of HSA was over 95%.