The ZnO films were deposited on c-plane sapphire, Si (0 0 1) and MgAl2O4 (1 1 1) substrates in pure Ar ambient at different substrate temperatures ranging from 400 to 750 degrees C by radio frequency magnetron sputtering. X-ray diffraction, photoluminescence and Hall measurements were used to evaluate the growth temperature and the substrate effects on the properties of ZnO films. The results show that the crystalline quality of the ZnO films improves with increasing the temperature up to 600 degrees C, the crystallinity of the films is degraded as the growth temperature increasing further, and the ZnO film with the best crystalline quality is obtained on sapphire at 600 degrees C. The intensity of the photoluminescence and the electrical properties strongly depend on the crystalline quality of the ZnO films. The ZnO films with the better crystallinity have the stronger ultraviolet emission, the higher mobility and the lower residual carrier concentration. The effects of crystallinity on light emission and electrical properties, and the possible origin of the n-type conductivity of the undoped ZnO films are also discussed. (C) 2009 Elsevier B. V. All rights reserved.

Relevância:

100.00% 100.00%

Publicador:

Resumo:

ZnS:Mn nanoparticles of the cubic zinc blende structure with the average sizes of about 3 nm were synthesized using a coprecipitation method and their optical and magnetic properties were investigated. Two emission bands were observed in doped nanoparitcles and attributed to the defect-related emission of ZnS and the Mn2+ emission, respectively. With the increase of Mn2+ concentration, the luminescence intensities of these two emission bands increased and the ZnS emission band shifted to lower energy. Based on the luminescence excitation spectra of Mn2+, the 3d(5) level structure of Mn2+ in ZnS nanoparticles is similar to that in bulk ZnS:Mn, regardless of Mn2+ concentration. Magnetic measurements showed that all the samples exhibit paramagnetic behavior and no antiferromagnetic interaction between Mn2+ ions exists, which are in contrast to bulk ZnS:Mn. (c) 2005 Elsevier B.V. All rights reserved.

Relevância:

100.00% 100.00%

Publicador:

Resumo:

A 275 mu m thick GaN layer was directly grown on the SiO2-prepatterned sapphire in a home-built vertical hydride vapour phase epitaxy (HVPE) reactor. The variation of optical and structure characteristics were microscopically identified using spatially resolved cathodeluminescence and micro-Raman spectroscopy in a cross section of the thick film. The D X-0(A) line with the FWHM of 5.1 meV and etch- pit density of 9 x 10(6) cm(-2) illustrated high crystalline quality of the thick GaN epitaxial layer. Optically active regions appeared above the SiO2 masks and disappeared abruptly due to the tapered inversion domains at 210 - 230 mu m thickness. The crystalline quality was improved by increasing the thickness of the GaN/sapphire interface, but the region with a distance of 2 mu m from the top surface revealed relatively low quality due to degenerate surface reconstruction by residual gas reaction. The x-ray rocking curve for the symmetric (0 0 2) and asymmetric (1 0 2) reflections also showed good quality and a small wing tilt of the epitaxial lateral overgrowth (ELO) GaN.

Relevância:

100.00% 100.00%

Publicador:

Resumo:

For both, (Al,Ga)N with low Al content grown on a GaN nucleation layer and (AI,Ga)N with high Al content gown on an AlN nucleation layer, the inhomogeneous distribution of the luminescence is linked to the distribution of defects, which may be due to inversion domains. In the former system, defect regions exhibit a much lower Al content than the nominal one leading to a splitting of the respective luminescence spectra. In the latter system, a domain-like growth is observed with a pyramidal surface morphology and non-radiative recombination within the domain boundaries. (c) 2007 WILEYNCH Verlag GmbH & Co. KGaA, Weinheim.

Relevância:

100.00% 100.00%

Publicador:

Resumo:

The chemical properties of AlxGa1-xN surfaces exposed to air for different time periods are investigated by atomic force microscopy (AFM), photoluminescence (PL) measurement and X-ray photoelectron spectroscopy (XPS). PL and AFM results show that AlxGa1-xN samples exhibit different surface characteristics for different air-exposure times and Al contents. The XPS spectra of the Al 2p and Ga 2p core levels indicate that the peaks shifted slightly, from an Al-N to an Al-O bond and from a Ga-N to a Ga-O bond. All of these results show that the epilayer surface contains a large amount of Ga and Al oxides. (c) 2006 Elsevier B.V. All rights reserved.

Relevância:

100.00% 100.00%

Publicador:

Resumo:

AlxInyGa1-x-yN epilayers have been grown by metalorganic chemical vapor deposition (MOCVD) at different temperatures from 800 to 870degreesC. The incorporation of indium is found to increase with decreasing growth temperature, while the incorporation of Al remains nearly constant. The optical properties of the samples have been investigated by photoluminescence (PL) and time-resolved photoluminescence (TRPL) at different temperatures. The results show that the sample grown at 820 C exhibits the best optical quality for its large PL intensity and the absence of the yellow luminescence. Furthermore the temperature-dependent PL and TRPL of the sample reveals its less exciton localization effect caused by alloy fluctuations. In the scanning electron microscopy measurement, much uniform surface morphology is found for the sample grown at 820degreesC, in good agreement with the PL results, The improvement of AlxInyGa1-x-yN quality is well correlated with the incorporation of indium into AlGaN and the possible mechanism is discussed. (C) 2002 Elsevier Science B.V. All rights reserved.

Relevância:

100.00% 100.00%

Publicador:

Resumo:

In this paper, we presents the characterization technique of high-speed optoelectronics devices based electrical and optical spectra, which is as important access to the devices performance as the prevalent vector network analyzer (VNA) sweeping method. The measurement of additional modulation of laser and frequency response of photodetector from electrical spectra, and the estimation of the modulation indexes and the chirp parameters of directly modulated lasers based on optical spectra analysis, are given as examples.

Relevância:

100.00% 100.00%

Publicador:

Resumo:

High quality ZnO films have been successfully grown on Si(100) substrates by Metal-organic chemical vapor deposition (MOCVD) technique. The optimization of growth conditions (II-VI ratio, growth temperature, etc) and the effects of film thickness and thermal treatment on ZnO films' crystal quality, surface morphology and optical properties were investigated using X-ray diffraction (XRD), atomic force microscopy (AFM), and photoluminescence (PL) spectrum, respectively. The XRD patterns of the films grown at the optimized temperature (300 degrees C) show only a sharp peak at about 34.4 degrees corresponding to the (0002) peak of hexagonal ZnO, and the FWHM was lower than 0.4 degrees. We find that under the optimized growth conditions, the increase of the ZnO films' thickness cannot improve their structural and optical properties. We suggest that if the film's thickness exceeds an optimum value, the crystal quality will be degraded due to the large differences of lattice constant and thermal expansion coefficient between Si and ZnO. In PL analysis, samples all displayed only ultraviolet emission peaks and no observable deep-level emission, which indicated high-quality ZnO films obtained. Thermal treatments were performed in oxygen and nitrogen atmosphere, respectively. Through the analysis of PL spectra, we found that ZnO films annealing in oxygen have the strongest intensity and the low FWHM of 10.44 nm(106 meV) which is smaller than other reported values on ZnO films grown by MOCVD.

Relevância:

100.00% 100.00%

Publicador:

Resumo:

ZnO complex 3D nano-structures have been self-organized on Al2O3 (0 0 0 1) substrate by laser molecular beam epitaxy (L-MBE). It is shown by AFM morphology that the structure is composed of ID quantum dot chains (QDCs) and larger nano-islands at the nodes of QDCs. The formation mechanism of the nano-structure is also investigated. XRD results indicate that the nano-structure is highly c-axis oriented, with the aligned in-plane oriented domains. Time-integrated photoluminescence (TIPL) of the sample shows obvious blue-shift and broadening of the near band-edge (NBE) emission at room temperature, which are related to the quantum confinement effects. Time-resolved PL (TRPL) result shows bi-exponential decay behavior of ZnO QDCs, with a fast decay time of 38.21 ps and a low decay time of 138.19ps, respectively, which is considered to be originated from the interdot coupling made by coherent emission and reabsorption of the photons in QDCs. (C) 2007 Elsevier B.V. All rights reserved.

Relevância:

100.00% 100.00%

Publicador:

Resumo:

Based on the density functional theory, we systematically study the optical and electronic properties of the insulating dense sodium phase (Na-hp4) reported recently (Ma et al., 2009). The structure is found optically anisotropic. Through Bader analysis, we conclude that ionicity exists in the structure and becomes stronger with increasing pressure.

Relevância:

100.00% 100.00%

Publicador:

Resumo:

The optical and structural properties of anodized AlxGa1-xAs films were investigated by using optical reflectance, X-ray photoemission and Auger electron spectroscopy (XPS and AES). II was found that the anodization process occurs progressively from the surface to the bulk of AlxGa1-xAs and the formed oxidation film comprises mainly oxides of Al and Ga together with a relatively small amount of As. The refractive indexes of the anodized Al0.8Ga0.2As film and Al0.8Ga0.2As film itself were deduced to be about 1.80 and 3.25, respectively, indicating that the anodization film is desirable for anti-reflection coating of the surface of AlxGa1-xAs/GaAs solar cells. (C) 1997 Elsevier Science S.A.

Relevância:

100.00% 100.00%

Publicador:

Resumo:

Lattice matched GaInP/GaAs heterostructures were grown by atmospheric pressure-metal organic vapor phase epitaxy (AP-MOVPE). Compositional intermixing of As/P and Ga/In near the heterointerfaces was studied by photoluminescence (PL) spectroscopy. Indium segregation, memory effect of In into GaAs and the carry-over of As in the GaInP layer during the growth process were considered as three major factors giving rise to the anomalous emissions in the PL spectra. Both thermal annealing and zinc doping strongly enhanced the compositional interdiffusion near the heterointerfaces.

Relevância:

100.00% 100.00%

Publicador:

Resumo:

The double perovskite oxide Sr2CrNbO6 has a cubic structure according to powder X-ray diffraction. After reducing in CO, Sr2CrNbO6 still exhibited a cubic structure refined by Rietveld technique. The TG analysis indicated that Sr2CrNbO6 loses 0.127 oxygen per formula unit from 400 to 700 degrees C in H-2. The morphology and compositions of this ceramic did not significantly change on reduction

Relevância:

100.00% 100.00%

Publicador:

Resumo:

Ce6-xDyxMoO15-delta (0.0 <= x <= 1.8) were synthesized by modified sol-gel method. Structural and electrical properties were investigated by means of X-ray diffraction (XRD), Raman, X-ray photoelectron spectroscopy (XPS) and electrochemical impedance spectroscopy (EIS). The XRD patterns showed that the materials were single phase with a cubic fluorite structure. Impedance spectroscopy measurement in the temperature range between 350 degrees C and 800 degrees C indicated a sharp increase in conductivity for the system containing small amount of Dy2O3. The Ce5.6Dy0.4MoO15-delta detected to be the best conducting phase with the highest conductivity (sigma(t) = 8.93 x 10(-3) S cm(-1)) is higher than that of Ce5.6Sm0.4MoO15-delta (sigma(t) = 2.93 x 10(-3) S cm(-1)) at 800 degrees C, and the corresponding activation energy of Ce5.6Dy0.4MoO15-delta (0.994 eV) is lower than that of Ce5.6Sm0.4MoO15-delta (1.002 eV).