470 resultados para Ultraviolet luminescence
Resumo:
The local structure and the valences of europium in SrBPO5:Eu prepared in air were checked by means of XAFS at Eu-L-3 edge. From the EXAFS results, it was discovered that the doped europium atoms were nine-coordinated by oxygen atoms and the distances of bond Eu-O were 2.42 Angstrom in the host. From the XANES data, it was found that the divalent and trivalent europium coexisted in the matrix. The emission spectra excited by VUV or UV exhibited a prominent broad band due to the 4f(6)5d-4f(7) transition of Eu2+ ions, which indicated that the trivalent europium ions were reduced in air in the matrix at high temperature by the defects [V-Sr]" formed by aliovalent substitution between Sr2+ and Eu3+ ions. The VUV excitation spectra in 100-200 nm range showed that the matrix had absorption bands with the maxima at about 130 and 150 nm, respectively.
Resumo:
Rare earth complex Eu(DBM)(3)phen (DBM: dibenzoylmethane, phen: 1.10-phenanthroline) hits been incorporated into unmodified MCM-41 and modified MCM-41s by aminopropyltriethoxysilane (APTES) or N-[(3-triethoxysilyl)propyl]ethylenediamine(TEPED). Thus, the assemblies of unmodified or modified MCM-41s with rare earth (RE) complex have been obtained. XRD spectra. NMR spectra. diffuse reflectance spectra. and the luminescence spectra were used to characterize the pure RE complex and the corresponding assemblies. The assemblies have better luminescence properties under UV irradiation. and their fluorescence lifetimes on the excited state are longer than that of the corresponding pure complex. The possible mechanisms are also discussed in the context.
Resumo:
Biphenyl- (Biph-) containing 1-alkynes (3 and 4) and their polymers (1 and 2) with varying bridge groups and spacer lengths were synthesized and the effects of the structural variation on their properties, especially their mesomorphism and photoluminescence behaviors, were studied. The acetylene monomers 3(3) [HCdropC(CH2)(3)O-Biph-OCO(CH2)(10)CH3] and 4(m) [HCdropC(CH2)(m)OCO-Biph-OCO(CH2)(10)-CH3, m = 3, 4] were prepared by sequential etherization and esterification reactions of 1-alkynes. While 3(3) exhibits enantiotropic crystal E and SmB mesophases, its structural cousin 4(3) displays only a monotropic SmB phase. Enantiotropic SmA and SmB mesophases are, however, developed when the spacer length is increased to 4. Polymerizations of the monomers are effected by Mo-, W-, Rh-, and Fe-based catalysts, with the WCl6-Ph4Sn catalyst giving the best results (isolation yield up to 85% and M-w up to 59000). The polymers were characterized by IR, UV, NMR, TGA, DSC, POM, XRD, and PL analyses. Compared to 1(3), 2(3) shows a red-shifted absorption, a higher T-i, and a better packed interdigitated bilayer SmA(d) structure, while the mesophase of 2(4) involves monolayer-packing arrangements of the mesogens. Upon photoexcitation, 1(3) emits almost no light but 2(m) gives a strong ultraviolet emission (lambda(max) similar to 350 nm), whose intensity increases with the spacer length.
Resumo:
Oxyapatite NaY9Si6O26 was prepared by sol-gel method. By choosing the precursors, a single phase compound was obtained. This soft chemical method lowered the reaction temperature by 100degreesC compared with the solid state method. Its morphology was studied by transmission electron microscopy (TEM). Several rare earth ions (Eu3+, Tb3+, Dy3+) and Pb2+ ion were doped in this compound. The high resolution emission spectrum of Eu3+ showed that rare earth ions occupied two yttrium sites. In spite of the charge imbalance of Pb2+ with the cations in this compound, it was found that Pb2+ could emit in UV range and transfer its excitation energy to Dy3+ ion.
Resumo:
XAFS (EXAFS and XANES) at Eu-L-3 edge were used to determine the local structure and the valences of europium in CaBPO5:Eu prepared in air. The results of EXAFS showed that the doped europium atoms were nine-coordinated by oxygen atoms and the distances of bond Eu-O were 2.39 Angstrom in the host lattice. XANES at Eu-L-3 edge exhibited that Eu2+ and Eu3+ coexisted in the matrix. The luminescent spectrum of the material excited by VUV at 147 nm presented a similar spectrum with that excited by f-f transition of Eu2+ at 396 nm and f-d transition of Eu2+ at 312 nm. The broad emission band due to both 4f(6)5d - 4f(7) transition of EU2+ and f - f transition of Eu3+ could be observed in emission spectra, which indicated that the trivalent europium ions were reduced in air in the matrix at high temperature by the defects [V-Cn]" formed by aliovalent substitution between Ca2+ and Eu3+ ions. The UV excitation spectrum showed the typical f-f transition of Eu3+ and f-d transition of Eu2+. The bands with the maxima at about 113 and 158 nm in VUV excitation spectrum were assigned to originate from the absorption of the host lattice.
Resumo:
In this presentation, nanocrystalline YVO4:A (A=Eu3+, Dy3+, SM3+, Er3+) phosphor films and their patterning were fabricated by a Pechini sol-gel process combined with a soft lithography (micro-molding in capillaries). XRD, FT-IR, AFM and optical microscope, absorption spectra, photoluminescence (PL) spectra as well as lifetimes were used to characterize the resulting films. The results of XRD indicated that the films began to crystallize at 400 degrees C and the crystallinity increased with the increase of annealing temperatures. Transparent nonpattemed phosphor films were uniform and crack free, which mainly consisted of grains with an average size of 90nm. Patterned crystalline phosphor film bands with different widths (5-30 mu m) were obtained. The doped rare earth ions (A) showed their characteristic emission in crystalline YVO4 phosphor films due to an efficient energy transfer from vanadate groups to them. The Sm3+ and Er3+ ions also showed upconversion luminescence in YVO4 film host. The optimum concentration for Eu3+ was determined to be 7 mol% and those for Dy3+, Sm3+, Er3+ were 2 Mol% of Y3+ in YVO4 films, respectively.
Resumo:
The europium complex, Eu(TTA)(3)phen (TTA = thenoyltrifluoroacetone, phen = 1,10-phenanthroline) was successfully doped into organically modified silicate (ormosil) matrix-SiO2/(VTMOS+PMMA) (VTMOS = vinyltrimethoxysilane, PMMA = polymethylmethacrylate) via sol-gel process, and the luminescence properties of the resultant ormosil composite phosphors [ormosil: Eu(TTA)(3)phen were investigated compared with those of the pure Eu(TTA)(3)phen complex powder. The ormosil composite materials incorporated with Eu(TTA)(3)phen show the characteristic red emission of Eu3+ ion. The Eu3+ possesses fewer emission lines and longer lifetime in the hybrid phosphor than in the pure Eu(TTA)(3)phen complex. This has been explained from the viewpoint of the surrounding environment where the Eu3+ ion lies. (C) 2000 Elsevier Science B.V. All rights reserved.
Resumo:
Rare earth complex Eu(phen)(2)Cl-3 was introduced into a SiO2-PEG-400 hybrid material by a sol-ger method. The result indicated that Poly(ethylene glycol) (PEG) could associate with Eu3+ and change the surroundings of Eu3+ in the hybrid material, greatly improving the decay time. Transparent SiO2-PEG400 hybrid doped with a very small amount of Eu(phen)(2)Cl-3 has better mechanical properties and can retain excellent luminescence properties of the rare earth complex. (C) 2000 Elsevier Science B.V. All rights reserved.
Resumo:
Vacuum ultraviolet excitation spectra of LnAl(3)B(4)O(12):Re (Ln = Y, Gd; Re = Eu, To), along with X-ray photoelectron spectra, were measured. The spectra are tentatively interpreted in terms of the optical properties of the rare earth ions and the band structure. It was found that there is an energy transfer from the hosts to the rare earth ions. It was also found that the top of the valence band in the Gd compound is mainly formed by the 2p levels of O2- and the 4f levels of Gd3+, and in the Y compound mainly by the 2p levels of O2-. (C) 2000 Elsevier Science Ltd. All rights reserved.
Resumo:
CaY1-xBO4: xEu was synthesied by solid state reaction method, and the displacement and luminescence of the Eu3+ in CaYBO4 host were studied. Two luminescent centers could be observed at certain Eu3+-concentration, indicating that the Eu3+ occupies two different crystallographic sites. This result shows that the Eu3+ occupies two different Y3+ sites in CaYBO4. The investigation on Eu-O charge transfer bands indicates that the larger distortion or the lower symmetry of Eu3+ site is,the shorter wavelength of the Eu-O charge transfer band is. When the Eu3+-concentration is high (x > 0.10), Eu3+ occupies the sites of Ca2+ and is reduced to Eu2+.
Resumo:
The nature of the emission centers and the valence change of Eu2+ in KCaF3:Eu2+ depends strongly on preparation conditions. Experimental results show that there are two different d-->f emission bands, located at 425 and 510 nm, respectively. Their origin, relationship, and the effect of doping concentration on them are discussed. A Eu2+-Eu3+ valence change process is proposed. (C) 2000 Elsevier Science Ltd. All rights reserved.
Resumo:
The efficient synthesis of 5-(5-bromovaleramido)-1,10-phenanthroline, 5-(6-bromohexanamido)-1,10-phenanthroline, and 5-(11-bromoundecanamido)-1,10-phenanthroline are described, which reacted with cis-Ru(bpy)(2)Cl-2. 2H(2)O and sodium hexafluorophosphate to form Ru(bpy)(2)[phen-NHCO(CH2)(n)Br](PF6)(2) (n = 4, 5 or 10; phen = 1,10-phenanthroline). The intricate H-1 NMR spectra at low field of these complexes were completely assigned in virtue of H-1-H-1 COSY technique. Cyclic voltammetry was used to study electrochemical behaviours of these complexes, and their luminescent properties were investigated with fluorescent spectra.
Resumo:
Plant extracellular calmodulin (CaM) has been purified from cauliflower and identified with NAD kinase(NADK) activation and inhibition effect of CaM antagonist W7, Tb-3.1 fluorescence titration showed that extracellular CaM contained four metal-binding sites, The excitation spectrum and emission specturm indicated that extracellular CaM contained one tyrosine residue which could transfer energy to bound Tb3+. Based on Forster type nonradiative energy transfer theory, the distances of Tyr-->sites III, IV have been determined, these are 1. 104 nm(Tyr --> III, site) and 1. 056 nm(Tyr --> N, site). By studing the effect of CaM antagonist W7 and CaM antibody on Tb3+-sensitized fluorescence, it was found that the binding sites of W7 and antibody were located on the c-terminal part of plant extracellular CaM which contains domain III and domain IV.
Resumo:
The BaMA(10)O(17) (M = Be, Mg, Ca, Zn, Cd, Mn, Co, Li) system has been synthesized by solid state method and characterized by XRD. The results show that when M is Mg, Zn, Mn, Co, Li, there exists the structure of beta-Al2O3 for BaMAl10O17 system, and when M indicates Cd, beta-Al2O3 structure is formed accompanying alpha-Al2O3 phase, and when M represents Be and Ca, beta-Al2O3 structure cannot be formed. This demonstrates that the condition forming beta-Al2O3 structure compounds for the system BaMAl10O17 is 0.05nm < R-M < 0.09nm (R-M represents the radius of M). The thought that if a M ion can form a stable spinel structure there exsits a corresponding magnetoplumbite and beta-alumina structure is proposed for BaMAl10O17 system according to the experimental results. When M is Li, Be, Zn, Eu2+ activator produces an emission of nearly 450 nm with half height width about 50 nm, when M is Mn, there are simultaneously the emissions of Eu2+ and Mn2+ and the excitation energy of Eu2+ can transfer to Mn2+ in the host, when M is Cd, Eu2+ displays a double-emission band, which can be explained by the Jahn-Teller's effect. It is possible for the system BaMAl10O17 with M being Li, Be, Zn to become blue-emitting component in three colour lamp through further study.
Resumo:
The p-toluene sulfonic acid (MA) in phenol matrix was separated and determined by capillary electrophoresis with ultraviolet detector. the effect of the concentration and pH of the buffer on separation was investigated. Cinnamic acid has been chosen as the internal standard from four compounds, the calibration curves of PTSA in 50 mg/L phenol matrix were obtained with and without the internal standard. The linear range was from 1.25 to 12.5 mg/L and the correlation coefficient was 0.9999 for both curves. The limit of detection of PISA was 0.75 mg/L at 3 times of SIN. Finally, the concentration of PTSA in four synthesized samples was determined with method of standard additions, and the effect of matrix was discussed. The values of MA in these samples were 1.01, 0.94, 1.56 and 0.00 mg/L respectively.