493 resultados para Photoluminescence spectrum


Relevância:

20.00% 20.00%

Publicador:

Resumo:

In this paper, we report a facile method for the fabrication of type-I collagen-silver nanoparticles (Ag NPs) multilayered films by utilizing type-I collagen as a medium. These samples were characterized by UV-vis spectra photometer, atomic force microscopy, scanning electron microscopy, and Fourier transform IR spectrum. Experimental results show that collagen molecules serve as effective templates to assemble Ag NPs into multilayer films. These samples exhibit high surface-enhanced Raman scattering (SERS) enhancement abilities.

Relevância:

20.00% 20.00%

Publicador:

Resumo:

A facile route to the synthesis of LnF(3) nanocrystals has been accomplished in three ionic liquids (ILs) (OmimPF(6), OmimBF(4), and BmimPF(6)). The partial hydrolysis of PF6- and BF4- was utilized to introduce a new fluoride source. Uniform LnF(3) (Ln = La, Ce, Pr, Nd, Sm, Eu, Er), Tb3+-doped CeF3, and Eu3+-doped LaF3 nanocrystals could be obtained in a large scale, and the products were up to 0.15 g per 10 mL solvents. In the "all-in-one" systems, the ILs acted as solvents, reaction agents, and templates.

Relevância:

20.00% 20.00%

Publicador:

Resumo:

A novel diimine Cu(I)complex [Cu(ABPQ)(DPEphos)]BF4 [ABPQ and DPEphos are acenaphtho[1,2-b]bipyrido[2,3-h:3,2-f]quinoxaline and bis(2-(diphenylphosphanyl)phenyl) ether, respectively] is synthesized, and its photophysical properties are experimentally and theoretically characterized. The emission bands centered at ca. 400/470 and 550 nm of [Cu(ABPQ)(DPEphos)]BF4 are attributed to the ligand-centered pi -> pi* transition and the metal-to-ligand charge transfer d pi(Cu) -> pi*(N-N) transition, respectively. The luminescence quantum yield of [Cu(ABPQ)(DPEphos)]BF4 in CHCl3 is found to be about five times higher than that of [Cu(Phen)(DPEphos)]BF4.

Relevância:

20.00% 20.00%

Publicador:

Resumo:

The quantum yield, lifetime, and absorption spectrum of four [Ru(bpy)(2)L](+) [where bpy is 2,2'-bipyridyl; L is represented by the deprotonated form of 2-(1H-tetrazol-5-yl)pyridine (L1) or 2-(1H-tetrazol-5-yl)pyrazine (L2)], as well as their methylated complexes [Ru(bpy)(2)LMe](2+) (RuL1Me and RuL2Me) are closely ligand dependent. In this paper, density functional theory (DFT) and time-dependent DFT (TDDFT) were performed to compare the above properties among these complexes. The calculated results reveal that the replacement of pyridine by pyrazine or the attachment of a CH3 group to the tetrazolate ring greatly increases the pi-accepting ability of the ancillary ligands.

Relevância:

20.00% 20.00%

Publicador:

Resumo:

A novel periodic mesoporous organosilica (PMO) material was synthesized through one-step co-condensation of 1,2-bis(triethoxysilyl)ethane (BTESE) and benzoic acid-functionalized organosilane (BA-Si) using cetyltrimethylammonium bromide (CTAB) as a structure-directing agent under basic conditions. The materials were fully characterized by FTIR, XRD, N-2 adsorption-desorption isotherms and FESEM. FTIR spectra proved that BA-Si was successfully incorporated into the PMO materials (PMOs) via benzyl group as a linker. XRD and N-2 adsorption-desorption isotherms revealed the characteristic mesoporous structure with highly uniform pore size distributions. FESEM confirmed that the morphology of the PMOs was significantly dependent cri the molar ratio of two organosilica precursors.

Relevância:

20.00% 20.00%

Publicador:

Resumo:

A urea-based bis-silylated bipyridine ligand derived from 4,4'-diamino-2,2'-bipyridine has been prepared. Organic-inorganic hybrid materials with a high loading of lanthanide 2,2-bipyridine moieties were obtained by using the silylated bipyridine as the only siloxane network precursor in the presence of lanthanide ions (or lanthanide complexes). The in-situ formation of lanthanide complexes from lanthanide ions and the silylated bipyridine during the sol-gel processing was confirmed by the luminescence behavior of the obtained hybrid materials and that of the corresponding pure lanthanide complex [Ln(bpy)(2)Cl-3 center dot 2H(2)O].

Relevância:

20.00% 20.00%

Publicador:

Resumo:

Three new metal-organic coordination polymers, [Cu(2,3-pydc)(bpp)]center dot 2.5H(2)O (1), [Zn(2,3-pydc)(bpp)]center dot 2.5H(2)O (2) and [Cd(2,3-pydc)(bpp)(H2O)]center dot 3H(2)O (3) (2,3-pydcH(2) = pyridine-2,3-dicarboxylic acid, bpp 1,3-bis(4-pyridyl)propane), have been synthesized at room temvperature. All complexes have metal ions serving as 4-connected nodes but represent two quite different structural motifs. Complexes 1 and 2 are isomorphous, both of which feature 2D -> 3D parallel interpenetration. Each two-dimensional (2D) layer with (4, 4) topology is interlocked by two nearest neighbours, one above and one below, thus leading to an unusual 3D motif. Complex 3 has a non-interpenetrating 3D CdSO4 framework with cavities occupied by uncoordinated water molecules.

Relevância:

20.00% 20.00%

Publicador:

Resumo:

LaInO3:Eu3+ phosphors were prepared by a Pechini sol-gel process. X-ray diffraction (XRD), field-emission scanning electron microscopy (FE-SEM), diffuse reflectance, photoluminescence, cathodoluminescence spectra, as well as lifetimes were utilized to characterize the synthesized phosphors. XRD results reveal that the sample begins to crystallize at 600 degrees C and pure LaInO3 phase can be obtained at 800 degrees C. The crystallinity increases upon raising the annealing temperature. The FE-SEM images indicate that LaInO3:Eu3+ phosphors are composed of fine and spherical grains around 40-80 nm in size. Under the excitation of UV light and low-voltage electron-beams, LaInO3:Eu3+ phosphors show the characteristic emissions of the Eu3+ (D-5(J)-F-7(J) J,J(')=0,1,2,3 transitions). The luminescence colors can be tuned from yellowish warm white to red by changing the doping concentration of Eu3+ to some extent. The corresponding luminescence mechanisms have been proposed.

Relevância:

20.00% 20.00%

Publicador:

Resumo:

LaPO4:Ce3+, Tb3+ nanoparticles were prepared by the reverse microemulsion with functional monomer, methyl methacrylate (MMA) as oil phase, and LaPO4:Ce3+, Tb3+/poly(methyl methacrylate) (PMMA) nanocomposite was obtained via polymerization of MMA monomer. The nanoparticles and nanocomposite have been well characterized by XRD, SEM, TEM, UV/vis spectrum, photoluminescence excitation and emission spectra and luminescence decays. The obtained solid nanocomposite LaPO4:Ce3+, Tb3+/PMMA is highly transparent and exhibits strong green photoluminescence upon UV excitation, due to the integration of luminescent LaPO4:Ce3+, Tb3+ nanoparticles. The luminescent lifetime of Tb3+ is determined to be 1.25 ms in the nanocomposite. (C) 2009 Elsevier Inc. All rights reserved.

Relevância:

20.00% 20.00%

Publicador:

Resumo:

Pyrazoline derivatives have been used widely in dyeing industry as fluorescent whitening agents due to their excellent capability. According to Schellhammer theory of the relation between chemical structure and fluorescent quality, six new fluorescent compounds were designed and synthesized which contained the benzothiazole group in the I-pyrazoline, the indole group in the 3-pyrazoline and the derivatives of phenyl in the 5-pyrazoline. The structure of target compounds was confirmed by IR, H-1 NMR, MS and elementary analysis. The fluorescence spectra showed that these compounds had good fluorescence. They could absorb ultraviolet light at near 353 nm. The fluorescence maximum emission wavelengths were about 430-443 nm. It was a kind of promising fluorescence compounds. The largest fluorescence emission wavelength and the fluorescence intensity were related to the substituted group of the compounds. When the 6-Br group was introduced into benzothiazole, the fluorescence emission wavelength exhibited a blue shift, and the fluorescence intensity increased.

Relevância:

20.00% 20.00%

Publicador:

Resumo:

One-dimensional Mn2+-doped ZnGa2O4 nanofibers were prepared by a simple and cost-effective electrospinning process. X-ray diffraction (XRD), Fourier transform infrared spectroscopy (FT-IR), thermogravimetric and differential thermal analysis (TG-DTA), scanning electron microscopy (SEM), energy-dispersive X-ray spectrum (EDS), transmission electron microscopy (TEM), high-resolution transmission electron microscopy (HRTEM), photoluminescence (PL) and cathodoluminescence (CL) spectra as well as kinetic decays were used to characterize the samples. SEM results indicated that the as-formed precursor fibers and those annealed at 700 degrees C are uniform with length of several tens to hundred micrometers, and the diameters of the fibers decrease greatly after being heated at 700 degrees C. Under ultraviolet excitation (246 nm) and low-voltage electron beams (1-3 kV) excitation, the ZnGa2O4:Mn2+ nanofibers presents the blue emission band of the ZnGa2O4 host lattice and the strong green emission with a peak at 505 nm corresponding to the T-4(1)-(6)A(1) transition of Mn2+ ion.

Relevância:

20.00% 20.00%

Publicador:

Resumo:

One-dimensional Mn2+-doped Zn2SiO4 rnicrobelts and microfibers were prepared by a simple and cost-effective electrospinning process. X-ray diffraction (XRD), Fourier transform infrared spectroscopy (FT-IR), thermogravimetric and differential thermal analysis (TG-DTA), scanning electron microscopy (SEM), energy-dispersive X-ray spectrum (EDS), transmission electron microscopy (TEM), high-resolution transmission electron microscopy (HRTEM), photoluminescence (PL), and cathodoluminescence (CL) spectra as well as kinetic decays were used to characterize the samples. The XRD and DTA results show that the Zn2SiO4 phase begins to crystallize at 800 degrees C and crystallizes completely around 1000 degrees C. SEM results indicate that the as-prepared microbelts/fibers are smooth, whose diameters decrease with increasing the annealing temperature. The average diameter of the Zn2SiO4:Mn2+ microfibers annealed at 1000 degrees C is 0.32 mu m, and their lengths reach up to several millimeters. The average width and thickness of the Zn2SiO4:Mn2+ microbelts fired at 1000 degrees C are around 0.48 and 0.24 mu m, respectively.

Relevância:

20.00% 20.00%

Publicador:

Resumo:

Nanocrystalline ZrO2 fine powders were prepared via the Pechini-type sol-gel process followed by annealing from 500 to 1000 degrees C. The obtained ZrO2 samples were characterized by X-ray diffraction (XRD), field emission scanning electron microscopy (FESEM), transmission electron microscopy (TEM), electron paramagnetic resonance (EPR), and photoluminescence spectra (PL), respectively. The phase transition process from tetragonal (T) to monoclinic (M) was observed for the nanocrystalline ZrO2 powders in the annealing process, accompanied by the change of their photoluminescence properties. The 500 degrees C annealed ZrO2, powder with tetragonal structure shows an intense whitish blue emission (lambda(max) = 425 nm) with a wide range of excitation (230-400 nm). This emission decreased in intensity after being annealed at 600 degrees C (T + M-ZrO2) and disappeared at 700 (T + M-ZrO2), 800 (T + M-ZrO2), and 900 degrees C (M-ZrO2). After further annealing at 1000 degrees C (M-ZrO2), a strong blue-green emission appeared again (lambda(max) = 470 nm).

Relevância:

20.00% 20.00%

Publicador:

Resumo:

Polycrystalline powder sample of KSr4(BO3)(3) was synthesized by high-temperature solid-state reaction. The influence of different rare earth dopants, i.e. Tb3+, TM3+ and Ce3+, on thermoluminescence (TL) of KSr4(BO3)(3) Phosphor was discussed. The TL, photoluminescence (PL) and some dosimetric properties of Ce3+-activated KSr4(BO3)(3) phosphor were studied. The effect of the concentration of Ce3+ on TL intensity was investigated and the result showed that the optimum Ce3+ concentration was 0.2 mol%. The TL kinetic parameters of KSr4(BO3)(3):0.002 Ce3+ phosphor were calculated by computer glow curve deconvolution (CGCD) method. Characteristic emission peaking at about 407 and 383 nm due to the 4f(0)5d(1) -> F-2((5/2),(7/2)) transitions of Ce3+ ion were observed both in PL and three-dimensional (3D) TL spectra. The dose-response of KSr4(BO3)(3):0.002 Ce3+ to gamma-ray was linear in the range from 1 to 1000 mGy. In addition, the decay of the TL intensity of KSr4(BO3)(3):0.002 Ce3+ was also investigated.