188 resultados para Solid phase reaction
Resumo:
A method with carbon nanotubes functioning both as the adsorbent of solid-phase extraction (SPE) and the matrix for matrix assisted laser desorption/ ionization mass spectrometry (MALDI-MS) to analyze small molecules in solution has been developed. In this method, 10 muL suspensions of carbon nanotubes in 50% (vol/vol) methanol were added to the sample solution to extract analytes onto surface of carbon nanotubes because of their dramatic hydrophobicity. Carbon nanotubes in solution are deposited onto the bottom of tube with centrifugation. After removing the supernatant fluid, carbon nanotubes are suspended again with dispersant and pipetted directly onto the sample target of the MALDI-MS to perform a mass spectrometric analysis. It was demonstrated by analysis of a variety of small molecules that the resolution of peaks and the efficiency of desorption/ ionization on the carbon nanotubes are better than those on the activated carbon. It is found that with the addition of glycerol and sucrose to the dispersant, the intensity, the ratio of signal to noise (S/N), and the resolution of peaks for analytes by mass spectrometry increased greatly. Compared with the previously reported method by depositing sample solution onto thin layer of carbon nanotubes, it is observed that the detection limit for analytes can be enhanced about 10 to 100 times due to solid-phase extraction of analytes in solution by carbon nanotubes. An acceptable result of simultaneously quantitative analysis of three analytes in solution has been achieved. The application in determining drugs spiked into urine has also been realized. (C) 2004 American Society for Mass Spectrometry.
Resumo:
Sm3Fe26.7V2.3N4 nitrides and Sm3Fe26.7V2.3Cy carbides have been synthesized by gas-solid phase reaction. Their hard magnetic properties have been investigated by means of additional ball-milling at room temperature. The saturation magnetization of Sm3Fe26.7V2.3N4 almost decreases linearly with increasing ball-milling time t, but that of Sm3Fe26.7V2.3Cy has no obvious change when the ball-milling time increases from t = 1 to 28 h. As a preliminary result, the maximum remanence B-r of 0.94 and 0.88 T, the coercivity mu(0i)H(C) of 0.75 and 0.25 T, and the maximum energy product (BH) of 108.5 and 39.1 kJ/m(3) for their resin-bonded permanent magnets are achieved, respectively, by ball-milling at 293 K. (C) 1999 Published by Elsevier Science B.V. All rights reserved.
Resumo:
(Y, Gd) BO3:Eu3+ particles coated with nano-hematite were prepared by a facile method I for example (humid) solid phase reaction at room temperature. The resulted hematite-coated (Y, Gd)BO3:Eu3+ particles were characterized by scanning electron microscopy (SEM), energy dispersive spectrometer (EDS) analysis, X-ray diffraction (XRD), X-ray photoelectron spectra (XPS), and photoluminescence spectra (PL). The SEM and EDS analyses indicate that the particles are coated with a very thin layer of iron oxide. XPS results further confirmed that the coating was hematite, and the coating thickness was in nanometer range. XRD patterns showed that either the hematite coating was too thin or the content of hematite was too small, so that the XRD cannot detect it. The emission spectra illustrate that the peak near 580 nm disappears due to the coating of iron oxide, and when the coating is very thin, the ratio of D-5(0)-> F-7(2) to D-5(2)-> F-7(1) of coated particles is higher than that of uncoated ones, which indicates that the color purity of the phosphor is increased by coating nano-hematite.
Resumo:
The phosphors MMgF(4)(M = Ca, Sr, Ba) doped with samarium ions are synthesized in different atmospheres using solid phase reaction at high temperature. Samarium has been first stabilized in the divalent state in SrMgF4 and BaMgF4 matrices. Effects of matrices on the valent state of samarium ions are briefly discussed.
Resumo:
On the basis of a brief review of the continuum theory for macroscopic descriptions and the kinetic theory for microscopic descriptions in solid/liquid two-phase flows, some suggestions are presented, i.e. the solid phase may be described by the Boltzmann equation and the liquid phase still be described by conservation laws in the continuum theory. Among them the action force on the particles by the liquid fluid is a coupling factor which connects the phases. For dilute steady solid/liquid two-phase flows, the particle velocity distribution function can be derived by analogy with the procedures in the kinetic theory of gas molecules for the equilibrium state instead of being assumed, as previous investigators did. This done, more detailed information, such as the velocity probability density distribution, mean velocity distribution and fluctuating intensity etc. can be obtained directly from the particle velocity distribution function or from its integration. Experiments have been performed for dilute solid/liquid two-phase flow in a 4 x 6 cm2 sized circulating square pipe system by means of laser Doppler anemometry so that the theories can be examined. The comparisons show that the theories agree very well with all the measured data.
Resumo:
Nd2CexO3+2x (x = 2.25, 2.5, 2.75, 3.0) were synthesized by solid-state reaction, and their phase stabilities and thermophysical properties were investigated. The X-ray diffraction (XRD) results indicated that Nd2CexO3+2x with fluorite structure were stable after long-term annealing at 1673 K. They have higher thermal expansion coefficients (TECs) than yttria-stabilized zirconia (YSZ) which is the typical thermal barrier coating (TBC) material, especially the thermal expansion as a function of temperature is parallel to that of the nickel-based superalloy.
Effects of Y2O3 addition on the phase evolution and thermophysical properties of lanthanum zirconate
Resumo:
Lanthanum zirconate (La2Zr2O7, LZ) powders with the addition of various Y2O3 contents for potential thermal barrier coatings (TBCs) application were synthesized by solid-state reaction. The structure evolution, sintering-resistance and thermophysical properties of the synthesized powders and sintered ceramics were systematically studied. X-ray diffraction (XRD) results indicate that LZ containing 3-12 wt.% Y2O3 mainly keeps a pyrochlore-type structure, and two new phases of LaYO3 and Y0.18Zr0.82O1.91 are also detected. Raman spectra confirm that the higher the Y2O3 content, the easier is the formation of LaYO3.
Resumo:
A series of solid electrolytes Ce1-xSmxO2-y (x=0similar to0.6) were prepared by sol-gel method. XRD measurement showed that single-phase solid solution was formed in all investigated ranges at 160 degreesC, which is a significantly lower synthesis temperature compared to traditional solid state reaction. High temperature X-ray, ESR, and Raman scattering were used to characterize the samples. ESR measurement showed that ESR with sample irradiated by high-energy particle is an effective way to study the defect structure. These changes in the Raman spectrum are attributed to O vacancies, which are introduced into the lattice when tetravalent Ce4+ is substituted by trivalent Sm3+.
Resumo:
A distorted layered perovskite compound BaTb2Mn2O7 was synthesized by the solid state reaction in pure argon. There is a structural phase transition in the BaTb2Mn2O7 compound. The phase transition was characterized by the DSC and high temperature Xray diffraction. The heat capacity of BaTb2Mn2O7 was calculated. The thermal anomaly corresponding to the phase transition was observed at about 740K. The lattice parameters were calculated by the CELL program for BaTb2Mn2O7, It has Tb-type orthorhombic symmetry with a = 0.3908 nm, b = 0.3866 nm, c = 2.0163 nm, and space group Immm at room temperature. With the increase of temperature, the lattice parameters gradually increase until 673K. From 723K to 973K, the compound translates to tetragonal with a = 0.39078 nm, c = 2.0277 nm and S.G. I4/mmm. This result is fairly in accordance with that of heat capacity.
Resumo:
Recent advances in the gas - phase reaction of aromatics with cationic electrophiles are reviewed. The overall substitution reaction is analyzed in terms of its elementary steps. Mechanistic studies have been focused on the structure and reactivity of covalent and non - covalent ionic intermediates, which display a rich chemistry and provide benchmark reactivity models. Particular attention has been devoted to proton transfer reactions, which may occur intra or intermolecularly in arenium intermediates.
Resumo:
High-quality Ce3+-doped Y3Al5O12 (YAG:Ce3+) phosphors were synthesized by a facile sol-gel combustion method. In this sol-gel combustion process, citric acid acts as a fuel for combustion, traps the constituent cations and reduces the diffusion length of the precursors. The XRD and FT-IR results show that YAG phase can form through sintering at 900 degrees C for 2 h. This temperature is much lower than that required to synthesize YAG phase via the solid-state reaction method. There were no intermediate phases such as YAlO3 (YAP) and Y4Al2O9 (YAM) observed in the sintering process. The average grain size of the phosphors sintered at 900-1100 degrees C is about 40 nm. With the increasing of sintering temperature, the emission intensity increases due to the improved crystalline and homogeneous distribution of Ce3+ ions. A blue shift has been observed in the Ce3+ emission spectrum of YAG:Ce3+ phosphors with increasing sintering temperatures from 900 to 1200 degrees C. It can be explained that the decrease of lattice constant affects the crystal field around Ce3+ ions. The emission intensity of 0.06Ce-doped YAG phosphors is much higher than that of the 0.04Ce and 0.02Ce ones. The red-shift at higher Ce3+ concentrations may be Ce-Ce interactions or variations in the unit cell parameters between YAG:Ce3+ and YAG. It can be concluded that the sol-gel combustion synthesis method provides a good distribution of Ce3+ activators at the molecular level in YAG matrix. (c) 2005 Elsevier B.V. All rights reserved.
Resumo:
Y4Al2O9:EU3+ phosphor was synthesized through a sol-gel combustion method. The Y4Al2O9 phase can form through sintering at 800 degrees C. This temperature is much lower than that required via the solid state reaction method. The average grain size of the phosphor was about 30 run. Compared with the amorphous phosphor, the charge transfer band of crystalline phosphor shows a blue shift. The emission Of Y4Al2O9:Eu3+ indicates the existence of two luminescent centers, in agreement with the crystal structure of Y4Al2O9. Higher doping concentration could be realized in Y4Al2O9 nanocrystal host lattice. This indicates that the sol-gel combustion synthesis method can increase emission intensity and quenching concentration due to a good distribution of EU3+ activators in Y4Al2O9 host. (c) 2005 Elsevier B.V. All rights reserved.
Resumo:
采用提拉法成功生长了氮化镓和氧化锌基外延薄膜晶格匹配的ScAlMgO4单晶衬底材料,晶体呈透明白色,尺寸为Ф30mm×59mm,表面部分沿解理面有裂纹.粉末X射线衍射(XRD)分析表明经1400℃固相反应烧结的原料基本合成了ScAlMgO4多晶相.初步的偏光显微镜观察、晶体的粉末XRD表征、透过光谱和双晶摇摆测试表明晶体具有较好的光学性质和结晶质量.研究表明晶体本身的层状结构、较大的温度梯度和热应力的不均匀性是生长过程中引起晶体开裂的几个主要原因.