Resumo:

Spherical MCM-41 particles with a diameter of about 150 nm have been successfully coated with CaWO4:Ln (Ln = Eu3+, Dy3+, Sm3+, Er3+) phosphor layers through a simple Pechini sol-gel process. The obtained CaWO4:Ln@MCM-41 composites, which kept the mesoporous structure of MCM-41 and the luminescent properties of phosphors, were investigated as a drug delivery system using aspirin (ASPL) as a model drug.

Relevância:

60.00% 60.00%

Publicador:

Resumo:

Several Chiral BINOL functionalized mesoporous silicas were prepared by post grafting of organosilane derivatives of (S)-BINOL (1,1'-bi-2-naphthol) on SBA-15 and characterized by C-13 CP/MAS NMR, FT-IR, UV-visible absorption spectra, elemental analysis, powder XRD, nitrogen adsorption-desorption isotherms and TEM techniques. Their catalytic properties were demonstrated in enantioselective Morita-Baylis-Hillman reaction of 3-phenylpropanal and cyclohexenone.

Relevância:

60.00% 60.00%

Publicador:

Resumo:

Ordered mesoporous silica (MCM-41) particles with different morphologies were synthesized through a simple hydrothermal process. Then these silica particles were functionalized with luminescent YVO4:EU3+ layers via the Pechini sol-gel process. The obtained YVO4:Eu3+ and MCM-41 composites, which maintained the mesoporous structure of MCM-41 and the red luminescence property of YVO4:Eu3+ were investigated as drug delivery systems using ibuprofen (IBU) as model drug. The physicochemical properties of the samples were characterized by X-ray diffraction (XRD), Fourier transform-infrared spectroscopy (FT-IR), scanning electron microscopy (SEM), transmission electron microscopy (TEM), N-2 adsorption, and photoluminescence (PL) spectra, respectively.

Relevância:

60.00% 60.00%

Publicador:

Resumo:

The crystal structure of a ternary Tm(DBM)(3)phen complex (DBM - dibenzoylmethane; phen = 1. 10-phenanthroline) and the synthesis of hybrid mesoporous material in which the complex covalently bonded to mesoporous MCM-41 are reported. Crystal data: Tm(DBM)(3)phen C59H47N2O7Tm, monoclinic P21/c, a = 19.3216(12) A, b = 10.6691(7) A, c = 23.0165(15)A, alpha = 90, beta = 91.6330(10), gamma = 90, V = 4742.8(5) A(3), Z = 4. The properties of the Tm(DBM)(3)phen complex and the corresponding hybrid mesoporous material [Tm(DBM)(3)phen-MCM-41] have been studied. The results reveal that the Tm(DBM)(3)phen complex is successfully covalently bonded to MCM-41.

Relevância:

60.00% 60.00%

Publicador:

Resumo:

Ordered N-methylimidazolium functionalized mesoporous silica (SBA-15) anion exchangers were directly synthesized by co-condensation of tetraethoxysilane with 1-methyl-3(triethoxysilylpropyl)imidazolium chloride. The prepared samples with rod-like morphology showed high surface areas (> 400 m(2) g(-1)), well-ordered pores (> 58 angstrom), and excellent thermal stability up to 387 degrees C. The adsorption behaviors of Cr(VI) from aqueous solution on the anion exchangers were studied using the batch method. The anion exchangers had high adsorption capacity ranging from 50.8 to 90.5 mg g(-1), over a wider pH range (1-8) than amino functionalized mesoporous silica. The adsorption rate was fast, and the maximum adsorption was obtained at pH 4.6. The adsorption data for the anion exchangers were consistent with the Langmuir isotherm equation. Most active sites of the anion exchangers were easily accessible. The mixed solution of 0.1 mol L-1 NH3 center dot H2O and 0.5 mol L-1 NH4Cl was effective desorption solution, and 95% of Cr(VI) could be desorbed.

Relevância:

60.00% 60.00%

Publicador:

Resumo:

Luminescence functionalization of ordered mesoporous MCM-41 silica was realized by depositing a YVO4:Eu3+ phosphor layer on its surface via the Pechini sol-gel process. This material, which combines the mesoporous structure of MCM-41 and the strong red luminescence property of YVO4: Eu3+, has been studied as a host carrier for drug delivery/release systems. The structure, morphology, texture and optical properties of the materials were well characterized by x-ray diffraction ( XRD), Fourier infrared spectroscopy ( FT-IR), transmission electron microscopy ( TEM), N-2 adsorption and photoluminescence ( PL) spectra. The results indicated that the specific surface area and pore volume of MCM-41, which were directly correlated to the drug-loading amount and ibuprofen ( IBU) release rate, decreased in sequence after deposition of YVO4:Eu3+ and loading of IBU as expected. The IBU-loaded YVO4:Eu3+@ MCM-41 system still showed red luminescence under UV irradiation ( 365 nm) and a controlled release property for IBU. In addition, the emission intensity of Eu3+ increases with an increase in the cumulative released amount of IBU, making the extent of drug release easily identified, tracked and monitored by the change of luminescence, which demonstrates its potential application in drug delivery/release systems.

Relevância:

60.00% 60.00%

Publicador:

Resumo:

An efficient, productive, and low-cost aerosol-assisted self-assembly process has been developed to produce organically modified mesoporous silica particles via a direct co-condensation of silicate species and organosilicates that contain nonhydrolyzable functional groups in the presence of templating surfactant molecules. Different surfactants including cetyltrimethylammonium bromide, nonionic surfactant Brij-56, and triblock copolymer P123 have been used as the structure-directing agents. The organosilanes used in this study include tridecafluoro-1, 1,2,2-tetrahydrooctyltriethoxysilane, methytriethoxysilane, vinyltrimethoxysilane, and 3-(trimethoxysilyl)propyl methacrylate. X-ray diffraction and transmission electron microscopy studies indicate the formation of particles with various mesostructures. Fourier transform infrared and solid-state nuclear magnetic resonance spectra confirm the organic ligands are covalently bound to the surface of the silica framework. The porosity, pore size, and surface area of the particles were characterized using nitrogen adsorption and desorption measurements.

Relevância:

60.00% 60.00%

Publicador:

Resumo:

The catalytic behavior of Mo-based zeolite catalysts with different pore structure and size, particularly with 8 membered ring ( M R), 10 M R, coexisted 10 and 12 M R, and 12 M R, was studied in methane aromatization under the conditions of SV=1500 ml/(g.h), p=0.1 MPa and T = 973 K. It was found that the catalytic performance is correlated with the pore structure of the zeolite supports. The zeolites that possess 10 MR or 10 and 12 MR pore structure with a pore diameter equal to or slightly larger than the dynamic diameter of benzene molecule, such as ZSM-5, ZSM-11, ZRP-1 and MCM-22, are fine supports. Among the tested zeolite supports, MCM-22 exhibits the highest activity and selectivity for benzene. A methane conversion of 10.5% with benzene selectivity of 80% was achieved over Mo/MCM-22 catalyst. The Mo/ERS-7 catalyst with 8 MR (0.45 nm) does not show any activity in methane dehydro-aromatization, while Mo/JQX-1 and Mo/SBA-15 catalysts with 12 MR pore exhibit little activity in the reaction. It can be concluded that the zeolites with 10 MR pore or coexisted 10 and 12 MR, having pore size equal to or slightly larger than the dynamic diameter of benzene molecule, are fine supports for methane activation and aromatization.

Relevância:

60.00% 60.00%

Publicador:

Resumo:

A new post-grafting process, consisting of two steps of substrate preparation and sol - gel post-grafting, has been developed to prepare titanium-doped mesoporous SBA-15 material with a double-layered structure and locally concentrated titanium content at the inner pore surface. With this novel technique, the single phased and originally ordered mesostructures can be well conserved; in the conventional direct synthesis they can be partially damaged when the frameworks are doped with high content heteroatoms. Titanium species exist in an isolated, tetrahedral structure and are localized at the pore surface; this is beneficial to both reactant access and product release. Characterization with XRD, N-2 adsorption/desorption isotherms, HREM/ EDS, ICP, UV - Vis, and the newly developed UV - Raman spectroscopy confirm these results. Preliminary catalytic tests with the selective epoxidation of cyclohexene show good catalytic activity. Among them, sample TiSBA-15-10 with a Si : Ti molar ratio of 10 shows a TON value of 75 and a highest product ( epoxide) yield of 55%.

Relevância:

20.00% 20.00%

Publicador:

Resumo:

通过接近玻璃转变温度的等温退火获得不同弛豫状态的Zr64.13Cu15.75Ni10.12Al10块体非晶合金样品。利用维氏显微硬度计和洛氏硬度计研究结构弛豫对合金硬度和压痕周围剪切带特征的影响规律。结果表明:在590K等温退火处理使Zr64.13Cu15.75Ni10.12Al10块体非晶合金发生焓弛豫行为,其维氏显微硬度随退火时间的延长较快增加后趋于稳定,而大载荷洛氏硬度对结构弛豫不敏感。通过洛氏压痕周围剪切带特征的研究,定量比较了结构弛豫对剪切带间距、数量的影响规律。

Relevância:

20.00% 20.00%

Publicador:

Resumo:

采用共沉淀法先合成出氢氧化物前驱体Ni0.85-xCo0.15Mnx(OH)2,其中X=0、0.1、0.2和0.4,前驱体与Li2CO3在空气气氛中固相烧结制得正极材料LiNi0.85-xCo0.15MnxO2。用XRD、SEM研究了锰含量对材料结构和形貌的影响。研究发现,LiNi0.85Co0.15O2的X射线衍射图中存在微量第二相,而锰掺杂有利于减小反应过程中锂离子损失和镍离子占据锂位,容易形成有序层状结构材料。随着Mn离子替代Ni离子量的增加,晶胞参数a减小,晶胞参数c、c/a及I003/I104值增大。SEM结果表明前驱体和最终产物形貌均随锰含量增加颗粒均匀性增强,粒子尺寸变小,粒径分布变窄。

Relevância:

20.00% 20.00%

Publicador:

Resumo:

Three kinds of Er3+-doped tellurite glasses with different hydroxyl groups are prepared by the conventional melt-quenching method. Infrared spectra are measured to estimate the exact content of OH- groups in samples. The maximum phonon energy in glasses are obtained by measuring the Raman scattering spectra. The strength parameters Omega(t) (t = 2, 4, 6) for all the samples are calculated and compared. The nonradiative decay rate of the Er3+ I-4(13/2) -> I-4(15/2) transition are calculated for the glass samples with different phonon energy and OH- group contents. Finally, the effect of OH- groups on fluorescence decay rate of Er3+ is analysed, the constant KOH-Er Of TWN, TZPL and TZL glasses are calculated to be 9.2 x 10(-19) cm(4)s(-1), 5.9 x 10(-19) cm(4)s(-1), and 3.5 x 10(-19) cm(4)s(-1), respectively.

Relevância:

20.00% 20.00%

Publicador:

Resumo:

A series of zinc tellurite glasses of 75TeO(2)-20ZnO-(5-x)La2O3-xEr(2)O(3) (x=0.02, 0.05, and 0.1 mol%) with the different hydroxl groups were prepared by the conventional melt-quenching method. Infrared spectra were measured in order to estimate the exact content of OH- groups in samples. The observed increase of the fluorescence lifetime with the oxygen bubbling time has been related to the reduction in the OH- content concentration as evidenced by IR transmission spectra. Various nonradiative decay rates from I-4(13/2) of Er3+ with. the change of OH content were determined from the fluorescence lifetime and radiative decay rates were calculated on the basis of Judd-Ofelt theory. (c) 2005 Elsevier B.V. All rights reserved.

Relevância:

20.00% 20.00%

Publicador:

Resumo:

Yb: YAlO3 (YAP) (15 at %) and Yb: Y3Al5O12 (YAG)(15 at %) have been grown using the Czochralski method. Their absorption and fluorescence spectra were measured at room temperature and important spectroscopic parameters were calculated. Through the comparison of spectroscopic parameters of Yb:YAP and Yb: YAG, all results indicate that 15 at % Yb:YAP crystal is a potential candidate used for compact, efficient thin chip lasers when the laser output wavelength is 1012 or 103 8 nm. (C) 2004 Elsevier B.V. All rights reserved.