458 resultados para europium ions
Resumo:
The europium-substituted heteropolytungstate K13Eu(SiW11O39)(2) was successfully assembled into two lipids by LB technique for the first time. X-ray diffraction has shown a well defined lamellar for the LB films. The LB films have been characterized by fluorescence spectra and the characteristic luminescence behaviors were discussed. The ligand-metal charge transfer band could be observed in the spectra of the LB films, which could not be found in that of heteropolytungstate solid. The results of fluorescence spectra indicate the energy could be effectively transferred from ligands to the Eu3+ ions in the LB films and the luminescence efficiency was increased greatly. The influences of various lipids on the luminescence of polyoxometalates were investigated. The various interactions between monolayer and polyanions have different effect on the luminescence properties of europium-substituted heteropolytungstate.
Resumo:
Monoclonal antibody technique was employed to detect the conformational difference of CaM induced by metal ions. A trivalent europium ion induced conformation-specific anti-calmodulin monoclonal antibody was successfully prepared with europium-saturated calmodulin as antigen.
Resumo:
The luminescent materials SrB4O7:Eu and BaB8O13:Eu were synthesized, and the valence states of europium in the materials were measured by means of XANES at Eu-L-3 edge. It is found that the Ed(3+) and Eu2+ ions are all present in the materials, and more Eu3+ ions can be reduced in SrB4O7:Eu than in BaB8O13:Eu. The excitation and emission spectra of Eu3+ in SrB4O7:Eu and BaB8O13:Eu were determined.
Resumo:
New kinds of hybrid materials containing covalently bonded Eu3+ (Tb3+) bipyridine complexes in a silica network have been prepared and their luminescence properties reported.
Resumo:
In-situ synthesis of ternary europium complex with thenoyltrifluoacetone (TTA) and 1,10-phenanthroline (phen) in titania matrix in the presence of dimethylformamide (DMF) by a sol-gel process was described, which was confirmed by the luminescence excitation spectra and infrared spectra. The titania gel that contains europium complex exhibits Eu3+ characteristic emission bands and presents a longer fluorescence lifetime than the pure complexes dissolved in ethanol solution. The concentration effect on the luminescence intensity was also investigated.
Resumo:
Ternary europium complexes with thenoyltrifluoroacetone (TTA) and phenanthroline (phen) were incorporated into SiO2/polymer matrix by a sol-gel method. The gels exhibit the characteristic emission bands of europium ion. In addition, Eu3+ presents a longer fluorescence lifetime in gel than in the corresponding pure complex powder. Concentration effects on the luminescence intensity were investigated. The reasons that are responsible for above results are also discussed in the context.
Resumo:
In-situ synthesis of europium and terbium complexes with 1,10-phenanthroline (phen) in silica matrix by a two-step sol-gel process has been proposed. The formation of europium and terbium complexes with phen in sol-gel derived silica gel were confirmed by the luminescence excitation spectra. The silica gels that contain in-situ synthesized europium and terbium complex exhibit the characteristic emission bands of the rare earth ions. Furthermore. the rare earth ions present longer fluorescence lifetimes than the comparable pure complex powder and the complexes dissolved in ethanol solutions. The luminescence properties of the silica gels codoped with europium (or terbium) and phen were also investigated with respect to the gels doped with europium (or terbium). (C) 1999 Elsevier Science B.V. All rights reserved.
Resumo:
Photophysical properties (e.g. luminescence and energy transfer) of binary and ternary complexes of Gd3+, Eu3+, and Tb3+ with aminobenzoic acids and 1,10-phenanthroline were studied in connection with their spectroscopic characterization. Intramolecular energy transfer between center ions and ligands as well as between ligands is discussed in detail.
Resumo:
The luminescence properties of Bi3+, EU(3+), Dy3+ and energy transfer from Bi3+ to Dy3+ and EU(3+) have been studied in two modifications of Y2SiO5 (low-temperature X(1) type and high-temperature X(2) type) and discussed in relation to their crystal structures. The Bi3+ ion luminesces in the blue region of the spectrum in X(1)-Y2SiO5 but in the UV region in X(2)-Y2SiO5. Two obviously different luminescent centres have been observed for Bi3+ and Eu3+ ill X(1)-Y2SiO5, but only one has been seen in X(2)-Y2SiO5. The Stokes shift (9200 cm(-1)) for Bi3+ in X(1)-Y2SiO5 is much larger than that (5000 cm(-1)) in X(2)-Y2SiO5. This suggests that the host lattice is more rigid in X(2)-Y2SiO5 than in X(1)-Y2SiO5. As a result, the Bi3+, EU(3+) and Dy3+ ions show higher emission intensity in the former than in the latter type. X(1)-Y2SiO5 is more suitable for Bi3+ --> EU(3+) energy transfer and X(2)-Y2SiO5 is more suitable for Bi3+ --> Dy3+ energy transfer.
Resumo:
The criterion on 4f~7(~6P_J)→4f~7 (~8S_(7/2))(i. e. f→f)transition emission of Eu~(2+) ions was established based on chemical band properties and crystal field effects. By means of the criterion, we have predioted, designed and synthesized 40 Eu~(2+)-doped complex fluorides. The sharp emissions of f→f transition of Eu~(2+) ions were observed in these doped compounds. The condition for applying this criterion is briefly discussed.
Resumo:
CaF_2 single crystal is very useful as optical host materials. It has been systematically studied and widely used in thermoluminescence that rare earth ions were doped into CaF_2 single crystal with chemical methods. However, the ion implan-
Resumo:
Under the environment of seawater, durability of concrete materials is one of the chief factors considered in the design of structures. The decrease of durability of structures is induced by the evolution of micro-damage due to the erosion of chlorine and sulfate ions, which is characterized by the reduction of modulus, strength, and toughness of the material. In this paper, the variation of the flexural strength of cement mortar under sulfate erosion is investigated. The results obtained in present work indicate that the erosion time, concentration of sulfate solution, and water-to-cement ratio will significantly affect the flexural strength. Crown Copyright (c) 2008 Published by Elsevier Ltd. All rights reserved.
Resumo:
The energy, velocity, angle distribution of ions in magnetoactive electron cyclotron resonance plasma have been studied with a two-dimension hybrid mode. The dependence of these distribution functions versus position and pressure are discussed. Our simulation results are in good agreement with many experimental measurements. (C) 1997 American Institute of Physics.
Resumo:
The ablation rate of a hydrogen isotopic spherical pellet G(is) due to the impact of energetic ions of the respective isotopes and its scaling law are obtained using the transsonic neutral-shielding model, where subscript s might refer to either hydrogen or deuterium. Numerical results show that if E0s/E0e2 greater-than-or-equal-to 1.5, G(is)/G(es) greater-than-or-equal-to 20%, where E0s and E0e are the energy of undisturbed ion and electron, respectively, and G(es) is the ablation rate of a pellet due to the impact of electrons. Hence, under the NBI heating, the effect of the impact of energetic ions on the pellet ablation should be taken into consideration. This result also gives an explanation of the observed enhancement of pellet ablation during NBIH.
Resumo:
Under the environment of seawater, durability of concrete materials is one of the chief factors considered in the design of structures. The decrease of durability of structures is induced by the evolution of micro-damage due to the erosion of chlorine and sulfate ions, which is characterized by the reduction of modulus, strength, and toughness of the material. In this paper, the variation of the flexural strength of cement mortar under sulfate erosion is investigated. The results obtained in present work indicate that the erosion time, concentration of sulfate solution, and water-to-cement ratio will significantly affect the flexural strength. Crown Copyright (c) 2008 Published by Elsevier Ltd. All rights reserved.