A master-oscillator fiber power amplifier (MOPA) system with a 4-m-long Yb3+-doped homemade large mode area (LMA) double-clad fiber is reported. The system emits up to 133.8 W of amplified radiation at a wavelength of 1064 nm and a repetition rate of 100 kHz, limited only by the available pump power. Peak power of 300 kW at 20 kHz with a pulse duration of 15 ns is obtained. (c) 2006 Society of Photo-Optical Instrumentation Engineers.

Relevância:

20.00% 20.00%

Publicador:

Resumo:

A master-oscillator fiber power amplifier (MOPA) system with a 4-m-long Yb3+-doped homemade large mode area (LMA) double-clad fiber is reported. The system emits up to 133.8 W of amplified radiation at a wavelength of 1064 nm and a repetition rate of 100 kHz, limited only by the available pump power. Peak power of 300 kW at 20 kHz with a pulse duration of 15 ns is obtained. (c) 2006 Society of Photo-Optical Instrumentation Engineers.

Relevância:

20.00% 20.00%

Publicador:

Resumo:

A phase-locking fibre laser array with up to 60 W of coherent output power based on two large-core fibre is reported. The slope efficiency of the in-phase mode is 37%. For two cases of spacings between the cores, steady high-contrast interference stripes are observed. When the whole system operates under a high pump power level, no thermal effects for the spatial filter have been observed, which means that we can increase the coherent output power further by increasing the individual fibre laser power.

Relevância:

20.00% 20.00%

Publicador:

Resumo:

To get high output power with good beam quality, a tapered section is introduced to large-mode-area (LMA) Yb-doped fiber laser. Output characteristics of the fiber laser without tapered section and with tapered section are compared experimentally. When the launched pump power is 119.1 W, 77.9 W with M-2 3.08 and 56.4 W with M-2 1.14 can be obtained, respectively. The corresponding slope efficiencies are 71.8% and 54.1%, respectively. Although output power of the tapered fiber laser has 30.6% penalty, brightness of it is as much as 5.28 times of the fiber laser without tapered section. Moreover, spectra of them are measured. It is found that tapered section makes lasing wavelength of the fiber laser shorter. (c) 2007 Elsevier B.V. All rights reserved.

Relevância:

20.00% 20.00%

Publicador:

Resumo:

Large ruby with the size of circle divide75 x 45 mm was grown by temperature gradient technique for the first time. Absorption spectrum was carried out in the range of 190-800 nm by spectrophotometer, and the concentration spatial distribution of Cr3+ in ruby was calculated from the absorption coefficient that based on the Beer-Lambert's Law. Cr3+ ions gradually increase alone both the growth axis and the radial direction. The shape and ingredient of the inclusions were measured by means of Leitz ride field microscopy and scanning electron microscopy. Lane photos and X-ray omega scan show the good quality of as grown ruby. The optimized growth conditions were pointed out based on the observation. (C) 2004 Elsevier B.V. All rights reserved.

Relevância:

20.00% 20.00%

Publicador:

Resumo:

A finite-element model is employed to analysis the thermal environments in Temperature Gradient Technique (TGT) furnace during the growth of large-sized Nd:YAG crystal. The obtained results show that when the crucible is located at the lower position inside of the heater, a flatter solid-liquid interface is established, which makes it easier to obtain the core-free Nd:YAG crystal. Meanwhile, the lower crucible position can induce higher axial temperature gradient, which is beneficial to the release of latent heat. (c) 2007 WILEY-VCH Verlag GmbH & Co. KGaA, Weinheim.

Relevância:

20.00% 20.00%

Publicador:

Resumo:

According to the parameter requirements of a graded reflectivity mirror with a Gaussian profile, the layer structure and the mask pattern are designed using a graded-thickness middle layer. The mask and the automatic mask-switchover equipment are designed considering the actual requirement of the thin films and the specific deposit facility. The uniformity of the layer thickness is analyzed. The measurement results indicate that samples prepared with this technique are basically in accordance with the design parameter. The scattering effect between the material molecules and the mask, thickness errors, and the alignment error between the mask and the substrate are the main factors that influence the deposit result. (c) 2008 Society of Photo-Optical Instrumentation Engineers. [DOI: 10.1117/1.3027595]