253 resultados para Cr : Yb : YAG crystal
Resumo:
For the first time, a high optical quality Yb3+-doped lutetium pyrosilicate laser crystal Lu2Si2O7 (LPS) was grown by the Czochralski (Cz) method. The segregation coefficient of ytterbium ion in Yb:LPS crystal detected by the inductively coupled plasma atomic emission spectrometer (TCP-AES) method is equal to 0.847. X-ray powder diffraction result confirms the C2/m phase monoclinic space group of the grown crystal and the peaks corresponding to different phases were indexed. The absorption and fluorescence spectra, as well as fluorescence decay lifetime of Yb3+ ion in LPS have been investigated. The absorption and fluorescence cross-sections of the transitions F-2(7/2) <-> F-2(5/2) of Yb3+ ion in LPS crystal have been determined. The advantages of the Yb:LPS crystal including high crystal quality, quasi-four-level laser operating scheme, high absorption cross-sections (1.33 x 10(-2) cm(2)) and particularly broad emission bandwidth (similar to 62 nm) indicated that the Yb:LPS crystal seemed to be a promising candidate used as compact, efficient thin chip lasers when LD is pumped at 940 and 980 nm due to its low-symmetry monoclinic structure and single crystallographic site. (c) 2007 Elsevier B.V. All rights reserved.
Resumo:
In this paper, single crystal of ytterbium (Yb) doped Ca-5(PO4)(3)F (FAP) has been grown along the c-axis by using the Czochralski method. The segregation coefficients of Yb3+ in the Yb:FAP crystal has been determined by ICP-AES method. The absorption spectrum, fluorescence spectrum and fluorescence lifetime of the Yb:FAP crystal has been also measured at room temperature. In the absorption spectra, there are two absorption bands at 904 and 982 nm, respectively, which are suitable for InGaAs diode laser pumping. The absorption cross-section (sigma(abs)) is 5.117 x 10(-20) cm(2) with an FWHM of 4 nm at 982 nm. The emission cross-section is (sigma(em)) 3.678 x 10(-20) cm(2) at 1042 nm. Favorable values of the absorption cross-section at about 982 nm are promising candidates for laser diode (LD) pumping. (c) 2005 Elsevier B.V. All rights reserved.
Resumo:
Yb:Y3Al5O12 (Yb:YAG) single crystals with Yb doping concentration 0.5 at.%, 5 at.%, 15 at.%, 25 at.%, 50 at.%, 100 at.% and Yb:YAlO3 (Yb:YAP) single crystals with Yb doping concentration 0.5 at.%, 5 at.%, 15 at.%, 30 at.% were grown by the Czochralski process. The fluorescence spectra of these crystals and the effects of self-absorption on the shape of the fluorescence spectra were studied. Through comparing the fluorescence spectra of Yb:YAG and Yb:YAP, all results indicate that the effects of self-absorption on the fluorescence spectra of Yb:YAP are remarkably stronger than that of Yb:YAG at the same Yb concentration. (c) 2006 Elsevier B.V. All rights reserved.
Resumo:
采用提拉法生长Y3Al5O12(YAG)晶体和Yb3+掺杂原子数分数分别为5%, 10%, 15%, 20%, 25%, 50%和100%的Yb∶Y3Al5O12(Yb∶YAG)晶体。系统表征和分析了Yb3+掺杂浓度对拉曼光谱的影响。随着Yb3+掺杂浓度的增加,晶体的振动模式没有明显的变化,晶体结构没有改变;在370 cm-1和785 cm-1附近,振动吸收峰的半峰全宽逐渐增大。分析得出,Yb3+掺杂浓度对晶体的晶格、对称性、荧光寿命均有影响,从而可能影响到晶体的光谱和激光性能。
Resumo:
采用热键合技术,制作中运用不同的工艺参量制作出12片Yb∶Y3Al5O12/Y3Al5O12(Yb∶YAG/YAG)复合晶体。利用偏光显微镜对其键合界面进行了观察,研究了样品的透射光谱,从而确定出复合晶体合适的制作工艺。通过透射光谱的形状和透射率来表征复合晶体键合界面的质量。研究表明Yb∶YAG/YAG复合晶体键合质量较好,可实现一体化。
Resumo:
Ytterbium-doped calcium pyroniobate single crystal has been grown for the first time. Spectral properties of Yb: Ca2Nb2O7 were investigated by emission and absorption spectra. Its cooperative luminescence and fluorescence lifetime were also studied. Yb ions in Ca2Nb2O7 showed very broad absorption and emission bandwidth and relatively large absorption and emission cross-sections. Along with other optical properties, this Yb-doped crystal would be a potential self-frequency doubling femtosecond laser gain material. (C) 2007 Published by Elsevier B.V.
Resumo:
A bulk crystal of Yb:Sc2SiO5 (Yb:SSO) with favorable thermal properties was successfully obtained by the Czochralski method. The energy level diagrams for Yb:SSO crystal were determined by optical spectroscopic analysis and semi-empirical crystal-field calculations using the simple overlap model. The full width at half maximum of the absorption band centering at 976 nm was calculated to be 24 nm with a peak absorption cross-section of 9.2x10(-21) cm(2). The largest ground-state splitting of Yb3+ ions is up to 1027 cm(-1) in a SSO crystal host. Efficient diode-pumped laser performance of Yb:SSO was primarily demonstrated with a slope efficiency of 45% and output power of 3.55 W.
Resumo:
采用热键合技术制备了Yb:Y3Al5O12/Y3Al5O12(Yb:YAG/YAG)复合晶体,对复合晶体进行了结构表征和键合质量检测,利用光学显微镜和扫描电镜观察了复合晶体横截面的形貌;在偏光显微镜下观察键合区域的应力,利用干涉条纹来表征复合晶体的光学均匀性;通过红外透过光谱的测量来检测复合晶体的键合质量.实验结果表明:热键合技术制备的Yb:YAG/YAG复合晶体键合界面处无界面缺陷,不存在复合界面空间过渡层,光学均匀性良好.
Resumo:
通过助熔剂固相反应法制备了5%Yb掺杂的硫氧化钇(Y2O2S)粉体。通过对其漫反射光谱和荧光光谱的测量,估算得Yb3+离子在Y2O2S晶格中的晶场分裂。由光谱数据计算得Yb3+离子的2F7/2能级在Y2O2S中的分裂值为709cm-1,适合于Yb3+离子的准三能级的激光运转。由5%Yb:Y2O2S的发射光谱拟合得出其峰位,峰高及峰宽。为了比较,相关的5%Yb:YAG的数据也被给出。
Resumo:
为了同时补偿固体增益介质的热致双折射及热透镜效应,进一步提高重复频率1 kHz激光二极管(LD)侧向抽运高平均功率电光调Q Nd:YAG激光器的输出功率,设计了一种完全消除热退偏损耗的双调Q开关谐振腔结构,此结构在传统调Q谐振腔的基础上沿着偏振片的退偏方向增加了一个调Q谐振支路,并使得激光从增益介质方向输出。实验结果表明,此激光器的单脉冲能量比单Q开关结构的非补偿腔输出能量高出74.7%。当侧面抽运的激光二极管输出脉冲能量达到307 mJ时,激光输出能量达到26.2 mJ,光-光转换效率为8.5%,光束发
Resumo:
For the first time, to the best of our knowledge, a radially polarized laser pulse was produced from a passively Q-switched Nd:YAG ceramic microchip laser with a piece of Cr4+:YAG crystal as the saturable absorber and multilayer concentric subwavelength grating as the polarization-selective output coupler. The averaged laser power reached 450 mW with a slope efficiency of 30.2%. The laser pulse had a maximum peak power of 759 W, a minimum pulse duration of 86 ns, and a 6.7 kHz repetition rate at 3.7 W absorbed pump power. The polarization degree of the radially polarized pulse was measured to be as high as 97.4%. Such a radially polarized laser pulse with a high peak power and a short width is important to numerous applications such as metal cutting. (C) 2008 Optical Society of America
Resumo:
Yb:YAG single crystals with Yb doping concentration 5.4, 16.3, 27.1, 53.6, and 100 at.% were grown by the Czochralski process. The effects of Yb concentration on the absorption spectra (190-1 100nm), fluorescence spectra under 940nm and X-ray excitation were studied. The concentration quenching of fluorescence was observed when the Yb doping concentration reaches to as high as 27.1 at.% for Yb:YAG. Under 940 nm excitation, the influence of the self-absorption at 969 and 1029 nrn on the fluorescence spectra is not evident when the Yb doping concentration is as high as 27.1 at.%. However, it can greatly change the shape of fluorescence spectra of Yb:YAG when the Yb doping concentration reaches to above 53.6 at.%. (c) 2005 Elsevier B.V. All rights reserved.
Resumo:
The dark-brown colored 5 at% Yb-doped YAlO3 (Yb:YAP) single crystal was grown successfully by temperature gradient technique (TGT) for the first time. The TGT-grown Yb:YAP crystal with the perovskite structure and excellent crystallization perfection were confirmed by the X-ray diffractions techniques. The dark-brown color of TGT-Yb:YAP crystal turned into the colorless after annealing in the air at 1200 degrees C for 10h. The absorption spectra, LD-excited infrared emission and X-ray excited luminescence spectra of the air-annealed Yb:YAP single crystal were investigated at the room temperature. The results indicate that the TGT-Yb:YAP single crystals can be used for the laser and scintillation applications. (c) 2005 Elsevier B.V. All rights reserved.
Resumo:
采用石墨电阻加热的温梯法生长了V:YAG晶体,晶体的不同部位呈现两种不同的颜色:浅绿色和黄褐色.通过对比分析不同颜色V:YAG晶体的室温吸收光谱,推断出石墨发热体高温下扩散出来的C可以起到还原作用,提高晶体中V^3+tetra离子的浓度,同时诱导了F心的形成.在1300℃下,对不同颜色的V:YAG晶体进行真空退火处理,发现处于八面体格位中的V^3+离子在热激发作用下与近邻的四面体格位Al^3+离子存在置换反应,由此产生一定浓度的四面体格位V^3+离子.同时,F心在退火过程中被完全消除,释放出来的自由电子被
Resumo:
采用提拉法生长了Yb掺杂原子数分数为0.5%的Yb:Y3Al5O12。(Yb2YAG)晶体,对晶体的吸收光谱和荧光光谱进行了分析。与Yb掺杂原子数分数为5%的Yb:YAG晶体进行了对比,得出采用940nm激光二极管(LD)抽运晶体最为合适。原子数分数为0.5%的Yb:YAG晶体相对于原子数分数为5%的Yb:YAG晶体白吸收效应的影响要小。测量了原子数分数为0.5%的Yb:YAG晶体的荧光寿命为0.95ms,与理论值很接近。因此采用原子数分数为0.5%的Yb:YAG晶体作为激光工作物质将有利于高效、小型集成