158 resultados para HZSM-5 esterification


Relevância:

100.00% 100.00%

Publicador:

Resumo:

Variations in the structure and acidity properties of HZSM-5 zeolites with reduction in crystal sizes down to nanoscale (less than 100 nm) have been investigated by XRD, TEM and solid-state NMR with a system capable of in situ sample pretreatment. As evidenced by a combination of Al-27 MAS NMR, Si-29 MAS, CP/MAS NMR and H-1 MAS NMR techniques, the downsize of the zeolite crystal leads to an obvious line broadening of the Al-27, Si-29 MAS NMR spectrum, an increasing of the silanol concentration on the external surface, and a pronounced alteration of the acidity distribution between the external and internal surfaces of the zeolite. In a HZSM-5 zeolite with an average size at about 70 nm, the nonacidic hydroxyl groups (silanols) are about 14% with respect to the total amount of Si, while only 4% of such hydroxyl groups exist in the same kind of zeolite at 1000 nm crystal size. The result of H-1 MAS NMR obtained using Fluorinert(R) FC-43 (perfluorotributyl amine) as a probe molecule demonstrates that most of the silanols are located on the external surface of the zeolite. Moreover, the concentration of Bronsted acid sites on the external surface of the nano-structured zeolite appears to be distinctly higher than that of the microsized zeolite.

Relevância:

100.00% 100.00%

Publicador:

Resumo:

The conversion of n-C4H10 was undertaken on MoO3/HZSM-5 catalyst at 773-973K and the phases of molybdenum species were detected by XRD. The XRD results show that bulk MoO3 on HZSM-5 can be readily reduced by n-C4H10 to MoO2 at 773 K and MoO2 can be gradually carburized to molybdenum carbide above 813 K. The molybdenum carbide formed from the carburization of MoO2 with n-C4H10 below 893 K is alpha-MoC1-x with fcc-structure, while hcp-molybdenum carbide formed above 933 K. During the evolution of MoO3 to MoO2 (>773 K) or the carburization of MoO2 to molybdenum carbide (>813 K), deep oxidation, cracking and coke deposition are serious, in particular at higher reaction temperatures, these lead to the poor selectivity to aromatics. Aromatization of n-C4H10 can proceed catalytically on both Mo2C/HZSM-5 and MoO2/HZSM-5, the distribution of the products for the two catalysts is similar below 813 K, but the, activity for Mo2C/HZSM-5 is much higher than that for MoO2/HZSM-5. (C) 2002 Elsevier Science B.V. All rights reserved.

Relevância:

100.00% 100.00%

Publicador:

Resumo:

The addition of ZnO or ZrO2 into CuO/HZSM-5 was investigated for DME synthesis from syngas by using the reactive frontal chromatography method, TPR and in situ TPR. These promoters enhanced the catalytic activity of Cu/HZSM-5 and promotion with ZnO and ZrO2 produced a maximum activity, which could be explained by the improvement of the dispersion of Cu and the promotion of CuO reduction. The Cu+ species existing during the reaction have been detected, based on which a Cu-0 <-> Cu+1 redox cycle model was put forward.