116 resultados para Viscosity and digestion
Resumo:
Direct numerical simulation (DNS) of supercritical CO2 turbulent channel flow has been performed to investigate the heat transfer mechanism of supercritical fluid. In the present DNS, full compressible Navier-Stokes equations and Peng-Robison state equation are solved. Due to effects of the mean density variation in the wall normal direction, mean velocity in the cooling region becomes high compared with that in the heating region. The mean width between high-and low-speed streaks near the wall decreases in the cooling region, which means that turbulence in the cooling region is enhanced and lots of fine scale eddies are created due to the local high Reynolds number effects. From the turbulent kinetic energy budget, it is found that compressibility effects related with pressure fluctuation and dilatation of velocity fluctuation can be ignored even for supercritical condition. However, the effect of density fluctuation on turbulent kinetic energy cannot be ignored. In the cooling region, low kinematic viscosity and high thermal conductivity in the low speed streaks modify fine scale structure and turbulent transport of temperature, which results in high Nusselt number in the cooling condition of the supercritical CO2.
Resumo:
From the partial differential equations of hydrodynamics governing the movements in the Earth's mantle of a Newtonian fluid with a pressure- and temperature-dependent viscosity, considering the bilateral symmetry of velocity and temperature distributions at the mid-plane of the plume, an analytical solution of the governing equations near the mid-plane of the plume was found by the method of asymptotic analysis. The vertical distribution of the upward velocity, viscosity and temperature at the mid-plane, and the temperature excess at the centre of the plume above the ambient mantle temperature were then calculated for two sets of Newtonian rheological parameters. The results obtained show that the temperature at the mid-plane and the temperature excess are nearly independent of the rheological parameters. The upward velocity at the mid-plane, however, is strongly dependent on the rheological parameters.
Resumo:
Direct numerical simulation (DNS) of supercritical CO2 turbulent channel flow has been performed to investigate the heat transfer mechanism of supercritical fluid. In the present DNS, full compressible Navier-Stokes equations and Peng-Robison state equation are solved. Due to effects of the mean density variation in the wall normal direction, mean velocity in the cooling region becomes high compared with that in the heating region. The mean width between high-and low-speed streaks near the wall decreases in the cooling region, which means that turbulence in the cooling region is enhanced and lots of fine scale eddies are created due to the local high Reynolds number effects. From the turbulent kinetic energy budget, it is found that compressibility effects related with pressure fluctuation and dilatation of velocity fluctuation can be ignored even for supercritical condition. However, the effect of density fluctuation on turbulent kinetic energy cannot be ignored. In the cooling region, low kinematic viscosity and high thermal conductivity in the low speed streaks modify fine scale structure and turbulent transport of temperature, which results in high Nusselt number in the cooling condition of the supercritical CO2.
Resumo:
以硅酸四乙酯(TEOS)和甲基三乙氧基硅烷(MTEOS)为前驱材料,用溶胶-凝胶(sol-gel)方法在钛宝石表面制备得到均匀性良好且具有高激光损伤阈值的有机硅复合凝胶增透膜。膜层在钛宝石激光器输出波段(750~850nm)的增透效果显著,其平均透过率超过98.6%;激光破坏阈值为2.2J/cm^2(800nm,300ps);膜层表面均匀性达到激光波面的要求,在皮秒、飞秒超短脉冲高功率激光领域具有应用价值。溶胶的性能测试结果表明,溶胶粘度和成膜折射率均随溶液中CH3SiO1.5溶胶体含量的增加而增大,而膜
Resumo:
糯小麦在食品加工业、淀粉加工业及其它工业上有着重要用途,是近年来许多国家小麦研究的重要课题。国外糯小麦选育尚未突破高产与糯性相结合的难点,国内目前还没有培育出高蛋白强筋型的糯小麦品种,这在一定程度上与缺乏合适的育种方法和高效、实用的糯小麦分子标记辅助育种技术有关。国内外对Wx基因效应的研究主要利用缺体-四体系、重组自交系或近等基因系,还未见有利用遗传背景相同的BC5F2代回交改良群体的报道。 糯性位点近等基因系是小麦淀粉品质育种的重要材料,而我国目前还没有一套中国栽培小麦遗传背景的糯性位点近等基因系。为了选育部分糯小麦、全糯小麦和中国栽培小麦遗传背景的糯性位点近等基因系,我们利用Wx蛋白电泳和高效实用的分子标记技术体系来鉴定糯小麦杂交后代的基因型,结果证明该体系能有效地用于糯小麦的分子标记辅助育种。以中国春糯性位点全套近等基因系为研究材料,对小麦Wx基因的6个STS标记和1个CAPS标记进行了筛选,改良PCR扩增条件以及产物检测方式后,从这些标记中筛选出3个标记,包括鉴定Wx-A1、Wx-D1位点的2个共显性STS标记和Wx-B1位点的1个显性STS标记。利用上述3个分子标记从BC5F2 代回交改良群体中筛选出了8种Wx基因型,经卡方检验,其分离比符合3对基因的分离比例,其中基因型为aabbdd的植株有2株,直链淀粉含量分别为1.81%和0.82%,为全糯小麦;基因型为AAbbdd,aabbDD的部分糯性植株各有1株,直链淀粉含量分别为15.24%和17.57%。以上4株植株的农艺性状和品质性状接近回交亲本“川育12”,并明显优于全糯材料“98Y1441”,表明采用回交法与Wx基因分子标记辅助选择相结合,有助于培育高产、优质的全糯和部分糯小麦。同时,本研究中建立的分子标记技术体系,也为选育具有中国栽培小麦遗传背景的糯性位点近等基因系奠定了基础。 在基因型鉴定的基础上,利用糯小麦杂交后代BC5F2代回交改良群体研究了各基因缺失降低直链淀粉含量的效果和各基因合成直链淀粉的能力,以及直链淀粉含量与农艺性状、品质性状、淀粉糊化特性等的相关性。缺失不同Wx基因的8种基因型,直链淀粉含量差异显著。研究单缺失基因型发现,减少效应最大的是Wx-B1b基因,Wx-B1b和Wx-D1b基因没有显著差异,减少效应最小的是Wx-A1b基因。研究双缺失基因型发现,Wx基因合成直链淀粉的能力,Wx-B1a基因最高,Wx-A1a基因最低,而Wx-B1a和Wx-D1a基因差异很小;直链淀粉含量与株高、穗长、小穗数、穗粒数、千粒重等农艺性状相关不显著,表明淀粉品质育种可以与高产育种实现有机结合;直链淀粉含量与SDS-沉降值呈显著负相关(r=-0.726),说明直链淀粉含量降低在一定程度上有利于提高小麦营养与加工品质,这一结果至今未见有文献报道;全糯类型的淀粉糊化特性与其他类型显著不同,具有最高的峰值粘度和稀懈值,最低的低谷粘度、最终粘度、反弹值、峰值时间、糊化温度、起始糊化温度,表明糯小麦淀粉在食品和工业上具有特殊用途;稀懈值与直链淀粉含量呈极显著负相关(r=-0.969),其他粘度参数与直链淀粉含量呈显著正相关(最终粘度r=0.797,低谷粘度r=0.910、反弹值r=0.954、峰值时间r=0.970、糊化温度r=0.962、起始糊化温度r=0.932)。以上结论可为糯小麦品种选育和淀粉品质改良提供理论依据。 Waxy wheat is very important in food processing industry, starch processing industry and the other industries, so it is a focus of wheat research in many countries these years. Foreign wheat breeders have not conquered the difficulty of high yield combined with waxy character, and there is no waxy wheat variety with high protein and strong gluten in China at present,all of which were caused by lacking proper breeding methods and effective, applied molecular markers-assisted selection technique at a certain extent. Until now, research about the effect of waxy genes mainly depended on nullisomic-tetrasomic lines, recombinant lines or near-isogenic lines, and it is lacking the reports of using improved BC5F2 backcross progenies under the common genetic background. Near-isogenic lines at the Wx loci are important materials for wheat starch quality breeding. However, there are no such lines under the Chinese cultivated wheat genetic background. To develop partial waxy wheats, waxy wheats and near-isogenic lines at the Wx loci under the Chinese cultivated wheat genetic background, we use SDS-PAGE of waxy proteins and effective, applied molecular marker-assisted selection technical system to identify the genotype of waxy wheat’s progenies. The results indicated that such a system is applicable in waxy wheat’s molecular marker-assisted selection effectively. A series of Chinese Spring Wx loci near-isogenic lines were used to identify the specific bands of six STS markers and one CAPS marker of Wx genes. After optimizing PCR amplification and separating of PCR products, three co-dominant and dominant STS-markers were identified at the Wx-A1, Wx-D1 and Wx-B1 loci, respectively, which were used to identify the genotype of waxy wheat’s progenies. Eight Wx genotypes were developed from the improved BC5F2 backcross progenies, which follows Mendelian segregation. Among them, there were two aabbdd waxy plants whose amylose content in the BC5F3 seeds were 1.81% and 0.82%, respectively. In addition, there were partial waxy plants (AAbbdd and aabbDD) whose amylose content in the BC5F3 seeds were 15.24 % and 17.57%, respectively. Most agronomic and quality traits of these four plants resembled those of the recurrent parent “Chuanyu 12”, and superior to waxy wheat parent “98Y1441”. This shows that backcross approach in combination with molecular marker-assisted selection of waxy genes is helpful to develop partial and full waxy wheat with good traits in the waxy wheat breeding program. At the same time, molecular marker-assisted selection technical system in this paper, also establish the base for breeding the near-isogenic lines at the Wx loci under the Chinese cultivated wheat genetic background. According to the results of genotype identification, we use waxy wheat’s improved BC5F2 backcross progenies to verify the effects of null alleles on reducing amylose content and determine the amylose synthesis capacity of each Wx gene independently, and investigate the relativity among amylose content with agonomic traits, quality traits, starch pasting properties respectively. There was significant difference in amylose content of the eight genotypes carrying different null Wx alleles. The reducing effect of the single null alleles was the most significant in Wx-B1b, followed by Wx-D1b and Wx-A1b, and there was no significant difference between Wx-B1b and Wx-D1b. The results of the double null lines further demonstrated that for the capacity of amylose synthesis, Wx-B1a was the highest, followed by Wx-D1a and Wx-A1a, and there was no significant difference between Wx-B1a and Wx-D1a. Amylose contents of the eight genotypes were not significantly correlated with plant height, spike length, spikelets per spike, grains per spike, 1000-grain weight, which showed that starch quality breeding could integrate with high yield breeding. Amylose contents of the eight genotypes were negatively significantly correlated with SDS-sedimentation value(r=-0.726), which suggested that reduction in amylose content is propitious to improve quality at a certain extent. Starch pasting properties of the full waxy type was significantly different from the other seven types, with the highest peak viscosity and breakdown, and lowest valley viscosity, final viscosity, setback, peak time, pasting temperature and starting pasting temperature. It indicated that waxy wheat starch has special use in food and industry. Breakdown was negatively significantly correlated with amylose contents (r=-0.969), and the other parameters were positively significantly correlated with amylose contents (r=0.797 for final viscosity, r=0.910 for trough viscosity, r =0.954 for setback, r =0.970 for peak time, r=0.962 for pasting temperature and r=0.932 for starting pasting temperature ). The results of the study are very useful for waxy wheat variety breeding and starch quality improvement.
Resumo:
We present a numerical study of shear viscosity and thermal conductivity of symmetric nuclear matter, pure neutron matter, and beta-stable nuclear matter, in the framework of the Brueckner theory. The calculation of in-medium cross sections and nucleon effective masses is performed with a consistent two- and three-body interaction. The investigation covers a wide baryon density range as needed in the applications to neutron stars. The results for the transport coefficients in beta-stable nuclear matter are used to make preliminary predictions on the damping time scales of nonradial modes in neutron stars.
Sulfonated poly(arylene-co-imide)s as water stable proton exchange membrane materials for fuel cells
Resumo:
A novel sulfonated poly(arylene-co-imide)s were synthesized by Ni(0) catalytic copolymerization of sodium 3-(2,5-dichlorobenzoyl)benzenesulfonate and naphthalimide dichloride monomer. The synthesized copolymers with the - SO3H group on the side-chain of polymers possessed high molecular weights revealed by their high viscosity and the formation of tough and flexible membranes. Because of the introduction of electron donating phenoxy groups into naphthalimide moieties, the hydrolysis of the imide rings was depressed. The resulting copolymers exhibited excellent water stability. The copolymer membranes display no apparently change in appearance, flexibility, and toughness after a soaking treatment in pressurized water at 140 degrees C for 250 h.
Resumo:
Polycarbodiimide (CDI) was used to improve the thermal stability of poly(L-lactic acid) (PLA) during processing. The properties of PLA containing various amounts of CDI were characterized by GPC, DSC, rheology, and tensile tests. The results showed that an addition of CDI in an amount of 0.1-0.7 wt% with respect to PLA led to stabilization of PLA at even 210 degrees C for up to 30 min, as evidenced by much smaller changes in molecular weight. melt viscosity, and tensile strength and elongation compared to the blank PLA samples. In order to examine the possible stabilization mechanism, CDI was reacted with water, acetic acid, L-lactic acid, ethanol and low molecular weight PLA. The molecular structures of the reaction products were measured with FTIR.
Resumo:
We prepared four new ionic liquids consisting of N-methyl-N-allylpyrrolidinium cation in conjunction with anions including iodide, nitrate, thiocyanate, and dicyanamide, respectively, and measured their physical properties of density, viscosity, and conductivity. Owing to the relatively lower melting point of electroactive N-methyl-N-allylpyrrolidinium iodide, in combination with three other nonelectroactive ionic liquids, we could construct solvent-free electrolytes possessing high iodide concentrations for dye-sensitized solar cells. We correlated temperature-dependent electrolyte viscosity with molar conductivity and triiodide mobility through applying an empirical Walden's rule and a modified Stokes-Einstein equation, respectively. We have further found that these anions (nitrate, thiocyanate, and dicyanamide) have different influences on surface states and electron transport in the mesoporous titania film, resulting in different photovoltages and photocurrents of dye-sensitized solar cells.
Resumo:
High-solids, low-viscosity, stable poly(acrylamide-co-acrylic acid) aqueous latex dispersions were prepared by the dispersion polymerization of acrylamide (AM) and acrylic acid (AA) in an aqueous solution of ammonium sulfate (AS) medium using anionic polyelectrolytes as stabilizers. The anionic polyelectrolytes employed include poly(2-acrylamido-2-methylpropanesulfonic acid sodium) (PAMPSNa) homopolymer and random copolymers of 2-acrylamido-2-methylpropanesulfonic acid sodium (AMPSNa) with methacrylic acid sodium (MAANa), acrylic acid sodium (AANa) or acrylamide (AM). The influences of stabilizer's structure, composition, molecular weight and concentration, AA/AM molar feed ratio, total monomer, initiator and aqueous solution of AS concentration, and stirring speed on the monomer conversion, the particle size and distribution, the bulk viscosity and stability of the dispersions, and the intrinsic viscosity of the resulting copolymer were systematically investigated. Polydisperse spherical as well as ellipsoidal particles were formed in the system. The broad particle size distributions indicated that coalescence of the particles takes place to a greater extent.
Resumo:
A series of sulfonated polymides containing benzimidazole groups were synthesized using 4,4'-binaphthyl-1,1',8,8'-tetracarboxylic dianhydride (BTDA), 4,4'-diaminodiphenyl ether-2,2'-disulfonic acid (ODADS) as the sulfonated diamine, and 2-(3',5-diaminophenyl)benzimidazole (a) or 6,4'-diamino-2-phenylbenzimidazole (b) as the nonsulfortated diamine. The electrolyte properties of the synthesized polyimides Ia-x, Ib-x, x refers to molar percentage of the sulfonated diamine) were investigated and compared with those of polyimides (Ic-x) from BTDA, ODADS, and m-phenylenediamine (c). All synthesized polyimides possessed high molecular weights revealed by their high viscosity, and formation of tough and flexible membranes. Polyintides with benzimidazole groups exhibited much better swelling capacity than those without benzimiclazole groups. This was attributed to the strong interchain interaction through basic benzimidazole functions and sulfonic acid groups. The sulfortated polyimides that are incorporated with 1, 1',8,8'-binaphthalimide exhibited better hydrolytic stability than that with 1,4,5,8-naphthalimide. Polyimide membranes with good water stability as well as high proton conductivity were developed. Polyimide membrane (Ia - 90), for example, did not lose mechanical properties after being soaked in boiling water for tOOO h, while its proton conductivity was still at a high level (compared to that of Nafion 117).
Resumo:
Polylactide (PLA) was melt blended with a biodegradable hyperbranched poly(ester amide) (HBP) to enhance its flexibility and toughness without sacrificing comprehensive performance. The advantage of using HBP was due to its unique spherical shape, low melt viscosity, and abundant functional end groups together with its easy access. Rheological measurement showed that blending PLA with as little as 2.5% HBP resulted in a 40% reduction of melt viscosity. The glass transition temperature (T-g) of PLA in the blends decreased slightly with the increase of HBP content, indicating partial miscibility which resulted from intermolecular interactions via H-bonding. The H-bonding involving CO of PLA with OH and NH of HBP was evidenced by FTIR analysis for the first time. The HBP component, as a heterogeneous nucleating agent, accelerated the crystallization rate of PLA. Remarkably, with the increase of HBP content, the elongation at break of PLA blends dramatically increased without severe loss in tensile strength, even the tensile strength increased within 10% content of HBP. The stress-strain curves and the SEM photos of impact-fractured surface showed the material changed from brittle to ductile failure with the addition of HBP. Reasonable interfacial adhesion via H-bonding and finely dispersed particulate structure of HBP in PLA were proposed to be responsible for the improved mechanical properties.
Resumo:
Sulfonated poly(p-phenylene)s (SPPs) containing sulfonic acid groups in their side chains had been directly synthesized by Ni(0) catalytic coupling of sodium 3-(2,5-dichlorobenzoyl)benzenesulfonate and 2,5-dichlorobenzophenone. The synthesized copolymers possessed high molecular weights revealed by their high viscosity, and the formation of tough and flexible membranes by casting from DMAc solution. The copolymers exhibited excellent oxidative stability and mechanical properties due to their fully aromatic structure extending through the backbone and pendent groups. Transmission electron microscopic (TEM) analysis revealed that these side-chain type SPP membranes have a microphase-separated structure composed of hydrophilic side-chain domains and hydrophobic polyphenylene main chain domains. The proton conductivities of copolymer membranes increased with the increase of IEC and temperature, reaching values above 3.4 x 10(-1) S/cm at 120 degrees C, which are almost 2-3 times higher than that of Nafion 117 at the same measurement conditions. Consequently, these materials proved to be promising as proton exchange membranes.
Resumo:
Reactive compatibilization of ethylene-propylene copolymer functionalized with allyl (3-isocyanato-4-tolyl) carbamate (TAI) isocyanate (EPM-g-TAI) and polyamide 6 (PA6) was investigated in this paper, FTIR analysis revealed the evidence of a chemical reaction between the end groups of PA6 and EPM-g-TAI. Thermal, rheological, morphological, and mechanical properties of the resultant system were examined, DSC analysis indicated that the crystallization of PA6 in Pa6/EPM-g-TAI blends was inhibited, due to the chemical reaction that occurs at the interface of PA6 and EPM-g-TAI. Rheological measurement showed that complex viscosity and storage modulus of PA6/EPM-g-TAI were both dramatically enhanced compared to those of PA6/EPM at the same blending composition. After examining the morphology of both blending systems, smaller particile sizes, more homogeneous distribution of domains and improved interfacial adhesion between matrix and domains were observed in the compatibilized system. Mechanical properties such as tensile strength. Young's modulus, flexural strength and modulus, as well as notched and un-notched impact strength of PA6/EPM-g-TAI blends were also found to improve gradually with increasing the content of grafted TAI.
Resumo:
A series of polyimides (PIs) based on 2,3,3',4'-benzophenonetetracarboxylic dianhydride (2,3,3',4'-BTDA) and 3,3',4,4'-BTDA were prepared by the conventional two-step process. The properties of the 2,3,3',4'-BTDA based polyimides were compared with those of polyimides prepared from 3,3',4,4'-BTDA. It was found that PIs from 2,3,3,4'-BTDA have higher glass transition temperature and better solubility without sacrificing their thermal properties. Furthermore the theological properties of PMR-15 type polyimide resins based on 2,3,3',4'-BTDA showed lower melt viscosity and wider melt flow region (flow window) compared with those from 3,3',4,4'-BTDA. The structure-property relations resulted from isomerism were discussed.