Poly(vinyl acetate-co-vinyl alcohol) copolymers (P(VAc-co-VA)) were synthesized by hydrolysis-alcoholysis of PVAc. The miscibility, crystallization, and morphology of poly(P-hydroxybutyrate) (PHB) and P(VAc-co-VA) blends were studied by differential scanning calorimetry, optical microscopy (OM), and SAXS. It is found that the P(VAc-co-VA)s with vinyl alcohol content of 9, 15, and 22 mol % will form a miscible phase with the amorphous part of PHB in the solution-cast samples. The melting-quenched samples of PHB/P(VAc-co-VA) blends with different vinyl alcohol content show different phase behavior. PHB and P(VAc-co-VA9) with low vinyl alcohol content (9% mel) will form a miscible blend in the melt state. PHB and P(VAc-co-VA15) with 15 mol % vinyl alcohol will not form miscible blends while PHB/P(VAc-co-VA15) blend with 20/80 composition will form a partially miscible blend in the melt state. PHB and P(VAc-co-VA22) with 22 mol % vinyl alcohol are not miscible in the whole composition range. The single glass transition temperature of the blends within the whole composition range suggests that PHB and P(VAc-co-VA9) are totally miscible in the melt. The crystallization kinetics was studied from the whole crystallization and spherulite growth for the miscible blends. The equilibrium melting point of PHB in the PHB/P(VAc-co-VA9) blends, which was obtained from DSC results using the Hoffman-Weeks equation, decreases with the increase in P(VAc-co-VA9) content. The negative value of the interaction parameter determined from the equilibrium melting point depression supports the miscibility between the components. The kinetics of spherulitic crystallization of PHB in the blends was analyzed according to nucleation theory in the temperature range studied in this work. The best fit of the data to the kinetic theory is obtained by employing WLF parameters and the equilibrium melting points obtained by DSC. The addition of P(VAc-co-VA) did not affect the crystalline structure of PHB, as shown by the WAXD results. The long periods of blends obtained from SAXS increase with the increase in P(VAc-co-VA) content. It indicates that the amorphous P(VAc-co-VA) was rejected to interlamellar phase corporating with the amorphous part of PHB.

Relevância:

100.00% 100.00%

Publicador:

Resumo:

The multilayer Langmuir-Blodgett (LB) films of pr,ly 3-(2-(5-chlorobenzotriazole)ethyl) thiophene (PCBET) blended with amphibious arachidic acid (AA) were prepared and characterized. The photoluminescence intensity of the blend film was enhanced as the AA increased by a certain amount. The PCBET excimers were not formed in the blend LB films.

Relevância:

100.00% 100.00%

Publicador:

Resumo:

The miscibility and crystallization behavior of poly(beta-hydroxybutyrate) (PHB) and poly(p-vinylphenol) (PVPh) blends were studied by differential scanning calorimetry and optical microscopy (OM). The blends exhibit a single composition-dependent glass transition temperature, characteristic of miscible systems, A depression of the equilibrium melting temperature of PHB is observed. The interaction parameter values obtained from analysis of the melting point depression are of large negative values, which suggests that PHB and PVPh blends are thermodynamically miscible in the melt. Isothermal crystallization kinetics in the miscible blend system PHB/PVPh was examined by OM. The presence of the amorphous PVPh component results in a reduction in the rate of spherulite growth of PHB. The spherulite growth rate is analyzed using the Lauritzen-Hoffman model, The isothermally crystallized blends of PHB/PVPh were examined by wide-angle X-ray diffraction and smell-angle X-ray scattering (SAXS). The long period obtained from SAXS increases with the increase in PVPh component, which implies that the amorphous PVPh is squeezed into the interlamallar region of PHB.

Relevância:

100.00% 100.00%

Publicador:

Resumo:

The miscibility and specific interactions in poly (beta-hydroxybutyrate) (PHB)/poly(p-vinylphenol) (PVPh) blends were studied by differential scanning calorimetry(DSC) , fourier transform infrared(FTIR) spectrometer and high resolution solid state C-13 NMR, A single composition-dependent glass transition temperatures were obtained by DSC which indicate the blends of PHB/PVPh were miscible in the melt state, The experimental glass transition temperatures were fitted quite well with those obtained from Couchman-Karasz equation. The FTIR study shows that the strong intermolecular hydrogen bonding exists in blends of PHB with strong proton acceptor and PVPh with strong proton donor and is the origin of its compatibility. The CPMAS C-13 NMR spectra also show that the strong hydrogen bonding exists in PHB/PVPh blends. From the T-1 rho(H) relaxation time it follows that the blends of PHB/PVPh(40/60, 20/80) studied are completely homogeneous on the scale of about 3.2 nm.

Relevância:

100.00% 100.00%

Publicador:

Resumo:

Small amplitude potential step experiments were carried out to study the counterion transfer process in oxidized poly(3-methylthiophene) (PMT) film. The results demonstrate that anion transfer process in PMT film is migration rather than diffusion. A porous metal electrode model-single hole model, which takes into account both the ionic resistance of the film and the uncompensated solution resistance, was found suitable to describe the potential step experiments. According to this model, the ionic resistivity of oxidized PMT film was calculated to be 5.0 x 10(4) OMEGA.cm, and, in turn, the diffusion coefficent of ClO4- ion in PMT film 3.7 x 10(-9) cm2/s.

Relevância:

100.00% 100.00%

Publicador:

Resumo:

The miscibility of poly(hydroxyether of bisphenol A) (phenoxy) with a series of poly(ethylene oxide-co-propylene oxide) (EPO) has been studied. It was found that the critical copolymer composition for achieving miscibility with phenoxy around 60-degrees-C is about 22 mol % ethylene oxide (EO). Some blends undergo phase separation at elevated temperatures, but there is no maximum in the miscibility window. The mean-field approach has been used to describe this homopolymer/copolymer system. From the miscibility maps and the melting-point depression of the crystallizable component in the blends, the binary interaction energy densities, B(ij), have been calculated for all three pairs. The miscibility of phenoxy with EPO is considered to be caused mainly by the intermolecular hydrogen-bonding interactions between the hydroxyl groups of phenoxy and the ether oxygens of the EO units in the copolymers, while the intramolecular repulsion between EO and propylene oxide units in the copolymers contributes relatively little to the miscibility.

Relevância:

100.00% 100.00%

Publicador:

Resumo:

Blends of poly[3,3-bis(chloromethyl)oxetane] (Penton) with poly(vinyl acetate) were prepared. Compatibility, morphology, thermal behavior, and mechanical properties of blends with various compositions were studied using differential scanning calorimetry (DSC), dynamic mechanical measurements (DMA), tensile tests, and scanning electron microscopy (SEM). DMA study showed that the blends have two glass transition temperatures (T(g)). The T(g) of the PVAc rich phase shifts significantly to lower temperatures with increasing Penton content, suggesting that a considerable amount of Penton dissolves in the PVAc rich phase, but that the Penton rich phase contains little PVAc. The Penton/PVAc blends are partially compatible. DSC results suggest that PVAc can act as a beta-nucleator for Penton in the blend. Marked negative deviations from simple additivity were observed for the tensile strength at break over the entire composition range. The Young's modulus curve appeared to be S-shaped, implying that the blends are heterogeneous and have a two-phase structure. This was confirmed by SEM observations.

Relevância:

100.00% 100.00%

Publicador:

Resumo:

The C=C stretching Raman shifts and photoluminescence (PL) for poly(3-methylthiophene) (P3MT) are measured at various doping levels by in situ electrochemical Raman and PL spectroscopic techniques. It is found that the doping for P3MT induces the nonlinear excitations (soliton, Polaron, bipolaron), but also affects the polymer-chain structure, including the conjugated length and the interchain distance.

Relevância:

100.00% 100.00%

Publicador:

Resumo:

In situ monitoring of conductivity and potential response of conductive polymers during electrochemical process had been described. A renewable carbon fibre array ring-glassy carbon disk electrode was used for this purpose. Poly(3-methylthiophene) and polythiophene were investigated with this method, and some 5 orders in magnitude of conductivity changes were observed during the electrochemical redox process.

Relevância:

100.00% 100.00%

Publicador:

Resumo:

The Electrochemical stability of poly(3-methylthiophene) (PMT) thin film modified glassy carbon electrodes was investigated experimentally with successive cyclic voltammetry(CV) The effects of electrolyte solutions on the stability were studied. In the presence of small hydrated anions (less-than-or-equal-to 3.5nm) in the solution, the electroactivity of PMT films decreased with the characteristics of second order kinetics. In a solution with large hydrated anions (greater-than-or-equal-to 4 nm), PMT films have good stability. PMT/GO electrode can electrocatalyse the oxidation of Br- and Cl- anions, and loses its electroactivity rapidly. X-ray photoelectron spectra (XPS) have demonstrated that chlorine has bonded covalently onto the PMT structure after OV cycles in NaCl solutions.

Relevância:

100.00% 100.00%

Publicador:

Resumo:

The transesterification of poly(beta-hydroxybutyrate) (PHB) and poly(epsilon-caprolactone) (PCL) was carried out by using stannous octoate as catalyzer in liquid phase. The effects of reaction conditions on the transesterification, including reaction temperature, reaction time and catalyzer content, were investigated. The sequence distribution, crystallization behavior and thermal stability of PHB-co-PCL copolyesters were studied by C-13-NMR, FTIR, DSC, WAXD and TGA. The results showed that the transesterification of PHB with PCL was confirmed to produce a block copolymer, and enhancing reaction temperature and increasing reaction time were advantageous to the transesterification. With the increase in PCL content in the block copolymer, the crystallization behavior of PHB-co-PCL copolyesters changed evidently. On the other hand, the introduction of PCL segment into PHB chains did not change its crystalline structure; moreover, thermal stability of PHB-co-PCL copolyesters was a little improved in air, comparing with that of pure PHB.

Relevância:

100.00% 100.00%

Publicador:

Resumo:

1,4,10,13,16-Pentaazatricycloheneicosane-9,17-dione (macrocyclic polyamine)-modified polymer-based monolithic column for CEC was prepared by ring opening reaction of epoxide groups from poly(glycidyl methacrylate-co-ethylene dimethacrylate) (GMA-co-EDMA) monolith with macrocyclic polyamine. Conditions such as reaction time and concentration of macrocyclic polyamine for the modification reaction were optimized to generate substantial EOF and enough chromatographic interactions. Anodic EOF was observed in the pH range of 2.0-8.0 studied due to the protonation of macrcyclic polyamine at the surface of the monolith. Morphology of the monolithic column was examined by SEM and the incorporation of macrocyclic polyamine to the poly(GMA-co-EDMA) monolith was characterized by infrared (IR) spectra. Successful separation of inorganic anions, isomeric benzenediols, and benzoic acid derivatives on the monolithic column was achieved for CEC. In addition to hydrophobic interaction, hydrogen bonding and electrostatic interaction played a significant role in the separation process.

Relevância:

100.00% 100.00%

Publicador:

Resumo:

The objective of this study was to evaluate degradation behavior and the feasibility of biodegradable polymeric stents in common bile duct (CBD) repair and reconstruction. Various molar ratios of lactide (LA) and glycolide (GA) in poly(L-lactide-co-glycolide) (PLGA) were synthesized and processed into a circular tubing of similar to 10.0 mm outer diameter and a wall thickness of about 2.0 mm.