Ag/PPy (polypyrrole) composite colloids were prepared through the reaction of silver nitrate with pyrrole solution in DNIF either in the dark, or under the irradiation of femtosecond laser (fs) pulse or UV lamp. The UV-vis spectra of the nanocomposite colloid display an intense absorption band around 620 nm, accompanied by a weak one around 470 nm. The colors and optical absorption spectra of as-synthesized colloids can be reversibly tuned between blue and red, corresponding to absorption band of 620 urn and 526 urn, within few seconds by adding base and acid solutions or gases in turn into the composite colloid suspension. In addition, excess of H+ solution enhanced the absorption band around 470 nm and, at the same time, depressed that around 620 nm. The possible mechanism for the formation and optical absorption properties of the Ag/PPy composite colloid was proposed. (C) 2006 Elsevier B.V. All rights reserved.

Relevância:

100.00% 100.00%

Publicador:

Resumo:

Hybrid TiO2/ormosil waveguiding films have been prepared by the sol-gel method at low thermal treatment temperature of 150° C. The influence of processing parameters including the molar ratios of titanium butoxide (Ti(OBu)(4))/3-glycidoxypropyltrimethoxysilane (GLYMO) and H2O/Ti(OBu)(4) (expressed as R), especially aging of sot on the optical properties was investigated. The optical properties of films were measured with scanning electron microscope (SEM), UV/VIS/NIR spectrophotometer (UV-Vis), m-line and the scattering-detection method. The results indicate that the film thickness increases with the increase of sol aging time, but the variation of refractive index as a function of sot aging time depends on the relative ratios of GLYMO to Ti(OBu)(4). Higher transmittance and lower attenuation of the planar waveguide can be obtained in the sol with lower Ti(OBu)(4) contents and shorter aging time.

Relevância:

100.00% 100.00%

Publicador:

Resumo:

Sol-gel derived TiO2/SiO2/ormosil hybrid planar waveguides have been deposited on soda-lime glass slides and silicon substrates, films were heat treated at 150 degreesC for 2 h or dried at room temperature. Different amounts of water were added to sols to study their impacts on microstructures and optical properties of films. The samples were characterized by m-line spectroscopy, Fourier transform infrared spectroscopy (FT-IR), UV/VIS/NIR spectrophotometer (UV-vis), atomic force microscopy (AFM), thermal analysis instrument and scattering-detection method. The refractive index was found to have the largest value at the molar ratio H2O/OR = 1 in sol (OR means -OCH3, -OC2H5 and -OC4H9 in the sol), whereas the thickest film appears at H2O/OR = 1/2. The rms surface roughness of all the films is lower than 1.1 nm, and increases with the increase of water content in sol. Higher water content leads to higher attenuation of film. (C) 2004 Elsevier B.V. All rights reserved.

Relevância:

100.00% 100.00%

Publicador:

Resumo:

The effect of Al(PO3)(3) content on physical, chemical and optical properties of fluorophosphate glasses for 2 mu m application, such as thermal stability, chemical durability, surface hardness, absorption spectra and emission spectra, is investigated. With the increment of Al(PO3)(3) content, the thermal stability characterized by the gap of T-g and T,, increases first and then decreases, and reaches the maximum level containing 5 mol% Al(PO3)(3) content. The density and chemical durability decrease monotonously with the introduction of Al(PO3)(3) content increasing, while the refractive index and surface hardness increase. Above properties of fluorophosphate glasses are also compared with fluoride glasses and phosphate glasses. The Judd-Ofelt parameters, absorption and emission cross sections are discussed based on the absorption spectra of Tm-doped glasses. The emission spectra are also measured and the 1.8 mu m fluorescence of the sample is obvious indicating that it is suitable to 2 mu m application. (c) 2008 Elsevier B.V. All rights reserved.

Relevância:

100.00% 100.00%

Publicador:

Resumo:

Gd1.99-xYxCe0.01SiO5 (Ce:GYSO) crystals (x = 0, 0.0995, 0.199) have been grown by the Czochralski (Cz) method. Crystal structure and the distribution coefficients of Ce have been determined for all three crystals. Spectroscopic measurements indicate that optical transmittance and luminescence intensity of Gd1.99-xYxCe0.01SiO5 (x = 0.0995, 0.199) crystals are Substantially higher than those of Ce:Gd2SiO5 (Ce:GSO), especially at x = 0.0995, which makes them good candidate materials for scintillation applications. The particularly important result is that the alloyed Ce:GYSO crystals can be grown easily by the Cz method and, unlike Ce:GSO, they do not undergo cleavage during the growth process or subsequent mechanical treatment. (c) 2005 Elsevier B.V. All rights reserved.

Relevância:

100.00% 100.00%

Publicador:

Resumo:

We report on the optical property changes for Ce3+-doped Gd2SiO5 crystal irradiated by a femtosecond (fs) laser. Absorption spectra showed that Ce-related color centers were formed in this crystal after an 800 nm fs laser irradiation. The annealing temperature-dependence of the refractive index and absorption intensity changes have been investigated. Furthermore, a new way of writing overlapped gratings inside the crystal by use of birefringence of fs laser beam in this crystal was proposed. (c) 2005 Elsevier B.V. All rights reserved.

Relevância:

100.00% 100.00%

Publicador:

Resumo:

High-quality Ce3+-doped Y3Al5O12 (YAG:Ce3+) phosphors were synthesized by a facile sol-gel combustion method. In this sol-gel combustion process, citric acid acts as a fuel for combustion, traps the constituent cations and reduces the diffusion length of the precursors. The XRD and FT-IR results show that YAG phase can form through sintering at 900 degrees C for 2 h. This temperature is much lower than that required to synthesize YAG phase via the solid-state reaction method. There were no intermediate phases such as YAlO3 (YAP) and Y4Al2O9 (YAM) observed in the sintering process. The average grain size of the phosphors sintered at 900-1100 degrees C is about 40 nm. With the increasing of sintering temperature, the emission intensity increases due to the improved crystalline and homogeneous distribution of Ce3+ ions. A blue shift has been observed in the Ce3+ emission spectrum of YAG:Ce3+ phosphors with increasing sintering temperatures from 900 to 1200 degrees C. It can be explained that the decrease of lattice constant affects the crystal field around Ce3+ ions. The emission intensity of 0.06Ce-doped YAG phosphors is much higher than that of the 0.04Ce and 0.02Ce ones. The red-shift at higher Ce3+ concentrations may be Ce-Ce interactions or variations in the unit cell parameters between YAG:Ce3+ and YAG. It can be concluded that the sol-gel combustion synthesis method provides a good distribution of Ce3+ activators at the molecular level in YAG matrix. (c) 2005 Elsevier B.V. All rights reserved.

Relevância:

100.00% 100.00%

Publicador:

Resumo:

Optical properties were investigated of ZnO thin films grown oil (100) gamma-LiAlO2 (LAO) substrates by pulsed laser deposition method. C-axis oriented ZnO film was grown oil (100) LAO substrate at the substrate temperature of 550 degrees C. The transmittances of the films were over 85%. Peaks attributed to excitons were seen in the absorption spectra, indicating that the thin films have high crystallinity. Photoluminescence spectra were observed at room temperature; the peak at 550 urn is ascribed to oxygen vacancies in the ZnO films caused by the diffusion of Li from the substrate into the film during deposition. (c) 2005 Elsevier B.V. All rights reserved.

Relevância:

100.00% 100.00%

Publicador:

Resumo:

ZnO thin films were deposited on the substrates of (100) gamma-LiAlO2 at 400, 550 and 700 degrees C using pulsed laser deposition (PLD) with the fixed oxygen pressure of 20 Pa, respectively. When the substrate temperature is 400 degrees C, the grain size of the film is less than 1 mu m observed by Leitz microscope and measured by X-ray diffraction (XRD). As the substrate temperature increases to 550 degrees C, highly-preferred c-orientation and high-quality ZnO film can be attained. While the substrate temperature rises to 700 degrees C, more defects appears on the surface of film and the ZnO films become polycrystalline again possibly because more Li of the substrate diffused into the ZnO film at high substrate temperature. The photoluminescence (PL) spectra of ZnO films at room temperature show the blue emission peaks centered at 430 nm. We suggest that the blue emission corresponds to the electron transition from the level of interstitial Zn to the valence band. Meanwhile, the films grown on gamma-LiAlO2 (LAO) exhibit green emission centered at 540 nm, which seemed to be ascribed to excess zinc and/or oxygen vacancy in the ZnO films caused by diffusion of Li. from the substrates into the films during the deposition.