Resumo:
Urea bridged organic-inorganic hybrid mesoporous SiO2 materials (U-BSQMs) were synthesized through a sol-gel procedure by co-condensation of bis(triethoxysilyl propyl) urea (BSPU) under basic conditions using cetyltrimethylammonium bromide (CTAB) as organic template. X-ray diffraction (XRD) and transmission electron microscopy (TEM) confirmed the mesoporous structure of the sample. Fourier-transform infrared spectroscopy (FT-IR), solid state CP-MAS NMR spectroscopy of Si-29 (Si-29, CP-MAS NMR) and C-13 (C-13 CP NMR) indicated that most of the Si-C bonds are unbroken during the synthesis process.
Resumo:
A novel biodegradable diblock copolymer, poly(L-cysteine)-b-Poly(L-lactide) (PLC-b-PLLA), was synthesized by ring-opening polymerization (ROP) of N-carboxyanhydride of beta-benzyloxycarbonyl-L-Cysteine (ZLC-NCA) with amino-terminated Poly(L-lactide) (NH2-PLLA) as a macroinitiator in a convenient way. The diblock copolymer and its precursor were characterized by H-1 NMR, Fourier transform infrared (FT-IR), gel permeation chromatography (GPC), and X-ray photoelectron spectroscopy (XPS) measurements. The length of each block polymer could be tailored by molecular design and the ratios of feeding monomers.
Resumo:
A novel series of compounds with different counter anions, i.e. 1-{[4-(4-nitrophenylazo)phenyloxy]}alkyl-3-methyl-1H-imidazol-3-ium bromide salts (C-n , n=3, 6, 10) and tetrafluoroborate salts (D-n , n=3, 6, 10), were synthesised by the incorporation of an imidazolium group into paraffin side chain-terminated 4-nitroazobenzene derivatives. Their chemical structures were determined by H-1 NMR, C-13 NMR, UV spectroscopy and elemental analysis.
Resumo:
A novel strategy in which the benzimidazole group and sulfonic group are simultaneously attached to an aromatic polymer has been reported in this paper. For this purpose, sulfonated poly(arylene ether ketone) copolymers containing carboxylic acid groups (SPAEK-x-COOH, x refers to the molar percentage Of sulfonated repeating units) are prepared by the aromatic nucleophilic polycondensation of sodium 5,5'-carbonyl-bis(2-fluobenzene-sulfonate) (SDFBP), 4,4'-difluorobenzophenone (DFBP) and phenolphthalin (PPL). Then the carboxylic acid groups attached to the SPAEK-x-COOH are transformed to benzimidazole units through condensation reactions (referred to as SPAEK-x-BI). Fourier transform infrared spectroscopy and H-1 NMR measurements are used to characterize and confirm the structures of these copolymers.
Resumo:
Four cyclometalated Pt(II) complexes, i.e., [(L-2)PtCl] (1b), [(L-3)PtCl] (1c), [(L-2)PtC CC6H5] (2b) and [(L-3)PtC CC6H5] (2c) (HL2 = 4-[p-(N-butyl-N-phenyl)anilino]-6-phenyl-2,2'-bipyridine and HL3 = 4-[p(-N,N'-dibutyl-N'-phenyl)phenylene-diamino]-phenyl-6-phenyl-2,2'-bipyridine), have been synthesized and verified by H-1 NMR, C-13 NMR and X-ray crystallography. Unlike previously reported complexes [(L-1)PtCl] (1a) and [(L-1)PtC CC6H5] (2a) (HL1 = 4,6-diphenyl-2,2'-bipyridine), intense and continuous absorption bands in the region of 300-500 nm with strong metal-to-ligand charge transfer ((MLCT)-M-1) (d pi(Pt) -> pi*(L)) transitions (epsilon similar to 2 x 10(4) dm(3) mol (1) cm (1)) at 449-467 nm were observed in the UV-Vis absorption spectra of complexes 1b, 1c, 2b and 2c.
Resumo:
Synthetic routes to aluminium ethyl complexes supported by chiral tetradentate phenoxyamine (salan-type) ligands [Al(OC6H2(R-6-R-4)CH2)(2){CH3N(C6H10)NCH3}-C2H5] 7: R = H ; 5, 8: R = Cl; 6, 9: R = CH3) are reported. Enantiornerically pure salan ligands 1-3 with (R,R) configurations at their cyclohexane rings afforded the complexes 4, 5, and 6 as mixtures of two diastereoisomers (a and b). Each diastereoisomer a was, as determined by X-ray analysis, monomeric with a five-coordinated aluminium central core in the solid state, adopting a cis-(O,O) and cis-(Me,Me) ligand geometry. From the results of variable-temperature (VT) H-1 NMR in the temperature range of 220-335 K, H-1-H-1 NOESY at 220 K, and diffusion-ordered spectroscopy (DOSY), it is concluded that each diastereoisomer b is also monomeric with a five-coordinated aluminium central core.
Resumo:
Cationic corn starch derivatives with a high degree of substitution are prepared in alkaline solution or in mixed media of organic solvent and water with different levels of the cationic reagent, 2,3-epoxypropyltrimethylammonium chloride. The starch cationization yield is investigated, and the results indicate that the degree of substitution (DS) of the samples depends on the reaction conditions and reaction media. The maximum DS values are up to 1.37 in 1,4-dioxane alkali ne-aqueous solution. Meanwhile, the structures of the cationic starch derivatives are characterized by elemental analyses, FTIR spectroscopy, X-ray diffraction, and C-13 NMR spectroscopy, as well as by SEM techniques.
Resumo:
Pyrazoline derivatives have been used widely in dyeing industry as fluorescent whitening agents due to their excellent capability. According to Schellhammer theory of the relation between chemical structure and fluorescent quality, six new fluorescent compounds were designed and synthesized which contained the benzothiazole group in the I-pyrazoline, the indole group in the 3-pyrazoline and the derivatives of phenyl in the 5-pyrazoline. The structure of target compounds was confirmed by IR, H-1 NMR, MS and elementary analysis. The fluorescence spectra showed that these compounds had good fluorescence. They could absorb ultraviolet light at near 353 nm. The fluorescence maximum emission wavelengths were about 430-443 nm. It was a kind of promising fluorescence compounds. The largest fluorescence emission wavelength and the fluorescence intensity were related to the substituted group of the compounds. When the 6-Br group was introduced into benzothiazole, the fluorescence emission wavelength exhibited a blue shift, and the fluorescence intensity increased.
Resumo:
A novel diamine, 1,4-bis [3-oxy-(N-aminophthalimide)] benzene (BOAPIB), was synthesized from 1,4-bis [3-oxy-(N-phenylphthalimide)] benzene and hydrazine. Its structure was determined via IR, H-1 NMR, and elemental analysis. A series of five-member ring, hydrazine-based polyimides were prepared from this diamine and various aromatic dianhydrides via one-step polycondensation in p-chlorophenol. The inherent viscosities of these polyimides were in the range of 0.17-0.61 dL/g. These polymers were soluble in polar aprotic solvents and phenols at room temperature. Thermogravimetric analysis (TGA) showed that the 5% weight-loss temperatures of the polyimides were near 450 degrees C in air and 500 degrees C in nitrogen. Dynamic mechanical thermal analysis (DMTA) indicated that the glass-transition temperatures (T(g)s) of these polymers were in the range of 265-360 degrees C. The wide-angle X-ray diffraction showed that all the polyimides were amorphous.
Resumo:
Ionic liquid monomer 1-vinyl-3-ethylimidazolium bromide (ViEtIM(+)Br(-)) was first used to copolymerize with acrylonitrile (AN) successfully under various conditions. This was achieved with azobisisobutyronitrile as the initiator and dimethyl sulfoxide as the solvent. The kinetics of this copolymerization were studied. The values of the monomer apparent reactivity ratios were calculated by the Kelen-Tudos method. The apparent reactivity ratios of ViEtIM(+)Br(-) (r(ViEtIM+Br-)) and AN (r(AN)) were similar at polymerization conversions of less than 10%, (r(AN) = 0.954, r(ViEtIM+Br-) = 0.976). The copolymers were obtained with high molecular weights and high hydrophilicides. The copolymers were characterized by H-1-NMR, differential scanning calorimetry, and thermogravimetric analysis. These copolymers may be potentially useful in the preparation of precursor fibers and carbon fibers.
Resumo:
A smart biodegradable cationic polymer (CBA-PEI) based on the disulfide bond-containing cross-linker cystamine bisacrylamide (CBA) and low molecular weight branched polyethylenimine (1800-Da, PEI1800) was successfully synthesized by Michael addition reaction in our recent study. Furthermore, a series of copolymers (CBA-PEI-PEG) with different PEGylation degree were obtained by the mPEG-SPA (5000-Da) reacting with CBA-PEI at various weight ratios directly. The molecular structures of the resulting polymers CBA-PEI and CBA-PEI-PEG were evaluated by nuclear magnetic resonance spectroscopy (H-1-NMR) and capillary viscosity measurements, all of which had successfully verified formation of the copolymers. The polymer/DNA complexes based on CBA-PEI and CBA-PEI-PEG were measured by dynamic light scattering and gel retardation assay. The results showed that the particle size and zeta potential of complexes were reduced with increasing amount of PEG grafting, even no particle formation. The particle size of CBA-PEI/DNA complexes was in range of 103.1 to 129.1 nm, and the zeta potential was in range of 14.2 to 24.3 mV above the 2:1 weight ratio. In the same measure condition, the particle size of CBA-PEI-PEG complexes was reduced to a range of 32.2 to 55 nm, and the zeta potential was in range of 9.3 to 13.8 mV at the 2:1 weight ratio.
Resumo:
A new process for the preparation of 3,5-dihydroxy-1-pentylbenzene, which is used as medicinal intermediate and raw material for the synthesis of HIV restrainer, is proposed in this paper. Technical 3,5-dimethoxybenzoic acid reacted with lithium hydride to form a salt (I) which acylated n-butyllithium directly to give 1-(3,5-dimethoxyphenyl)-1-pentanone (II) in 85.06% yield. Then (II) was reduced through a Wolff-K-Huangminglong reaction at 210 degrees C to give 3,5-dimethoxy-1-pentylbenzene (III). Finally, (III) refluxed with melt pyridine hydrochloride at 200 degrees C for 2 h to afford the target product 3,5-dihydroxy-1-pentylbenzene (IV). The total yield of (IV) amounted to 61.50% and its mass percentage was 98.22%. The products were characterized by means of IR, H-1-NMR, GC and HLPC-MS. The results indicated that this synthetic route was feasible, characterized by simple process and higher yield, and superior to the published ones.
Resumo:
A new vinyl acyl azide monomer, 4-(azidocarbonyl) phenyl methacrylate, has been synthesized and characterized by NMR and FTIR spectroscopy. The thermal stability of the new monomer has been investigated with FTIR and thermal gravimetry/differential thermal analysis (TG/DTA), and the monomer has been demonstrated to be stable below 50 degrees C in the solid state. The copolymerizations of the new monomer with methyl acrylate have been carried out at room temperature under Co-60 gamma-ray irradiation in the presence of benzyl 1-H-imidazole-1-carbodithioate. The results show that the polymerizations bear all the characteristics of controlled/living free-radical polymerizations, such as the molecular weight increasing linearly with the monomer conversion, the molecular weight distribution being narrow (< 1.20), and a linear relationship existing between In([M](0)/[M]) and the polymerization time. The data from H-1 NMR and FTIR confirm that no change in the acyl azide groups has occurred in the polymerization process and that acyl azide copolymers have been obtained. The thermal stability of the polymers has also been investigated with TG/DTA and FTIR.
Resumo:
A novel fluorescent dye labeled H-shaped block copolymer, (PMMA-Fluor-PS)(2)-PEO-(PS-Fluor-PMMA)(2), is synthesized by the combination of atom transfer radical polymerization (ATRP) and anionic polymerization (AP). To obtain the designated structure of the copolymer, a macroinitiator, 2,2-dichloro acetyl-PEO-2,2-dichloro acetyl (DCA-PEO-DCA), was prepared from DCAC and poly(ethylene oxide). The copolymer was characterized by H-1 NMR, GPC and fluorescence spectroscopy.
Resumo:
Order-disorder transition (ODT) behavior in eicosylated polyethyleneimine (PEI20C) comblike polymer obtained by grafting n-eicosyl group on polyethyleneimine backbone was systematically investigated by the combination of differential scanning calorimetry (DSC), wide-angle X-ray diffraction (WAXD), Fourier transform infrared (FTIR) spectroscopy as well as solid-state high resolution nuclear magnetic resonance (NMR) spectroscopy. DSC investigations showed two obvious transitions, assigned to the transitions (1) from orthorhombic to hexagonal and (2) from hexagonal to amorphous phase, respectively. These transitions are induced by the variations of alkyl side chain conformation and packing structure with temperature changing, which consequently lead to the destruction of original phase equilibrium. The ODT behavior can also be confirmed by spectroscopic methods like WAXD, FTIR and NMR. The ordered structure and the transition behavior of the alkyl side chains confined by the PEI backbone are obviously different from those of pristine normal alkanes. The transition mechanism of ODT and the origin of the phase transition behavior in PEI20C comblike polymer were discussed in detail in this paper.