118 resultados para semi conducting polymers, electroluminescence, photovoltaics


Relevância:

30.00% 30.00%

Publicador:

Resumo:

By selecting polyfluorene as the polymer host, choosing 2,1,3-benzothiadiazole derivative moieties as the red dopant units and covalently attaching 0.3 mol% of the dopant units to the side chain of the polymer host, we developed a novel series of red electroluminescent polymers of dopant/host system with molecular dispersion feature. Their EL spectra exhibited predominant red emission from the dopant units because of the energy transfer and charge trapping from the polymer backbone to the dopant units. The emission wavelength of the polymers could be tuned by modifying the chemical structures of the dopant units.

Relevância:

30.00% 30.00%

Publicador:

Resumo:

Three series of poly(phenylene vinylene) (PPV) derivatives containing hole-transporting triphenylamine derivatives [N-(4-octoxylphenyl)diphenylamine, N,N'-di(4-octyloxylphenyl)-N,N'-diphenyl-1,4-phenylenediamine, and N,N'-di(4-octoxylphenyl)-N,N'-diphenylbenzidine] (donor) and electron-transporting oxadiazole unit (2,5-diphenyl-1,3,4-oxadiazole) (acceptor) in the main chain were synthesized by improved Wittig copolymerization. The resulting donor-acceptor (D-A) polymers are readily soluble in common organic solvents, such as chloroform, dichloroethane, THF, and toluene.

Relevância:

30.00% 30.00%

Publicador:

Resumo:

Two new stepladder conjugated polymers, that is, poly(7,7,15,15-tetraoctyldinaphtho[1,2-a:1',2'-g]-s-indacene) (PONSI) and poly(7,7,15,15-tetra(4-octylphenyl)dinaphtho[1,2-a:1',2'-g]-s-indacene) (PANSI) with alkyl and aryl substituents, respectively, have been synthesized and characterized. In comparison with poly(indenofluorene)s, both polymers have extended conjugation at the direction perpendicular to the polymer backbone because of the introduction of naphthalene moieties. The emission color of the polymers in film state is strongly dependent on the substituents. While PONSI emits at a maximum of 463 nm, PANSI with the same backbone but aryl substituents displays dramatically redshifted emission with a maximum at 494 nm.

Relevância:

30.00% 30.00%

Publicador:

Resumo:

Three low bandgap conjugated polymers, i.e., PDTPBT-C8, PDTPBT-C6 and PDTPBT-C5, which consist of alternating N-alkyl dithieno[3,2-b: 2',3'-d] pyrrole and 2,1,3-benzothiadiazole units and carry 1-octylnonyl, 1-hexylheptyl and 1-pentylhexyl as side chains, respectively, were synthesized. These polymers show strong absorption in the wavelength range of 600-900 nm with enhanced absorption coefficient as the length of alkyl chain decreases. The film morphology of the polymers and 1-(3-methoxycarbonyl) propyl-1-phenyl-[6,6]-C-61 (PCBM) blends is also dependent on the alkyl chain length. As the length decreases, the film becomes more uniform and the domian size decreases from 400-900 nm for PDTPBT-C8 to similar to 50 nm for PDTPBT-C5.

Relevância:

30.00% 30.00%

Publicador:

Resumo:

A novel strategy for obtaining white electroluminescence (EL) is based on the mechanism of electron trapping on host. Phosphonate-functionalized polyfluorene is chosen as host owing to its strong electron affinity. Electrons are confined mostly by host pendants in the EL process, which suppresses charge transfer from host to dopant. White EL with CIE coordinates of (0.34,0.35) is achieved.

Relevância:

30.00% 30.00%

Publicador:

Resumo:

A sulfonated poly[bis(benzimidazobenzisoquinolinones)] (SPBIBI) possessing a conjugated pyridinone ring was shown to be effective for dispersing multiwalled carbon nanotubes (MWCNTs) in DMSO. The dispersions in which the SPBIBI to MWCNTs mass ratio was 4:1 demonstrated the highest MWCNTs concentrations, i.e., 1.5-2.0 mg mL(-1), and were found to be stable for more than six months at room temperature. Through casting of these dispersions, MWCNTs/SPBIBI composite membranes were successfully fabricated on substrates as proton exchange membranes for fuel cell applications and showed no signs of macroscopic aggregation. The properties of composite membranes were investigated, and it was found that the homogeneous dispersion of the MWCNTs in the SPBIBI matrix altered the morphology structures of the composite membranes, which lead to the formation of more regular and smaller cluster-like ion domains.

Relevância:

30.00% 30.00%

Publicador:

Resumo:

One mu-dichloro bridged diiridium complex and three mononuclear iridium(III) complexes based on the 1,3,4-oxadiazole derivatives as cyclometalated ligands and acetylacetonate (acac) or dithiolates O,O'-diethyldithiophosphate (Et(2)dtp) or N,N'-diethyldithiocarbamate (Et(2)dtc) as ancillary ligands have been synthesized and systematically studied by X-ray diffraction analysis. The results reveal that three mononuclear complexes all adopt distorted octahedral coordination geometry around the iridium center by two chelating ligands with cis-C-C and trans-N-N dispositions, which have the same coordination mode as the diiridium dimer. The dinuclear complex crystallizes in the monoclinic system and space group C2/c, whereas three mononuclear iridium complexes are all triclinic system and space group P(1) over bar. In the stacking structure of the dimer, one-dimensional tape-like chains along the b-axis are formed by hydrogen bondings, which are strengthened by pi stacking interactions between phenyl rings of 1,3,4-oxadiazole ligands. Then these chains assemble a three-dimensional alternating peak and valley fused wave-shape structure. In each stacking structure of three mononuclear complexes, two molecules form a dimer by the C-H center dot center dot center dot O hydrogen bondings, and these dimers are connected by pi stacking interactions along the b-axis, constructing a zigzag chain.

Relevância:

30.00% 30.00%

Publicador:

Resumo:

Four single polymers with two kinds of attachment of orange chromophore to blue polymer host for white electroluminescence (EL) were designed. The effect of the side-chain attachment and main-chain attachment on the EL efficiencies of the resulting polymers was compared. The side-chain-type single polymers are found to exhibit more efficient white EL than that of the main-chain-type single polymers. Based on the side-chain-type white single polymer with 4-(4-alkyloxy-phenyl)-7-(4-diphenylamino-phenyl)-2,1,3-benzothiadiazoles as the orange-dopant unit and polyfluorene as the blue polymer host, white EL with simultaneous orange (lambda(max) = 545 nm) and blue emission (lambda(max) = 432 nm/460 nm) is realised. A single-layer device (indium tin oxide/poly(3,4-ethylenedioxythiophene)/polymer/Ca/Al) made of these polymers emits white light with the Commission Internationale de l'Eclairage coordinates of (0.30,0.40), possesses a turn-on voltage of 3.5 V, luminous efficiency of 10.66 cd A(-1), power efficiency of 6.68 lm W-1, and a maximum brightness of 21240 cd m(-2).

Relevância:

30.00% 30.00%

Publicador:

Resumo:

A family of supramolecular polymers was prepared via Cd2+-directed self-assembly polymerization of his (2,2':6',2 ''-terpyridine)-based ligand monomers, using oligofluorenes and triphenylamine as bridges under mild conditions. The polymers were fully characterized using thermogravimetric analysis, inherent viscosity, electrochemical measurements, UV-visible spectroscopy, photoluminescence (PL) and electroluminescence (EL). Polymers with oligofluorenes as spacers exhibited blue emission (434-442 nm) in dimethyl acetamide (DMAc) solution, while polymers with triphenylamine as spacer presented an emission peak at 494 nn in DMAc solution. Complexation polymerization of bis(2,2':6',2 ''-terpyridine)-based ligand monomers with cadmium(II) improved fluorescence quantum yields dramatically, and the film PL quantum yields of these polymers were about 0.38-0.54. Single-layer light-emitting diodes were fabricated with the configuration indium tin oxide (ITO)/polymer/Ca/Al; the EL showed green emission and the onset voltages of the devices were 8-11 V.

Relevância:

30.00% 30.00%

Publicador:

Resumo:

2-(4-Biphenylyl)-5-(4-tert-butylphenyl)-1,3,4-oxdiazole (PBD) is a good electron-transporting material and can form single crystals from solution. In this work, solution cast PBD single crystals with different crystallographic axes (b, c) perpendicular to the Au/S substrates in large area are achieved by controlling the rate of solvent evaporation in the presence and absence of external electrostatic field, respectively. The orientation of these single crystals on Au/S substrate was characterized by transmission electron microscopy (TEM) and atomic force microscopy (AFM). Conducting probe atomic force microscopy (CP-AFM) was used to measure the charge transport characteristics of PBD single crystals grown on Au/S substrates. Transport was measured perpendicular to the substrate between the CP-AFM tip and the Au/S substrate. The electron mobility of 3 x 10(-3) cm(2)/(V s) for PBD single crystal along crystallographic b-axis is determined. And the electron mobility of PBD single crystal along the c-axis is about 2 orders of magnitude higher than that along the b-axis due to the anisotropic charge transport at the low voltage region.

Relevância:

30.00% 30.00%

Publicador:

Resumo:

Triphenyl pyrazoline derivatives (TPPs) bearing electron withdrawing and pushing substitutents were synthesized. Their photoluminescence (PL) properties in the solution and doped in poly(N-vinylcarbazole) (PVK) thin films were investigated. When TPPs were doped into PVK films the photoluminescence intensity was enhanced with increasing TPPs concentration. It indicated that the energy transfer from PVK to TPPs has happened. Double and three-layer electroluminescence (EL) devices based on PVK doped with TPPs as an active layer were fabricated and investigated and the electroluminescent mechanism was followed by energy transfer from PVK to TPPs. The pyrazoline derivative with both electron withdrawing and pushing substituents was the optimistic candidate for electroluminescent emitter due to higher transfer efficiency from electric energy to light energy as well as larger luminance.

Relevância:

30.00% 30.00%

Publicador:

Resumo:

An efficient white light-emitting polymer was developed with blue polyfluorene (PFO) chemically doped with orange fluorescent 1, 8-naphthalimide moieties. The emission spectrum can be easily tuned by varying the content of 1, 8-naphthalimide moieties. A white polymeric light-emitting diode (WPLED) with a structure of indium tin oxide (ITO)/the complex of (3,4-ethylenedioxythiophene) and polystyrene sulfonic acid (PEDOT)/polymer/Ca/Al showed a current efficiency of 5.3 cd/A and a power efficiency of 2.8 Lm/W at 6 V with the Commission Internationale de L'Eclairage (CIE) coordinates at (0.25,0.35). Moreover, the WPLED from the copolymer showed a very stable white light emission at different driving voltage and brightness. The CIE coordinates of the WPLED were (0.25, 0.35), (0.26, O.36), and (0.26, 0.36) under driving voltages of 6, 8, and 10 V, corresponding to the brightness of 82, 3555, and 7530 cd/m(2), respectively. This approach for realization of white light emission is promising over the polymer blending system in terms of both efficiency and color stability.

Relevância:

30.00% 30.00%

Publicador:

Resumo:

Efficient blue polymer light-emitting diodes (PLEDs) have been fabricated with a neutral alcohol-soluble polyfluorene, i.e., poly(9,9-bis(6(')-diethoxylphosphorylhexyl)fluorene) (PF-EP), as the emitting layer, high work-function Al as the cathode, and poly(vinyl carbazole) as the hole-transporting layer. The PLEDs display a maximum luminous efficiency of 4.0 cd/A and the luminous efficiency > 2.4 cd/A in a wide range of current densities. It is found that the promising performance of the devices is attributed to the fact that the PF-EP is not only an efficient blue light-emitting polymer, but it also can facilitate efficient electron injection at the Al/PF-EP interface.

Relevância:

30.00% 30.00%

Publicador:

Resumo:

Hybrid organic/inorganic white light-emitting diodes (LEDs) were fabricated of semiconductor polymer poly(N-vinylcarbazole) (PVK) doped with CdSe/CdS core-shell semiconductor quantum dots (QDs). The device, with a structure of indium-tin-oxide (ITO)vertical bar 3,4-polyethylene-dioxythiophene- polystyrene sulfonate (PEDOT:PSS)vertical bar PVK:CdSe/CdS vertical bar Al, emitted a pure white light spanning the whole visible region from 400 to 800 nm. The Commission Internationale del'Eclairage coordinates (CIE) remained at x = 0.33, y = 0.34 at wide applied voltages. The maximum brightness and electroluminescence (EL) efficiency reached 180 cd m(-2) at 19 V and 0.21 cd A(-1) at current density of 2 mA cm(-2), respectively. The realization of the pure white light emission is attributed to the incomplete energy and charge transfer from PVK to CdSe/CdS core-shell QDs.