Poly(ether ether ketone) and poly(ether diphenyl ether ketone) homopolymers are prepared by nucleophilic substitution routes. Miscibility of PEEK/PEDEK blends has been studied by wide-angle X-ray diffraction (WAXD) and differential scanning calorimetry (d.s.c.). The results indicate that for PEEK/PEDEK blends, when the PEDEK content (weight fraction) is greater than 0.20 and less than 0.75, PEEK and PEDEK components form independent crystalline regions, i.e. they are immiscible; when the PEDEK content is in the range W-PEDEK less than or equal to 0.20 or greater than or equal to 0.75, a rich PEEK- or PEDEK-rich content crystallizes from a mixed melt and PEEK and PEDEK are miscible. Copyright (C) 1996 Elsevier Science Ltd.

Relevância:

20.00% 20.00%

Publicador:

Resumo:

The crystal structure of poly(ether ketone ketone) (PEKK) is predicted by using Cerius2 software according to the wide angle X-ray diffraction (WAXD) experiment result. The predicted structure has a planar zigzag chain conformation between ether oxygen and ketone carbons in an orthorhombic lattice. Average zigzag angle is 126 degrees and average torsion angle is 30.32 degrees. The WAXD powder pattern calculated from the crystal packing model is in good agreement with the experiment result.

Relevância:

20.00% 20.00%

Publicador:

Resumo:

The melting behavior of semicrystalline poly(ether ether ketone ketone) (PEEKK) has been studied by differential scanning calorimetry (DSC). When PEEKK is annealed from the amorphous state, it usually shows two melting peaks. The upper melting peaks arise first, and the lower melting peaks are developed later. The upper melting peaks shown in the DSC thermogram are the combination (addition) of three parts: initial crystal formed before scanning; reorganization; and melting-recrystallization of lower melting peaks in the DSC scanning period. In the study of isothermal crystallization kinetics, the Avrami equation was used to analyze the primary process of the isothermal crystallization; the Avrami constant, n, is about 2 for PEEKK from the melt and 1.5 for PEEKK from the glass state. According to the Lauritzen-Hoffman equation, the kinetic parameter of PEEKK from the melt is 851.5 K; the crystallization kinetic parameter of PEEKK is higher than that of PEEK, and suggests the crystallizability of PEEKK is less than that of PEEK. The study of crystallization on PEEKK under nonisothermal conditions is also reported for cooling rates from 2.5 degrees C/min to 40 degrees C/min, and the nonisothermal condition was studied by Mandelkern analysis. The results show the nonisothermal crystallization is different from the isothermal crystallization. (C) 1996 John Wiley & Sons, Inc.

Relevância:

20.00% 20.00%

Publicador:

Resumo:

On the basis of DSC measurements, the Delta H-f(0) values of the fusion heat for PEEKK-PEBEKK copolymers with various biphenyl contents were obtained by using thermodynamics statistical theory proposed by Flory and graphical method of the specific volume-fusion heat. The results reveal that Delta H-f(0) values determined by these two methods for PEEKK-PEBEKK copolymers with various biphenyl content are nearly the same, and that Delta H-f(0) values are closely dependent on biphenyl content. Delta H-f(0) value is minimum at n(B)=0.35.

Relevância:

20.00% 20.00%

Publicador:

Resumo:

The variations of unit cell parameters and crystallite size of nine PEEK samples treated at various temperatures have been studied by using Wide-Angle X-ray Diffraction (WAXD), The results indicate a decrease in unit cell parameter a,b and c but an increase in crystallite size L(hkl) With the increase beat treatment temperature. Based on X-ray scattering intensity theory and using the graphic multipeak resolution method, the formula of degree of crystallinity (W-c,W-X) for PEEK is derived. The results calculated are compatible with the density measurement and calorimetry.

Relevância:

20.00% 20.00%

Publicador:

Resumo:

The electrochemically deposited poly(o-phenylenediamine) film on a Pt electrode has been investigated utilizing in situ external reflection FTIR spectroelectrochemistry technique. The prepared ladder polymer film is found to be partially ring-opened. The dopant ClO4- is evidenced to orient in such a way that more than one oxygen atom attach to the charge sites of the polymer. This suggests that positive charges of oxidized polymer are partially delocalized over the whole chains. The proton movement observed during the oxidation reaction is associated with the solvated MeCN molecule. It is proposed that the proton diffusion, dissolvation and protonation of the film may be essential to the electrochemical reduction reaction of the film. Copyright (C) 1996 Elsevier Science Ltd.

Relevância:

20.00% 20.00%

Publicador:

Resumo:

Polyurethane (PU) based on polyepichlorohydrin/poly(methyl methacrylate) (PECH/PMMA) interpenetrating polymer networks (IPNs) was synthesized by a simultaneous method. The effects of composition, hydroxyl group number of PECH, NCO/OH ratio and crosslinking agent content in IPNs were investigated in detail. Some other glycols, such as poly(ethylene glycol), poly(propylene glycol) and hydroxyl-terminated polybutadiene, were also used to obtain PU/PMMA IPNs. The interpenetrating and fracture behaviors of the IPNs are explained briefly.

Relevância:

20.00% 20.00%

Publicador:

Resumo:

The morphology of a novel poly(aryl ether ketone) [PEDEKmK] was investigated via polarizing optical microscopy (POM), TEM, DSC, SAXS and electron diffraction (ED). A distinct change in lamellar thickness, orientation, and spherulitic morphology was observed due to crystal melting and recrystallization. However, the crystal packing mode is found to be identical before and after the recrystallization process.