504 resultados para Gd@C82
Resumo:
Calcium lanthanide oxyborate doped with rare-earth ions LnCa(4)O(BO3)(3):RE3+ (LnCOB:RE, Ln = Y, La, Gd, RE = Eu, Tb, Dy, Cc) was synthesized by the method of solid-state reaction at high temperature. Their fluorescent spectra were measured from vacuum ultraviolet (VUV) to visible region at room temperature. Their excitation spectra all have a broadband center at about 188 nm, which is ascribed to host absorption. Using Dorenbos' and J phi rgensen's work [P. Dorenbos, J. Lumin. 91 (2000) 91, R. Resfeld, C.K. J phi rgensen. Lasers and Excite States of Rare Earth [M], Springer, Berlin, 1977, p. 45], the position of the lowest 5d levels E(Ln,A) and charge transfer band E-ct were calculated and compared with their excitation spectra.Eu3+ and Tb3+ ions doped into LnCOB show efficient luminescence under VUV and UV irradiation. In this system, Ce3+ ions do not show efficient luminescence and quench the luminescence of Tb3+ ions when Tb3+ and Ce3+ ions are co-doped into LnCOB. GdCOB doped with Dy3+ shows yellowish white light under irradiation of 254 nm light for the reason that Gd ions transfer the energy from itself to Dy.
Resumo:
Ce3+ and/or Tb3+-doped (La,Gd)MgB5O10 nanocrystalline thin films were deposited on silica glass substrates by a sol-gel dip-coating process using triethyl borate B(OC2H5)(3) as the boron source. The results of XRD indicated that the films have fully crystallized after annealing at 800 degrees C. The films are transparent, uniform and crack free with a thickness of about 300 nm, consisting of particles with an average grain size of 50 nm. The luminescence and energy transfer properties of Ce3+ and Tb3+ have been studied in the films. It is confirmed that the excitation energy of Ce3+ transfers to the Gd3+, migrates over the Gd3+ sublattices, trapped by the Tb3+ and resulted in its characteristic green emission (D-5(4)-F-7(5) at 543 nm) in GdMgB5O10 nanocrystalline films as in the powder phosphors.
Resumo:
(Y, Gd) BO3:Eu3+ particles coated with nano-hematite were prepared by a facile method I for example (humid) solid phase reaction at room temperature. The resulted hematite-coated (Y, Gd)BO3:Eu3+ particles were characterized by scanning electron microscopy (SEM), energy dispersive spectrometer (EDS) analysis, X-ray diffraction (XRD), X-ray photoelectron spectra (XPS), and photoluminescence spectra (PL). The SEM and EDS analyses indicate that the particles are coated with a very thin layer of iron oxide. XPS results further confirmed that the coating was hematite, and the coating thickness was in nanometer range. XRD patterns showed that either the hematite coating was too thin or the content of hematite was too small, so that the XRD cannot detect it. The emission spectra illustrate that the peak near 580 nm disappears due to the coating of iron oxide, and when the coating is very thin, the ratio of D-5(0)-> F-7(2) to D-5(2)-> F-7(1) of coated particles is higher than that of uncoated ones, which indicates that the color purity of the phosphor is increased by coating nano-hematite.
Resumo:
The speciation and distribution of Zn(II) and the effect of Gd(III) on Zn(II) speciation in human blood plasma were studied by computer simulation. The results show that, in normal blood plasma, the most predominant species of Zn(II) are [Zn(HSA)] (58.2%), [Zn(IgG)](20.1%), [Zn(Tf)] (10.4%), ternary complexes of [Zn(Cit)(Cys)] (6.6%) and of [Zn(Cys)(His)H] (1.6%), and the binary complex of [Zn(CYS)(2)H] (1.2%). When zinc is deficient, the distribution of Zn(II) species is similar to that in normal blood plasma. Then, the distribution changes with increasing zinc(II) total concentration. Overloading Zn(II) is initially mainly bound to human serum albumin (HSA). As the available amount of HSA is exceeded, phosphate metal and carbonate metal species are established. Gd(III) entering human blood plasma predominantly competes for phosphate and carbonate to form precipitate species. However, Zn(II) complexes with phosphate and carbonate are negligible in normal blood plasma, so Gd(III) only have a little effect on zinc(II) species in human blood plasma at a concentration above 1.0x10(-4) M.
Resumo:
Thin film phosphors with compositions of RP1-xVxO4: A (R = Y, Gd, La; A = Sm3+, Et3+; x = 0, 0.5, 1) have been prepared by a Pechini sol-gel process. X-Ray diffraction, atomic force microscopy (AFM), photoluminescence excitation and emission spectra were utilized to characterize the thin film phosphors. The results of XRD showed that a solid solution formed in YVxP1-xO4: A film series from x = 0 to x = 1 with zircon structure, which also held for GdVO4: A film. However, LaVO4: A film crystallized with a different structure, monazite. AFM study revealed that the phosphor films consisted of homogeneous particles ranging from 90 to 400 nm depending on the compositions. Upon short ultraviolet excitation, the films exhibit the characteristic Sm(3+ 4)G(5/2)-H-6(J) (J=5/2, 7/2, 9/2) emission in the red region and Er3+ H-2(11/2), S-4(3/2)-I-4(15/2) emission in the green region, respectively With the increase of x values in YVxP1-xO4: SM3+ (Er3+) films, the emission intensity Of SM3+ (Er3+) increases due to the increase of energy transfer probability from VO43- to Sm3+ (Er3+). Due to the structural effects, the Sm3+ (Er3+) shows similar spectral properties in YVO4 and GdVO4 films, which are much different from those in LaVO4 film.
Resumo:
采用共沉淀法制备了稀土正磷酸盐荧光粉 ( La,Gd) PO4∶ RE3 +( RE=Eu,Tb) .红外光谱分析发现Gd PO4的红外光谱吸收峰与 La PO4一致 ,只是峰位向高波数方向移动 . ( La,Gd) PO4∶ RE3 +的真空紫外光谱特性研究表明 ,Gd3 +在能量传递过程中起中间体作用 .XPS研究揭示 ,La PO4的价带由 O2 -的 2 p能级构成 ,而 Gd PO4的价带则是由 O2 - 的 2 p能级和 Gd3 +的 4 f能级共同构成.
Resumo:
Macromolecular conjugates of two kinds of natural polysaccharides, that from Panax quinquefolium linn (PQPS) and Ganoderma applanatum pat (GAPS), with gadolinium-diethylenetriaminepenta-acetic acid (Gd-DTPA) have been synthesized and characterized by means of FTIR, elementary analysis and ICP-AES. Their stability was investigated by competition study with Ca2+, EDTA (ethylenediaminetetraacetic acid) and DTPA. Polysaccharide-bound complexes exhibit T-1 relaxivities of 1.5-1.7 times that of Gd-DTPA in D2O at 25degreesC and 9.4T. MR imaging of Sprague-Dawley (SD) rats showed remarkable enhancement in rat liver and kidney after i.v. injection of these two complexes: liver parenchyma 60.9+/-5.6%, 57.8+/-7.4% at 65-85 min; kidney 144.9+/-14.5%, 199.9+/-25.4% at 10-30 min for PQPS-GdDTPA, GAPS-Gd-DTPA at gadolinium dose of 0.083 and 0.082 mmol/kg, respectively. Our preliminary in vivo and in vitro study indicates that the two kinds of polysaccharide-bound complexes are potential tissue-specific contrast agents for MRI.
Resumo:
Four neutral gadolinium complexes of diethylenetriaminepentaacetic acid (DTPA)-bisamide derivatives have been synthesized and characterized. Their potential application as tissue-specific and low-osmolarity MRI contrast agents has been evaluated by in vitro and in vivo experiments. Their measured relaxivities in D2O, bovine serum albumin and human serum transferrin solutions showed favorable relaxation ability. In vivo studies have proven that Gd(DTPA-BDMA), Gd(DTPA-BIN), and Gd(cyclic-DTPA-1,2-pn) could be promising liver-specific MRI contrast agents and Gd(DTPA-BDMA), and Gd(cyclic-DTPA-1,2-pn) have favorable renal excretion capability. Among them, Gd(cyclic-DTPA-1,2-pn) is a more powerful hepatic contrast agent and Gd(DTPA-BIN) provides the stable imaging contrast for several hours. They also show a lower toxicity.
Resumo:
The speciation and distribution of Gd(III) in human interstitial fluid was studied by computer simulation. Meantime artificial neural network was applied to the estimation of log beta values of complexes. The results show that the precipitate species, GdPO4 and Gd-2(CO3)(3), are the predominant species. Among soluble species, the free Gd(III), [Gd(HSA)], [Gd(Ox)] and then the ternary complexes of Gd(III) with citrate arc main species and [Gd-3(OH)(4)] becomes the predominant species at the Gd(III) total concentration or 2.2x10(-2)mol/L.
Resumo:
A series of novel indigo light emitting long-lasting phosphors CdSiO3: RE3+ (RE = Y, La, Gd, Lu) was prepared by the conventional high-temperature solid-state method. The XRD, photoluminescence (PL) spectra and afterglow intensity decay were used to characterize the synthesized phosphors. These phosphors emitted indigo light and showed long-lasting phosphorescence. The phosphorescence can be seen with the naked eye in the dark clearly even after the 254-nm UV irradiation have been removed for more than 30 min.
Resumo:
Vacuum ultraviolet excitation spectra of phosphors (La,Gd)PO4:RE3+ (RE = Eu or Tb) and X-ray photoelectron spectra of LaPO4 and GdPO4 are investigated. The vacuum ultraviolet excitation intensity of (La,Gd)PO4:RE3+ is enhanced with the increasing of Gd3+ content, which implies that Gd3+ plays an intermediate role in energy transfer from host absorption band to RE3+. When Gd3+ is doped into LaPO4:Eu, charge transfer band (CT band) begins to shift to higher energy region and the overlap degree of CT band and the host absorption band gets greater with more Gd3+ doped into LaPO4. These results suggest that the dopant (Gd3+) gives an important influence on energy transfer efficiency. The top of LaPO4 valance band is formed by the 2p level of O2-, whereas that of GdPO4 valance band is formed by the 2p level of O2- and the 4f level of Gd3+, showing the differences in band structures between LaPO4 and GdPO4.
Resumo:
Photoluminescence characteristics and the energy transfer between Gd3+ and Eu2+ in BaLiF3,, matrix have been investigated. A series of concentrations of Gd3+ ion with a fixed Eu2+ concentration doped in BaLiF3 : Gd3+, Eu2+ has been studied. When the doping concentration for Gd3+ was 0.3%,, the system reached the highest energy transfer efficiency. Due to the competitive absorption for the Gd3+ and the Eu2+ ions in BaLiF3 : Gd3+ : Eu2+, when the doping concentration for Gd3+ ion exceeded 0.3 Vo, the continuously increasing concentration of Gd3+ ions caused the competitive absorption ratio for Gd3+ increasing and the emission intensity of Eu2+ decreasing. The energy transfer processes were discussed, while the transfer probability was calculated to be 1.35 X 10(5) s(-1).
Resumo:
Rare-earth and lead ions (Eu3+, Tb3+, Dy3+, Pb2+) doped Ca2Y8 (SiO4)(6)O-2 and Ca2Gd8(SiO4)(6)O-2 thin films have been dip- coated on silicon and quartz glass substrates through the sol- gel route. X- Ray diffraction (XRD), TG- DTA, scanning electron microscopy (SEM), atomic force microscopy (AFM), FT- IR and luminescence excitation and emission spectra as well as luminescence decays were used to characterize the resulting films. The results of XRD reveal that these films remain amorphous below 700 degreesC, begin to crystallize at 800 degreesC and crystallize completely around 1000 degreesC with an oxyapatite structure. The grain structure of the film can be seen clearly from SEM and AFM micrographs, where particles with various shapes and average size of 250 nm can be resolved. Eu3+ and Tb3+ show their characteristic red (D-5(0)-F-7(2)) and green (D-5(4) - F-7(5)) emission in the films with a quenching concentration of 10 and 6 mol% (of Y3+), respectively. The lifetime and emission intensity of Eu3+ increase with the temperature treatment from 700 to 1100 degreesC, while those of Tb3+ show a maximum at 800 degreesC. Energy transfer phenomena have been observed by activating the oxyapatite film host- lattice Ca2Gd8(SiO4)(6)O-2 with Tb3+ (Dy3+). In addition, Pb2+ can sensitize the Gd3+ sublattice in Ca2Gd8(SiO4)(6)O-2.
Resumo:
研究了 Ba Li F3中 Gd3+和 Eu2 +的光谱性质及 Gd3+对 Eu2 +的能量传递过程 ,讨论了传递机理 .Gd3+的含量 (物质的量分数 )为 0 .3 %时 ,传递效率最高 ,传递几率 PSA=1 .3 5× 1 0 5s- 1 .当 Gd3+的含量高于 0 .3 %时 ,由于 Gd3+ 和 Eu2 + 竞争吸收 Gd3+ 占优势 ,增加 Gd3+ 含量 ,竞争吸收比相应增加 ,Eu2 + 自身吸收光子数目减少 ,发射强度降低
Resumo:
笼内金属富勒烯以其独特的结构性质和潜在的应用价值而引起了人们极大的注意 [1~ 3] ,但因制备技术复杂、产率低以及将其从伴生的空心富勒烯中分离出来比较困难而使其研究受到很大的限制 .笼内金属富勒烯的分离提取始终是金属富勒烯研究的一个重要分支 .通常的方法是将放电得到的烟炱采用甲苯索氏提取的方法粗提 ,然后用高压液相色谱法分离得到纯品 ,笼内金属富勒烯的产率仅为烟炱的 0 .1 % [4~ 6] .我们改进了常规的提取方法 ,建立了一种新的提取方法—高温高压提取法 .具体的做法是采用甲苯索氏提取法从烟炱中提取出空心富勒烯和少量金属富勒烯 ,对剩余物用 1 ,2 ,4-氯苯高温高压法提取 .笼内金属富勒烯的产率增大了 5倍 ( 0 .5 % ) ,这一结果目前尚未见文献报道 .1 实验部分1 .1 金属富勒烯的合成 笼内金属富勒烯 Lnm@C2 n( Ln=Y,Tb,Gd)采用电弧放电法 ,在自制的一套电弧放电器中合成 .将 8mm× 2 0 0 mm的光谱纯级石墨棒钻出 5 mm× 1 5 0 mm的深孔 ,充填经预先处理的各种稀土氧化物和石墨粉的混合物 ,混合物中稀土原子和碳原子物质的量比为 1∶ 5 ...