373 resultados para D. optical properties
Resumo:
Gd1.99-xYxCe0.01SiO5 (Ce:GYSO) crystals (x = 0, 0.0995, 0.199) have been grown by the Czochralski (Cz) method. Crystal structure and the distribution coefficients of Ce have been determined for all three crystals. Spectroscopic measurements indicate that optical transmittance and luminescence intensity of Gd1.99-xYxCe0.01SiO5 (x = 0.0995, 0.199) crystals are Substantially higher than those of Ce:Gd2SiO5 (Ce:GSO), especially at x = 0.0995, which makes them good candidate materials for scintillation applications. The particularly important result is that the alloyed Ce:GYSO crystals can be grown easily by the Cz method and, unlike Ce:GSO, they do not undergo cleavage during the growth process or subsequent mechanical treatment. (c) 2005 Elsevier B.V. All rights reserved.
Resumo:
We report on the optical property changes for Ce3+-doped Gd2SiO5 crystal irradiated by a femtosecond (fs) laser. Absorption spectra showed that Ce-related color centers were formed in this crystal after an 800 nm fs laser irradiation. The annealing temperature-dependence of the refractive index and absorption intensity changes have been investigated. Furthermore, a new way of writing overlapped gratings inside the crystal by use of birefringence of fs laser beam in this crystal was proposed. (c) 2005 Elsevier B.V. All rights reserved.
Resumo:
High-quality Ce3+-doped Y3Al5O12 (YAG:Ce3+) phosphors were synthesized by a facile sol-gel combustion method. In this sol-gel combustion process, citric acid acts as a fuel for combustion, traps the constituent cations and reduces the diffusion length of the precursors. The XRD and FT-IR results show that YAG phase can form through sintering at 900 degrees C for 2 h. This temperature is much lower than that required to synthesize YAG phase via the solid-state reaction method. There were no intermediate phases such as YAlO3 (YAP) and Y4Al2O9 (YAM) observed in the sintering process. The average grain size of the phosphors sintered at 900-1100 degrees C is about 40 nm. With the increasing of sintering temperature, the emission intensity increases due to the improved crystalline and homogeneous distribution of Ce3+ ions. A blue shift has been observed in the Ce3+ emission spectrum of YAG:Ce3+ phosphors with increasing sintering temperatures from 900 to 1200 degrees C. It can be explained that the decrease of lattice constant affects the crystal field around Ce3+ ions. The emission intensity of 0.06Ce-doped YAG phosphors is much higher than that of the 0.04Ce and 0.02Ce ones. The red-shift at higher Ce3+ concentrations may be Ce-Ce interactions or variations in the unit cell parameters between YAG:Ce3+ and YAG. It can be concluded that the sol-gel combustion synthesis method provides a good distribution of Ce3+ activators at the molecular level in YAG matrix. (c) 2005 Elsevier B.V. All rights reserved.
Resumo:
Optical properties were investigated of ZnO thin films grown oil (100) gamma-LiAlO2 (LAO) substrates by pulsed laser deposition method. C-axis oriented ZnO film was grown oil (100) LAO substrate at the substrate temperature of 550 degrees C. The transmittances of the films were over 85%. Peaks attributed to excitons were seen in the absorption spectra, indicating that the thin films have high crystallinity. Photoluminescence spectra were observed at room temperature; the peak at 550 urn is ascribed to oxygen vacancies in the ZnO films caused by the diffusion of Li from the substrate into the film during deposition. (c) 2005 Elsevier B.V. All rights reserved.
Resumo:
ZnO thin films were deposited on the substrates of (100) gamma-LiAlO2 at 400, 550 and 700 degrees C using pulsed laser deposition (PLD) with the fixed oxygen pressure of 20 Pa, respectively. When the substrate temperature is 400 degrees C, the grain size of the film is less than 1 mu m observed by Leitz microscope and measured by X-ray diffraction (XRD). As the substrate temperature increases to 550 degrees C, highly-preferred c-orientation and high-quality ZnO film can be attained. While the substrate temperature rises to 700 degrees C, more defects appears on the surface of film and the ZnO films become polycrystalline again possibly because more Li of the substrate diffused into the ZnO film at high substrate temperature. The photoluminescence (PL) spectra of ZnO films at room temperature show the blue emission peaks centered at 430 nm. We suggest that the blue emission corresponds to the electron transition from the level of interstitial Zn to the valence band. Meanwhile, the films grown on gamma-LiAlO2 (LAO) exhibit green emission centered at 540 nm, which seemed to be ascribed to excess zinc and/or oxygen vacancy in the ZnO films caused by diffusion of Li. from the substrates into the films during the deposition.
Resumo:
We report the space selective precipitation of Pd nanoparticles in Pd2+ -doped silicate glass by ultrashort laser pulses irradiation and further annealing. Absorption spectra, transmission electron microscopy, refractive index measurement and Z-scan technique demonstrated that metallic Pd nanoparticles were precipitated in the glass sample after irradiation by an 800-nm femtosecond laser and subsequent annealing at 600 degrees C. We discuss a refractive index change and nonlinear absorption that combines the precipitation of Pd nanoparticles. Crown Copyright (c) 2005 Published by Elsevier B.V. All rights reserved.
Resumo:
beta-Ga2O3: Cr single crystals were grown by floating zone technique. Absorption spectra and fluorescence spectra were measured at room temperature. The values of field splitting parameter Dq and Racah parameter B were obtained by the peak values of absorption spectra. The value 10Dq/B=23.14 manifests that in beta-Ga2O3 crystals Cr3+ ions are influenced by low energy crystal field. After high temperature annealing in air, the Cr3+ intrinsic emission was enhanced and the green luminescence disappeared. The strong and broad 691 nm emission was obtained at 420 nm excitation due to the electron transition occurred from T-4(2) to (4)A(2). The studies manifest that the beta-Ga2O3 crystals have the potential application for tunable laser.
Resumo:
Nanocrystalline Zn0.95 - xNi0.05AlxO (x = 0.01, 0.02, 0.05 and 0.10) diluted magnetic semiconductors have been synthesized by an auto-combustion method. X-ray diffraction measurements indicate that all Al-doped Zn0.95Ni0.05O samples have the pure wurtzite structure. Transmission electron microscope analyses show that the as-synthesized powders are of the size 40 - 45 nm. High-resolution transmission electron microscope, energy dispersive spectrometer and X-ray photoemission spectroscope analyses indicate that Ni2+ and Al3+ uniformly substitute Zn2+ in the wurtzite structure without forming any secondary phases. The Al doping concentration dependences of cell parameters (a and c), resistance and the ratio of green emission to UV emission have the similar trends. (c) 2007 Elsevier B.V. All rights reserved.
Resumo:
Nonpolar a-plane (1120) ZnO thin films have been fabricated on gamma-LiAlO2 (302) substrates via the low-pressure metal-organic chemical vapor deposition. An obvious intensity variation of the E-2 mode in the Raman spectra indicates that there exhibits in-plane optical anisotropy in the a-plane ZnO thin films. Highly-oriented uniform grains of rectangular shape can be seen from the atomic force microscopy images, which mean that the lateral growth rate of the thin films is also anisotropic. It is demonstrated experimentally that a buffer layer deposited at a low temperature (200 degrees C) can improve the structural and optical properties of the epilayer to a large extent. (c) 2007 Elsevier B.V. All rights reserved.
Resumo:
We report the structural and optical properties of nonpolar m-plane GaN and GaN-based LEDs grown by MOCVD on a gamma-LiAlO2 (100) substrate. The TMGa, TMIn and NH3 are used as sources of Ga, In and N, respectively. The structural and surface properties of the epilayers are characterized by x-ray diffraction, polarized Raman scattering and atomic force microscopy (AFM). The films have a very smooth surface with rms roughness as low as 2nm for an area of 10 x 10 mu m(2) by AFM scan area. The XRD spectra show that the materials grown on gamma-LiAlO2 (100) have < 1 - 100 > m-plane orientation. The EL spectra of the m-plane InGaN/GaN multiple quantum wells LEDs are shown. This demonstrates that our nonpolar LED structure grown on the gamma-LiAlO2 substrate is indeed free of internal electric field. The current voltage characteristics of these LEDs show the rectifying behaviour with a turn on voltage of 1-3 V.