461 resultados para ethylene polymerization
Resumo:
The kinetics of the polymerization of isoprene with the heterogeneous rare earth catalyst system isopropoxyneodymium dichloride/triethylaluminium (Nd(OPri)Cl-2-AlEt(3)) was examined in a specially designed dilatometer. The rate of polymerization is expressed as R(p) approximate to -d[M]/dt = k'(p)[Nd](1.40)[M]. The main kinetical parameters such as the concentration of active propagating chain, the efficiency of lanthanide catalyst used (ELCU), the absolute rate constant of propagation as well as the average life time of growing chains, were determined at 30 degrees C, 40 degrees C, 45 degrees C and 50 degrees C.
Resumo:
The isothermal crystallization and melting behavior of the poly(epsilon-caprolactone) (PCL)/poly(ethylene oxide)(PEO) diblock copolymer has been studied by WAXD, SAXS, and DSC methods. Only the PCL block is crystallizable; the PEO block of weight fraction 20% cannot crystallize, although its corresponding homopolymer has strong crystallizability. The long period, amorphous layer, and crystalline lamella of the PCL/PEO block copolymer all increase with the rise in the crystallization temperature, and the thickness of the amorphous layer is much larger than that of crystalline lamella due to the existence of the PEO block in the amorphous region. The isothermal crystallization of the PCL/PEO block copolymer is investigated by using the theory of Turnbull and Fischer. It is found that the amorphous PEO block has a great influence on the nucleation of PCL block crystallization, and the extent of this influence depends on crystallization conditions, especially temperature. The outstanding characteristics are the phenomenon of the double melting peaks in the melting process of the PCL/PEO block copolymer after isothermal crystallization at different temperatures and the transformation of melting peaks from double peaks to a single peak with variations in the crystallization condition. They are related mainly to the existence of the PEO block bonding chemically with the PCL block. In summing up results of investigations into the crystallization and melting behavior of the PCL/PEO block copolymer, it is interesting to notice that when the PCL/PEO block copolymer crystallizes at three different crystallization temperatures, i.e., below 0 degrees C, between 0 and 35 degrees C, and above 35 degrees C, the variation of peak melting temperature is similar to that of overall crystallization rates in the process of isothermal crystallization. The results can be elucidated by the effect of the PEO block on the crystallization of the PCL block, especially its nucleation. (C) 1996 John Wiley & Sons, Inc.
Resumo:
A new mono-substituted titanocene, (eta(5)-cyclopentadienyl) [eta(5)-(1-(4-methoxyphenyl) cyclohexyl) cyclopentadienyl] dichlorotitanium (I), has been prepared via a novel modified synthesis, and its X-ray crystal structure has been determined. It crystallizes in the orthorhombic space group P2(1)2(1)2(1) with cell constants a=0.968 0(5) nm, b=1.284 6(5) nm, c=1.694 4(6) nm, Z=4, R=0.066. The I/methylaluminoxane (MAO) catalyst system produces at different polymerization temperatures either an isotactic or a syndiotactic polypropylene, both of which have the combined influence of enantiomorphic-site control and chain-end control, or an atactic polypropylene controlled by Bernoullian propagation mechanism.
Resumo:
Morphology and mechanical properties of polypropylene (PP)/high density polyethylene (HDPE) blends modified by ethylene-propylene copolymers (EPC) with residual PE crystallinity were investigated. The EPC showed different interfacial behavior in PP/HDPE blends of different compositions. A 25/75 blend of PP/HDPE (weight ratio) showed improved tensile strength and elongation at break at low EPC content (5 wt %). For the PP/HDPE = 50/50 blend, the presence of the EPC component tended to make the PP dispersed phase structure transform into a cocontinuous one, probably caused by improved viscosity matching of the two components. Both tensile strength and elongation at break were improved at EPC content of 5 wt %. For PP/HDPE 75/25 blends, the much smaller dispersed HDPE phase and significantly improved elongation at break resulted from compatibilization by EPC copolymers. (C) 1995 John Wiley & Sons, Inc.
Resumo:
Three new bimetallic complexes were synthesized and crystalized by reactions of (CF3CO2)(3)Ln With R(1) AlR(2)(Ln=Nd and Y, R(1)=H, R=i-C4H9; Ln=Eu, R=R(1)=C2H5) in tetrahydrofuran solution, and their crystal structures were determined using a X-ray diffraction method. The structures and the questions on valence state and noncoplanarity in the structures were confirmed and cracked by means of H-1 NMR and C-13 NMR spectra, especially by C-13-H-1 COSY 2D NMR technique. A general formula of molecules of the three rare earth complexes was defined as follows: [(mu-CF3CO2)(2)Ln(mu-CF3CHO2)AlR(2) . 2THF](2) A mechanism on the formation of the new complexes was also proposed through the following five steps: alkylating, beta-elimination (or hydrogenation), hydrogen transfer, linkage and association. Both Y-Al and Eu-Al complexes function as a catalyst in polymerization of MMA and ECH. The polymer obtained from the first monomer is mainly syndiotactic chain structure and the polymerization of the last monomer shows higher catalytic activity. The Y-Al complex also capable of ring-opening polymerization of THF in case of adding-vary small amount of ECH and a oxonium ion mechanism of THF polymerization was suggested from the analysis of THF polymer terminal.
Resumo:
Thermal behavior and morphology of blends prepared by solution casting of mixtures of chitosan and poly( ethylene oxide) were studied by means of differential scanning calorimetry (DSC) and scanning electron microscopy (SEM). The preliminary results indicate that both melting point and crystallinity depend on the composition of the blends, and that they exhibit minimum values when the blend contains 50% chitosan. From the prediction of melting point depression analysis, the compatibility of the blends shows a transition at this specific composition. This conclusion was further confirmed by observation of the morphology.
Resumo:
The polymerization of acrylonitrile initiated by organolanthanide complexes alone is studied for the first time. The effect df polymerization conditions on catalytic activity of the title complex and molecular weight of the polymers produced have been studied.
Resumo:
The intrinsic viscosities of poly(ethylene oxide)-poly(vinyl acetate) blends (PEO-PVA) have been measured in chloroform as a function of molecular weights of blend components and compositions. The interaction parameters Delta b obtained from the modified Krigbaum and Wall theory and the differences between the intrinsic viscosities of polymer mixtures and the weight-average intrinsic viscosities of the two blend components were both used to characterize the extent of miscibility of the blend mixtures. (C) 1995 John Wiley and Sons, Inc.
Resumo:
The compatibilization of incompatible polypropylene (PP)/poly(ethylene oxide) (PEO) blends was studied. The experimental results showed that the graft copolymer [(PP-MA)-g-PEO] of maleated PP (PP-MA) and mono-hydroxyl PEO (PEO-OH) was a good compatibilize
Resumo:
Graft copolymers of polyethylene (PE) with polyisoprene (PI) were synthesized through polymerization of ethylene in toluene solution of PI (cis-1,4-: 95%; 3,4-: 5%) using a homogeneous V(acac)3/Et3Al2Cl3 catalyst. Copolymers are formed when the growing po
Resumo:
The dependence of thermal degradation behaviour on vinyl acetate (VA) content of ethylene-vinyl acetate (EVA) copolymers was studied by thermogravimetric analysis (t.g.a.). Among the parameters investigated, the maximum rate of weight loss at the stage of
Resumo:
The oxygen permselectivity of a poly[1-(trimethylsilyl)-1-propyne) (PTMSP) membrane was drastically improved by plasma polymerization of fluorine-containing monomers. The effects of such plasma polymerization conditions as deposition time, plasma power an
Resumo:
(eta(3)-C3H5)(2)CeCl5Mg2(tmed)(2) combined with HAl(i-Bu)(2) or Al(i-Bu)(3) can initiate the polymerization of isoprene with about 50% of the cis-1, 4 microstructure contained in the polymer. The insertion reaction of isoprene occurring between Ce3+ and e