467 resultados para FLUORESCENCE-SPECTRA
Resumo:
The self-assembly of oligo(o-phenylenediamine) (OPD) into 1-D nanostructures on a macroscopic length scale was found when they were transferred from N-methyl pyrrolidone to deionized water. Field emission scanning electron microscopy and confocal fluorescence microscopy were used to investigate the morphology of the precipitates. Results showed that large amounts of OPD 1-D supertructures could be obtained through the simple reprecipitation route, and the length of the fibers could be tuned from microscale to macroscale by adjusting the ratio of two solvents. X-ray diffraction patterns and UV-vis spectra revealed that pi-pi interactions between OPD molecules that facilitated the formation of 1-D structures became predominant when they were transferred from a good solvent to a bad one. Accordingly, a possible formation mechanism was proposed.
Resumo:
Nanocyrstalline LaGaO3 and Dy3+- and Eu3+-doped LaGaO3 were prepared through a Pechini-type sol-gel process. X-ray diffraction (XRD), field emission scanning electron microscopy (FE-SEM), photoluminescence, cathodoluminescence spectra, and lifetimes were utilized to characterize the samples. XRD reveals that the samples begin to crystallize at 900 degrees C and pure LaGaO3 phase can be obtained at 1000 degrees C. FE-SEM images indicate that the Dy3+- and Eu3+-doped LaGaO3 samples are both composed of aggregated spherical particles with sizes ranging from 40 to 80 nm. Under the excitation of ultraviolet light and low voltage electron beams (1-5 kV), the undoped LaGaO3 sample shows a strong blue emission peaking at 433 nm, and the Dy3+- and Eu3+-doped LaGaO3 samples show their characteristic emissions of Dy3+ (F-4(9/2)-H-6(15/2) and F-4(9/2)-H-6(13/2) transitions) and Eu3+ (D-5(0,1,2)-F-7(1,2,3,4) transitions), respectively. The relevant luminescence mechanisms are discussed.
Resumo:
In this article, we firstly reported on the synthesis and characterization of ultratine CeF3 nanoparticles (NPs) modified by catanionic surfactant via a reverse micelles-based route. The catanionic surfactant PN was prepared by mixing the di(2-ethylhexyl) phosphoric acid (DEHPA) and primary amine (N1923) with 1:1 molar ratio. It exhibited a high surface activity and formed much small reverse micelles in comparison with its individual component (DEHPA or N1923). The PN reverse micelles were then used as templates to prepare ultrafine CeF3 NPs. The narrow distributed nanoparticles have an average diameter 1.8 nm. FTIR spectra indicated that there existed strong chemical interactions between nanoparticles and the adsorbed surfactants. The modification resulted in the FFIR peak position of P=O shifting to lower energy. Due to the effect of modification and small size, the CeF3 NPs showed a remarkable red shift of 54 mn in the fluorescence emission in comparison with that of bulk material and a red shift of 18 nm in contrast with that of the normal CeF3 NPs with an average diameter of 16 nm.
Resumo:
The phase diagram of a cetyltrimethyl ammonium bromide( CTAB)/n-butanol/n-octane/KNO3-Mg( NO3)(2) system was drawn. Nanoparticles of Eu2+-doped KMgF3 were prepared from the quaternary microemulsions of cetyltrimethyl ammonium bromide(CTAB), n-butanol, n-octane and water. The X-ray diffraction(XRD) patterns were indexed to a pure KMgF3 cubic phase. The environmental scanning electron microscopic (ESEM) images show the presence of spherical Eu2+-doped KMgF3 nanoparticles with a diameter of ca. 20 nm. The emission of KMgF3: Eu2+ nanoparticles peaks at 360 mn. The excitation band was observed at 250 nm with a blue shift of ca. 70 nm compared with that of KMgF3: Eu2+ single crystal. The preparation method of nano-KMgF3: Eu2+/PMMA composite films was inquired into.
Resumo:
Organically modified silica xerogels (OMSX) and Eu3+ (Tb3+)-doped OMSX were prepared by the reaction of (3-aminopropyl) triethoxysilane (APS) with 3-isocyanatepropyltriethoxysilane (ICPTES) followed by the subsequent hydrolysis and condensation in the presence of Eu3+ (Tb3+) via sol-gel method, which were characterized by FT-IR, XRD, fluorescence excitation and emission spectra. The as-formed OMSX shows a strong blue emission with the maximum excitation and emission wavelength at 351 and 420 nm, respectively. Due to the spectral overlap between the emission band of OMSX and f-f absorption lines of Eu3+ and Tb3+ in the UV-blue region, an energy transfer was observed from OMSX host to Eu3+ and Tb3+ in OMSX/Eu3+ and OMSX/Tb3+, respectively. Excitation at 350-360 nm resulted in a very weak emission around 420 nm from OMSX host and strong emission of Eu3+ and Tb3+ in OMSX/Eu3+ and OMSX/Tb3+, respectively. The emission spectra of Eu3+ and Tb3+ consist of D-5(0)-F-7(J) (J = 0, 1, 2, 3, 4) and D-5(4)-F-7(J) (J = 6, 5, 4, 3), respectively. Furthermore, the predicted structure of OMSX/Eu3+ and OMSX/Tb3+ is presented.
Resumo:
Novel composite resins possessing good luminescent properties have been synthesized through a free radical copolymerization of styrene, alpha-methylacrylic acid and the binary or ternary complexes of lanthanide ions (Eu3+ and Tb3+). These polymer-based composite resins not only possess good transparency and mechanical performance but also exhibit an intense narrow band emission of lanthanide complexes under UV excitation. We characterized the molecular structure, physical and mechanical performance, and luminescent properties of the composite resins. Spectra investigations indicate that alpha-methyl-acrylic acid act as both solubilizer and ligand. Photoluminescence measurements indicate that the lanthanide complexes show superior emission lines and higher intensities in the resin matrix than in the corresponding pure complex powders, which can be attributed to the restriction of molecular motion of complexes by the polymer chain networks and the exclusion of water molecules from the complex. We also found that the luminescence intensity decreased with increasing content of alpha-methylacrylic acid in the copolymer system. The lifetime of the lanthanide complexes also lengthened when they were incorporated in the polymer matrix. In addition, we found that the relationships between emission intensity and Tb (Eu) content exhibit some extent of concentration quenching.
Resumo:
We report on the preparation of luminescent silica mesoporous molecular sieves (MCM-48) activated by the europium complex Eu(DBM)(3) . 2H(2)O (where DBM = dibenzoylmethane), using a simple wet impregnation method. Different concentrations of Eu(DBM)(3) . 2H(2)O were introduced into the MCM-48 cubic structure, and the resulting samples were washed with ethanol for different times. UV-Vis absorption measurements and thermogravimetric analysis were used to estimate the amount of Eu complex that has been incorporated within the pores of the MCM-48 host. The various samples were characterized by X-ray powder diffraction (XRD), infrared spectroscopy, diffuse reflectance (DR) and fluorescence measurements. The results reveal that Eu complexes have been successfully introduced into the pores of MCM-48 without disrupting the structure. All the impregnated MCM-48 materials show the typical red luminescence of Eu3+ when excited with a UV lamp. Shifts of the absorption maxima were observed in the DR and fluorescence excitation spectra and will be discussed in relation with guest-host interactions between the organic complex and the silica matrix. The decay profiles of the europium luminescence in the different samples were also measured and discussed.
Resumo:
Several ultrathin luminescent Langmuir-Blodgett (LB) films have been prepared by using the subphase containing the rare earth ions (Eu3+, Tb3-). The effect of the rare earth ions on the monolayer of 2-n-heptadecanoylbenzoic acid (HBA) was investigated. IR and UV spectra showed the rare earth ions were bound to the carboxylic acid head groups and the coordination took place between the polar head group and the rare earth ions. The layer structure of the LB films was demonstrated by low-angle X-ray diffraction. UV absorbance intensity increases linearly with the number of LB films layers, which indicate that the LB films are homogeneously deposited. The LB films can give off strong fluorescence. and the signal can be detected from a single layer. The characteristic luminescence behaviors of LB films have been discussed compared with those of the complexes.
Resumo:
In this work, the LB films based on heteropolytungstate of Dy and Sm have been prepared. The X-ray diffraction shows the LB films have a highly ordered lamella structure. The luminescence characteristics of the LB films were studied. The charge transfer bands of LB films are in higher energies than those of the corresponding solids. It is noticed that the yellow to blue intensity ratio (Y:B) of Dy3+ in the LB films is different from that of the solid. The differences in the spectra show that the Dy3+ site symmetry in LB film was changed due to the interaction between the surfactant and the polyanions. The differences could also be found in the luminescence spectra of the LB films of Sm complex.
Resumo:
Several new hybrid organic-inorganic Langmuir-Blodgett (LB) films containing europium-substituted hetero-polytungstate Eu (XW11O39)(2)''(-) (X=Ge, Si, B) were successfully obtained using LB technique. When the heteropolytungstate anions are dissolved in the subphase, dimethyldioctadecylammonium bromide compression isotherms have been modified, which shows that the polyanions interact with the monolayer. Y-type LB films were obtained from the systems. Low-angle X-ray has shown that these LB films have well-defined lamella. The LB films were characterized by luminescence spectra and the characteristic luminescence behavior for europium-substituted heteropolytungstate complexes and their LB films were discussed. The results of excitation spectra indicate that the energy could be effectively transferred from ligands to the Eu3+ ions in the LB films and the luminescence efficiency could be greatly increased. The results of luminescence spectra indicate that the formations of hybrid organic-inorganic LB films have a great effect on the luminescence of europium-substituted heteropolytungstate. The lifetime shortening was observed in LB films.
Resumo:
The complex fluoride LiBaF3 and LiBaF3:M(M = Eu, Ce) is solvothermally synthesized at 180 degreesC and characterized by means of X-ray powder diffraction, scanning electron microscopy, thermogravimetric analysis and infrared spectroscopy. In the solvothermal process, the solvents, molar ratios of initial mixtures and reaction temperature play important roles in the formation of products. The excitation and emission spectra of the LiBaF3:M(M= Eu,Ce) have been measured by fluorescence spectrophotometer. In the LiBaF3: Eu emission spectra, there is one sharp line emission located at 360 nm arising from f --> f transition of Eu2+ in the host lattice, and typical doublet 5d-4f emission of Ce3+ in LiBaF3 powder is shown.
Resumo:
The different ions doped KMgF3 single crystals are prepared by the vertical Bridgman method. The near-infrared absorption spectra for different parts of all as-growth crystals indicate that there is the best transparency in middle part. The correlation between the vibronic frequencies of Eu2+ and the site displacement of Cu+ co-doped ions is firstly studied, which indicates that Cu+ ions replace the site of the Mg2+ ions. The co-doped Eu2+ counteracts the charge misfit causing by the replacement of Mg2+ with Cu+. The overlapping of the emission spectra of the Eu2+ and the excitation spectra of the Cu+ results in the energy transfer from Eu2+ to Cu+.
Resumo:
The rare earth (Eu3+, Dy3+)-polyoxometalate thin films were fabricated on quartz plate by the sol-gel method. The thin films were demonstrated by the luminescence spectra. The thin films exhibit the characteristic emission bands of the rare-earth ions. It is noticed that the yellow to blue intensity ratio (Y:B) of Dy3+ and the red to orange ratio (R:O) of Eu3+ in the films are different from that of the corresponding solids. Furthermore, the thin films present shorter fluorescence lifetime than the pure complexes. The reasons that were responsible for these results were also discussed.
Resumo:
Luminescent thin films of heteropolytungstate complexes containing lanthanide (europium or samarium) were successfully fabricated by the Langmuir-Blodgett (LB) technique. The pressure-area isotherm of the monolayer of dimethyldioctadecylammonium. bromide (DODA) is modified rather markedly when the subphase contains the complex of Na9EuW10O36 or Na9SmW10O36. The above results indicate that the monolayer of DODA has a strong interaction with the polyanions of EuW10O369-. (or SmW10O369-). X-ray photoelectron spectra and fluorescent spectra verify that europium and tungsten atoms are 36 36 incorporated into the LB films. Ultraviolet (UV), fluorescent spectra and low-angle X-ray diffraction experiments demonstrate that these LB films have a well-defined lamellar structure. The LB film containing EuW10O369- can give off strong fluorescence 16 on UV irradiation. The characteristic emission behaviors of europium ions in LB films and in the powder of Na9EuW10O369- are discussed. It is found that the intensity ratio of the D-5(0)-F-7(2) transition to the D-5(0)-->F-7(1) transition in LB film is quite different from that in the powder of Na9EuW10O36. The difference of the ratio indicates that the site symmetry of europiurn is distorted in LB film, which is probably due to the strong electrostatic interactions between DODA and polyanions.
Resumo:
The measurements of VUV-UV photoluminescence emission (PL) and photoluminescence excitation (PLE) spectra of rare earth ions activated strontium orthophosphate [Sr-3(PO4)(2):RE, RE = Ce, Sm, Eu, Tb] are performed. Whenever the samples are excited by VUV or UV light, the typical emission of Ce-3+,Ce- Sm3+, Eu3+, Eu2+ and Tb3+ ions can be observed in PL spectra, respectively. The charge transfer bands (CTBs) of Sm3+ and Eu3+ are found, respectively, peaking at 206 and 230nm. The absorption bands peaking in the region of 150-160 nm are assigned to the host lattice sensitization bands, i.e., the band-to-band transitions of PO43- grouping in Sr-3(PO4)(2). It is speculated that the first f-d transitions of Sm3+ (Eu3+), and the CTB of Tb3+ are, respectively, located around 165 (14 3) and 167 urn by means of VUV-UV PLE spectra and relational empirical formula, these f-d transitions or CT bands are included in the bands with the maxima at 150-160 nm, respectively. The valence change of europium from trivalent to divalent in strontium orthophosphate prepared in air is observe by VUV-UV PL and PLE spectra.