82 resultados para Atterberg settling tubes
Resumo:
A prototype of time-of-flight positron emission computed tomography (TOF-PET) has been developed for acquiring the coincident detection of 511 keV gamma-rays produced from positron annihilation. It consists of two 80.5 mmx80.5 mm LYSO scintillator arrays (composed of 35 x35 pixel finger crystals) with the position sensitive photomultiplier tubes R2487 as the readout. Each array is composed of 2 mm x2 mm x 15 mm finger crystals and the average pixel pitch is 2.30 mm. The measured results indicate that the TOF information has the potential to significantly enhance the image quality by improving the noise variance in the image reconstruction. The best spatial resolution (FWHM) of the prototype for the pairs of 511 keV gamma-rays is 1.98 mm and 2.16 mm in the x and y directions, respectively, which are smaller than the average pixel pitch of 2.30 mm.
Synthesis of carbon nanotube bundles with mesoporous structure by a self-assembly solvothermal route
Resumo:
A kind of carbon nanotube bundle has been synthesized by a simple one-step solvothermal reaction between Na and hexachlorobenzene (HCB) using NiCl2 as catalyst precursor. Before the reaction, NiCl2 was initially dispersed ultrasonically in cyclohexane then prereduced by Na at 230degreesC to produce small Ni particles in reduced state. The tubes thus-produced have a uniform outer diameter of about 20 nm, an inner diameter of 4 nm, and are highly ordered assembled as bundles which have a 2D hexagonal arrangement as proven by SAXS and TEM experiments.
Resumo:
细颗粒泥沙的絮凝或分散对土壤渗透性、土壤可蚀性有重要作用 ,是水土保持研究的重要内容。在 Ca Cl2 浓度为 0~ 1.0 mmol/L ,泥沙浓度为 10 g/L时 ,用吸管法研究了 Ca Cl2 对细颗粒泥沙絮凝沉降的影响。结果表明 :泥沙沉降分 2个阶段 ,分选沉降段和絮凝沉降段 ;在絮凝沉降段 ,Ca Cl2 浓度越大 ,絮凝沉降越快。但较高浓度时 ,细颗粒泥沙平均沉速反而随 Ca Cl2浓度增大而逐渐减小 ;泥沙浓度随时间呈指数衰减 ;细颗粒泥沙絮凝临界粒径为 0 .0 3mm。
Resumo:
在CaCl2和MgCl2浓度为0~1.0mmol/L,泥沙浓度为10g/L时,用吸管法研究了有机质、CaCl2和MgCl2对细颗粒泥沙静水絮凝沉降的影响,结果表明,去除有机质后,细颗粒泥沙絮凝沉降加快,其絮凝所需的最佳电解质浓度降低;CaCl2和MgCl2的絮凝能力无明显差异,有机质含量对其几乎没有影响;在相同盐度下,细颗粒泥沙的絮凝沉降速度随电解质摩尔浓度的增大而增大.
Resumo:
铝类絮凝剂对细颗粒泥沙絮凝沉降有重要作用 ,常应用于浑水澄清、农业污水处理等研究中。在AlCl3 浓度为 0~ 1 7mmol/L ,泥沙浓度为 1 0g/L时 ,用吸管法研究了AlCl3 对细颗粒泥沙絮凝沉降的影响 ,结果表明 :在液面下同一深度 ,泥沙浓度随时间呈指数衰减 ;悬液经多次搅拌后再沉降 ,其沉速减缓 ;当AlCl3 浓度为 0 9~ 1 7mmol/L时 ,出现明显的清浑水交界面 ,交界面随时间等速下降 ,平均沉速为 4 75 6cm/min ,对应的絮团平均粒径为 0 0 31 5mm ;土娄土絮凝临界粒径为 0 0 2 7mm。
Resumo:
通过对单厢式矩形断面、单厢式梯形断面、迷宫式、旋流式等 4种结构形成的沉沙池沉沙效率对比试验表明 ,以迷宫式沉沙池效果最佳 ,平均沉沙效率可达 88.3%。此种结构形式的断面尺寸为 1m、宽 0 .4m ,迷宫室底部比集水渠低 0 .2 m,迷宫分成 5个小厢室 ,每个厢室长 0 .146 m,沉沙池首部的静水池深 0 .2 5 m
Resumo:
在CaCl2 和MgCl2 浓度为 0~ 1.0mmol L ,泥沙浓度为 10g L时 ,本文用吸管法研究了有机质对细颗粒泥沙絮凝沉降的影响 ,结果表明 :在液面下同一深度 ,有机质并不影响泥沙浓度随时间呈指数衰减的变化规律。但去除有机质后 ,细颗粒泥沙絮凝的最佳电解质浓度降低 ;对于相同的电解质浓度 ,其絮凝沉降加快 ,泥沙平均沉速明显增大
Resumo:
Hollow carbon nanofibers with circular and rectangular opening were prepared by using electrospun silica fibers as templates. Silica fibers were synthesized by electrospinning, and they were coated with a carbon layer formed by thermal decomposition and carbonization of polystyrene under a nitrogen atmosphere. Hollow carbon nanofibers with circular and rectangular openings were then obtained after the silica core was etched by hydrofluoric acid. The carbon nanofibers with different morphologies also could be used as templates to fabricate silicon carbide fibers. The silicon carbide fibers with circular and rectangular openings could be obtained by using hollow carbon nanofibers and carbon belts as templates, respectively.
Resumo:
Nanocomposites based on poly(iminosebacoyl imino-decamethylene) (PA1010) and multiwall carbon nanotubes (MWNTs) were successfully prepared by melt blending technique. environmental scanning electron microscope micrographs of the fracture surfaces showed that not only is there an evenly dispersion of MWNTs throughout the PA1010 matrix but also a strongly interfacial adhesion with the matrix. The combined effect of more defects on MWNTs and low temperature buckling fracture is mainly responsible for the broken tubes. Differential scanning calorimeter results showed that the MWNTs acted as a nucleation agent and increased the crystallization rate and decreased crystallite size. In the linear region, rheological measurements showed a distinct change in the frequency dependence of storage modulus, loss modulus, and complex viscosity particularly at low frequencies. We conclude that the rheological percolation threshold might occur when the content of MWNTs is over 2 wt% in the composites.
Resumo:
High-performance polyimide fibers possess man), excellent properties, e.g., outstanding thermal stability and mechanical properties and excellent radiation resistant and electrical properties. However, the preparation of fibers with good mechanical properties is very difficult. In this report, a biphenvl polyimide from 3,3',4,4'-biphenyltetracarboxylic dianhydride and 4,4'-oxydianiline is synthesized in p-chlorophenol by one-step polymerization. The solution is spun into a coagulation bath of water and alcohol via dry-jet wet-spinning technology. Then, the fibers are drawn in two heating tubes. Thermal gravimetric analysis, thermal mechanical analysis, and dynamic mechanical analysis (DMA) are performed to study the properties of the fibers. The results show that the fibers have a good thermal stability at a temperature of more than 400degreesC. The linear coefficient of thermal expansion is negative in the solid state and the glass transition temperature is about 265degreesC. DMA spectra indicate that the tandelta of the fibers has three transition peaks, namely, alpha, beta, and gamma transition. The alpha and gamma transition temperature, corresponding to the end-group motion and glass transition, respectively, extensively depends on the applied frequency, while the beta transition does not.
Resumo:
An aromatic polyimide was synthesized via a one-step polycondensation reaction between biphenyltetracarboxylic dianhydride (BPDA) and 4,4'-oxydianiline (ODA) in p-chlorophenol. The polyimide (BPDA-ODA) solution dopes were spun into fibers by means of dry-jet wet spinning. The as-spun fibers were drawn and treated in heating tubes for improving the mechanical properties. The thermal treatment on the fibers resulted in a relatively high tensile strength and modulus. Thermal mechanical analysis (TMA) was employed to study the linear coefficient of thermal expansion (CTE). Thermal gravimetry analysis (TGA) spectra showed that the BPDA-ODA fibers possessed an excellent property of thermo-oxidative degradation resistance. The sonic modulus E-s of the polyimide fibers was measured.
Resumo:
As the leading nanodevice candidate, single-walled carbon nano-tubes (SWNTs) have potential therapeutic applications in gene therapy and novel drug delivery. We found that SWNTs can inhibit DNA duplex association and selectively induce human telomeric i-motif DNA formation by binding to the 5'-end major groove under physiological conditions or even at pH 8.0. SWNT binding to telomeric DNA was studied by UV melting, NMR, S1 nuclease cleavage, CD, and competitive FRET methods. These results suggest that SWNTs might have the intriguing potential to modulate human telomeric DNA structures in vivo, like biologically relevant B-A and B-Z DNA transitions, which is of great interest for drug design and cancer therapy.
Resumo:
Gradient colloidal crystals with a thickness gradient were prepared by the vertical deposition technique with vertically graded concentration suspensions. The thickness of the gradient colloidal crystal gradually changes at different positions along the specific gradient direction of the crystal. The thickness gradient was determined by the concentration gradient, depending on the initial colloidal concentration and the settling time. The optical transmission intensity at the dip wavelength can be tuned by changing the thickness of the colloidal crystals. The gradient colloidal crystals lead to a gradient of optical intensity at the dip in transmission light. The gradient of optical intensity at the dip increases as the thickness gradient of the colloidal crystal increases.
Resumo:
Graft chain propagation rate coefficients (k(p.g)) for grafting AA onto linear low density polyethylene (LLDPE) in the melt in ESR tubes have been measured via Fourier transform infrared (FTIR) spectroscopy and electron spin resonance (ESR) spectroscopy in the temperature range from 130 to 170 degrees C. To exclude the effect of homopolymerization on the grafting. the LLDPE was pre-irradiated in the air by electron beam to generate the peroxides and then treated with iodide solution to eliminating one kind of peroxides, hydroperoxide. The monomer conversion is determined by FTIR and the chain propagation free-radical concentration is deduced from the double integration of the well-resolved ESR spectra, consisting nine lines in the melt. The temperature dependence of k(p.g) is expressed:The magnitude of k(p.g) from FTIR and ESR analysis is in good agreement with the theoretical data deduced from ethylene-AA copolymerization, suggesting this method could reliably and directly provide the propagation rate coefficient. The comparison of k(p.g) with the data extrapolated from solution polymerization at modest temperature indicates that the extrapolated data might not be entirely fitting to discuss the kinetics behavior in the melt.
Resumo:
Fullerenes-extracted soot (FES) is the by-product of fullerenes production. Retention characteristics at different temperatures for 17 volatile organic compounds (VOCs) on FES are measured. The adsorption and desorption efficiencies for VOCs on FES adsorbent tubes range from 40.8 to 117%, most of them being 100+/-20%. The values are compared with Tenax GR, an adsorbent commonly used in environmental analysis. FES can be used as an adsorbent of low cost to collect VOCs in environmental samples. (C) 2000 Elsevier Science B.V. All rights reserved.