An improved aqueous impregnation method was used to prepare 40 wt% Pt/C electrocatalysts. TEM analysis of the samples showed that the Pt particles impregnated for a short time have a very narrow size distribution in the range of 1-4 nm with an average size of 2.6 nm. UV-vis spectroscopy measurements verified that the redox reaction between PtCl62- and formaldehyde took place with a slow rate at ambient temperature via a two-step reaction path, where PtCl42- serves as an intermediate. The use of the short-time-impregnated 40 wt% Pt/C as cathode electrocatalysts in direct methanol fuel cells yields better performance than that of commercial 40 wt% Pt/C electrocatalyst. Experimental evidence provides clues for the fundamental understanding of elementary steps of the redox reactions, which helps in guiding the design and preparation of highly dispersed Pt catalyst for fuel cells.

Relevância:

50.00% 50.00%

Publicador:

Resumo:

The domain-structure of samples containing a series of starch/poly(sodium acrylate)-grafted superabsorbents, pure starch, pure poly(sodium acrylate), and blend of starch/poly(sodium acrylate) has been studied by high-resolution solid-state C-13 NMR spectroscopy at room temperature. The result shows that the crystallinity of starch decreases greatly in the grafted and blended samples.

Relevância:

50.00% 50.00%

Publicador:

Resumo:

Hydrogenation of maleic anhydride (MAH) with Pd/C catalysts in supercritical carbon dioxide (scCO(2)) was investigated. The selectivity for gamma-butyrolactone (GBL) reached 97.3% in scCO(2) at 100% conversion of MAH, which was notably higher than that of 77.4% obtained in organic solvent of ethylene glycol dimethyl ether (EGDME). The particle size of Pd exhibited large influence on the reaction rate and selectivity of GBL. Higher selectivity of GBL was obtained with Pd/C catalyst of smaller Pd particle size, and the rate of GBL selectivity increase as a function of CO2 pressure was found to be significantly correlated with Pd particle size.

Relevância:

50.00% 50.00%

Publicador:

Resumo:

The structural stability and redox properties of yeast iso-1-cytochrome c and its mutant, F82H, were studied by surface-enhanced resonance Raman scattering (SERRS) spectroscopy. Phenylalanine, which exists at the position-82 in yeast iso-1-cytochrome c, is replaced by histidine in the mutant. The SERRS spectra of the proteins on the bare silver electrodes indicate that the mutant possesses a more stable global structure with regard to the adsorption-induced conformational alteration. The redox potential of the mutant negatively shifts by about 400 mV, relative to that of yeast iso-1-cytochrome c. This is ascribed to axial ligand switching and higher solvent accessibility of the heme iron in the mutant during the redox reactions.

Relevância:

50.00% 50.00%

Publicador:

Resumo:

The interaction of [(C(5)H(4)R)(2)NdCl.2LiCl] (R = H, Bu(t)) with one equivalent of Li[(CH2)(CH2)PPh(2)] in refluxing tetrahydrofuran gave the purplish-blue complex [(C(5)H(4)R)(3)NdCH2P(Me)Ph(2)] in 50% yield. The compounds have been fully characterized by analytical, spectroscopic and X-ray diffraction methods. Variable temperature P-31{H-1} NMR spectroscopy indicated the existence of the following equilibrium: [(C(5)H(4)R)(3)NdCH2P(Me)Ph(2)] + THF reversible arrow (C(5)H(4)R)(3)Nd(THF) + CH2=P(Me)Ph(2). At room temperature, the exchange between the coordinated and free ylide ligand is slow on the NMR time scale.

Relevância:

50.00% 50.00%

Publicador:

Resumo:

Ammonia synthesis over ruthenium catalysts supported on different carbon materials using Ba or K compounds as promoters has been investigated. Ba(NO3)(2), KOH, and KNO3 are used as the promoter or promoter precursor, and activated carbon (AC), activated carbon fiber (ACF). and carbon molecular sieve (CMS) are used as the support. The activity measurement for ammonia synthesis was carried out in a flow micro-reactor under mild conditions: 350-450 degreesC and 3.0 MPa. Results show that KOH promoter was more effective than KNO3. and that Ba(NO3)(2) was the most effective promoter among the three. The roles of promoters can be divided into the electronic modification of ruthenium, the neutralization of surface functional groups on the carbon support and the ruthenium precursor. The catalyst with AC as the support gave the highest ammonia concentration in the effluent among the supports used, while the catalyst with ACF as the support showed the highest turnover-frequency (TOF) value. It seems that the larger particles of Ru on the carbon supports are more active for ammonia synthesis in terms of TOF value. (C) 2001 Elsevier Science B.V. All rights reserved.

Relevância:

50.00% 50.00%

Publicador:

Resumo:

In this work, high-surface supported PtRu/C were prepared with Ru(NO)(NO3)(3) and [Pt(H2NCH2CH2NH2)(2)]Cl-2 as the precursors and hydrogen as a reducing agent. XRD and TEM analyses showed that the PtRu/C catalysts with different loadings possessed small and homogeneous metal particles. Even at high metal loading (40 wt.% Pt, 20 wt.% Ru) the mean metal particle size is less than 4 nm. Meanwhile, the calculated Pt crystalline lattice parameter and Pt (220) peak position indicated that the geometric structure of Pt was modified by Ru atoms. Among the prepared catalysts, the lattice parameter of 40-20 wt.% PtRu/C contract most. Cyclic voltammetry (CV), chronoamperometry (CA), CO stripping and single direct methanol fuel cell tests jointly suggested that the 40-20 wt.% PtRu/C catalyst has the highest electrochemical activity for methanol oxidation. (c) 2004 Elsevier Ltd. All rights reserved.