344 resultados para Mn:YAP
Resumo:
We report the continuous-wave and acousto-optical Q-switched operation of a diode-end-pumped Tm:YAP laser. Continuous-wave output power of 3.5 W at 1.99 mu m was obtained under the absorbed pump power of 14 W. Under Q-switched laser operation, the average output power increased from 1.57 W to 2.0 W, with an absorbed pump power of 12.6 W, as the repetition rate increased from 1 kHz to 10 kHz. The maximum Q-switched pulse energy was 1.57 mJ with a repetition rate of 1 kHz. The minimum pulse width was measured to be about 80 ns, corresponding to a peak power of 19.6 kW.
Resumo:
The magnetic behavior of Mn-doped beta-Ga2O3 is Studied from first-principles calculations within the generalized gradient approximation method. Calculations show that ferromagnetic ordering is always favorable for configurations in which two Mn ions substitute either tetrahedral or octahedral sites, and the ferromagnetic ground state is also sometimes favorable for configurations where one Mn ion substitutes a tetrahedral site and another Mn ion substitutes an octahedral site. However, the configurations of the latter case are less stable than those of the former. (c) 2008 Acta Materialia Inc. Published by Elsevier Ltd. All rights reserved.
Resumo:
We reported on a diode end-pumped AO Q-switched Tm:YAP laser at 1937 nm. The average output power was 3.9 W, with a slope efficiency of 29.4% and optical-optical conversion efficiency of 21.6% at a 5-kHz repetition rate. The temperature dependency of the output power and the pulse width at different repetition rates were investigated in details.
Resumo:
We report on efficient actively Q-switched Ho: YAP laser double-pass pumped by a 1.91-mu m laser. At room temperature, when the incident pump power was 20.9 W, a maximum average output power of 10.9W at 2118 nm was obtained at the repetition rate of 10 kHz, and this corresponds to a conversion efficiency of 52.2% and a slope efficiency of 63.5%. Moreover, a maximum pulse energy of similar to 1.1 mJ and a minimum pulse width of 31 ns were achieved, with the peak power of 35.5 kW. (C) 2009 Optical Society of America
Resumo:
The Ho:YAP crystal is grown by the Czochralski technique. The room-temperature polarized absorption spectra of Ho:YAP crystal was measured on a c-cut sample with 1 at% holmium. According to the obtained Judd-Ofelt intensity parameters Omega(2) = 1.42 x 10(-20) cm(2), Omega(4) = 2.92 x 10(-20) cm(2), and Omega(6) = 1.71 x 10(-20) cm(2), this paper calculated the fluorescence lifetime to be 6 ms for I-5(7) -> I-5(8) transition, and the integrated emission cross section to be 2.24 x 10(-18) cm(2). It investigates the room-temperature Ho:YAP laser end-pumped by a 1.91-mu m Tm:YLF laser. The maximum output power was 4.1 W when the incident 1.91-mu m pump power was 14.4W. The slope efficiency is 40.8%, corresponding to an optical-to-optical conversion efficiency of 28.4%. The Ho:YAP output wavelength was centred at 2118 nm with full width at half maximum of about 0.8 nm.