30 resultados para Y zeolite
Resumo:
PbS clusters in zeolite-Y have been prepared with the reaction of Pb2+-ion-exchanged zeolite-Y with Na2S in solution at room temperature. Their absorption spectra show dramatic blue shifts from that of the bulk PbS. Obvious change of both the absorption edges and peak positions upon PbS concentrations have been observed. These phenomena provide evidences that PbS clusters have been formed within the zeolite. The absorption spectra show featureless structure and have no tails near the absorption edges. As the PbS loading density becomes higher, the absorption bands become stronger and sharpen. Order PbS clusters lattice with high quality might be formed in the supercages of zeolite-Y. (C) 1996 American Institute of Physics.
Resumo:
Ultrafine zeolite Y crystals (ca. 100-200 nm) have been successfully grown on metakaolin microspheres (< 100 mu m) for which good hydrothermal stability was observed; products were characterized by powder X-ray diffraction, scanning electronic microscopy and transmission electronic microscopy.
Resumo:
CdS clusters are formed in the pores of a mesoporous zeolite in which the size of the clusters may be adjusted. The size of the clusters increases as the CdS loading is increased. X-ray diffraction investigation shows that the lattice constants of the clusters contract upon increasing size. This contraction is attributed to an increase of the static pressure exercised by the zeolite framework as the clusters grow bigger. Both the excitonic and trapped emission bands are detected and become more intensive upon decreasing size. Three absorption bands appear in the photoluminescence excitation (PLE) spectra and they shift to the blue as cluster size decreases. Based on the effective-mass approximation, the three bands are assigned to the 1S-1S, 1S-1P and 1S-1D transitions, respectively. The size-dependence of the PLE spectra can also be explained. (C) 1997 Elsevier Science Ltd.
Resumo:
The TiO2-supported zeolite with core/shell heterostructure was fabricated by coating aluminosilicate zeolite (ASZ) on the TiO2 inoculating seed via in situ hydrothermal synthesis. The catalysts were characterized by transmission electron microscope (TEM), X-ray diffraction (XRD), nitrogen physisorption (BET), and Fourier transform infrared spectroscopy (FT-IR). The surface acidity of the catalysts was measured by pyridine-TPD method. The catalytic performance of the catalysts for ethanol dehydration to ethylene was also investigated. The results show that the TiO2-supported zeolite composite catalyst with core/shell heterostructure exhibits prominent conversion efficiency for ethanol dehydration to ethylene.
Resumo:
TiO2/4A zeolite composite catalysts were prepared by coating TiO2 on 4A zeolite via liquid phase deposition. The TiO 2/4A zeolite composite catalysts wtih higher surface weak acidity and lower mediate strong acidity exhibit much better catalytic performance on ethanol dehydration to ethylene compared with 4A zeolite. It is suggested that the TiO2 promoter could improve the effective Lewis acidity of composite catalyst which consequently enhanced the catalytic performance.
Resumo:
A high quality pure hydroxy-sodalite zeolite membrane was successfully synthesized on an alpha-Al2O3 support by a novel microwave-assisted hydrothermal synthesis (MARS) method. Influence of synthesis conditions, such as synthesis time, synthesis procedure, etc., on the formation of hydroxy-sodalite zeolite membrane by MAHS method was studied by X-ray diffraction (XRD), scanning electron microscopy (SEM) and gas permeation measurements. The synthesis of hydroxy-sodalite zeolite membrane by MAHS method only needed 45 min and synthesis was more than 8 times faster than by the conventional hydrothermal synthesis (CHS) method. A pure hydroxy-sodalite zeolite membrane was easily synthesized by MAHS method, while a zeolite membrane, which consisted of NaX zeolite, NaA zeolite and hydroxy-sodalite zeolite, was usually synthesized by CHS method. The effect of preparation procedures had a dramatic impact on the formation of hydroxy-sodalite zeolite membrane and a single-stage synthesis procedure produced a pure hydroxy-sodalite zeolite membrane. The pure hydroxy-sodalite zeolite membrane synthesized by MARS method was found to be well inter-grown and the thickness of the membrane was 6-7 mum. Gas permeation results showed that the hydrogen/n-butane permselectivity of the hydroxy-sodalite zeolite membrane was larger than 1000. (C) 2004 Elsevier Inc. All rights reserved.
Resumo:
The density functional theory has been used to study the isomorphously substituted MCM-22 zeolite for the first time. The effect of the basis sets on the calculation results is discussed in details. Data of several index properties for characterizing the relative acidity of T-MCM-22 (T = B, Al, Ga, and Fe), including proton affinity, bond length and bond angle, OH stretching frequency, and charge on the acidic proton, show that the acidity of T-MCM-22 increases in the sequence of B-MCM-22 < Fe-MCM-22 < Ga-MCM-22 < Al-MCM-22. After making a correction, the calculated OH stretching frequencies for Al-MCM-22 and Fe-MCM-22 show a reasonable agreement with the experimental data. On the basis of an equilibrium structure of the B-MCM-22 zeolite, the effect of the B element in the synthesis of the Ti-MCM-22 is also discussed. The adding of the B element during the synthesis of the Ti-MCM-22 can decrease greatly the Ti substitution energy because of the forming of a structure quite similar to the terminal silanol group. The results can provide some constructively information for zeolite synthesis.
Resumo:
By using the solid-state MAS NMR technique, the hydrothermal stabilities (under 100% steam at 1073 K) of HZSM-5 zeolites modified by lanthanum and phosphorus have been studied. They are excellent zeolite catalysts for residual oil selective catalytic cracking (RSCC) processes. It was indicated that the introduction of phosphorus to the zeolite via impregnation with orthophosphoric acid led to dealumination as well as formation of different Al species, which were well distinguished by Al-27 3Q MAS NMR. Meanwhile, the hydrothermal stabilities of the zeolites (P/HZSM-5, La-P/HZSM-5) were enhanced even after the samples were treated under severe conditions for a prolonged time. It was found that the Si-O-Al bonds were broken under hydrothermal conditions, while at the same time the phosphorous compounds would occupy the silicon sites to form (SiO)(x)Al(OP)(4 - x) species. With increasing time, more silicon sites around the tetrahedral coordinated Al in the lattice can be replaced till the aluminum is completely expelled from the framework. The existence of lanthanum can partially restrict the breaking of the Si-O-Al bonds and the replacement of the silicon sites by phosphorus, thus preventing dealumination under hydrothermal conditions. This was also proved by P-31 MAS NMR spectra. (C) 2004 Elsevier Inc. All rights reserved.
Resumo:
MCM-41 zeolite and Tron (II)-Phen/MCM-41 zeolite have been prepared and characterized by XRD, IR, NH3-TPD, HET and UV-Vis. The Iron( II)-Phen/MCM-41 zeolite+30% H2O2 system is capable for catalyzing hydroxylation of phenol.
Resumo:
MCM-41 mesoporous molecular sieve and iron(II)-Phen/MCM-41 have been prepared and characterized by XRD, IR, NH3-TPD, BET and UV-Vis. The iron(II)-Phen/MCM-41 molecular sieve + 30% H2O2 system is capable of performing hydroxylation of phenol.
Resumo:
The synthesis of zeolite X is characterized by UV Raman spectroscopy, NMR spectroscopy, and X-ray diffraction. UV Raman spectra of the liquid phase of the synthesis system indicate that AI(OH); species are incorporated into silicate species, and the polymeric silicate species are depolymerized into monomeric silicate species during the early stage of zeolite formation. An. intermediate species possessing Raman bands at 307, 503, 858 and 1020 cm(-1) is detected during the crystallization ill the solid phase transformation. The intermediate species is attributed to the beta cage, the secondary building unit of zeolite X. A model for the formation of zeolite X is proposed, which involves four-membered rings connecting to each other via six-membered ring to form beta cages, then the beta cages interconnect via double six-membered rings to form the framework of zeolite X. (C) 2001 Elsevier Science B.V. All rights reserved.