165 resultados para Melting point
Resumo:
The isothermal melt and cold crystallization kinetics of poly(aryl ether ketone ether ketone ketone) are investigated by differential scanning calorimetry over two temperature regions. The Avrami equation describes the primary stage of isothermal crystallization kinetics with the exponent n approximate to 2 for both melt and cold crystallization. With the Hoffman-Weeks method, the equilibrium melting point is estimated to be 406 degrees C. From the spherulitic growth equation proposed by Hoffman and Lauritzen, the nucleation parameter (K-g) of the isothermal melt and cold crystallization is estimated. In addition, the K-g value of the isothermal melt crystallization is compared to those of the other poly(aryl ether ketone)s. (C) 2000 John Wiley & Sons, Inc.
Resumo:
The miscibility, spherulite growth kinetics, and morphology of binary blends of poly(beta-hydroxybutyrate) (PHB) and poly(methyl acrylate) (PMA) were studied with differential scanning calorimetry, optical microscopy, and small-angle X-ray scattering (SAXS). As the PMA content increases in the blends, the glass-transition temperature and cold-crystallization temperature increase, but the melting point decreases. The interaction parameter between PHB and PMA, obtained from an analysis of the equilibrium-melting-point depression, is -0.074. The presence of an amorphous PMA component results in a reduction in the rate of spherulite growth of PRE. The radial growth rates of spherulites were analyzed with the Lauritzen-Hoffman model. The spherulites of PHB were volume-filled, indicating the inclusion of PMA within the spherulites. The long period obtained from SAXS increases with increased PMA content, implying that the amorphous PMA is entrapped in the interlamellar region of PHB during the crystallization process of PHB. All the results presented show that PHB and PMA are miscible in the melt. (C) 2000 John Wiley & Sons, Inc.
Resumo:
Nonisothermal and isothermal melt crystallization kinetics of a novel aryl ether ketone polymer containing meta-phenylene linkages, PEKEKK (T/I), were studied by differential scanning calorimetry (DSC). The Avrami equation modified by Jeziorny and a new approach by combining the Avrami equation with the Ozawa equation could describe the nonisothermal crystallization. Isothermal crystallization could also be described by the Avrami equation. The activation energies were 187 and 159 kJ/mol for nonisothermal and isothermal crystallization, respectively. Using the Hoffman-Weeks method, the equilibrium melting point T-m(o) was estimated as 353 degrees C. From the spherulitic growth equation proposed by Hoffman and Lauritzen, the nucleation parameter K-g of the isothermal melt crystallization was estimated as 5.49 x 10(5) K-2. The crystallization characteristics of PEKEKK (T/I) were compared with those of all-para PEKEKK. The differences were explained by differences in the chain flexibility of the two polymers.
Resumo:
Poly(ethylene oxide) (PEO) and silica (SiO2) organic-inorganic hybrid materials have been synthesized by sol-gel approach. The crystallization behavior of PEO in silica networks has been investigated by differential scanning calorimeter (DSC) and scanning electron micrograph (SEM). The degree of PEO crystallinity in PEO/SiO2 hybrid networks reduces with the increase of SiO2. PEO is in amorphous state when the concentration of PEO is lower than 50 wt% in the hybrid materials. The melting points of PEO in the networks are lower than that of pure PEG, but the melting point of PEO in the networks almost has the same melting point. WAXD and SEM results show that the crystalline behavior of PEO in PEO/SiO2 hybrid system is sternly confined. (C) 1999 Elsevier Science Ltd. All rights reserved.
Resumo:
Radiation crosslinking of polymers mainly depends on the structure of polymer chain. The flexibility and mobility of chain directly influence the possibility of the reactive radicals recombination. Flexible chain is easier to crosslink than rigid-chain polymer. The latter must be crosslinked at high temperature, as most polymers can only crosslink above their melting point. Structural effect also influences the mechanism of radiation crosslinking of polymers. We find from the results in literature and in our laboratory that, the flexibility chain polymer mainly crosslinked with H type, but the rigid chain polymer mainly crosslinked with Y type. (C) 2001 Published by Elsevier Science Ltd.
Resumo:
Poly (ethylene oxide) (PEO) and poly (trimethopropane trimethacrylate) (PTMPTMA) interpenetrate networks have been synthesized. The confined crystallization behavior of PEO in the PTMTYTMA networks has been investigated by a differential scanning calorimeter and scanning electron microscope. The degree of PEO crystallinity in PEO/PTMPTMA interpenetrate networks reduces with the increase of PTMPTMA. PEO is in an amorphous state when the concentration of PEO is lower than 50% in the interpenetrate networks system. The melting points of crystalline PEO in the networks are lower than that of pure PEG, and the melting point of PEO in the networks is higher and increases with the increase of PEO in the interpenetrate networks. Wide-angle X-ray diffraction results show that the PEO crystallite size perpendicular to the (120) plane is not affected as much as PEO in silica networks. (C) 2001 Elsevier Science Ltd. All rights reserved.
Resumo:
In order to investigate the influence of different alkyl side chain substitution on the structures and properties of P3ATs, X-ray diffraction, differential scanning calorimetry (DSC), thermal gravity analysis (TGA), Fourier transform infrared spectra (FTIR) and ultraviolet-visible spectra (W-VIS) were applied to characterizing the samples of ploy(3-octylthiophene) (P3OT), poly(3-dodecylthiophene) (P3DDT) and poly(3-octadecylthiophene) (P3ODT). It is found that the different length of alkyl group substitution leads to great difference in molecular chain packings, according to the room temperature X-ray diffraction results. The temperature dependence of X-ray diffraction experiments were also performed to study the melting processes of P3ATs. With the increase in the number of carbon atoms in alkyl side chains, the melting point decreases, and the thermal stability decreases too. The results of both FTIR and W-VIS spectra indicate that the conjugation length of P3DDT is the longest. among the three P3ATs. (C) 2001 Elsevier Science B.V. All rights reserved.
Resumo:
By using different catalyst systems, two trans-1,4-polybutadiene (TPBD) samples with different tr trans-content and molecular weight were synthesized. The phase transition of two samples from monoclinic form to hexagonal phase was revealed by differential calorimeter scanning and X-ray, respectively. The small-angle X-ray scattering measurements showed the remarkable discrepancy of phase transition and melting point between the two samples was attributed to the different lamellar thickness of crystals: The crystals with different crystalline morphology and lamellar thickness were developed by casting different concentration TPBD solutions. Transmission electron microscopy morphology observations proved that annealing the specimen at the temperature above the phase transition point for different times resulted in the different lamellae thickening of monoclinic form. It means that annealing the TPBD in its hexagonal phase will also slightly favor the increase of both the phase transition temperature and melting point of hexagonal phase. (C) 2001 Elsevier Science Ltd. All rights reserved.
Resumo:
Poly(epsilon -caprolactone) (PCL) and silica (SiO2) organic-inorganic hybrid materials have been synthesized by the sol-gel method. The crystallization behavior of PCL in silica networks has been investigated using differential scanning calorimetry (DSC) and scanning electron microscopy (SEM). The degree of PCL crystallinity in PCL/SiO2 hybrid networks reduces with increase of SiO2. PCL is in an amorphous state when the concentration of PCL is lower than 40wt% in the hybrid system. The melting point of PCL in the networks is lower than, but close to that of pure PCL. WAXD and SEM results show that the crystalline behavior of PCL in PCL/SiO2 hybrid system is strictly confined. (C) 2001 Elsevier Science Ltd. All rights reserved.
Resumo:
Isothermal and nonisothermal melt crystallization kinetics of a novel poly(aryl ether ketone), PEDEKK, were investigated by differential scanning calorimetry. Several kinetic analyses were used to describe the crystallization behavior. The activation energies were determined as 425 and 176 KJ/mol for isothermal and nonisothermal crystallization, respectively. The equilibrium melting point T-m(o) was estimated to be 444 degrees C by using the Hoffman-Weeks approach. The observed crystallization characteristics of PEDEKK were compared with those of the other members of the poly(arpl ether ketone) family.
Resumo:
Poly(vinyl acetate-co-vinyl alcohol) copolymers (P(VAc-co-VA)) were synthesized by hydrolysis-alcoholysis of PVAc. The miscibility, crystallization, and morphology of poly(P-hydroxybutyrate) (PHB) and P(VAc-co-VA) blends were studied by differential scanning calorimetry, optical microscopy (OM), and SAXS. It is found that the P(VAc-co-VA)s with vinyl alcohol content of 9, 15, and 22 mol % will form a miscible phase with the amorphous part of PHB in the solution-cast samples. The melting-quenched samples of PHB/P(VAc-co-VA) blends with different vinyl alcohol content show different phase behavior. PHB and P(VAc-co-VA9) with low vinyl alcohol content (9% mel) will form a miscible blend in the melt state. PHB and P(VAc-co-VA15) with 15 mol % vinyl alcohol will not form miscible blends while PHB/P(VAc-co-VA15) blend with 20/80 composition will form a partially miscible blend in the melt state. PHB and P(VAc-co-VA22) with 22 mol % vinyl alcohol are not miscible in the whole composition range. The single glass transition temperature of the blends within the whole composition range suggests that PHB and P(VAc-co-VA9) are totally miscible in the melt. The crystallization kinetics was studied from the whole crystallization and spherulite growth for the miscible blends. The equilibrium melting point of PHB in the PHB/P(VAc-co-VA9) blends, which was obtained from DSC results using the Hoffman-Weeks equation, decreases with the increase in P(VAc-co-VA9) content. The negative value of the interaction parameter determined from the equilibrium melting point depression supports the miscibility between the components. The kinetics of spherulitic crystallization of PHB in the blends was analyzed according to nucleation theory in the temperature range studied in this work. The best fit of the data to the kinetic theory is obtained by employing WLF parameters and the equilibrium melting points obtained by DSC. The addition of P(VAc-co-VA) did not affect the crystalline structure of PHB, as shown by the WAXD results. The long periods of blends obtained from SAXS increase with the increase in P(VAc-co-VA) content. It indicates that the amorphous P(VAc-co-VA) was rejected to interlamellar phase corporating with the amorphous part of PHB.
Resumo:
Isothermal melt and cold crystallization kinetics of PEEKK have been investigated by differential scanning calorimetry in two temperature regions. During the primary crystallization process, the relative crystallinity develops with a time dependence described by the Avrami equation, with exponent n = 2 for both melt and cold crystallization. The activation energies are -544.5 and 466.7 kJ/mol for crystallization from the melt and amorphous glassy state, respectively. The equilibrium melting point T-m(o) is estimated to be 371 degrees C by using the Hoffman-Weeks approach. The lateral and end surface free energies derived from the Lauritzen-Hoffman spherulitic growth rate equation are sigma=10 erg/cm(2) and sigma(e) = 60 erg/cm(2), respectively. The work of chain folding q is determined as 3.98 kcal/mol. These observed crystallization kinetic characteristics of PEEKK are compared with those of PEEK. (C) 1997 Elsevier Science Ltd.
Resumo:
The thermal properties and crystalline structure of the amphiphilic graft copolymers CR-g-PEG600, CR-g-PEG2000, and CR-g-PEG6000 using chloroprene rubber (CR) as the hydrophobic backbone and poly(ethylene glycol) (PEG) with different molecular weights as the hydrophilic side chains were studied by DSC and WAXD. The results showed that a distinct phase-separated structure existed in CR-g-PEGs because of the incompatibility between the backbone segments and the side-chain segments. For all the polymers studied, T-m2, which is the melting point of PEG crystalline domains in CR-g-PEG, decreased compared to that of the corresponding pure PEG and varied little with PEG content. For CR-g-PEG600 and CR-g-PEG2000, T-m1, which is the melting point of the CR crystalline domains, increased with increasing PEG content when the PEG content was not high enough, and at constant PEG content, the longer were the PEG side chains the higher was the T-m1. The crystallite size L-011 of CR in CR-g-PEGs increased compared to that of the pure CR and decreased with increasing PEG content. (C) 1997 John Wiley & Sons, Inc.
Resumo:
The miscibility and crystallization behavior of poly(beta-hydroxybutyrate) (PHB) and poly(p-vinylphenol) (PVPh) blends were studied by differential scanning calorimetry and optical microscopy (OM). The blends exhibit a single composition-dependent glass transition temperature, characteristic of miscible systems, A depression of the equilibrium melting temperature of PHB is observed. The interaction parameter values obtained from analysis of the melting point depression are of large negative values, which suggests that PHB and PVPh blends are thermodynamically miscible in the melt. Isothermal crystallization kinetics in the miscible blend system PHB/PVPh was examined by OM. The presence of the amorphous PVPh component results in a reduction in the rate of spherulite growth of PHB. The spherulite growth rate is analyzed using the Lauritzen-Hoffman model, The isothermally crystallized blends of PHB/PVPh were examined by wide-angle X-ray diffraction and smell-angle X-ray scattering (SAXS). The long period obtained from SAXS increases with the increase in PVPh component, which implies that the amorphous PVPh is squeezed into the interlamallar region of PHB.
Resumo:
Isothermal melt and cold crystallization kinetics of PEDEKmK linked by meta-phenyl and biphenyl were investigated by differential scanning calorimetry in two temperature regions. Avrami analysis is used to describe the primary stages of the melt and cold crystallization, with exponent n = 2 and n = 4, respectively. The activation energies are -118 kJ/mol and 510 kJ/mol for crystallization from the melt and the glassy states, respectively. The equilibrium melting point T-m(0) is estimated to be 309 degrees C by using the Hoffman-Weeks approach, which compares favorably with determination from the Thomson-Gibbs method. The lateral and end surface free energies derived from the Lauritzen-Hoffman spherulitic growth rate equation are sigma = 8.45 erg/cm(2) and sigma(e) = 45.17 erg/cm(2), respectively. The work of chain folding q is determined as 3.06 kcal/mol. These observed crystallization characteristics of PEDEKmK are compared with those of the other members of poly(aryl ether ketone) family. (C) 1997 John Wiley & Sons, Inc.