GaN epilayers grown on pre-nitridated (0001) sapphire substrates by metallorganic vapor phase epitaxy were investigated by wavelength dispersive X-ray spectroscopy and energy dispersive S-ray spectroscopy. Precipitates were observed to mainly consist of O impurity whose strengths were weaker than surrounding matrix. The precipitates were larger in size and distributed more sparsely and inhomogeneously in < 11-20 > directions of the epilayers grown on substrates pre-nitridated for longer periods. The larger precipitates often joined to cracks in the TEM specimens. The crack formation seems to be attributed to the compressive stress concentration at edge angles of the larger precipitates. Yellow luminescence of the epilayers was imaged by cathodoluminescence. The distribution similarity between the cathodoluminescence and the precipitates suggested that the precipitates were responsible for the yellow luminescence band. (C) 2000 Elsevier Science S.A, All rights reserved.

Relevância:

10.00% 10.00%

Publicador:

Resumo:

GaN epilayers grown on sapphire substrates nitridated for various lengthy periods were investigated by light scattering tomography (LST) and Raman scattering. In the LST images of the plane-view epilayers, the light scattering defects distribute in [<11(2)over bar 0>] directions. The defect density is lower in epilayer grown on substrate nitridated for a longer period. The defects are believed to be straight threading edge dislocations on {<1(1)over bar 00>} planes. The Raman shift of E-2 mode is larger in the sample grown on substrate nitridated for a longer period. Our results show that the stress is higher in the sample with fewer dislocations.

Relevância:

10.00% 10.00%

Publicador:

Resumo:

We report on an 880 nm LD pumped passive mode-locked TEM00 Nd:YVO4 laser based on a semiconductor saturable absorber mirror (SESAM) for the first time. When the incident pump power was 16 W, 4.76 W average output power of continuous-wave mode-locked laser with an optical-to-optical conversion efficiency of 30% was achieved. The repetition rate of mode-locked pulse was 80 MHz with 25 ps pulse width. The maximum pulse energy and peak power were 60 nJ and 2.4 kW, respectively.

Relevância:

10.00% 10.00%

Publicador:

Resumo:

An electrical-to-green efficiency of more than 10% was demonstrated by intracavity-frequency-doubling a Q-switched diode-side-pumped Nd:YAG laser with a type II lithium triborate (LBO) crystal in a straight plano-concave cavity. An average power of 69.2 W at 532 nm was generated when electrical input power was 666 W. The corresponding electrical-to-green conversion efficiency is 10.4%. To the best of our knowledge, this is the highest electrical-to-green efficiency of second harmonic generation laser systems with side-pumped laser modules, ever reported. At about 66 W of green output power, the power fluctuation over 4 hours was better than +/-0.86%.

Relevância:

10.00% 10.00%

Publicador:

Resumo:

We report an LD side-pumped continuous-wave passive mode-locked Nd:YAG laser with a Z-type folded cavity based on a semiconductor saturable absorber mirror (SESAM). The average output power 2.95 W of mode-locked laser with electro-optical conversion efficiency of 1.3% and high beam quality (M-x(2) = 1.25 and M-y(2) = 1.22) is achieved. The repetition rate of mode-locked pulse of 88 MHz with pulse energy of 34 nJ is obtained.

Relevância:

10.00% 10.00%

Publicador:

Resumo:

An electrically bistable device has been fabricated using nanocomposite films consisting of silver nanoparticles and a semiconducting polymer by a simple spin-coating method. The current-voltage characteristics of the as-fabricated devices exhibit an obvious electrical bistability and negative differential resistance effect. The current ratio between the high-conducting state and low-conducting state can reach more than 103 at room temperature. The electrical bistability of the device is attributed to the electric-filed-induced charge transfer between the silver nanoparticles and the polymer, and the negative differential resistance behavior is related to the charge trapping in the silver nanoparticles. The results open up a simple approach to fabricate high quality electrically bistable devices by doping metal nanoparticles into polymer.

Relevância:

10.00% 10.00%

Publicador:

Resumo:

We have proposed a novel type of photonic crystal fiber (PCF) with low dispersion and high nonlinearity for four-wave mixing. This type of fiber is composed of a solid silica core and a cladding with a squeezed hexagonal lattice elliptical airhole along the fiber length. Its dispersion and nonlinearity coefficient are investigated simultaneously by using the full vectorial finite element method. Numerical results show that the proposed highly nonlinear low-dispersion fiber has a total dispersion as low as +/- 2.5 ps nm(-1) km(-1) over an ultrabroad wavelength range from 1.43 to 1.8 mu m, and the corresponding nonlinearity coefficient and birefringence are about 150 W-1 km(-1) and 2.5 x 10(-3) at 1.55 mu m, respectively. The proposed PCF with low ultraflattened dispersion, high nonlinearity, and high birefringence can have important application in four-wave mixing. (C) 2010 Optical Society of America

Relevância:

10.00% 10.00%

Publicador:

Resumo:

We describe our research on the employment of an infrared upconversion screen made of electron trapping material (ETM) in combination with the high sensitivity of the S-20 photocathode responsive to visible radiation to produce a streak camera arrangement capable of viewing and recording infrared incident pulses. The ETM-based upconversion screen converts 800-1600 nm infrared radiation to visible light which is viewed or recorded by the S-20 photocathode. The peak values of the upconversion efficiency are located at 1165 nm for CaS:Eu, Sm and 1060 nm for CaS:Ce, Sm. The present experiment showed time resolution was 12.3 ps for a CaS:Eu, Sm screen and 8.4 ps for a CaS:Ce, Sm screen. The minimum detectability is 4.8 x 10(-9) J/mm(2) (minimum detectability of the coupled visible streak camera is 8.3x10(-10) J/mm(2)). Other parameters, such as spatial resolution and dynamic range, have also been measured and analyzed. The results show ETM can be used in the measurement of infrared ultrafast phenomena up to picosecond time domain. In consideration of the limited number of trapped electrons in ETM, the infrared-sensitive streak camera consisting of an ETM-based upconversion screen is suitable to operate in the single shot mode. (C) 1999 American Institute of Physics. [S0034-6748(99)00112-4].

Relevância:

10.00% 10.00%

Publicador:

Resumo:

Without introducing concentration quenching phenomenon, a few wt% of Tb3+ and Yb3+ ions were doped into a group of easily-fiberized tellurite glasses characterized by loose polyhedron structures and rich interstitial positions. Intense green upconversion emission from Tb3+ ions centered at 539 nm due to transition 5D4→7F5 was observed by direct excitation of Yb3+ ions with a laser diode at 976 nm. Optimizing the concentration ratio of Tb3+/Yb3+, a tellurite glass with composition of 80TeO2-10ZnO-10Na2O (mol%)+1.0wt% Tb2O3+3.0wt% Yb2O3 was found to present the highest green light intensity and therefore is especially suitable for efficient green fiber laser development.