427 resultados para ENERGY TRANSFER


Relevância:

60.00% 60.00%

Publicador:

Resumo:

The near infrared long lasting phosphorescence of Yb3+ is observed in Yb3+ and Mn2+ codoped zinc borosilicate glasses. Compared with the glasses solely activated by Mn2+, when the Yb3+ ion is codoped, the red long lasting phosphorescence of the samples is largely improved in both brightness and persistent time but the photostimulated long lasting phosphorescence is greatly depressed. It is considered that the appearance of the phosphorescence of Yb3+ is due to the alteration of the energy transfer channel; additionally, Yb3+ also changes the trap depth of the glasses with the shallower trap predominating therefrom the red long lasting phosphorescence is improved and the photostimulated long lasting phosphorescence is degraded.

Relevância:

60.00% 60.00%

Publicador:

Resumo:

The line emission peak of Eu2+ ion in crystal KMgF3 is at 360 nm. The probability of stimulated emission on 4f(7) (P-6(7/2))-> 4f(7)(S-8(7/2)) transition was predicted with a four-level decay model of Eu2+6P7/2 excited states proposed by the authors. Optic gain and net gain coefficient (g = 11.4 +/- 3.2)cm(-1) of 360 nm emission in crystal KMgF3 : Eu2+ were measured by ASE method, and the predication was proved by experiment. The net gain coefficient can be increased by annealing or doping crystal KMgF3 : Eu2+ with Gd3+ or Ce3+.

Relevância:

60.00% 60.00%

Publicador:

Resumo:

We demonstrated high-efficiency red organic light-emitting diodes (OLEDs) employing a europium complex, Eu (III) tris( thenoyltrifluoroacetone) 3,4,7,8-tetramethyl-1,10-phenanthroline (Eu(TTA)(3)(Tmphen)), as an emitter and a blue electrophosphorescent complex, Iridium ( III) bis[4,6-di-fluorophenyl-pyridinato-N,C-2] picolinate (FIrpic), as an assistant dopant codoped into 4,4-N, N-dicarbazole-biphenyl (CBP) host as an emissive layer. A pure red electroluminescence (EL) only from Eu3+ ions at 612 nm with a full width at half maximum of 3 nm was observed and the EL efficiency was significantly enhanced. The maximum EL efficiency reached 7.9 cd A(-1) at 0.01 mA cm(-2) current density, which is enhanced by 2.8 times compared with electrophosphorescence-undoped devices. The large improvements are attributed to energy transfer assistance effects of FIrpic, indicating a promising method for obtaining efficient red OLEDs based on rare-earth complexes.

Relevância:

60.00% 60.00%

Publicador:

Resumo:

A series of europium complexes were synthesized and their electroluminescent (EL) characteristics were studied. It was found by comparison that the different substituted groups, such as methyl, chlorine, and nitryl, on ligand 1,10-phenanthroline affect significantly the EL performance of devices based on these complexes. The more methyl-substituted groups on ligand 1,10-phenanthroline led to higher device efficiency. A chlorine-substituted group showed the approximate EL performance as two methyl-substituted groups, whereas a nitryl substituent reduced significantly the EL luminous efficiency. However, beta-diketonate ligand TTA and DBM exhibited similar EL performance. The improved EL luminous efficiency by proper substituted groups on the 1, 10-phenanthroline was attributed to the reduction of the energy loss caused by light hydrogen atom vibration, as well as concentration quenching caused by intermolecular interaction, and the match of energy level between the ligand and Eu3+.

Relevância:

60.00% 60.00%

Publicador:

Resumo:

A well-known red fluorescent dye 4-(dicy-anomethylene)-2-t-butyl-6(1,1,7,7-tetramethyljulolidyl-9-enyl)4H-pyran (DCJTB) was codoped with an electron transport organic molecule tris(8-hydroxyquinohne) aluminum (Alq3) in a host matrix of polystyrene (PS), and the amplified spontaneous emission (ASE) was studied by optically pumping. It was found that the ASE performance was significantly improved by the introduction of Alq3. The Alq3:DCJTB:PS blending thin films showed a low threshold (2.4 mu J/pulse) and a high net gain coefficient (109.95 cm(-1)) compared with the pure DCJTB:PS system (threshold of 15.2 mu J/pulse and gain of 35.94 cm(-1)). The improvement of the ASE performance was considered to be attributable to the effective Foster energy transfer from Alq(3) to DCJTB. Our results demonstrate that the Alq(3):DCJTB could be a promising candidate as gain medium for red organic diode lasers.

Relevância:

60.00% 60.00%

Publicador:

Resumo:

Amplified spontaneous emission (ASE) characteristics of a red fluorescent dye, 4-(dicy-anomethylene)-2-t-butyl-6(1,1,7,7-tetramethyljulolidyl-9-enyl)-4H-pyran (DCJTB), and a green fluorescent dye, (10-(2-benzothiazolyl)-1,1,7,7-tetramethyl-2,3,6,7-tetrahydro-1H,5H,11H-[1] benzopyrano [6,7,8-ij]quinohzin-11-one) (C545T) codoped polystyrene (PS) as the active medium were studied. It was found that the performance of ASE is greatly improved due to the introduction of C545T. By optimizing the concentrations of C545T and DCJTB in PS, an ASE threshold of 0.016 mJ pulse(-1), net gain of 52.71 cm(-1), and loss of 11.7 cm(-1) were obtained. The efficient Forster energy transfer from C545T to DCJTB was used to explain the improvement of the ASE performance in the coguest system.

Relevância:

60.00% 60.00%

Publicador:

Resumo:

Single-walled carbon nanotubes (SWNTs) binding to human telomeric i-motif DNA can significantly accelerate S1 nuclease cleavage rate by increasing the enzyme turnover number.

Relevância:

60.00% 60.00%

Publicador:

Resumo:

A red long lasting phosphor Zn-3(PO4)(2): Mn2+ Ga3+ (ZPMG) was prepared by ceramic method, and phase conversion and spectral properties were investigated. Results indicated that the phase conversion from alpha-Zn-3(PO4), beta-Zn-3(PO4)(2) to gamma-Zn-3(PO4)(2) occurs with different manganese concentration incorporated and sinter process. The structural change induced by the phase transformation results in a remarkable difference in the spectral properties. The possible luminescence mechanism for this red LLP with different forms has been illustrated.

Relevância:

60.00% 60.00%

Publicador:

Resumo:

A series of Eu3+-doped ZnO films have been prepared by a sol-gel method. These films were characterized by X-ray diffraction (XRD) and photoluminecent spectra (PL). Effects of synthetic parameters, such as annealing atmosphere, temperature and concentration of doped ions, on the highly oriented crystal growth were studied in detail. The crystalline structures of films annealed in vacuum have a wurtzite symmetry with highly c-axis orientation. A characteristic D-5(0) -> F-7(J)(J = 1, 2, 3 and 4) red emission is observed due to energy transfer from the ZnO host to the doped Eu3+ in the c-oriented ZnO films.

Relevância:

60.00% 60.00%

Publicador:

Resumo:

A single-crystalline EuF3 nanoflower with a novel three-dimensional (3D) nanostructure has been successfully synthesized via a facile, fast, efficient, and mild ultrasonic irradiation solution route employing the reaction of Eu(NO3)(3) and KBF4 under ambient conditions without any template or surfactant. The ultrasonic irradiation plays an important role and is necessary for the synthesis of EuF3 with the complex structure. The formation mechanism of this complex nanostructure is proposed in this paper. No template or surfactant is used in this method, which avoids the subsequent complicated workup for the removal of the template or surfactant. Furthermore, a substantial reduction in the reaction time as well as the reaction temperature is observed compared with the hydrothermal process.

Relevância:

60.00% 60.00%

Publicador:

Resumo:

We successfully prepared a new kind of thermoresponsive and fluorescent complex of Tb(III) and PNIPAM-g-P(NIPAM-co-St) (PNNS) core-shell nanoparticle. It was found that Tb(III) mainly bonded to 0 of the carbonyl groups of PNNS, forming the novel (PNIPAM-g-P(NIPAM-co-St))-Tb(III) (PNNS-Tb(III)) complex. The maximum emission intensity of the complex at 545 nm is enhanced about 223 times comparing to that of the pure Tb(III). The intramolecular energy transfer efficiency from PNNS to Tb(III) reaches 50%. When the weight ratio of Tb(III) and the PNNS-Tb(III) complex is 1.2 wt.%, the enhancement of the emission fluorescence intensity at 545 nm is highest.

Relevância:

60.00% 60.00%

Publicador:

Resumo:

A highly efficient white electroluminescent polymer with simultaneous blue, green, and red emission is reported, developed using a dopant/host strategy by covalently attaching both a green- and a red-light-emitting dopant to the side chain of a blue-light-emitting polymer host (see figure). In a single-layer device a maximum luminance efficiency of 7.3 cd A(-1) with CIE coordinates of (0.31,0.32) is achieved.

Relevância:

60.00% 60.00%

Publicador:

Resumo:

Two orange phosphorescent iridium complex monomers, 9-hexyl-9-(iridium (III)bis(2-(4'-fluorophenyl)-4-phenylquinoline-N, C-2')(tetradecanedionate-11,13))-2,7-dibromofluorene (Br-PIr) and 9-hexyl-9-(iridium(III)bis(2-(4'-fluorophenyl)-4-methylquinoline-N, C-2')(tetradecanedionate-11,13))-2,7-dibromofluorene (Br-MIr), were successfully synthesized. The Suzuki polycondensation of 2,7-bis(trimethylene boronate)-9,9-dioctylfluorene with 2,7-dibromo-9,9-dioetylfluorene and Br-Plr or Br-MIr afforded two series of copolymers, PIrPFs and MIrPFs, in good yields, in which the concentrations of the phosphorescent moieties were kept small (0.5-3 mol % feed ratio) to realize incomplete energy transfer. The photoluminescence (PL) of the copolymers showed blue- and orange-emission peaks. A white-light-emitting diode with a configuration of indium tin oxide/poly(3,4-ethylenedioxythiophene):poly(styrenesulfonate)/PIr05PF (0.5 mol % feed ratio of Br-PIr)/Ca/Al exhibited a luminous efficiency of 4.49 cd/A and a power efficiency of 2.35 lm/W at 6.0 V with Commission Internationale de L'Eclairage (CIE) coordinates of (0.46, 0.33). The CIE coordinates were improved to (0.34, 0.33) when copolymer MIr10PF (1.0 mol % feed ratio of Br-MIr) was employed as the white-emissive layer. The strong orange emission in the electroluminescence spectra in comparison with PL for these kinds of polymers was attributed to the additional contribution of charge trapping in the phosphorescent dopants.

Relevância:

60.00% 60.00%

Publicador:

Resumo:

Y2(1-x) Gd2xSiWO8 : A ( 0 <= x <= 1; A= Eu3+, Dy3+, Sm3+, Er3+) phosphor films have been prepared on silica glass substrates through the sol - gel dip-coating process. X-ray diffraction (XRD), Fourier transform infrared spectroscopy (FT-IR), thermogravimetric and differential thermal analysis (TG-DTA), atomic force microscope (AFM), scanning electron microscopy (SEM) and photoluminescence spectra as well as lifetimes were used to characterize the resulting films. The results of the XRD indicated that the films began to crystallize at 800 degrees C and crystallized completely at 1000 degrees C. The AFM and SEM study revealed that the phosphor films, which mainly consisted of closely packed grains with an average size of 90 - 120 nm with a thickness of 660 nm, were uniform and crack free. Owing to an efficient energy transfer from the WO42- groups to the activators, the doped lanthanide ion ( A) showed its characteristic f - f transition emissions in crystalline Y2(1-x) Gd2xSiWO8 (0 <= x <= 1) films. The optimum concentrations for Eu3+, Dy3+, Sm3+, Er3+ were determined to be 21, 5, 3 and 7 mol% of Y3+ in Y2SiWO8 films, respectively.

Relevância:

60.00% 60.00%

Publicador:

Resumo:

Rare earth ions (Eu3+ and Dy3+)-doped Gd-2(WO4)(3) phosphor films were prepared by a Pechini sol-gel process. X-ray diffraction (XRD), Fourier transform infrared spectroscopy (FT-IR), atomic force microscopy (AFM) and photoluminescence (PL) spectra as well as lifetimes were used to characterize the resulting powders and films. The results of XRD indicate that the films begin to crystallize at 600degreesC and the crystallinity increases with the elevation of annealing temperatures. The film is uniform and crack-free, WO(4)(2-)mainly consists of closely packed fine particles with an average grain size of 80 nm. Owing to an energy transfer from 4 groups, the rare earth ions show their characteristic emissions in crystalline Gd-2(WO4)(3) phosphor films, i.e., D-5(J) -F-7(J), (J = 0, 1, 2, 3; J' = 0 1, 2, 3, 4, not in all cases) transitions for Eu3+ and F-4(9/2)-H-6(J) (J = 13/2, 15/2) transitions for D Y3+, with the hypersensitive transitions D-5(0)-F-7(2) (Eu3+) and F-4(9/2) - H-6(13/2) (Dy3+) being the most prominent groups, respectively.