The dark-brown colored 5 at% Yb-doped YAlO3 (Yb:YAP) single crystal was grown successfully by temperature gradient technique (TGT) for the first time. The TGT-grown Yb:YAP crystal with the perovskite structure and excellent crystallization perfection were confirmed by the X-ray diffractions techniques. The dark-brown color of TGT-Yb:YAP crystal turned into the colorless after annealing in the air at 1200 degrees C for 10h. The absorption spectra, LD-excited infrared emission and X-ray excited luminescence spectra of the air-annealed Yb:YAP single crystal were investigated at the room temperature. The results indicate that the TGT-Yb:YAP single crystals can be used for the laser and scintillation applications. (c) 2005 Elsevier B.V. All rights reserved.
Resumo:
The broadband luminescence covering 1.2-1.6 mu m was observed from bismuth and aluminum co-doped germanium oxide glasses pumped by 808 nm laser at room temperature. The spectroscopic properties of GeO2:Bi,Al glasses strongly depend on the glass compositions and the pumping sources. To a certain extent, the Al3+ ions play as dispersing reagent for the infrared-emission centers in the GeO2:Bi,Al glasses. The broad infrared luminescence with a full width at half maximum larger than 200 nm and a lifetime longer than 200 mu s possesses these glasses with the potential applications in broadly tunable laser sources and ultra-broadband fiber amplifiers in optical communication field. (c) 2005 Elsevier B.V. All rights reserved.
Resumo:
Near-infrared broadband emission from bismuth-tantalum-codoped germanium oxide glasses was observed at room temperature when the glasses were pumped by an 808 nm laser diode. The emission band covered the 0, E, S, C, and L bands (1260-1625 nm), with a maximum peak at similar to 1310 nm, a FWHM broader than 400 nm, and a lifetime longer than 200 lis. The observed broadband luminescence was attributed to bismuth clusters in the glasses. Bismuth-tantalum-codoped germanium oxide glass might be promising as amplification media for broadly tunable lasers and wideband amplifiers in optical communications. (c) 2005 Optical Society of America.
Resumo:
Beta gallium oxide (beta-Ga2O3) single crystals were grown by the floating zone technique. The absorption spectra and the luminescence of the crystals were measured. The absorption spectra showed an intrinsic short cutoff edge around 260 nm with two shoulders at 270 and 300 nm. Not only the characteristic UV (395 nm), blue (471 nm) and green (559 nm) lights, but also the red (692 nm) light can be seen in the emission spectra. The deep UV light was attributed to the existing of quantum wells above the valence band and the red light was owed to the electron-hole recombination via the vicinity donors and acceptors. (c) 2006 Elsevier Ltd. All rights reserved.
Resumo:
研究了Yb:YAG晶体的合作发光现象。当用940hm的近红外光激发时,Yb:YAG晶体有明显的上转换蓝色发光。实验发现498nm的蓝色发光强度与激发功率的平方成正比,而且Yb^3+掺杂浓度越高,蓝色发光越强。分析表明这是Yb^3+间强的相互作用导致的合作发光,是由于Yb^3+在共价性的YAG基质中,它的4f^I3电子易于与近邻离子发生相互作用导致的。
Resumo:
EU3+ -doped Y3Al5O12 (YAG:Eu3+) phosphors were synthesized by a facile sol-gel combustion method. In this process, citric acid traps the constituent cations and reduces the diffusion length of the precursors. YAG phase is obtained through sintering at 900 degrees C for 2h. There were no intermediate phases such as YAlO3 (YAP) and Y4Al2O9 (YAM) observed. The charge transfer band of nanocrystalline phosphors shows a shift toward the high-energy side, compared with that of amorphous ones due to lower covalency of Eu-O bond for nanocrystalline phosphors. The higher concentration quenching in YAG:EU3+ nanophosphors may be caused by the confinement effect on resonant energy transfer of nanocrystalline. It also indicates that the sol-gel combustion synthesis method provides a good distribution of Eu3+ activators in YAG host. (c) 2005 Elsevier B.V. All rights reserved.
Resumo:
High-quality Ce3+-doped Y3Al5O12 (YAG:Ce3+) phosphors were synthesized by a facile sol-gel combustion method. In this sol-gel combustion process, citric acid acts as a fuel for combustion, traps the constituent cations and reduces the diffusion length of the precursors. The XRD and FT-IR results show that YAG phase can form through sintering at 900 degrees C for 2 h. This temperature is much lower than that required to synthesize YAG phase via the solid-state reaction method. There were no intermediate phases such as YAlO3 (YAP) and Y4Al2O9 (YAM) observed in the sintering process. The average grain size of the phosphors sintered at 900-1100 degrees C is about 40 nm. With the increasing of sintering temperature, the emission intensity increases due to the improved crystalline and homogeneous distribution of Ce3+ ions. A blue shift has been observed in the Ce3+ emission spectrum of YAG:Ce3+ phosphors with increasing sintering temperatures from 900 to 1200 degrees C. It can be explained that the decrease of lattice constant affects the crystal field around Ce3+ ions. The emission intensity of 0.06Ce-doped YAG phosphors is much higher than that of the 0.04Ce and 0.02Ce ones. The red-shift at higher Ce3+ concentrations may be Ce-Ce interactions or variations in the unit cell parameters between YAG:Ce3+ and YAG. It can be concluded that the sol-gel combustion synthesis method provides a good distribution of Ce3+ activators at the molecular level in YAG matrix. (c) 2005 Elsevier B.V. All rights reserved.
Resumo:
The effects of gamma irradiation on as-grown 5 at% Yb:YAlO3 (YAP) and air annealing on gamma-irradiated 5 at% Yb: YAP have been studied by the difference in the absorption spectra before and after treatment. The gamma irradiation and air annealing led to opposite changes of the absorption properties of the Yb: YAP crystal. After air annealing, the gamma-irradiation effects were totally removed over the wavelength range 390-800 nm and the concentrations of Fe3+ and Yb3+ were slightly increased. For the first time, the gamma-irradiation-induced valence changes between Yb3+ and Yb2+ ions in Yb: YAP crystals have been observed. (c) 2005 WILEY-VCH Verlag GmbH & Co. KGaA, Weinheim.
Resumo:
Optical properties were investigated of ZnO thin films grown oil (100) gamma-LiAlO2 (LAO) substrates by pulsed laser deposition method. C-axis oriented ZnO film was grown oil (100) LAO substrate at the substrate temperature of 550 degrees C. The transmittances of the films were over 85%. Peaks attributed to excitons were seen in the absorption spectra, indicating that the thin films have high crystallinity. Photoluminescence spectra were observed at room temperature; the peak at 550 urn is ascribed to oxygen vacancies in the ZnO films caused by the diffusion of Li from the substrate into the film during deposition. (c) 2005 Elsevier B.V. All rights reserved.
Resumo:
Y3Al5O12:Eu nanophosphors were synthesized by a gel combustion method. The structure of phosphors was characterized by XRD and FTIR. YAG phase came to occur when YAG:Eu precursors were sintered at 800 ℃, although the phase was mainly amorphous. The organ
Resumo:
通过研究提拉法生长的掺杂Ti浓度为0.2at%的LiAlO2晶体吸收光谱,荧光光谱和红外光谱,来分析此新型晶体的结构.分析发现光谱中仅出现了四价Ti离子的196nm的特征吸收峰,用235nm光激发得到384nm的特征发射峰;针对吸收光谱中660-820nm出现的四个弱小吸收峰提出了一个色心模型,从而解释了空气和富Li气氛处理后吸收峰消失的现象;对比纯LiAlO2晶体的红外光谱发现,Ti的掺入仅影响了[AlO4]键强,而[LiO4]及相关键强几乎不变;结合ICP测试估算出直径50mm,厚1mm的Ti:LiA
Resumo:
A new kind of Nd3+, -doped high silica glass (SiO2 > 96% (mass fraction)) was obtained by sintering porous glass impregnated with Nd3+, ions. The absorption and luminescence properties of high silica glass doped with different Nd3+, concentrations were studied. The intensity parameters Omega(t) (t = 2, 4, 6), spontaneous emission probability, fluorescence lifetime, radiative quantum efficiency, fluorescence branching ratio, and stimulated emission cross section were calculated using the Judd-Ofelt theory. The optimal Nd3+ concentration in high silica glass was 0.27% (mole fraction) because of its high quantum efficiency and emission intensity. By comparing the spectroscopic parameters with other Nd3+ doped oxide glasses and commercial silicate glasses, the Nd3+-doped high silica glasses are likely to be a promising material used for high power and high repetition rate lasers.
Resumo:
ZnO thin films were deposited on the substrates of (100) gamma-LiAlO2 at 400, 550 and 700 degrees C using pulsed laser deposition (PLD) with the fixed oxygen pressure of 20 Pa, respectively. When the substrate temperature is 400 degrees C, the grain size of the film is less than 1 mu m observed by Leitz microscope and measured by X-ray diffraction (XRD). As the substrate temperature increases to 550 degrees C, highly-preferred c-orientation and high-quality ZnO film can be attained. While the substrate temperature rises to 700 degrees C, more defects appears on the surface of film and the ZnO films become polycrystalline again possibly because more Li of the substrate diffused into the ZnO film at high substrate temperature. The photoluminescence (PL) spectra of ZnO films at room temperature show the blue emission peaks centered at 430 nm. We suggest that the blue emission corresponds to the electron transition from the level of interstitial Zn to the valence band. Meanwhile, the films grown on gamma-LiAlO2 (LAO) exhibit green emission centered at 540 nm, which seemed to be ascribed to excess zinc and/or oxygen vacancy in the ZnO films caused by diffusion of Li. from the substrates into the films during the deposition.
Resumo:
采用传统无压烧结工艺制备出透明性良好的掺Cr3+氧化铝陶瓷;测定了陶瓷的吸收光谱、发射光谱和激发光谱。结果表明,氧化铝陶瓷吸收峰与红宝石单晶一致,吸收截面大小与单晶相近;陶瓷中Cr3+离子所处格位的晶体场强较单晶弱,但其发射谱仍有较好的锐线发射;陶瓷中微量添加剂以及晶界的存在使得Al2O3晶胞发生畸变,造成其发射峰宽化。
Resumo:
总结了飞秒激光与晶体和玻璃相互作用产生的新现象,如光致折射率改变、光致晶体相变、光还原稀土离子及光致发光等。并分析了它们可能的应用。同时简要的介绍了各种现象产生的机理,展望了飞秒激光与其它物质相互作用可能的研究方向及可能出现的新现象。指出了进行这些研究时可能采用的新方法。