The crystal structure of poly(ether ketone ketone) (PEKK) is predicted by using Cerius2 software according to the wide angle X-ray diffraction (WAXD) experiment result. The predicted structure has a planar zigzag chain conformation between ether oxygen and ketone carbons in an orthorhombic lattice. Average zigzag angle is 126 degrees and average torsion angle is 30.32 degrees. The WAXD powder pattern calculated from the crystal packing model is in good agreement with the experiment result.

Relevância:

100.00% 100.00%

Publicador:

Resumo:

The melting behavior of semicrystalline poly(ether ether ketone ketone) (PEEKK) has been studied by differential scanning calorimetry (DSC). When PEEKK is annealed from the amorphous state, it usually shows two melting peaks. The upper melting peaks arise first, and the lower melting peaks are developed later. The upper melting peaks shown in the DSC thermogram are the combination (addition) of three parts: initial crystal formed before scanning; reorganization; and melting-recrystallization of lower melting peaks in the DSC scanning period. In the study of isothermal crystallization kinetics, the Avrami equation was used to analyze the primary process of the isothermal crystallization; the Avrami constant, n, is about 2 for PEEKK from the melt and 1.5 for PEEKK from the glass state. According to the Lauritzen-Hoffman equation, the kinetic parameter of PEEKK from the melt is 851.5 K; the crystallization kinetic parameter of PEEKK is higher than that of PEEK, and suggests the crystallizability of PEEKK is less than that of PEEK. The study of crystallization on PEEKK under nonisothermal conditions is also reported for cooling rates from 2.5 degrees C/min to 40 degrees C/min, and the nonisothermal condition was studied by Mandelkern analysis. The results show the nonisothermal crystallization is different from the isothermal crystallization. (C) 1996 John Wiley & Sons, Inc.

Relevância:

100.00% 100.00%

Publicador:

Resumo:

On the basis of DSC measurements, the Delta H-f(0) values of the fusion heat for PEEKK-PEBEKK copolymers with various biphenyl contents were obtained by using thermodynamics statistical theory proposed by Flory and graphical method of the specific volume-fusion heat. The results reveal that Delta H-f(0) values determined by these two methods for PEEKK-PEBEKK copolymers with various biphenyl content are nearly the same, and that Delta H-f(0) values are closely dependent on biphenyl content. Delta H-f(0) value is minimum at n(B)=0.35.

Relevância:

100.00% 100.00%

Publicador:

Resumo:

Five narrowly distributed fractions of phenolphthalein poly(ether sulfone) (PES-C) were studied in CHCl3 by both static and dynamic laser light scattering (LLS) at 25 degrees C. The dynamic LLS showed that the PES-C samples contain some large polymer clusters as in previously studied phenolphthalein poly(ether ketone)(PEK-C). These large clusters can be removed by a 0.1-mu m filter. Our results showed that [R(g)(2)](1/2)(z) = (3.35 +/- 0.13) x 10(-2) M(w)((0.52 +/- 0.03)) and [D] = (2.26 +/- 0.02) x 10(-4)M(w)-((0.54) +/- 0.03)) with [R(g)(2)](1/2)(z), M(w) and [D] being the z-average radius of gyration, the weight-average molecular weight, and the z-average translational diffusion coefficient, respectively. A combination of static and dynamic LLS results enabled us to determine D = (2.45 +/- 0.04) x 10(-4)M-((0.55 +/- 0.05)), where D and M correspond to monodisperse species. Using this scaling relationship, we have successfully converted the translational diffusion coefficient distribution into the molecular weight distribution for each of the five PES-C fractional The weight-average molecular weights obtained from dynamic light scattering have a good agreement with that obtained from static laser light-scattering measurements.

Relevância:

100.00% 100.00%

Publicador:

Resumo:

C-13 and H-1 relaxation times were measured as a function of temperature in two magnetic fields for dilute solutions of phenolphthalein poly(ether sulfone) (PES-C) in deuterated chloroform. The spin-lattice relaxation times were interpreted in terms of segmental motion characterized by the sharp cutoff model of Jones and Stockmayer (J. S. model). The phenyl group rotation is treated as a stochastic diffusion by the J. S. model. The restricted butterfly motion of the phenyl group attached to the cardo ring in PES-C is mentioned but is not discussed in detail in this work. Correlation times for the segmental motion are in the picosecond range which indicates the high flexibility of PES-C chains. The correlation time for the phenyl group internal rotation is similar to that of the segmental motion. The temperature dependence of these motions is weak. The apparent activation energy of the motions considered is less than 10 kJ/mol. The simulating results for PES are also reasonable considering the differences in structure compared with PES-C. The correlation times and the apparent activation energy obtained using the J. S. model for the main chain motion of PES-C are the same as those obtained using the damped orientational diffusion model and the conformational jump model.

Relevância:

100.00% 100.00%

Publicador:

Resumo:

The miscibility and phase behavior of polysulfone (PSF) and poly(hydroxyether of bisphenol A) (phenoxy) with a series of copoly(ether ether ketone) (COPEEK), a random copolymer of poly(ether ether ketone) (PEEK), and phenolphthalein poly(ether ether ketone) (PEK-C) was studied using differential scanning calorimetry. A COPEEK copolymer containing 6 mol % ether ether ketone (EEK) repeat units is miscible with PSF, whereas copolymers containing 12 mol % EEK and more are not. COPEEK copolymers containing 6 and 12 mol % EEK are completely miscible with phenoxy, but those containing 24 mol % EEK and more are immiscible with phenoxy. Moreover, a copolymer containing 17 mol % EEK is partially miscible with phenoxy; the blends show two transitions in the midcomposition region and single transitions at either extreme. Two T(g)s were observed for the 50/50 blend of phenoxy with the copolymer containing 17 mol % EEK, whereas a single composition-dependent T-g appeared for all the other compositions. An FTIR study revealed that there exist hydrogen-bonding interactions between phenoxy and the copolymers. The strengths of the hydrogen-bonding interactions in the blends of the COPEEK copolymers containing 6 and 12 mol % EEK are the same as that in the phenoxy/PEK-C blend. However, for the blends of copolymers containing 17, 24, and 28 mol % EEK, the hydrogen-bonding interactions become increasingly unfavorable and the self-association of the hydroxyl groups of phenoxy is preferable as the content of EEK units in the copolymer increases. The observed miscibility was interpreted qualitatively in terms of the mean-field approach. (C) 1996 John Wiley & Sons, Inc.

Relevância:

100.00% 100.00%

Publicador:

Resumo:

Structures of poly(ether ether ketone ketone)-poly(ether biphenyl ether ketone ketone) copolymers were studied by using small angle X-ray scattering and the one-dimensional electron density correlation function method. The results revealed that structures of the aggregated state of the copolymers depend closely on the biphenyl content (n(b)). When n(b) = 0.35, invariant Q, long period L, average thickness of crystal lamellae (d) over bar, electron density difference eta(c) - eta(a) and degree of crystallinity W-c,W-x assume minimum values.

Relevância:

100.00% 100.00%

Publicador:

Resumo:

The mechanical properties of glass fiber-reinforced phenolphthalein poly(ether ketone)/poly(phenylene sulfide) (PEK-C/PPS) composites have been studied. The morphologies of fracture surfaces were observed by scanning electron microscope. Blending a semicrystalline component, PPS, can improve markedly the mechanical properties of glass fiber-reinforced PEK-C composites. These results can be attributed to the improvement of fiber/matrix interfacial adhesion and higher fiber aspect ratio. (C) 1996 John Wiley & Sons, Inc.

Relevância:

100.00% 100.00%

Publicador:

Resumo:

Block copolymers of poly(ethersulphone) (PES) oligomers with liquid crystalline polyester units were synthesized by the reaction of dihydroxy-terminated poly(ether sulphone) oligomers (number-average molecular weights: 704, 1,158 and 2570) and terephthaloyl bis(4-oxybenzoyl chloride), and their properties were investigated. The results indicated that the copolymer with PES segments of molecular weight of 704 possessed birefringent features when annealed at 360 degrees C, while the copolymer with PES segments of molecular weight of 2,570 became isotropic. Also, the block copolymers had a better chemical resistance and high-temperature stability than PES.

Relevância:

100.00% 100.00%

Publicador:

Resumo:

According to stress relaxation curves of phenolphthalein poly(ether ketone) (PEK-C) at different temperatures and the principle of time-temperature equivalence, the master curves of PEK-C at arbitrary reference temperatures are obtained. A coupling model (Kohlrausch-Williams-Watts) is applied to explain quantitatively the different temperature dependence of stress relaxation behavior and the relationship between stress relaxation and yield phenomenon is established through the coupling model.

Relevância:

100.00% 100.00%

Publicador:

Resumo:

Based on Jeziorny theory, the kinetics of phase transition of poly(ester-imide) has been determined under non-isothermal condition by using differential scanning calorimetry (DSC). Avrami exponent n, kinetic parameters G(c) and rate constant Z(c) were derived and discussed.

Relevância:

100.00% 100.00%

Publicador:

Resumo:

The Izod impact fracture behaviour of notched specimens of phenolphthalein poly(ether ketone) (PEK-C) has been studied over a temperature range from room temperature to 240 degrees C by using an instrumented impact tester. The temperature dependence of the maximum load, total impact energy, initiation energy, propagation energy, ductility index (DI) and the relationships between these parameters and the relaxation processes have been investigated.

Relevância:

100.00% 100.00%

Publicador:

Resumo:

Stress relaxation and dynamic mechanical behavior of phenolphthalein poly(ether ketone) (PEK-C) have been investigated. Using Ferry's reduction method, the master curve was obtained. From the experimental results, we found that the WLF equation is not appropriate in the lower-temperature range (T < T-g). The relaxation spectrum was calculated according to the first approximation method proposed by Schwarzl and Staverman. In addition to the alpha-transition region, a second transition zone is revealed at low temperature. This transition is probably due to a restricted motion of its main chain. (C) 1995 John Wiley and Sons, Inc.

Relevância:

100.00% 100.00%

Publicador:

Resumo:

Phenolphthalein poly(ether ketone) (PEK-C) was tested using an instrumented impact tester to determine the temperature effect on the fracture toughness K-c and critical strain energy release rate G(c). Two different mechanisms, namely the relaxation processes and thermal blunting of the crack tip were used to explain the temperature effect on the fracture toughness. Examination of the fracture surfaces revealed the presence of crack growth bands. It is suggested that these bands are the consequence of variations in crack growth along crazes that are formed in the crack tip stress field. As the crack propagates, the stress is relaxed locally, decreasing the growth rate allowing a new bundle of crazes to nucleate along which the crack advances.

Relevância:

100.00% 100.00%

Publicador:

Resumo:

Fracture toughness values of phenolphthalein poly(ether ketone) (PEK-C) at 190 degrees C were determined by two different methods, i. e. the conventional crack growth method and the crack stress whitening zone method, which show consistent results. This indicates that the crack stress whitening zone method can be used to determine the crack initiation of some polymers for which the blunting line concept is unsuitable.